• Title/Summary/Keyword: electron microscope analysis

Search Result 1,022, Processing Time 0.029 seconds

Scientific Analysis of Gilt-Bronze Plaquettes with Buddhist Images(Panbul) from Anapji Pond, Gyeongju (안압지 금동판불의 과학적 분석)

  • Yu, Heisun;Park, Haksoo;Shin, Yongbi
    • Conservation Science in Museum
    • /
    • v.8
    • /
    • pp.49-69
    • /
    • 2007
  • This is about the scientific analysis of the 10 items of the gilt-bronze Panbul excavated from Anapji, Gyeongju. First, the composition of the Panbul was confirmed, using X-ray fluorescence spectrometer (XRF), and the patinas covering the surface of the Panbul were analyzed, using X-ray diffractometer (XRD). And the micro structures and gilt layer of the Panbul were investigated, using microscope and scanning electron microscope with energy dispersive spectrometer (SEM/EDS), and in order to investigate the internal conditions of the Panbul, X-radiography was conducted. As the result, it is found out that the material of the Panbul excavated from Anapji was the bronze of copper (86~95%) and tin (4~12%), and coated with gold. And cuprite (Cu2O) was detected from red patina of the gilt-bronze Panbul, and chalcocite(Cu2S) also was detected from the black patina. As the result of the observation of the micro structure through microscope, it is estimated that it was manufactured, using the wax molding method, and, judging from the fact that the thickness of gilt layer was not even, and that the groove had been filled, it was presumed that the amalgam coating method had been used, but some questions still remain, because mercury was not detected. Lastly, through the X-radiography, it was observed that the tiny round spots existed, which was presumed to have been generated during the casting.

A Fatigue Failure Analysis of Fractured Fixing Bolts of a Mobile Elevating Work Platform using Finite Element Methods (유한요소기법을 이용한 고소작업대의 파손된 고정볼트의 피로 파손 분석)

  • Choi, Dong Hoon;Kim, Jae Hoon
    • Journal of the Korean Society of Safety
    • /
    • v.35 no.5
    • /
    • pp.1-8
    • /
    • 2020
  • Mobile elevating work platforms (MEWPs) consist of a work platform, extending structure, and chassis, and are used to move persons to working positions. MEWPs are useful but are composed of pieces of equipment, and accidents do occur owing to equipment defects. Among these defects, accidents caused by the fracture of bolts fixed to the extension structure and swing system are increasing. This paper presents a failure analysis of the fixing bolts of MEWP. Standard procedure for failure analysis was employed in this investigation. Visual inspection, chemical analysis, tensile strength measurement, microstructural characterization, fractography analysis by Optical Microscope(OM) and Scanning Electron Microscopy(SEM), and finite element analysis (FEA) were used to analyze the failure of the fixing bolts. Using this failure analysis approach, we found the root cause of failure and proposed a means for solving this type of failure in the future. First, the chemical composition of the fixing bolt is obtained by a spectroscopy chemical analysis method, which determined that the chemical composition matched the required standard. The tensile test showed that the tensile and yield strengths were within the required capacity. The stress analysis was carried out at five different boom angles, and it was determined that the fixing bolt of MEWP can withstand the loads at all the boom angles. The outcomes of the fatigue analysis revealed that the fixing bolt fails before reaching the design requirements. The results of the fatigue analysis showed primarily that the failure of the fixing bolt was due to fatigue. A visual inspection of the fractured section of the fixing bolt also confirmed the fatigue failure. We propose a method to prevent failure of the fixing bolt of the MEWP from four different standpoints: the manufacturer, safety certification authority, safety inspection agency, and owner.

The particle properties and luminescence properties of Gd2O3:Eu using solution-combustion with various Eu content were analysis (X선 검출기를 위해 특수용매 액상법으로 합성한 Gd2O3:Eu의 Europium(Eu) 함량에 따른 입자특성과 발광특성의 분석)

  • Kim, Sung-Hyun;Kim, Young-Bin;Jung, Suk-Hee;Kim, Min-Woo;Oh, Kyung-Min;Park, Ji-Gun
    • Journal of the Korean Society of Radiology
    • /
    • v.2 no.3
    • /
    • pp.11-18
    • /
    • 2008
  • In this study, the particle properties and luminescence properties of Gd2O3 nano powder with various Eu content were studied. Gd2O3:Eu nano powder was fabricated using special solvent which mixed the alcohol and the distilled water at specific ratio. This solvent by the solution method showed short fabrication time because solution time of Gd and Eu was reduced. From this experiment with Gd2O3:Eu, the particle properties og nano powder phosphor way analysed using SEM (scanning electron microscope) and EDX(Energy Dispersive X-ray). Also the luminescence properties of nano powder was measured using PL(Photoluminescence) and CL (CathodeLuminescence). The size of powder was 30nm~40nm. The magnitude of powder showed the best peak at 620nm. Among 1,3,5wt% of Eu content, the more Eu content was added in powder, the more photons wre generated. Also it shows luminescence efficiency was improved adding 5% of Eu content.

  • PDF

Fabrication and Evaluation Properties of Micro-Tubular Solid Oxide Fuel Cells (SOFCs) (마이크로 원통형 SOFC 제작 및 특성평가)

  • Kim, Hwan;Kim, Wan-Je;Lee, Jong-Won;Lee, Seung-Bok;Lim, Tak-Hyoung;Park, Seok-Joo;Song, Rak-Hyun;Shin, Dong-Ryul
    • Korean Chemical Engineering Research
    • /
    • v.50 no.4
    • /
    • pp.749-753
    • /
    • 2012
  • In present work, anode support for micro-tubular SOFC was fabricated with outer diameter of 3 mm and characterized with microstructure, mechanical properties and gas permeability. The microstructure of surface and cross section of a porous anode support were analyzed by using SEM (Scanning Electron Microscope) image. The gas permeability and the mechanical strength of anode support was measured and analysed by using differential pressure at the flow rates of 50, 100, 150 cc/min. and using universal testing machine respectively. The unit cell composed of NiO-YSZ, YSZ, YSZ-LSM/LSM/LSCF was fabricated and operated with reaction temperature and fuel flow rate and showed maximum power density of $1095mW/cm^2$ on the condition of $800^{\circ}C$. The performance of single cell for micro-tubular SOFC increased with the increasing the reaction temperature due to the decrement of ohmic resistance of cell by the increment of the ionic conductivity of electrolyte through the evaluation of electrochemical impedance analysis for single cell with reaction temperature.

Synthesis of Hexagonal β-Ni(OH)2 Nanosheet as a Template for the Growth of ZnO Nanorod and Microstructural Analysis (ZnO 나노 막대 성장을 위한 기판층으로서 hexagonal β상 Ni(OH)2 나노 시트 합성 및 미세구조 분석)

  • Hwang, Sung-Hwan;Lee, Tae-Il;Choi, Ji-Hyuk;Myoung, Jae-Min
    • Korean Journal of Materials Research
    • /
    • v.21 no.2
    • /
    • pp.111-114
    • /
    • 2011
  • As a growth-template of ZnO nanorods (NR), a hexagonal $\beta-Ni(OH)_2$ nanosheet (NS) was synthesized with the low temperature hydrothermal process and its microstructure was investigated using a high resolution scanning electron microscope and transmission electron microscope. Zinc nitrate hexahydrate was hydrolyzed by hexamethylenetetramine with the same mole ratio and various temperatures, growth times and total concentrations. The optimum hydrothermal processing condition for the best crystallinity of hexagonal $\beta-Ni(OH)_2$ NS was determined to be with 3.5 mM at $95^{\circ}C$ for 2 h. The prepared $Ni(OH)_2$ NSs were two dimensionally arrayed on a substrate using an air-water interface tapping method, and the quality of the array was evaluated using an X-ray diffractometer. Because of the similarity of the lattice parameter of the (0001) plane between ZnO (wurzite a = 0.325 nm, c = 0.521 nm) and hexagonal $\beta-Ni(OH)_2$ (brucite a = 0.313 nm, c = 0.461 nm) on the synthesized hexagonal $\beta-Ni(OH)_2$ NS, ZnO NRs were successfully grown without seeds. At 35 mM of divalent Zn ion, the entire hexagonal $\beta-Ni(OH)_2$ NSs were covered with ZnO NRs, and this result implies the possibility that ZnO NR can be grown epitaxially on hexagonal $\beta-Ni(OH)_2$ NS by a soluble process. After the thermal annealing process, $\beta-Ni(OH)_2$ changed into NiO, which has the property of a p-type semiconductor, and then ZnO and NiO formed a p-n junction for a large area light emitting diode.

Synthesis of Ultrafine LaAlO$_3$ Powders with Good Sinterability by Self-Sustaining Combustion Method Using (Glycine+Urea) Fuel ((Glycine+Urea) 혼합연료를 이요한 자발착화 연소반응법에 의한 우수한 소결성의 초미분체 LaAlO$_3$ 분말 합성)

  • Nam, H.D.;Choi, W.S.;Lee, B.H.;Park, S.
    • Journal of the Korean Ceramic Society
    • /
    • v.36 no.2
    • /
    • pp.203-209
    • /
    • 1999
  • LaAlO3d single phase used as the butter layer on Si wafer for YBa2Cu3O7-$\delta$ superconductor application were prepared by solid state reaction method and by self-sustaining combustion process. The microstructure and crystallity of synthesiszed LaAlO3 powder studied using scanning electron microscope (SEM) and X-ray diffractometer(XRD), specific surface area and sintering characteristics fo powder were investigated by Brunauer-Emmett-Teller (BET) method and dilatometer respectively. In solid state reaction method, it is difficult to obtain LaAlO3 single phase up to 150$0^{\circ}C$ period. However, in self-sustaining combustion process, it is to easy to do it only $650^{\circ}C$. Based on the results of analysis of dilatometer it is easier to obtain high sintering density (98.87%) in self-sustaining combustion process than in the solid state reaction method. This reason is that the average particle size prepared by self-sustaining combustion process is nano crystal size and has high specific surface are value(56.54 $m^2$/g) compared with that by solid state reaction method. Also, LaAlO3 layer on the Si wafer has been achieved by screen printing and sintering method. Even though the sintering temperature is 130$0^{\circ}C$, the phenomena of silicon out diffusion in LaAlO3/Si interphase are not observed.

  • PDF

Preparation of Porous Polyacrylonitrile Nanofibers Membrane for the MF Application (MF 적용을 위한 다공성 PAN 나노섬유막의 제조)

  • Ahn, Hyeonryun;Jang, Wongi;Tak, Taemoon;Byun, Hongsik
    • Membrane Journal
    • /
    • v.23 no.2
    • /
    • pp.112-118
    • /
    • 2013
  • Polyancrylonitrile nanofiber membrane (PAM) was prepared by using the electrospinning method with a solution of polyacrylonitrile (PAN) in DMF. The pore-diameter of PAMs and the number of PAM's layer were controlled for the microfiltration (MF) application. In addition, in order to improve the water-flux, AN-PEGMA copolymers have been synthesized via free radical polymerization with poly (ethylene glycol) methyl ether methacrylate and azobisisobutylronitrile (AIBN), and then PAN/AN-PEGMA nanofiber membranes (PAM/APM) were prepared by electrospinning with a mixture of PAN (9 wt%) and AN-PEGMA (3 wt%) in DMF (88 wt%). The prepared membranes were investigated with FT-IR and E.D.S. It was confirmed through scanning electron microscope (SEM), porometer, and porosity analysis that the porous membrane with a uniform diameter (400~600 nm) and a uniform pore characteristics (0.5~0.4 ${\mu}m$) was prepared. For the MF application, water-flux measurements were investigated and then the result was shown that the water permeability value of PAM/APMs introduced AN-PEGMA copolymers was relatively higher than that of the PVdF commercial membrane. From these results, PAN nanofiber membranes prepared by electrospinning could be utilized as a MF membrane.

The Structural Stability and Electrochemical Properties of Fe Doped Li[Ni0.575Co0.1Mn0.325]O2 (Fe을 도핑한 Li[Ni0.575Co0.1Mn0.325]O2의 구조적인 안정성 및 전기화학적 특성)

  • Yang, Su-Bin;Yoo, Gi-Won;Jang, Byeong-Chan;Son, Jong-Tae
    • Journal of the Korean Electrochemical Society
    • /
    • v.17 no.3
    • /
    • pp.149-155
    • /
    • 2014
  • In this study, a positive-electrode material in a lithium secondary battery $Li[Ni_{0.575}Co_{0.1}Mn_{0.325}]O_2$ was synthesized as precursor by co-precipitation. Cathode material was synthesized by adding iron. The synthesized cathode material was analyzed by scanning electron microscope and x-ray diffraction. The analysis of x-ray diffraction showed that the a-axis and c-axis is increased by doping iron. And $I_{(003)}/I_{(104)}$ is increased and $I_{(006)}+I_{(102)}/I_{(101)}$ is decreased. Through this result, it was confirmed that the structural stability is improved. And impedance measurements show that the charge transfer resistance ($R_{ct}$) is lowered by doping iron. Consequently, electrochemical properties are improved by doping iron. In particular, the cycle characteristics are improved at a high temperature condition (328 K). Structural stabilities are contributing to the cycle properties.

Mössbauer Studies of Manganese Iron Oxide Nanoparticles (망간-철산화물 나노입자의 뫼스바우어 분광 연구)

  • Hyun, Sung-Wook;Shim, In-Bo;Kim, Chul-Sung;Kang, Kyung-Su;Park, Chu-Sik
    • Journal of the Korean Magnetics Society
    • /
    • v.18 no.1
    • /
    • pp.24-27
    • /
    • 2008
  • We have prepared $MnFe_2O_4$ nanoparticles with polyol method. The crystallographic and magnetic properties were measured by using X-ray diffraction(XRD), vibrating sample magnetometer(VSM) and $M\"{o}ssbauer$ spectroscopy. The high resolution transmission electron microscope(HRTEM) shows uniform nanoparticle-sizes with $6{\sim}8$ nm. The crystal structure is found to be single-phase cubic spinel with space group of Fd3m. The lattice constant of $MnFe_2O_4$ nanparticles is determined to be $8.418{\pm}0.001{\AA}$. $M\"{o}ssbauer$ spectrum of $MnFe_2O_4$ nanparticles at room temperature(RT) shows a superparamagnetic behavior. In VSM analysis, the diagnosis of the superparamagnetic behavior is also shown in hysteresis loop at RT. $M\"{o}ssbauer$ spectrum at 4.2K shows that the well developed two sextets are with different hyperfine field $H_{hfA}=498$(A-site) and $H_{hfB}=521$(B-site) kOe.

Characteristics of Tremolite Asbestos from Abandoned Asbestos Mines in Boryeong Area, Chungnam (충남 보령지역의 폐석면 광산에서 산출하는 투각섬석 석면의 특성)

  • Yoon, Keun-Taek;Hwang, Jin-Yeon;Oh, Ji-Ho;Lee, Hyo-Min
    • Journal of the Mineralogical Society of Korea
    • /
    • v.23 no.1
    • /
    • pp.73-84
    • /
    • 2010
  • We studied the geological occurrence, associated minerals, mineralogical properties and formation process of tremolites from two abandoned asbestos mines, Jungang (Sinsuk) and Daebosuksan, located in Boryoung area, Chungnam. Morphologically different tremolites such as long fibrous, needle-like, bladed and prismatic forms coexisted. Fibrous tremolite, known for its high toxieity to human health, was systematically analyzed by polarized light microscopy and scanning electron microscopy. The average length of tremolite fibers was 31.2 ${\mu}m$ although the maximum length of some asbestos was 210.0 ${\mu}m$. The average width and aspect ratio were 1.6 ${\mu}m$ and 19.9, respectively. Tremolite showed inclined extinction in the range of 6.1~20.2$^{\cric}$. X-ray diffraction patterns were slightly different between fibrous (asbestiform) and prismatic (non-asbestiform) tremolites. EPMA analysis of tremolites in the study area indicated extremely high Mg content with very low Fe content, close to the composition of tremolite in end-member in the tremolite-actinolite solid solution series. The formational conditions of asbestiform and non-asbestiform tremolite appear to be different. Asbestiform tremolite was estimated to have been formed in later stage.