• 제목/요약/키워드: firing strength

검색결과 173건 처리시간 0.023초

Thin and Hermetic Packaging Process for Flat Panel Display Application

  • Kim, Young-Cho;Jeong, Jin-Wook;Lee, Duck-Jung;Choi, Won-Do;Lee, Sang-Geun;Ju, Byeong-Kwon
    • Journal of Information Display
    • /
    • 제3권1호
    • /
    • pp.11-16
    • /
    • 2002
  • This paper presents a study on the tubeless Plasma Display Panel (PDP) packaging using glass-to-glass electrostatic bonding with intermediate amorphous silicon. The bonded sample sealing the mixed gas with three species showed high strength ranging from 2.5 MPa to 4 MPa. The glass-to-glass bonding for packaging was performed at a low temperature of $180^{\circ}C$ by applying bias of 250 $V_{dc}$ in ambient of mixed gases of He-Ne(27 %)-Xe(3 %). The tubeless packaging was accomplished by bonding the support glass plate of $30mm{\times}50mm$ on the rear glass panel and the capping glass of $20mm{\times}20mm$. The 4-inch color AC-PDP with thickness of 8 mm was successfully fabricated and fully emitted as white color at a firing voltage of 190V.

Characterization of Lightweight Earthenware Tiles using Foaming Agents

  • Lee, Won-Jun;Cho, Woo-Suk;Hwang, Kwang-Taek;Kim, Jin-Ho;Hwang, Hae-Jin;Lee, Yong-Ouk
    • 한국세라믹학회지
    • /
    • 제52권6호
    • /
    • pp.473-478
    • /
    • 2015
  • Green bodies of earthenware tile were prepared from a mixture of earthenware tile powder and SiC as forming agents by applying a conventional process. Granule powder for tile samples was prepared using the spray drying method with commercial earthenware raw material with a quantity of SiC of 0.3 wt%. The applied pressure was $250kg{\cdot}f/m^2$ and the firing temperature was $1050-1200^{\circ}C$. The effects of the SiC particle size and sintering temperature on the open porosity and total porosity were investigated and the correlative mechanism was also discussed. While total porosity was not significantly changed by decreasing the SiC particle size, the open porosity showed a gradual decrease, which represents an increase of the closed porosity. As the sintering temperature increased, coarsening was made among the pores due to excessive oxidation. The volume shrinkage and bending strength were demonstrated for the sintered tile samples. The sintered bulk density was also measured to determine the weight reduction value.

공침법에 의한 Cordierite분말의 합성 및 소결에 관한 연구 (Synthesis and Sintering of Cordierite by using Coprecipitation Method)

  • 한문희;박금철
    • 한국세라믹학회지
    • /
    • 제27권7호
    • /
    • pp.899-906
    • /
    • 1990
  • The cordierite powders were prepared from Mg(NO3)2.6H2O, Al(NO3)3.9H2O and colloidal silica by the coprecippitation method, and the sintering behavior of the powders were investigated. Two different methods were applied for producing the precursor powders. The one was to added the aqueous solution of Mg(NO3)2.6H2O and Al(NO3)3.9H2O to NH4OH to adjust pH at 10 where the colloidal silica of pH 10 was added. The other wa to add the aqueous solution of Mg(NO3)2.6H2O and Al(NO3)3.9H2O to the colloidal silica with NH4OH to control the final mixture to be at pH 10. It was confirmed that more homogeneous powders were obtained from the latter method. The firing linear shrinkage of the powder compacts fabricated from the calcined powder between 90$0^{\circ}C$ and 110$0^{\circ}C$ was found to be larger as the calcination temperature was low. But all of them stopped shrinking around 120$0^{\circ}C$. The powder compacts, fabricated using the calcined powders at 90$0^{\circ}C$ and 95$0^{\circ}C$ for 2hours and sintered at 142$0^{\circ}C$ for 2hours, showed relative density of 93-96%, 3-point bending strength of 81-83MPa, KIC of 1.9-2.4 MPam1/2 and thermal expansion coefficient of 0.213-0.732$\times$10-6$^{\circ}C$.

  • PDF

상용 치과 법랑질 도재의 광학적 및 기계적 특성 (Optical and Mechanical Properties of Commercial Dental Enamel Porcelain)

  • 박형랑
    • 대한치과기공학회지
    • /
    • 제26권1호
    • /
    • pp.115-128
    • /
    • 2004
  • In this study, optical and mechanical properties were investigated with 4 kinds of commercial dental enamels. As a result of EDS analysis $SiO_2,\;Na_{2}O,\;Al_{2}O_3\;and\;K_{2}O$ were the main components of commercial dental enamels. In case of H specimen, content of $SiO_2\;and\;K_2O$ were more than that of another specimens. Starting powder and fired specimens were glass ceramics which were consist of amorphous phase and leucite (crystalline) phase. Crystallization did not occurred during firing process, since the XRD peak intensity was similar between starting powder and fired specimens. As a result of differential thermal analysis, $T_g$ and crystalline temperature was varied with composition in the range of $548\sim576^{\circ}C$ and $735\sim780^{\circ}C$ respectively. 0.5mm thickness dental enamel specimens showed sufficient translucent properties. However, transmittance and reflectance were lower than 5% result from scattering due to the refractive index difference between glass and crystalline phase. 3 point bending strength was in the range of 73.9$\sim$101.8MPa which was similar or slightly higher than enamel of natural teeth and Vickers hardness was higher than enamel of natural teeth more than 100.

  • PDF

Low k Materials for High Frequency High Integration Modules

  • Na, Yoon-Soo;Lim, Tae-Young;Kim, Jin-Ho;Shin, Hyo-Soon;Hwang, Jong-Hee;Cho, Yong-Soo
    • 한국세라믹학회지
    • /
    • 제46권4호
    • /
    • pp.413-418
    • /
    • 2009
  • Glass systems based on Ca, Sr, Ba, and Zn modified alumino-boro silicates were investigated in order to improve the dielectric and mechanical properties of a typical LTCC (low temperature co-fired ceramic) which was developed for high frequency highly-integrated modules. The glass was prepared by a typical melting procedure and then mixed with cordierite fillers to fabricate glass/ceramic composite-type LTCC materials. The amount of cordierite filler was fixed at 50 volumetric%. For an optimal glass composition of 7.5% CaO, 7.5% BaO, 5% ZnO, 10% $Al_2O_3$, 30% $B_2O_3$, and 40% $SiO_2$ in mole ratio, the resultant LTCC composite showed a dielectric constant of 5.8 and a dielectric loss ($tan{\delta}$) of 0.0009 after firing at $900^{\circ}C$. An average bending strength of 160MPa was obtained for the optimal composition.

Selective Laser Sintering of Alumina Using an Inorganic Binder Monoclinic $HBO_2$ and Post-Processing

  • 이인섭
    • 한국분말재료학회지
    • /
    • 제5권3호
    • /
    • pp.199-209
    • /
    • 1998
  • A new low melting inorganic binder, monoclinic $HBO_2$, has been developed for Selective Laser Sintering (SLS) of alumina powder by dehydration process of boron oxide powder in a vacuum oven at $120^{\circ}C$. It led to better green SLS parts and higher bend strength far green and fired parts compared to other inorganic binders such as aluminum and ammmonium phosphate. This appeared to be due to its low viscosity and better wettability of the alumina particle surface. A low density single phase ceramic, aluminum borate ($Al_{18}B_4O_{33}$), and multiphase ceramic composites, $A_{12}O_3-A_{14}B_2O_9$, were successfully developed by laser processing of alumina-monoclinic $HBO_2$ powder blends followed by post-thermal processing; both $Al_{18}B_4O_{33}$ and $A_{14}B_2O_9$ have whisker-like grains. The physical and mechanical properties of these SLS-processed ceramic parts were correlated to the materials and processing parameters. Further densification of the $A_{12}O_3-A_{14}B_2O_9$ ceramic composites was carried out by infiltration of colloidal silica, and chromic acid into these porous SLS parts followed by heat-treatment at high temperature ($1600^{\circ}C$). The densities obtained after infiltration and subsequent firing were between 75 and 80% of the theoretical densities. The bend strengths are between 15 and 33 MPa.

  • PDF

수산화알루미늄으로부터 수열법을 이용한 활성 알루미나 제조에 관한 연구 (Fabrication of Activated Alumina Using Aluminum Hydroxide by a Hydrothermal Process)

  • 배현철;이상진
    • 한국세라믹학회지
    • /
    • 제50권6호
    • /
    • pp.384-389
    • /
    • 2013
  • Activated alumina was fabricated with aluminum hydroxide in this study. High-purity alumina gel and boehmite were prepared from aluminum hydroxide by a hydrothermal process and fired to activate alumina having a surface area of 380 ~ 480 $m^2/g$ with less loss of ignition. The aging and drying condition during the fabrication process affected the loss of ignition, the sedimentation time of the alumina suspension, as well as the surface area of the activated alumina. For pellet-type activated alumina, the pre-fired alumina gel and boehmite were press-formed and fired at $400^{\circ}C$ and $550^{\circ}C$ for 6 h, respectively. The fired pellets showed a low density of 2.0 ~ 2.2 $g/cm^3$ with 20% firing shrinkage and sufficient handling strength. In this study, a new fabrication process for high-quality activated alumina with aluminum hydroxide is introduced. The effects of the processing parameters on the activated alumina properties are also examined.

AC-PDP특성평가를 위한 전압전달곡선 계측에 관한 연구 (Measurement of Voltage Transfer Curve in AC PDP)

  • 손진부;이성현;김동현;김영대;조정수;박정후
    • 한국전기전자재료학회:학술대회논문집
    • /
    • 한국전기전자재료학회 1999년도 춘계학술대회 논문집
    • /
    • pp.395-398
    • /
    • 1999
  • In ac PDP(plasma Display Panel), the discharge characteristics is very important to display clear images. In this paper, we have studied the measurement of voltage transfer curves which show the discharge characteristics in AC PDP. The change of the effective wall capacitance during a discharge is also studied. These depend on lateral spreading of charge distribution and the strength of the discharge. As a parameter of the frequency, we observed the effects of the frequency in voltage transfer curves and in effective wall capacitance changes. As frequency increases, minimum sustain voltage and firing voltage decrease. In upper region of gap voltage the chance of the effective wall capacitance is independent of frequency.

  • PDF

Anorthite의 합성 및 그 특성에 관한 연구 (A Study on the Synthesis of Anorthite and its Characteristics.)

  • 백용혁;이종권
    • 한국세라믹학회지
    • /
    • 제20권2호
    • /
    • pp.153-160
    • /
    • 1983
  • This study was carried out to research the change of mineral phases and the characteristics(apparent specific gra-vity water absorption firing shrinkage modulus of rupture thermal expansion and specific dielectric constant) of the sintered bodies manufactured by kaolin and limestone. Samples were composed of the same theoretical composition as it of anorthite and fired up to 145$0^{\circ}C$ Investigated the change and micro-structure of the mineral phases by XRD and SEM the characterisdtics of the sintered bodies by TMA Automatic Capacitance Bridge and etc. The results were as follow. 1. Reactions of sintering are occurred between 860-95$0^{\circ}C$ and 1200-138$0^{\circ}C$ and state of bloating is occurred at 1410-145$0^{\circ}C$ 2. For the inclusion of feldspar and its fine particles of materials the temperature of producing and collapsing is decreased. 3. Pseudo-wollastonite and gehlenite are formed about 95$0^{\circ}C$ 4. At 114$0^{\circ}C$ anorthite are begin to forming and increase continuously to 138$0^{\circ}C$. Above 141$0^{\circ}C$ content of anorthite are decreased. 5. The variations of bending strength with sintering temperature reflect similar trend of sintered contraction and in-crease continuously from 120$0^{\circ}C$. At 145$0^{\circ}C$ reached about 680kg/cm2. 6. Specific dielectric constant$($\varepsilon$_s)$ of specimen sintered at 141$0^{\circ}C$ is 7.12 and that value is most favorable.

  • PDF

KSR-III 추진제 탱크 압력 조절용 레귤레이터 개발 (The Development of Pressure Regulator of Propellant Tank for KSR-III)

  • 정영석;조기주;조인현;김용욱;오승협
    • 한국추진공학회지
    • /
    • 제6권4호
    • /
    • pp.47-58
    • /
    • 2002
  • 압력조절 레귤레이터는 KSR-III 추진제 탱크의 압력 조절용으로 개발하였다. KSR-III 가압 시스템은 가압 탱크, 압력조절용 레귤레이터, 추진제 탱크로 구성된 가장 기본적인 시스템이며 레귤레이터는 헬륨 탱크, 파이로밸브, 헬륨주입밸브와 더불어 가장 핵심적인 부품이다. 1차 시제품으로 기밀, 강도, 기본 성능을 만족하는 상세 설계를 완성하였고 2차 시제품으로 추진기관 종합수류시험을 수행하였다. 2차시험을 통해서 밸브의 용량(Cv)을 늘려야 할 필요성이 나타났다. 3차 시제품에 이를 개선하였으며 추진기관 종합 실추진제 시험과 연소시험을 통해 최종 검증하였다.