Commonly, the flocculant is dissolved in process or recycle water in industrial plant which has many ionic materials. Therefore, the polymer degradation in aqueous solution by chemical, mechanical or bacteriological may occur, sometimes rapidly. Even if the same flocculant is dissolved, the flocculation characteristics and the properties of dissolving polymer varied with the kind of dissolving water. In this study, we try to estimate the interaction between flocculants and ionic materials in dissolving water using self inversing emulsion polymer; polyacrylamide-co-trimethyl ammonium ethyl acrylate chloride flocculants which have varying molecular weights and structures at a several conditions. The polymeric flocculant is dissolved in artificial dissolving water with Potassium Chloride (PC), Calcium Chloride anhydrous (CC), Potassium Hydroxide (PH), Sodium Chloride (SC), Sodium Bromate (SB) and Iron (II) Sulfate Heptahydrate (IS) as ionic sources. Experimental results indicate that the cationic and anionic ions in dissolving water induce the hydrolysis, degradation of cationic functional group and uncoiling of polymeric flocculants, therefore, the flocculation efficiency decreased by undesired polymer. According that result, it is important to estimate not only its structures and physical properties but also the qualities of dissolving water to optimize the efficiency.
This research was studied dissolving pulp for rayon production, which is not KP, SP methods but steam explosion and oxygen alkali treatment. The variation of characterization in wood cellulose after steam explosion and oxygen alkali treatment this follows. In the oxygen alkali treatment of exploded pine wood, yield of dissolving pulp was lower than steam-exploded oak wood, and we have obtained dissolving pulp that high purity cellulose, but degree of polymerization was inclined to decrease less than 200. In the case of steam-exploded oak wood, degree of polymerization was higher than steam-exploded pine wood but purity of cellulose was lower than its.
Journal of Korea Technical Association of The Pulp and Paper Industry
/
v.36
no.4
s.107
/
pp.41-48
/
2004
To make a basepaper for multipurposed seed paper, old news print (ONP) and mixed office waste paper (MOW), modified and unmodified with a commercial cellulase, were investigated. Each handsheet was applied with different chemicals such as insecticides, germicides and herbicides. The interactions behaviors of chemicals used with base papers were evaluated by means of the contents of chemicals impregnation and dissolving behaviors in water and soil. The ONP and MOW treated with the cellulase had higher impregnation and dissolving capacities in both water and soil than untreated ONP and MOW. However, the modified ONP showed lower impregnation and dissolving capacities compared to the modified MOW. The content of impregnation of chemicals would be affected with the degree of microfibrils produced by the modification treatment. Otherwise, dissolving capacities of chemicals depend on the affinity of the residual lignin in the paper.
This research was studied for dissolving pulp preparation as the raw material of viscose rayon from woody biomass by solvolysis pretreatment. In the change of pulp characteristic after solvolysis pretreatment, the following results were obtained. In the case of solvolysis pretreatment, we have obtained pulp that high purity cellulose, and degree of polymerization was inclined to decrease less than 440 on the phosphoric acid as catalyst. Comparing phosphoric acid and formic acid as catalyst in the solvolysis pretreatment, using on formic acid catalyst is superior to phosphoric acid catalyst for making dissolving pulp.
Journal of Korea Technical Association of The Pulp and Paper Industry
/
v.29
no.3
/
pp.51-59
/
1997
Dissolving pulp is a low yield(30∼35%) bleached chemical pulp that has a high cellulose content (95% or higher) suitable for use in cellulose derivatives such as rayon, cellulose acetate. This research was studied for dissolving pulp preparation as the raw material of viscose rayon from commertial pulps. (TMP, CP, DIP) In the change of pulp(cellulose) characteristics after sodium hypochlorite and solvolysis treatment. the following results were obtained In the case of sodium hypochlorite pretreatment, we have obtained pulp that high purity cellulose, but degree of polymerization was inclined to decrease less than 170∼240. Comparing sodium hypochlorite pretreatment and solvolysis pretreatment, solvolysis pretreatment is superior to sodium hypochlorite process for making dissolving pulp. We think that the low degree of polymerization of cellulose because of increasing degradation of cellulose during delignification treatment.
The feasibility of lecithin as a material for dissolving microneedles to improve skin permeability of drugs and the effect of the composition of lecithin on the mechanical strength, solubility, and skin permeability of rhodamine B (RhB) of the dissolving microneedles were investigated. Dissolving microneedles with needles of uniform shape and size were fabricated with the mold made using the laser-writing technique, simpler and more efficient method compared to the photolithography method, the conventional method to fabricate the microneedle mold. The composition of lecithin in the microneedle affected the mechanical strength and solubility of the needle thus, the mechanical strength of the needle increased as the composition of lecithin in the needle increased, resulting in improving the skin permeability of RhB contained in the microneedles. When comparing the microneedles containing same composition of amylopectin (AP), the skin permeability of RhB of the microneedles containing lecithin was higher. These results indicate that lecithin can be used as a material for dissolving microneedles and the skin permeability of the microneedle could be controlled by changing the composition of lecithin.
Two types of polymeric micro-needles with 250 and $750{\mu}m$ lengths were prepared by a micromolding process. The geometry of dissolving micro-needles with minoxidil was investigated and the mechanical property of polymer micro-needles was also evaluated. Water dissolving micro-needles containing minoxidil were successfully inserted into skin and delivered minoxidil to the skin layer after 30 min of insertion. The observed hair growth was less when the minoxidil treatment was not applied or used without the micro-needles than that the minoxidil was applied by micro-needles. Histologically, these hair follicles became bigger, and the hair papillae were totally encircled by the hair bulbs. In this feasibility test, we show the successful delivery of minoxidil, and effective treatment of hair loss can be possible by using dissolving micro-needles with minoxidil.
The purpose of this study is to investigate the preparation of the carboxymethylcellulose from recycled fiber, especially on the reactivity of carboxymethylation. Using a deinked pulp and a dissolving pulp. Green's method is adapted to the carboxymethylation. We conformed that the carboxymethyl group is led for recycled fiber by FT-IR analysis. The recycled fiber is more reactive than the dissolving pulp because the recycled fiber had been defiberated and pretreated with alkali. It suggests that deinking process is in accordance with pretreatment of CMC process. Therefore, it may be possible to prepare CMC from the recylced fiber economically.
A fast dissolving tablet was developed using the freeze-drying technique. Hyeonggaeyeongyotang was selected as a model oriental medicine. Formulation and processing parameters were studied to obtain freeze-dried tablet with high drug loading, good palatability, and fast disintegration time. $Kollidon^{(R)}$ CLM served as both matrix former and taste masking agent. Ethanol used as co-solvent, decreased the disintegration time of tablet. Aspartame was employed to impart better taste. Drying condition was found to have a major effect in the morphology of the tablets. Freeze-drying process was optimized to decrease the processing time and improve the appearance of the tablets.
The Transactions of the Korean Institute of Electrical Engineers
/
v.41
no.2
/
pp.178-184
/
1992
This study treats the improvement of the dielectric strength of polymer by eliminating the air in it and dissolving electronegative gases. As experimental material, unsaturated polyester resin was used and the specimen was made by dissolving NS12T. SFS16T abd CCIS12TFS12T gases which have strong electron affinity. And also the electrical properties (tree growth and breakdown characteristics) of them were tested and discussed. The results are as follows. When the specimen dissolved with electronegative gas compared with one with air` 1) The tree breakdown voltage of the former is higher than that of the latter. 2) The tree growth of the former is slower than that of the latter. 3) The temperature dependence of the former is smaller than that of the latter. 4) The breakdown voltage of the specimen dissolved with electronegative gas is much higher than that dissolved with air.
이메일무단수집거부
본 웹사이트에 게시된 이메일 주소가 전자우편 수집 프로그램이나
그 밖의 기술적 장치를 이용하여 무단으로 수집되는 것을 거부하며,
이를 위반시 정보통신망법에 의해 형사 처벌됨을 유념하시기 바랍니다.
[게시일 2004년 10월 1일]
이용약관
제 1 장 총칙
제 1 조 (목적)
이 이용약관은 KoreaScience 홈페이지(이하 “당 사이트”)에서 제공하는 인터넷 서비스(이하 '서비스')의 가입조건 및 이용에 관한 제반 사항과 기타 필요한 사항을 구체적으로 규정함을 목적으로 합니다.
제 2 조 (용어의 정의)
① "이용자"라 함은 당 사이트에 접속하여 이 약관에 따라 당 사이트가 제공하는 서비스를 받는 회원 및 비회원을
말합니다.
② "회원"이라 함은 서비스를 이용하기 위하여 당 사이트에 개인정보를 제공하여 아이디(ID)와 비밀번호를 부여
받은 자를 말합니다.
③ "회원 아이디(ID)"라 함은 회원의 식별 및 서비스 이용을 위하여 자신이 선정한 문자 및 숫자의 조합을
말합니다.
④ "비밀번호(패스워드)"라 함은 회원이 자신의 비밀보호를 위하여 선정한 문자 및 숫자의 조합을 말합니다.
제 3 조 (이용약관의 효력 및 변경)
① 이 약관은 당 사이트에 게시하거나 기타의 방법으로 회원에게 공지함으로써 효력이 발생합니다.
② 당 사이트는 이 약관을 개정할 경우에 적용일자 및 개정사유를 명시하여 현행 약관과 함께 당 사이트의
초기화면에 그 적용일자 7일 이전부터 적용일자 전일까지 공지합니다. 다만, 회원에게 불리하게 약관내용을
변경하는 경우에는 최소한 30일 이상의 사전 유예기간을 두고 공지합니다. 이 경우 당 사이트는 개정 전
내용과 개정 후 내용을 명확하게 비교하여 이용자가 알기 쉽도록 표시합니다.
제 4 조(약관 외 준칙)
① 이 약관은 당 사이트가 제공하는 서비스에 관한 이용안내와 함께 적용됩니다.
② 이 약관에 명시되지 아니한 사항은 관계법령의 규정이 적용됩니다.
제 2 장 이용계약의 체결
제 5 조 (이용계약의 성립 등)
① 이용계약은 이용고객이 당 사이트가 정한 약관에 「동의합니다」를 선택하고, 당 사이트가 정한
온라인신청양식을 작성하여 서비스 이용을 신청한 후, 당 사이트가 이를 승낙함으로써 성립합니다.
② 제1항의 승낙은 당 사이트가 제공하는 과학기술정보검색, 맞춤정보, 서지정보 등 다른 서비스의 이용승낙을
포함합니다.
제 6 조 (회원가입)
서비스를 이용하고자 하는 고객은 당 사이트에서 정한 회원가입양식에 개인정보를 기재하여 가입을 하여야 합니다.
제 7 조 (개인정보의 보호 및 사용)
당 사이트는 관계법령이 정하는 바에 따라 회원 등록정보를 포함한 회원의 개인정보를 보호하기 위해 노력합니다. 회원 개인정보의 보호 및 사용에 대해서는 관련법령 및 당 사이트의 개인정보 보호정책이 적용됩니다.
제 8 조 (이용 신청의 승낙과 제한)
① 당 사이트는 제6조의 규정에 의한 이용신청고객에 대하여 서비스 이용을 승낙합니다.
② 당 사이트는 아래사항에 해당하는 경우에 대해서 승낙하지 아니 합니다.
- 이용계약 신청서의 내용을 허위로 기재한 경우
- 기타 규정한 제반사항을 위반하며 신청하는 경우
제 9 조 (회원 ID 부여 및 변경 등)
① 당 사이트는 이용고객에 대하여 약관에 정하는 바에 따라 자신이 선정한 회원 ID를 부여합니다.
② 회원 ID는 원칙적으로 변경이 불가하며 부득이한 사유로 인하여 변경 하고자 하는 경우에는 해당 ID를
해지하고 재가입해야 합니다.
③ 기타 회원 개인정보 관리 및 변경 등에 관한 사항은 서비스별 안내에 정하는 바에 의합니다.
제 3 장 계약 당사자의 의무
제 10 조 (KISTI의 의무)
① 당 사이트는 이용고객이 희망한 서비스 제공 개시일에 특별한 사정이 없는 한 서비스를 이용할 수 있도록
하여야 합니다.
② 당 사이트는 개인정보 보호를 위해 보안시스템을 구축하며 개인정보 보호정책을 공시하고 준수합니다.
③ 당 사이트는 회원으로부터 제기되는 의견이나 불만이 정당하다고 객관적으로 인정될 경우에는 적절한 절차를
거쳐 즉시 처리하여야 합니다. 다만, 즉시 처리가 곤란한 경우는 회원에게 그 사유와 처리일정을 통보하여야
합니다.
제 11 조 (회원의 의무)
① 이용자는 회원가입 신청 또는 회원정보 변경 시 실명으로 모든 사항을 사실에 근거하여 작성하여야 하며,
허위 또는 타인의 정보를 등록할 경우 일체의 권리를 주장할 수 없습니다.
② 당 사이트가 관계법령 및 개인정보 보호정책에 의거하여 그 책임을 지는 경우를 제외하고 회원에게 부여된
ID의 비밀번호 관리소홀, 부정사용에 의하여 발생하는 모든 결과에 대한 책임은 회원에게 있습니다.
③ 회원은 당 사이트 및 제 3자의 지적 재산권을 침해해서는 안 됩니다.
제 4 장 서비스의 이용
제 12 조 (서비스 이용 시간)
① 서비스 이용은 당 사이트의 업무상 또는 기술상 특별한 지장이 없는 한 연중무휴, 1일 24시간 운영을
원칙으로 합니다. 단, 당 사이트는 시스템 정기점검, 증설 및 교체를 위해 당 사이트가 정한 날이나 시간에
서비스를 일시 중단할 수 있으며, 예정되어 있는 작업으로 인한 서비스 일시중단은 당 사이트 홈페이지를
통해 사전에 공지합니다.
② 당 사이트는 서비스를 특정범위로 분할하여 각 범위별로 이용가능시간을 별도로 지정할 수 있습니다. 다만
이 경우 그 내용을 공지합니다.
제 13 조 (홈페이지 저작권)
① NDSL에서 제공하는 모든 저작물의 저작권은 원저작자에게 있으며, KISTI는 복제/배포/전송권을 확보하고
있습니다.
② NDSL에서 제공하는 콘텐츠를 상업적 및 기타 영리목적으로 복제/배포/전송할 경우 사전에 KISTI의 허락을
받아야 합니다.
③ NDSL에서 제공하는 콘텐츠를 보도, 비평, 교육, 연구 등을 위하여 정당한 범위 안에서 공정한 관행에
합치되게 인용할 수 있습니다.
④ NDSL에서 제공하는 콘텐츠를 무단 복제, 전송, 배포 기타 저작권법에 위반되는 방법으로 이용할 경우
저작권법 제136조에 따라 5년 이하의 징역 또는 5천만 원 이하의 벌금에 처해질 수 있습니다.
제 14 조 (유료서비스)
① 당 사이트 및 협력기관이 정한 유료서비스(원문복사 등)는 별도로 정해진 바에 따르며, 변경사항은 시행 전에
당 사이트 홈페이지를 통하여 회원에게 공지합니다.
② 유료서비스를 이용하려는 회원은 정해진 요금체계에 따라 요금을 납부해야 합니다.
제 5 장 계약 해지 및 이용 제한
제 15 조 (계약 해지)
회원이 이용계약을 해지하고자 하는 때에는 [가입해지] 메뉴를 이용해 직접 해지해야 합니다.
제 16 조 (서비스 이용제한)
① 당 사이트는 회원이 서비스 이용내용에 있어서 본 약관 제 11조 내용을 위반하거나, 다음 각 호에 해당하는
경우 서비스 이용을 제한할 수 있습니다.
- 2년 이상 서비스를 이용한 적이 없는 경우
- 기타 정상적인 서비스 운영에 방해가 될 경우
② 상기 이용제한 규정에 따라 서비스를 이용하는 회원에게 서비스 이용에 대하여 별도 공지 없이 서비스 이용의
일시정지, 이용계약 해지 할 수 있습니다.
제 17 조 (전자우편주소 수집 금지)
회원은 전자우편주소 추출기 등을 이용하여 전자우편주소를 수집 또는 제3자에게 제공할 수 없습니다.
제 6 장 손해배상 및 기타사항
제 18 조 (손해배상)
당 사이트는 무료로 제공되는 서비스와 관련하여 회원에게 어떠한 손해가 발생하더라도 당 사이트가 고의 또는 과실로 인한 손해발생을 제외하고는 이에 대하여 책임을 부담하지 아니합니다.
제 19 조 (관할 법원)
서비스 이용으로 발생한 분쟁에 대해 소송이 제기되는 경우 민사 소송법상의 관할 법원에 제기합니다.
[부 칙]
1. (시행일) 이 약관은 2016년 9월 5일부터 적용되며, 종전 약관은 본 약관으로 대체되며, 개정된 약관의 적용일 이전 가입자도 개정된 약관의 적용을 받습니다.