• Title/Summary/Keyword: gas metal arc weld

Search Result 141, Processing Time 0.027 seconds

Porosity Reduction during Gas Tungsten Arc-Gas Metal Arc Hybrid Welding of Zinc Coated Steel Sheets (II) - Hybrid Welding Results (GTA-GMA 하이브리드공정에 따른 자동차용 아연도금강판의 용접부 기공감소 (II) - 하이브리드공정 적용 결과)

  • Ahn, Young-Nam;Kim, Cheolhee
    • Journal of Welding and Joining
    • /
    • v.34 no.4
    • /
    • pp.48-54
    • /
    • 2016
  • The use of Zn coated steel has increased in the automotive industry due to its excellent corrosion resistance. Conventionally the BIW(body-in-white) structure and the hang-on parts have been made of Zn coated steel and more recently Zn coated steel began to be applied in the chassis parts. During gas metal arc (GMA) welding of the chassis part, lap fillet joint used to be adopted but spatter generation and porosities are most important concerns. In the industrial applications, an intentional joint gap was made to avoid the weld defects but it is not easy to control the size of joint gap. In this research, gas tungsten arc (GTA) is combined with GMA welding where GTA precedes GMA. As pulsed arc was adopted as GMA, GTA was oscillated along the longitudinal direction by pulsing GMA, but the arc oscillation did not disturb the molten droplet transfer of GMA welding. By increasing the distance between GTA and GMA, the length of weld pool increased and porosity could be reduced. Moreover porosity in the welds was fully removed when the distance between two arcs was 15 mm.

The Influence of Shield Gas Ratio on the Toughness of Al5083-O GMA Welding Zone (Al5083-O GMA 용접시 불활성가스 혼합비가 용접부의 인성에 미치는 영향에 관한 연구)

  • 이동길;조상곤;김건호
    • Journal of Advanced Marine Engineering and Technology
    • /
    • v.26 no.6
    • /
    • pp.653-660
    • /
    • 2002
  • In this study, the toughness was evaluated by using the instrumented Charpy impact testing procedures for A15083-O aluminum alloy used in the LNG carrying and storing tank. The specimens were GMAW welded with four different mixing shield gas ratios (Ar100%+He0%, Ar67%+He33%, Ar50%+He50%, and Ar33%+He67%), and tested at four different temperatures(+25, -30, -85, and $-196^{\circ}C$) in order to investigate the influence of the mixing shield gas ratio and the low temperature. The specimens were divided into base metal, weld metal, fusion line, and HAZ specimen according to the worked notch position. From experiment, the maximum load increased a little up to -$85^{\circ}C$ , and the maximum load and maximum displacement were shown the highest and the lowest at -$196^{\circ}C$ than the other test temperatures. The absorption energy of weld metal notched specimens was not nearly depends on test temperature and mixing shield gas ratio because the casting structure was formed in weld metal zone. In the other hand, the other specimens were shown that the lower temperature, the higher absorption energy slightly up to $-85^{\circ}C$ but the energy was decreased so mush at $-196^{\circ}C$.

Evaluation of Gas Metal Arc Welding Characteristics according to Contact Tip Materials (GMA용접에서 콘택트 팁 재질에 따른 용접특성 평가)

  • Kim, Dong Yoon;Hwang, In Sung;Kim, Dong Cheol;Kang, Moon Jin
    • Journal of Welding and Joining
    • /
    • v.32 no.6
    • /
    • pp.35-40
    • /
    • 2014
  • The contact tip for gas metal arc welding has important functions to transmit the welding current to the wire and to guide the wire to molten pool. If the contact tip is damaged, it is a cause of lowering the welding productivity due to removal of welding defects and replacement of contact tip. In case of the use of a contact tip for a long time the arc is unstable because the processed hole in the contact tip center is larger, and the variation of aiming position of the welding wire causes a seam tracking error. In this study, gas metal arc welding experiments using contact tip of three different materials were performed. The contact tips with Cu-P, Cu-Cr, and Cu-ODS were used at the experiments, and the welding characteristics by each contact tip were evaluated. After welding contact tip appearance, welding spatter adhesion amount of the nozzle, and weld bead appearance were evaluated. The welding current and welding voltage were measured to verify arc stability during arc welding.

An Experimental Investigation on Low Cycle Fatigue Behavior of Alloy 617 Base Metal and Alloy 617/Alloy 617 Weld Joints (Alloy 617 모재와 용접부재의 저사이클피로 거동에 관한 실험적 고찰)

  • Choi, Pil-Ho;Kim, Seon-Jin;Kim, Woo-Gon;Kim, Min-Hwan
    • Journal of Power System Engineering
    • /
    • v.18 no.5
    • /
    • pp.115-121
    • /
    • 2014
  • Alloy 617 is the one of the leading candidate materials for intermediate heat exchangers(IHX) of a very high temperature reactor(VHTR) system. Some of the components are joined by many welding techniques and therefore the welded joints are inevitable in the construction of systems. In the present paper, the low cycle fatigue(LCF) behaviors of Alloy 617 base metal(BM) and the gas tungsten arc welded (GTAWed) weld joints(WJ) are investigated experimentally under strain controlled LCF tests. Fully axial total-strain controlled tests have been conducted at room temperature with total strain ranges of 0.6, 0.9, 1.2 and 1.5%. The weld joints have shown a lower fatigue lives compared with base metals at all the testing conditions. The weld joints have shown a higher cyclic stress response behavior than base metal. Both BM and WJ exhibited cyclic strain hardening behavior, depending on the total strain range. In addition, the strain-life parameters for BM and WJ were determined, based on Coffin-Manson equations.

Development of Laser-Rotating An Hybrid Welding Process (레이저-회전 아크 하이브리드 용접공정의 개발)

  • Kim, Cheol-Hee;Chae, Hyun-Byung;Lee, Chang-Woo;Kim, Jeong-Han;Rhee, Se-Hun
    • Journal of Welding and Joining
    • /
    • v.24 no.1
    • /
    • pp.88-92
    • /
    • 2006
  • Laser-rotating arc hybrid welding was introduced by combining $CO_2$ laser and rotating gas metal arc welding. While the arc rotation enhances the weld pool motion, it reduces the undercut formation which is one of most critical weld defects in the conventional laser-arc hybrid welding. This research investigated the bead characteristics according to the welding parameters such as frequency of rotation, welding voltage, shielding gas composition and interspacing distance between laser and we. The welding parameters were selected to reduce spatter generation and ensure sound weld beads fur bead welding and butt welding with various joint gaps. Gap bridging ability was improved, such that the sound weld beads were achieved for butt joint with up to 2mm joint sap, with no adjustment of CTWD(Contact tip-to-workpiece distance) and electrode diameter.

A Study on Arc Sensor for Weld Seam Tracking by Using Fuzzy Control (퍼지제어를 이용한 용접선 추적용 아크센서에 관한 연구)

  • 조시훈;김재웅
    • Journal of Welding and Joining
    • /
    • v.13 no.1
    • /
    • pp.156-166
    • /
    • 1995
  • Experimental models which are able to determine the deviation between weld line and weaving center by measuring the weld current during welding were proposed for the gas metal arc welding process. The models were used for developing a weld seam tracking system which controls the weaving speed of a welding torch. However, it was revealed that the tracking result of the system is affected by the welding conditions. Thus an arc sensor system was developed by using fuzzy control approach for overcoming the difficulty of modelling the nonlinear process. The rule base and parameters of the fuzzy control system were determined on the basis of the results of experiments. This fuzzy control system has shown the successful tracking capability for the wide operating range of welding conditions.

  • PDF

Dynamic behavior of GMA considering metal transfer (금속이행을 고려한 GMA 용접 시스템의 동특성 해석)

  • 박세홍;김면희;강세령;최상균;이상룡
    • Proceedings of the Korean Society of Precision Engineering Conference
    • /
    • 2002.05a
    • /
    • pp.565-568
    • /
    • 2002
  • Welding variables and conditions in gas metal arc welding (GMAW) effect on the weld quality and productivity, extensive research efforts have been made to analyze the welding variables and conditions. In this study dynamic behavior of GMAW system is investigated using the characteristic equations of the power supply, wire and welding arc. Characteristic equation of wire is modified to include the effect of droplets attached at the electrode tip. The dynamic characteristics of arc length, current, voltage with respect to the step, ramp inputs of CTWD was simulated, seam tracking procedure using arc sensor was simulated with variable V-Groove geometries and weaving frequencies. From results of simulation, some predictions about dynamic characteristics of GMAW and welding process are available. The proposed simulator and results appear to be utilized to determine the proper welding conditions, to be improved by considering power supply dynamic characteristics.

  • PDF

Effects of Welding Parameters on Porosity Formation in Weld Beads of Galvanized Steel Pipes produced with Gas Metal Arc Welding (아연도금강관의 가스메탈아크용접에서 용접인자가 기공형성에 미치는 영향)

  • Lim, Young-Min;Jang, Bok-Su;Koh, Jin-Hyun
    • Journal of Welding and Joining
    • /
    • v.30 no.5
    • /
    • pp.46-50
    • /
    • 2012
  • This study was carried out to investigate the effect of welding parameters such as shielding gas compositions welding voltage and welding current on the pore formation in the weld beads of galvanized steel pipes produced with gas metal arc welding. The porosity was evaluated and rated by metallography and radiographic test in terms of weight percentage, number and distribution of pores in weld beads. The porosity increased with increasing welding voltage and current, in which Ar gas produced the most porosity while $Ar+5%O_2$ generated the least porosity. It was found that the porosity could be reduced by selection of the proper gas mixture composition such as $Ar+5%O_2$ and $Ar+10%CO_2$ and by using current (130~150A) and voltage(16~20V).

Microstructure and Tensile Properties of SS400 Carbon Steel and SUS430 Stainless Steel Butt Joint by Gas Metal Arc Welding

  • Poonnayom, Pramote;Chantasri, Sakchai;Kaewwichit, Jesada;Roybang, Waraporn;Kimapong, Kittipong
    • International Journal of Advanced Culture Technology
    • /
    • v.3 no.1
    • /
    • pp.61-67
    • /
    • 2015
  • The application of SS400 carbon steel and AISI430 ferritic stainless steel joint has been increased in industries because of the advantage of both metals was able to increase the service lifetime of the important structures. Therefore, a fusion welding process that could produce a sound weld and good joint properties should be optimized. This research is aimed to weld a butt joint of SS400 carbon steel and AISI430 ferritic stainless steel using Gas Metal Arc Welding (GMAW) welding process and to study the effects of welding parameters on joint properties. The experimental results were concluded as follows. The optimized welding parameter that produced the tensile strength of 448 MPa was the welding current of 110A, the welding speed of 400 mm/min and the mixed gas of $80%Ar+20%CO_2$. Increase of the welding current affected to increase and decrease the tensile strength of the joint, respectively. Lower welding current produced the incomplete bonding of the metals and indicated the low tensile strength. Microstructure investigation of the welded joint showed a columnar grain in the weld metal and a coarse grain in the heat affected zone (HAZ). The unknown hard precipitated phases were also found at the grain boundaries of the weld metal and HAZ. The hardness profile did not show the difference of the hardness on the joint that was welded by various welding currents but the hardness of the weld metal was higher than that of the other location.