• 제목/요약/키워드: duplex stainless

검색결과 206건 처리시간 0.026초

수퍼 2상 스테인리스강의 피로균열진전 특성에 미치는 미세조직의 영향 (Effect of Microstructure on the Characteristics of Fatigue Crack Propagation of Super Duplex Stainless Steel)

  • 도재윤
    • 한국해양공학회지
    • /
    • 제14권2호
    • /
    • pp.65-69
    • /
    • 2000
  • This study is to investigate the characteristics of fatigue crack propagation in rolled super duplex stainless steel that was changed austenite-ferrite volume fraction by heat treatment. It was used two kinds of specimen the rolling and the transverse directions δ-phase fraction affected sound velocity hardness and Young's modulus. Characteristics of fatigue crack propagation was affected by anisotropy and (δ+γ) phase volume fractions.

  • PDF

슈퍼 듀플렉스 스테인리스강의 응고·냉각 시 상석출에 미치는 냉각속도의 영향 (Influence of the Cooling Rate on the Phase Precipitation of Super Duplex Stainless Steel)

  • 장은석;김기영;김석준
    • 한국주조공학회지
    • /
    • 제35권2호
    • /
    • pp.23-28
    • /
    • 2015
  • This work presents the effect of the cooling rate on the precipitation of super duplex stainless steel. Specimens of super duplex stainless steel with a specific composition were cooled at various cooling rates after being melted at $1550^{\circ}C$ in a directional solidification furnace. Ferrite (${\delta}$), Austenite (${\gamma}$), Sigma (${\sigma}$), and Chi (${\chi}$) phases were precipitated when the cooling rate was lower than 0.22 K/s. When the cooling rate was 0.22 K/s or faster, ${\sigma}$ and ${\chi}$ phases were not precipitated.

Fe-Cr-Ni-Mn 2 상 스테인레스강의 인장성질에 미치는 변형온도 및 Mn 함량변화의 영향 (Effect of Deformation Temperature and Manganese Contents on the Tensile Properties of Fe-Cr-Ni-Mn Duplex Stainless Steel)

  • 강창룡;성장현
    • 열처리공학회지
    • /
    • 제4권4호
    • /
    • pp.44-52
    • /
    • 1991
  • The effect of deformation temperature and manganes contents on the tensile properties of duplex stainless steels with the structure of both ferrite and austenite were investigate. For this investigation, Fe-19% Cr-5% Ni-4~8% Mn alloys were prepared. The result obtained from this experiment are summerized as follows. With decreasing deformation temperature, tensile strengths of duplex stainless steel increased. Elongation showd to be increased and then decreased after representing the highest value at specific temperature. Tensile properties of duplex stainless steel were controlled by TRIP behavior in this experimental range of austenite contents. Tensile strengths decreased with increasing Mn contents. With increasing Mn contents, elongation decreased in the high temperature region, but increased in the low temperature region. The peak temperature representing the maximum elongation were changed to low temperature and the width of peak appeared to be broaden with increasing Mn contents.

  • PDF

Analysis of Phase Separation by Thermal Aging in Duplex Stainless Steels by Magnetic Methods

  • Kim, Sunki;Wonmok Jae;Kim, Yongsoo
    • Nuclear Engineering and Technology
    • /
    • 제29권5호
    • /
    • pp.361-367
    • /
    • 1997
  • The phase separation in ferrite phase of duplex stainless steel is the primary cause of thermal aging embrittlement of the LWR primary pressure boundary components. In this study the phase separation of simulated duplex stainless steel was detected by Mossbauer spectroscopy and magnetic property analysis by VSM(Vibrating Specimen Magnetometer). The simulated duplex stainless steels, Fe-Cr binary, Fe-Cr-Ni ternary, and Fe-Cr-Ni-Si quarternary allots, were aged at 370 and 40$0^{\circ}C$ up to 5,340 hours. It was observed from Mossbauer spectra analysis that internal magnetic field increases with aging time and from VSM that the specific saturation magnetization and Curie temperature increase with aging time. These result are indicative that phase separation into Fe-rich region and Cr-rich region is caused by thermal aging in the temperature range of 370~40$0^{\circ}C$ In cases of specimens containing Ni, the increase of specific saturation magnetization is much higher. This implies that Ni seems to promote Fe-Cr interdiffusion, which accelerates the phase separation into Fe-rich $\alpha$ phase and Cr-rich $\alpha$' phase.

  • PDF

Effects of Tungsten on the Precipitation Kinetics of Secondary Phases and the Associated Susceptibility to Pitting Corrosion in Duplex Stainless Steels

  • Park, Chan-Jin;Kwon, Hyuk-Sang
    • Corrosion Science and Technology
    • /
    • 제5권6호
    • /
    • pp.189-195
    • /
    • 2006
  • Effects of tungsten (W) on the precipitation kinetics of secondary phases and the associated resistance to pitting corrosion of 25%Cr duplex stainless steels were investigated through microstructural and electrochemical noise analyses. With the partial substitution of W for Mo in duplex stainless steel, the potential and current noises of the alloy were significantly decreased in chloride solution due to retardation of the ${\sigma}$ phase precipitation. The preferential precipitation of the $\chi$ phase in the W-containing alloy during the early period of aging contributed to retarding the precipitation of the $\sigma$ phase by depleting W and Mo along grain boundaries. In addition, the retardation of the nucleation and growth of the $\sigma$ phase in the W-containing alloy appears to be attributed to the inherently low diffusivity of W compared with that of Mo.

슈퍼 듀플렉스 용접부에 미치는 보호가스의 영향 (The effect of shielding gases on the characteristics of super duplex weld metal)

  • 홍인표;이철환;김유기;김대순
    • 대한용접접합학회:학술대회논문집
    • /
    • 대한용접접합학회 2005년도 춘계학술발표대회 개요집
    • /
    • pp.209-211
    • /
    • 2005
  • Super duplex stainless steels have been used for offshore oil and gas piping systems which are subject to corrosion atmosphere, because they have excellent resistance to Stress Corrosion Cracking (SCC) and Pitting corrosion and high strength/weight ratio. Normally, the welding for duplex stainless steels has been peformed using GTAW with Ar shielding gas. However, in case of using Ar as shielding gas, the corrosion resistance at root weld metal will be deteriorated due to loss of nitrogen from weld deposit during welding. It is wellknown that the corrosion resistance of super duplex stainless can be restored by addition of nitrogen as shielding gas. In this study, we made super duplex welding with using several kinds of shielding and purging gases and investigated the relationship between shielding gas and corrosion resistance. Consequently, it was shown that corrosion resistance of weld deposit can be restored by addition of $N_{2}$ as shielding gas.

  • PDF

Effect of Aging Time on the Resistance to Localized Corrosion of the Hyper Duplex Stainless Steel

  • Jeon, Soon-Hyeok;Kim, Soon-Tae;Lee, In-Sung;Kim, Ji-Soo;Kim, Kwang-Tae;Park, Yong-Soo
    • Corrosion Science and Technology
    • /
    • 제9권5호
    • /
    • pp.209-215
    • /
    • 2010
  • To elucidate the effect of aging time on resistance to localized corrosion of hyper duplex stainless steel, a double-loop electrochemical potentiokinetic reactivation test a potentiodynamic anodic polarization test, a scanning electron microscope-energy dispersive spectroscope analysis, and a thermodynamic calculation were conducted. With an increase in aging time, sigma phases are precipitated much more than chi phases due to the meta-stable chi phase acting as a transition phase. As aging time at $850^{\circ}C$ increases, the corrosion resistance decreases owing to an increase in Cr, Mo and W depleted areas adjacent to the intermetallic phases such as sigma phases and chi phases.

슈퍼 듀플렉스 내식강의 부식특성 및 경도에 미치는 텅스텐 첨가의 영향 (Influence of W Additions on the Corrosion Characteristics and Hardness of Super Duplex Stainless Steel)

  • 한윤기;김정민
    • 열처리공학회지
    • /
    • 제36권5호
    • /
    • pp.261-269
    • /
    • 2023
  • This study aims to investigate the effects of tungsten additions on the microstructure, corrosion characteristics, and hardness of super duplex stainless steel heat-treated at two different annealing temperatures. Under the annealing temperature of 1100℃, the microstructure of the stainless steels consisted mainly of ferrite, while under the annealing temperature of 1000℃, significant amounts of austenite and secondary phases were also observed. In terms of corrosion characteristics in 3.5 wt%NaCl solution, there was not a significant difference due to W addition at the 1100℃ conditions. However, at the 1000℃, a tendency of decreased corrosion resistance was observed with increasing the tungsten content. On the other hand, the micro-hardness of the stainless steel heat-treated 1000℃ showed an increasing trend with tungsten addition. This increase can be mainly attributed to the higher fraction of secondary phases, primarily sigma, known for their high hardness.

Materials Integrity Analysis for Application of Hyper Duplex Stainless Steels to Korean Nuclear Power Plants

  • Chang, Hyun-Young;Park, Heung-Bae;Park, Yong-Soo;Kim, Soon-Tae;Kim, Young-Sik;Kim, Kwang-Tae;Jhang, Yoon-Young
    • Corrosion Science and Technology
    • /
    • 제9권5호
    • /
    • pp.187-195
    • /
    • 2010
  • Hyper duplex stainless steels have been developed in Korea for the purpose of application to the seawater system of Korean nuclear power plants. This system supplies seawater to cooling water heat exchanger tubes, related pipes and chlorine injection system. In normal operation, seawater is supplied to heat exchanger through the exit of circulating water pump headers, and the heat exchanged sea water is extracted to the discharge pipes in circulating water system connected to the circulating water discharge lines. The high flow velocity of some part of seawater system in nuclear power plants accelerates damages of components. Therefore, high strength and high corrosion resistant steels need to be applied for this environment. Hyper duplex stainless steel (27Cr-7.0Ni-2.5Mo-3.2W-0.35N) has been newly developed in Korea and is being improved for applying to nuclear power plants. In this study, the physical & mechanical properties and corrosion resistance of newly developed materials are quantitatively evaluated in comparative to commercial stainless steels in other countries. The properties of weld & HAZ (heat affected zone) are analyzed and the best compositions are suggested. The optimum conditions in welding process are derived for ensuring the volume fraction of ferrite(${\alpha}$) and austenite(${\gamma}$) in HAZ and controlling weld cracks. For applying these materials to the seawater heat exchanger, CCT and CPT in weldments are measured. As a result of all experiments, it was found that the newly developed hyper duplex stainless steel WREMBA has higher corrosion resistance and mechanical properties than those of super austenitic stainless steels including welded area. It is expected to be a promising material for seawater systems of Korean nuclear power plants.

FABRICATION OF GD CONTAINING DUPLEX STAINLESS STEEL SHEET FOR NEUTRON ABSORBING STRUCTURAL MATERIALS

  • Choi, Yong;Moon, Byung M.;Sohn, Dong-Seong
    • Nuclear Engineering and Technology
    • /
    • 제45권5호
    • /
    • pp.689-694
    • /
    • 2013
  • A duplex stainless steel sheet with 1 wt.% gadolinium was fabricated for a neutron absorbing material with high strength, excellent corrosion resistance, and low cost as well as high neutron absorption capability. The microstructure of the as-cast specimen has typical duplex phases including 31% ferrite and 69% austenite. Main alloy elements like chromium (Cr), nickel (Ni), and gadolinium (Gd) are relatively uniformly distributed in the matrix. Gadolinium rich precipitates were present in the grains and at the grain boundaries. The solution treatment at $1070^{\circ}$ for 50 minutes followed by the hot-rolling above $950^{\circ}$ after keeping the sheet at $1200^{\circ}$ for 1.5 hours are important points of the optimum condition to produce a 6 mm-thick plate without cracking.