• Title/Summary/Keyword: gap N-joints

Search Result 8, Processing Time 0.017 seconds

An Experimental study on the behavior of gap N-joints in Cold-formed Square Hollow Sections with connection plate for a tension member (인장용 연결 플레이트를 갖는 각형강관 갭 N형 접합부의 거동에 관한 실험적 연구)

  • Park, Keum Sung;Bae, Kyu Woong;Moon, Tae Sup
    • Journal of Korean Society of Steel Construction
    • /
    • v.16 no.6 s.73
    • /
    • pp.769-780
    • /
    • 2004
  • This paper's objective is to evaluate the experimental behavior of gap N-joints made of cold-formed, square, hollow steel sections, with a connection plate as a tension member. The principal parameters for testing included the ratio of chord width to thickness, the ratio of brace width to chord width, eccentric ratio, the shape of the compression member, the branch angle, and the stiffening plate of the chord flange. The strength and failure mode were examined through the test for the gap N-joint, consisting of several parameters. Based on the results of the test, the gap N-joints were determined according to the capacity preceding the displacement of the tension, regardless of the width ratio, and the split failure mode-connected surface for a chord in joints. The strength of the gap N-joints increased proportionally as the $2\gamma$(B/T) ratio decreased, and as the width ratio(${\beta}$) of branch to chord increased. Particularly, $2\gamma$(B/T) decreased as the capacity of gap N-joint increased. The results of the test were summarized for the capacity, initial stiffness, ductility, and change of the failure mode of each gap N-joint.

Experimental evaluation of fatigue strength for small diameter socket welded joints under vibration loading condition

  • Oh, Chang-Young;Lee, Jun-Ho;Kim, Dong-Woo;Lee, Sang-Hoon
    • Nuclear Engineering and Technology
    • /
    • v.53 no.11
    • /
    • pp.3837-3851
    • /
    • 2021
  • To investigate how the fabrication and repair of socket welded joints could be used to enhance fatigue resistance under vibration condition, experimental test data of installation conditions that potentially influence fatigue strength were analyzed with the S-N curve. It was found that the decreasing fatigue strength of stainless steel socket welded joints was attributed to the effect of high heat input of welding process. The effect of welding method, slip-on gap and radial-gap conditions on fatigue strength was insignificant. The test data of repair technique application, 2 × 1 leg length and of socket weld overlay, clearly showed higher fatigue strength but there was a limitation for higher stress region because of the weld toe crack.

An Experimental Study on the Fatigue Strength of Repair Welded Joints of Old Steel Bridge (신판교체 보수 용접부의 피로강도에 관한 실험적 연구)

  • Park Hyeon-Chan;Lee Jin-Hyeong;Kim Jae-Hwan;Jang Gap-Cheol;Jang Gyeong-Ho
    • Proceedings of the KWS Conference
    • /
    • 2006.05a
    • /
    • pp.94-96
    • /
    • 2006
  • Recently, steel structures have been increasing because of its brilliant features. In general, cracks and corrosion are produced due to the numerous environmental factors in steel structures. However, the validity of repair method for the damaged steel structures has not been fully verified because of its lack of safety and reliability after application. Moreover, repair method by welding inevitably involves cutting and welding processes and reliability for the safety during the processes has net been established yet. Therefore, this study carried out experiments on the fatigue strength of repair welded joints of old steel bridge to investigate the fatigue characteristics in the repair welded joints. Fatigue tests were conducted by 250kN capacity MIS with the frequency of 5Hz under amplitude loading. From the results, it is known that fatigue strength grade of the repair welded joints was satisfied with C grade which specification requires.

  • PDF

Optimization of L-shaped Corner Dowel Joint in Modified Poplar using Finite Element Analysis with Taguchi Method

  • Ke, Qing;Zhang, Fan;Zhang, Yachi
    • Journal of the Korean Wood Science and Technology
    • /
    • v.44 no.2
    • /
    • pp.204-217
    • /
    • 2016
  • Modified poplar has emerged as a potential raw material for furniture production. Lack of specific modified poplar strength information; however, restricts applications in the furniture industry especially as related to strength in corner-joints. Optimization of strength in L-shaped corner dowel modified poplar joints under compression loads utilizing finite element analysis (FEA) by Taguchi method with the focus of this study. Four experiment factors (i.e., Structure Style, Tenon Length, Tenon Diameter, and Tenon Gap), each at three levels, were conducted by adopting a $L_9-3^4$ Taguchi orthodoxy array (OA) to determine the optimal combination of factors and levels for the von Mises stress utilizing ANSYS software. Results of Signal-to-Noise ratio (S/N) analysis and the analysis of variance (ANOVA) revealed the optimal L-shaped corner dowel joint in modified poplar is $45^{\circ}$ Bevel Butt in structure style, 24 mm in tenon length, 6 mm in tenon diameter, and 20 mm in tenon gap. Tenon length and tenon gap are determined to be significant design factors for affecting von Mises Stress. Confirmation tests with optimal levels and experimental test indicated the predicted optimal condition is comparable to the actual experimental optimal condition.

Behavior of N-joints using Square Hollow Sections in Truss (각형강관 트러스의 N형 접합부의 거동)

  • Lee, Sang Ho;Lee, Sang Sup;Bae, Kyou Woong;Moon, Tae Sup
    • Journal of Korean Society of Steel Construction
    • /
    • v.11 no.3 s.40
    • /
    • pp.251-258
    • /
    • 1999
  • The aim of this paper is to examine the behavior of the N-joints using square hollow sections and to improve the structural performance without reinforcing the joints. The selected parameters are the ratio of web to chord width, gap to chord width and eccentricity to chord width. Comparison between test results and codes shows the fact that the NPE-type has superior structural properties to the NSE-type in ultimate strength and deformation capacity. The experimental formulae based on the regression analysis are proposed. Ultimate strength formula employed in eurocode 3 is revised and proposed for the NSE-type. And ultimate strength formula including the eccentricity to chord width ratio which effects on the ultimate strength is proposed for the NPE-type.

  • PDF

A Study on the Mechanism of Crevice Corrosion for 430 Stainless Steel (430 스테인리스강의 틈부식 발생기구에 대한 연구)

  • 백신영;나은영
    • Journal of Advanced Marine Engineering and Technology
    • /
    • v.27 no.3
    • /
    • pp.447-452
    • /
    • 2003
  • Crevice corrosion is localized form of corrosion usually associated with a stagnant solution on the micro-environmental level. Such stagnant micro environments tend to occur in crevices (shielded areas) such as those formed under gaskets washers insulation material. fastener heads. surface deposits. disbonded coatings. threads. lap joints and clamps. Crevice corrosion is initiated by changes in located electrochemical reaction within the crevice such as a) depletion of inhibitor in the crevice b) depletion of oxygen in the crevice c) a shift to acid conditions in the crevice and d) build-up of aggressive ion species (e.g chloride) in the crevice. In this study. the mechanism of crevice corrosion for Type 430 stainless steel is investigated undercondition that the size of specimen is $15{\times}20\{times}3mm$, in 1N $H_2SO_4$ + 0.05N NaCl solution. and the artificial crevice gap size of 3 x 0.2 x 15 mm. Crevice corrosion is measured under applied potential -300mV(SCE) to the external surface. The obtained result of this study showed that 1) the induced time for initiation of crevice is 750 seconds. 2) potential of the crevice was about from -320mV to -399mV. which is lower than that of external surface potential of -300mV It is considered that potential drop in the crevice is one of mechanisms for the crevice corrosion

Influence of Plate Design on the Accuracy of Tibial Alignment after Center of Rotation of Angulation-Based Leveling Osteotomy in Toy-Breed Dogs

  • Han, Jae-Hong;Lee, Hae-Beom;Jeong, Jae-Min;Jeon, Young-Jin;Roh, Yoon-Ho
    • Journal of Veterinary Clinics
    • /
    • v.39 no.3
    • /
    • pp.100-106
    • /
    • 2022
  • The center of rotation of angulation-based leveling osteotomy (CBLO) has been introduced for the stabilization of cranial cruciate ligament rupture (CCLR) in small-breed dogs. This technique can be applied to the tibia without damaging its tuberosity. Although different designs of CBLO plates are available, tibial plateau leveling osteotomy (TPLO) plates have been still used for stabilization during CBLO. To the best of our knowledge, no studies have reported the effects of TPLO plates on the postoperative limb alignment after CBLO. Therefore, the present study (January 2020 to February 2021) aimed to compare the postoperative outcomes (postoperative tibial plateau angle [TPA] and tibial alignment) in patients receiving CBLO and TPLO plates during CBLO. Paired stifle joints (n = 16) were obtained from eight toy-breed cadaver dogs (mean weight, 4.4 kg) that underwent CBLO. The joints were randomly assigned to receive the CBLO (CBLO group) or TPLO plates (TPLO group). Pre-and postoperative radiographs were obtained, and the dissected tibiae were evaluated. The following postoperative parameters were compared to evaluate the surgical outcome: TPA, osteotomy location, mechanical medial proximal tibia angle, inter-segment gap, and tibial plateau translation. No significant differences were found in the postoperative alignment between the two groups. Therefore, TPLO plates may be considered as a viable alternative in toy-breed dogs undergoing CBLO.

Flip Chip Process for RF Packages Using Joint Structures of Cu and Sn Bumps (Cu 범프와 Sn 범프의 접속구조를 이용한 RF 패키지용 플립칩 공정)

  • Choi, J.Y.;Kim, M.Y.;Lim, S.K.;Oh, T.S.
    • Journal of the Microelectronics and Packaging Society
    • /
    • v.16 no.3
    • /
    • pp.67-73
    • /
    • 2009
  • Compared to the chip-bonding process utilizing solder bumps, flip chip process using Cu pillar bumps can accomplish fine-pitch interconnection without compromising stand-off height. Cu pillar bump technology is one of the most promising chip-mounting process for RF packages where large gap between a chip and a substrate is required in order to suppress the parasitic capacitance. In this study, Cu pillar bumps and Sn bumps were electroplated on a chip and a substrate, respectively, and were flip-chip bonded together. Contact resistance and chip shear force of the Cu pillar bump joints were measured with variation of the electroplated Sn-bump height. With increasing the Sn-bump height from 5 ${\mu}m$ to 30 ${\mu}m$, the contact resistance was improved from 31.7 $m{\Omega}$ to 13.8 $m{\Omega}$ and the chip shear force increased from 3.8 N to 6.8 N. On the contrary, the aspect ratio of the Cu pillar bump joint decreased from 1.3 to 0.9. Based on the variation behaviors of the contact resistance, the chip shear force, and the aspect ratio, the optimum height of the electroplated Sn bump could be thought as 20 ${\mu}m$.

  • PDF