• 제목/요약/키워드: dynamic Young's modulus

검색결과 121건 처리시간 0.023초

한국산(韓國産) 죽재(竹材)의 동력학적(動力學的) 성질(性質) (Dynamic Mechanical Properties of Bamboos in Korea)

  • 홍병화
    • Journal of the Korean Wood Science and Technology
    • /
    • 제16권1호
    • /
    • pp.45-54
    • /
    • 1988
  • This study was carried out to investigate the fiber length, fiber width and fiber thickness on the longitudinal direction by the parts of culm and also specific gravity in air dry, dyna.mic mechanical properties and internal frictions by the internode and the node in Phyllostachys bambusoides Phyllostachys nigra var. henonis and Phllostachys edulis which were grown in Korea. The results obtained were as follows; 1. The variations of fiber length and fiber width on the longitudinal direction had a tendency to increase slightly from the butt and then to decrease toward the top. but there was not a definite variation for fiber thickness according to the parts of culm. 2. The specific gravity in air dry of internode was increased from the butt toward the top, but the specific gravity in air dry of node was not correlations with the parts of culm. 3. Dynamic Young's modulus of internode on the longitudinal direction was increased according to the heights of culms within each species, and there were in order of P. edulis P. nigra var. henonis and P. bambusoides. 4. Correation coefficients between the specific gravity and the dynamic Young's modulus were 0.837 in P. bambusoides 0.871 in P. nigra var. henonis and 0.935 in P. edulis and there was also highly significant for dynamic Young's modulus between the specific gravities in air dry. 5. There were not correlations between the internal frictions and the parts of internode.

  • PDF

열처리(熱處理) 목재(木材)의 동적점탄성(動的粘彈性) (Dynamic Viscoelasticity of Heat Treated Wood)

  • 홍병화
    • Journal of the Korean Wood Science and Technology
    • /
    • 제14권2호
    • /
    • pp.13-20
    • /
    • 1986
  • The effect of heat treatment on the dynamic viscoelasticity of the woods of Picea sitchensis and Paulownia coreana which have been for musical instruments was investigated. The treatment was made in a temperature range of 60-180$^{\circ}C$ for periods of 3 hours to 24 hours. The results obtained are summarized as follows: Moisture absorption decreased with increasing temperature. Dynamic Young's modulus decreased with increasing temperature and hours. Dynamic viscoelasticity decreased with increasing moisture content, but internal friction increased with increasing amount of moisture content.

  • PDF

열처리(熱處理) 죽재(竹材)의 동적점탄성(動的粘彈性) (Dynamic Viscoelasticity of Heat-Treated Bamboo)

  • 홍병화;변희섭
    • Journal of the Korean Wood Science and Technology
    • /
    • 제23권4호
    • /
    • pp.67-73
    • /
    • 1995
  • This study was undertaken to investigate the effect of heat treatment on the dynamic viscoelasticity of three species of Phyllostachys bambusoides, Phyllostachys nigra var. henonis and Phyllostachys pubescens, grown in southern Korea. The bamboo was treated for 3~24 hours at $60{\sim}180^{\circ}C$, and then was treated in a climatic chamber for 3~48 hours at $40^{\circ}C$ and 95% relative humidity. The results obtained are summarized as follows : 1. Dynamic Young's modulus decreased with increasing temperature and duration of the heat treatment. 2. Internal friction decreased with increasing treatment duration. 3. Moisture absorption decreased with increasing temperature and duration of the heat treatment. 4. Dynamic viscoelasticity decreased, whereas internal friction slowly increased, with increasing moisture content.

  • PDF

하향식 탄성파를 통한 경기 편마암의 동탄성 특성연구 (A Study on the Characteristics of Dynamic Elastic Modulus in GyeongGi Gneiss Complex by Down Hole Test)

  • 이벽규;이수곤
    • 지질공학
    • /
    • 제18권4호
    • /
    • pp.371-379
    • /
    • 2008
  • 본 연구에서는 경기도 일대의 편마암지역 11곳에서 다운홀(down-hole) 탄성파탐사를 이용하여 획득한 탄성파속도를 이용, 편마암지역에서의 탄성파 속도와 동탄성계수와의 상관성을 조사하였다. 연구결과 편마암에서의 탄성파속도의 특성은 $V_s=0.5589{\times}V_p$ 상관관계를 보여준다. 탄성파 속도와 동탄성계수와의 상관관계는 두 개의 군으로 분리된다. 풍화가 진행됨에 따라 첫 번째 군은 암석의 비중에 큰 영향을 받지만 두 번째 군에서는 절리면의 간격에 영향을 받는다. 풍화가 진행됨에 따라 첫 번째 군은 감소하는 경향을 보인다. 경암반에서의 압축파속도($V_p$) 동탄성계수($E_d$, $G_d$, $K_d$)의 상관관계는 선형으로 분석되었지만, 보통암반에서의 압축파속도($V_p$)와 동탄성계수($E_d$, $G_d$, $K_d$)의 상관관계는 2차 함수 포물선 곡선의 형태를 띠는 것으로 분석되었다. 전단파속도($V_s$)와 동탄성계수($E_d$, $G_d$, $K_d$)의 상관관계 또한 압축파속도($V_p$)와 유사한 결과를 보이는 것으로 분석되었다.

정적 및 동적 하중을 받는 두 상이한 등방성 이종재료의 이종재료상수에 대한 연구 (A Study on the Bimaterial Constant of Two Dissimillar Isotropic Bimaterial Under Static and Dynamic Load)

  • 신동철;황재석
    • 대한기계학회논문집A
    • /
    • 제28권11호
    • /
    • pp.1776-1785
    • /
    • 2004
  • In this research, the relationships between static bimaterial constant and dynamic oscillation index are studied. It was certified that static bimaterial constant has the same form equation as the dynamic oscillation index. Bimaterial constant and oscillation index are increased with the increment of Young's modulus ratio and approached to the some value. Isochromatic fringe patterns are slanted to the left side with increment of bimaterial constants and oscillation index. Though patterns of stress components in above the crack surface are similar to each other, their magnitudes are different a little. In the ahead of crack tip, there are big differences in the isochromatic fringe patterns and their magnitudes. The influence of bimaterial with Young's modulus ratio is bigger in the propagation crack than in the stationary crack.

Comparison of the effects of irradiation on iso-molded, fine grain nuclear graphites: ETU-10, IG-110 and NBG-25

  • Chi, Se-Hwan
    • Nuclear Engineering and Technology
    • /
    • 제54권7호
    • /
    • pp.2359-2366
    • /
    • 2022
  • Selecting graphite grades with superior irradiation characteristics is important task for designers of graphite moderation reactors. To provide reference information and data for graphite selection, the effects of irradiation on three fine-grained, iso-molded nuclear grade graphites, ETU-10, IG-110, and NBG-25, were compared based on irradiation-induced changes in volume, thermal conductivity, dynamic Young's modulus, and coefficient of thermal expansion. Data employed in this study were obtained from reported irradiation test results in the high flux isotope reactor (HFIR)(ORNL) (ETU-10, IG-110) and high flux reactor (HFR)(NRL) (IG-110, NBG-25). Comparisons were made based on the irradiation dose and irradiation temperature. Overall, the three grades showed similar irradiation-induced property change behaviors, which followed the historic data. More or less grade-sensitive behaviors were observed for the changes in volume and thermal conductivity, and, in contrast, grade-insensitive behaviors were observed for dynamic Young's modulus and coefficient of thermal expansion changes. The ETU-10 of the smallest grain size appeared to show a relatively smaller VC to IG-110 and NBG-25. Drastic decrease in the difference in thermal conductivity was observed for ETU-10 and IG-110 after irradiation. The similar irradiation-induced properties changing behaviors observed in this study especially in the DYM and CTE may be attributed to the assumed similar microstructures that evolved from the similar size coke particles and the same forming method.

온도변화에 따른 플라스틱의 손실계수와 Young 률의 측정 (Measuring of Loss factor and Young's modulus of Plastics with Temperature Variation)

  • 신수현;정성수;이용봉;이두희
    • 한국음향학회:학술대회논문집
    • /
    • 한국음향학회 2004년도 추계학술발표대회논문집 제23권 2호
    • /
    • pp.321-322
    • /
    • 2004
  • It is well known that the loss factor and Young's modulus are fundamental mechanical properties of materials. In this study. the dynamic characteristics of plastics are evaluated by using two different standard test methods which are ASTM E 756 and ISO 6721. Polycarbonate and acrylonitrile butadiene styrene were used as test specimens. In order to evaluate vibration of damping properties with temperature, we measured loss factor and Young's modulus of the specimens the temperature range between $-10^{\circ}C$ and $60^{\circ}C$. The Young's modulus for polycarbonate decreased significantly as increasing temperature, while the loss factor increased. However, the Young's modulus and loss factor of acrylonitrile butadiene styrene are varied somewhat with temperature.

  • PDF

사력댐 동적물성 추정을 위한 현장조사기법 적용 및 분석 (Application and Analysis of Field Test and Geophysical Exploration for Dynamic Material Properties of Rockfill Dam)

  • 이종욱;김기영;전제성;조성은
    • 한국지반공학회:학술대회논문집
    • /
    • 한국지반공학회 2005년도 지반공학 공동 학술발표회
    • /
    • pp.352-359
    • /
    • 2005
  • In this study, seismic refraction survey and MASW at dam crest and down-hole test and cross hole test in the boring holes located in dam crest through the core are performed to fin out dynamic material properties, are needed to evaluate dynamic safety of rockfill dam using dynamic analysis method. From the field test and geophysical exploration, applied such as above, p-wave and s-wave velocity profile of each layer of dam body. Dynamic material properties, such as elastic modulus, shear modulus, poissong's ration, are obtained from p-wave and s-wave velocity profile and density profile from formation density logging test.

  • PDF

다양한 시험법으로 규명된 암반 탄성계수 비교 (Comparison of Rock Young's Moduli Determined from Various Measurement Methods)

  • 유근환;장찬동
    • 지질공학
    • /
    • 제16권1호
    • /
    • pp.1-14
    • /
    • 2006
  • 국내의 대표적 암종이라 할 수 있는 화강암체와 편마암체에 대해 탄성계수 측정 방법으로 자주 이용되고 있는 Goodman jack시험, PS검층, 초음파 속도측정, 일축압축 변형 시험을 실시하여 각 탄성계수를 측정하고 그 특징을 알아보았다. 실내에서 측정 된 동.정탄성계수는 측정시 가해진 응력의 크기, 측정시 이용된 주파수의 범위, 가압/감압 등의 측정 조건에 따라 상당히 다른 결과를 보였다. 실내 측정조건이 현장조건에 가까워질수록 현장암반의 탄성 계수와 비슷한 값으로 측정되는데 이는 실내시험시 현장 상태를 구현하는 것이 중요하다는 점을 시사한다. 동탄성계수는 정탄성계수에 비해 대체로 높게 측정되었으며 그 원인으로는 (미세)균열의 응력에 따른 거동양상, 측정시 이용한 주파수의 범위 차이, 그리고 변형 진폭의 차이 등의 효과로 설명 할 수 있다. 다양한 방법으로 측정된 각 탄성 계수 상호간의 관계 및 특징은 현장 암반 탄성계수의 적절한 판단을 위해 도움이 될 것으로 기대된다.

다자유도 곡선 맞춤법과 RKU 기법을 이용한 점탄성 감쇠재의 탄성 및 손실계수 추정방법 연구 (Study of the Measurement of Young's Modulus and Loss Factor for a Viscoelastic Damping Material Using a Multi Degree of Freedom Curve Fitting Method and RKU Equation)

  • 민천홍;박한일;배수룡;전재진
    • 한국해양공학회지
    • /
    • 제25권1호
    • /
    • pp.67-72
    • /
    • 2011
  • Offshore structures, such as a platform, a buoy, or a floating vessel, are exposed to several dynamic loads, and viscoelastic damping material is used to reduce the vibration of offshore structures. It is important to know the properties of viscoelastic materials because loss factor and Young's modulus of the viscoelastic damping material are dependent on frequency and temperature. In this study, an advanced technique for obtaining accurate loss factor and Young's modulus of the viscoelastic damping material is introduced based on a multi degree of freedom curve-fitting method and the RKU (Ross-Kerwin-Ungar) equations. The technique is based on a modified experimental procedure from ASTM E 756-04. Loss factor and Young's modulus of the viscoelastic damping material are measured for different temperatures by performing the test in a temperature-controlled vibration measurement room where temperature varies from 5 to 45 degrees Celsius.