로우스틸 마찰재의 마찰 및 마모특성에 미치는 구리계 재료의 영향 (Effects of Copper and Copper-Alloy on Friction and Wear Characteristics of Low-Steel Friction Material)

  • 정광기;이상우;권성욱;최성우;이희옥
    • Tribology and Lubricants
    • /
    • 제36권4호
    • /
    • pp.207-214
    • /
    • 2020
  • In this study, we investigated the effects of copper and copper-alloy on the frictional and wear properties of low-steel friction material. The proportions of copper and copper-alloy in the brake friction materials used in passenger cars are very high (approximately 5-20% weight), and these materials have significant effects on friction and wear characteristics. In this study, the effects of cupric ingredients, such as the copper fiber and brass fiber, are investigated using the friction materials based on commercial formulations. After the copper and brass fibers from the same formulation were removed, the frictional and wear characteristics were evaluated to determine the influence of the copper and copper-alloy. We evaluated the frictional and wear characteristics by simulating various braking conditions using a 1/5 scale dynamometer. The results show that the friction material containing copper and brass fibers have excellent frictional stability and a low wear rate compared to the friction material that does not contain copper and brass fibers. These results are attributed to the excellent ductility, moderate melting point, high strength, and excellent thermal conductivity of copper and copper-alloy. We analyzed the surfaces of the friction materials before and after the performing the friction tests using a scanning electron microscope-energy dispersive X-ray spectroscope, confocal microscope, and roughness tester to verify the frictional behavior of copper and copper-alloy. In future studies, it will be applied to the development of copper-free friction materials based on the results of this study.

스크래치 시험을 통한 DLC 박막 파손과 밀착 특성 평가 (Evaluation of Failure Modes and Adhesion of DLC Films by Scratch Test)

  • 김주희;박찬형;안효석
    • Tribology and Lubricants
    • /
    • 제33권4호
    • /
    • pp.127-133
    • /
    • 2017
  • In order to characterize the adhesive properties and failure mechanisms of diamond-like carbon (DLC) films of two different thicknesses (130 nm and $1.2{\mu}m$), deposited by plasma-enhanced chemical vapor deposition on a Si substrate, scratch testing with a micro-indenter ($12.5{\mu}m$ tip radius) was performed under a linearly increasing load. These scratch tests were conducted under the same test conditions for both films. The critical load of each film was estimated from the scratch test results, based on a sharp increase in the coefficient of friction and a clear distinction of failure modes. The critical load was the basis for evaluating the adhesion strength of the films, and the $1.2{\mu}m-thick$ DLC film had superior adhesion strength. For better understanding of the failure modes, the following analyses were conducted: friction behavior and scratch tracks analysis using scanning electron microscopy, energy-dispersive spectroscopy, and 3-D profilometry. The scratch test results showed that failure modes were related to the thickness of the films. The 130 nm-thick DLC film underwent cohesive failure modes (cracks and chipping) before reaching to a gross failure stage. On the other hand, the thicker DLC film ($1.2{\mu}m-thick$) did not exhibit micro cracks before a sudden gross failure of the film together with the evidence of cracking and chipping of the Si substrate.

Oxide Nanolayers Grown on New Ternary Ti Based Alloy Surface by Galvanic Anodizing-Characteristics and Anticorrosive Properties

  • Calderon Moreno, J.M.;Drob, P.;Vasilescu, C.;Drob, S.I.;Popa, M.;Vasilescu, E.
    • Corrosion Science and Technology
    • /
    • 제16권5호
    • /
    • pp.257-264
    • /
    • 2017
  • Film of new Ti-15Zr-5Nb alloy formed during galvanic anodizing in orthophosphoric acid solution was characterized by optical microscope, scanning electron microscope (SEM), energy dispersive spectroscopy (EDS), and Raman micro-spectroscopy. Its anticorrosive properties were determined by electrochemical techniques. The film had a layer with nanotube-like porosity with diameters in 500-1000 nm range. The nano layer contained significant amounts of P and O as well as alloying element. Additionally, Raman micro-spectroscopy identified oxygen as oxygen ion in $TiO_2$ anatase and phosphorous as $P_2O_7{^{4-}}$ ion in phosphotitanate compound. All potentiodynamic polarization curves in artificial Carter-Brugirard saliva with pH values (pH= 3.96, 7.84, and 9.11) depending on the addition of 0.05M NaF revealed nobler behavior of anodized alloy and higher polarization resistance indicating the film is thicker and more compact nanolayer. Lower corrosion rates of the anodized alloy reduced toxicity due to less released ions into saliva. Bigger curvature radii in Nyquist plot and higher phase angle in Bode plot for the anodized alloy ascertain a thicker, more protective, insulating nanolayer existing on the anodized alloy. Additionally, ESI results indicate anodized film consists of an inner, compact, barrier, layer and an outer, less protective, porous layer.

함침 오일 점도에 따른 나노동공 구조의 산화알루미늄 박막의 마찰 및 마멸 거동 (Tribological Influence of Kinematic Oil Viscosity Impregnated in Nanopores of Anodic Aluminum Oxide Film)

  • 김대현;안효석
    • 대한기계학회논문집A
    • /
    • 제37권5호
    • /
    • pp.625-630
    • /
    • 2013
  • 본 연구는 직경 45 nm인 원통형 나노동공을 가진 산화알루미늄(AAO) 박막에 오일을 함침시켰을때 동점도가 마찰 마멸에 미치는 영향을 규명하고자 실시하였다. 양극산화법으로 제조한 AAO 박막을 직경 1 mm의 440C 스테인리스 강구를 상대재로 하여 왕복동 미끄럼 접촉시험을 실시하였다. 마찰면과 마멸입자는 주사전자현미경과 에닥스(Energy-dispersive X-ray)를 이용해 분석하였다. 높은 동점도 오일의 윤활효과가 저점도 오일에 비해 크게 향상되었다. 동점도가 낮은 경우엔 모든 하중조건에서 심한 마찰흔적과 함께 두꺼운 소성변형층이 넓게 형성되었으며 경계윤활막의 손상으로 접촉면에 물질전이와 화학적 반응 현상이 모두 발생하였다. 오일의 점도가 높은 경우 마찰면에 존재하는 경계윤활막이 파괴되지 않아 마찰흔적과 소성변형층의 형성이 매우 적었으며 물질전이와 화학적 반응이 방지되었다.

수평횡파 송수신용 EMAT를 이용한 스틸 박판의 두께 감육 평가 (Evaluation of Thickness Reduction in Steel Plate by Using SH-EMATs)

  • 이진혁;박익근;김용권;김대현
    • 비파괴검사학회지
    • /
    • 제31권1호
    • /
    • pp.47-52
    • /
    • 2011
  • 전자기 초음파 탐촉자(electromagnetic acoustic transducer; EMAT)는 접촉 매질 없이 초음파의 송 수신이 가능하며 자석과 코일의 형상과 배열을 조절하여 SH파나 Lamb파 같은 유도 초음파 모드를 용이하게 발생시킬 수 있다. 또한 이러한 유도 초음파는 박판에서 판 두께 전체를 장거리로 전파하며 두께에 따른 분산특성이 있이 배관 등의 구조물을 탐상하는데 효과적인 비파괴검사 기법으로 연구되고 있다. 본 연구에서는 수평횡파(shear horizontal wave; SH)의 전파 거동을 해석하고 EMAT을 이용하여 SH파를 발생하여 스틸 박판의 두께 감육을 평가하였다. 그 결과 SH파의 분산특성은 두께 감육량의 증가에 따라 군속도가 감소하는 것을 확인할 수 있었으며, 이러한 군속도 변화를 통해 두께 감육량을 정량적으로 평가하는 것이 가능함을 확인하였다.

전기화학적 분석을 통해 산출된 코팅 결함율이 트라이볼로지적 특성에 미치는 영향 평가 (Influence of Coating Defect Ratio on Tribological Behavior Determined by Electrochemical Techniques)

  • 이영제;김우중;안승호;김호건;김정구;조정우
    • Tribology and Lubricants
    • /
    • 제20권6호
    • /
    • pp.306-313
    • /
    • 2004
  • Many of the current development in surface modification engineering are focused on multilayered coatings, which have the potential to improve the tribological properties. Four different multilayered coatings were deposited on AISI D2 steel in this study. The prepared samples are designed as $WC-Ti_{0.6}Al_{0.4}N,\;WC-Ti_{0.53}Al_{0.47}N,\;WC-Ti_{0.5}Al_{0.5}N\;and\;WC-Ti_{0.43}Al_{0.57}N$. The multilayered coatings were investigated with respect to coating surface and cross-sectional morphology, roughness, adhesion, hardness, porosity and tribological behaviors. Especially, wear tests of four multilayered coatings were performed by using a ball-on-disc configuration with a linear sliding speed of 0.017 m/sec and a normal load of 5.38 N load. The tests were carried out at room temperature in air by employing AISI 52100 steel ball $(H_R\;=\;66) $ having a diameter of 10 mm. The surface morphology, and topography of the wear scars of samples and balls have been determined by using scanning electron spectroscopy (SEM). Also, wear mechanism was determined by using SEM coupled with energy-dispersive spectroscopy (EDS). Results have showed an improved wear resistance of the $WC-Ti_{1-x}Al_xN$coatings with increasing of Al (aluminum) concentration.

Characterizations and Quantitative Estimation of Alkali-Activated Binder Paste from Microstructures

  • Kar, Arkamitra;Ray, Indrajit;Halabe, Udaya B.;Unnikrishnan, Avinash;Dawson-Andoh, Ben
    • International Journal of Concrete Structures and Materials
    • /
    • 제8권3호
    • /
    • pp.213-228
    • /
    • 2014
  • Alkali-activated binder (AAB) is recently being considered as a sustainable alternative to portland cement (PC) due to its low carbon dioxide emission and diversion of industrial wastes and by-products such as fly ash and slag from landfills. In order to comprehend the behavior of AAB, detailed knowledge on relations between microstructure and mechanical properties are important. To address the issue, a new approach to characterize hardened pastes of AAB containing fly ash as well as those containing fly ash and slag was adopted using scanning electron microscopy (SEM) and energy dispersive X-ray spectra microanalyses. The volume stoichiometries of the alkali activation reactions were used to estimate the quantities of the sodium aluminosilicate (N-A-S-H) and calcium silicate hydrate (CSH) produced by these reactions. The 3D plots of Si/Al, Na/Al and Ca/Si atom ratios given by the microanalyses were compared with the estimated quantities of CSH(S) to successfully determine the unique chemical compositions of the N-A-S-H and CSH(S) for ten different AAB at three different curing temperatures using a constrained nonlinear least squares optimization formulation by general algebraic modeling system. The results show that the theoretical and experimental quantities of N-A-S-H and CSH(S) were in close agreement with each other. The $R^2$ values were 0.99 for both alkali-activated fly ash and alkali-activated slag binders.

양극산화와 열수처리한 순수 니오비움 금속의 생체활성 평가 (Evaluation of Biocompatibility of Anodized and Hydrothermally Treated Pure Niobium Metal)

  • 원대희;최운재;이민호;배태성
    • 대한치과기공학회지
    • /
    • 제27권1호
    • /
    • pp.79-88
    • /
    • 2005
  • This study was performed to investigate the surface properties of electrochemically oxidized pure niobium by anodic oxide and hydrothermal treatment technique. Niobium specimens of $10\times10mm$ in dimension were polished sequentially from #600, #800, #1000 emery paper. The surface pure niobium specimens were anodized in an electrolytic solution that was dissolved calcium and phosphate in water. The electrolytic voltage was set in the range of 250 V and the current density was 10 $mA/cm^2$. The specimen was hydrothermal treated in high-pressure steam at 300$^{\circ}C$ for 2 hours using an autoclave. Then, specimens were immersed in the Hanks' solution with pH 7.4 at 37$^{\circ}C$ for 30 days. The surface of specimen was characterized by scanning electron microscope(SEM), energy dispersive X-ray microanalysis(EDX), potentiostat/galvanostat test, and cytotoxicity test. The results obtained was summarized as follows; According to the result of measuring corrosion behavior at 0.9% NaCl, corrosion resistance was improved more specimens treated with anodic oxide than in hydrothermal treated ones. The multi-porous oxide layer on surface treated through anodic oxidation showed a structure that fine pores overlap one another, and the early precipitation of apatite was observed on the surface of hydrothermal treated samples. According to the result of EDX after 30 days deposition in Hanks' solution, Ca/P was 1.69 in hydrothermal treated specimens. In MTT test, specimens treated through anodic oxidation and hydrothermal treated ones showed spectrophotometer similar to that of the control group. Thus no significant difference in cytotoxicity was observed (P>0.05).

  • PDF

Electrochemical Behavior of Nanostructured Fe-Pd Alloy During Electrodeposition on Different Substrates

  • Rezaei, Milad;Haghshenas, Davoud F.;Ghorbani, Mohammad;Dolati, Abolghasem
    • Journal of Electrochemical Science and Technology
    • /
    • 제9권3호
    • /
    • pp.202-211
    • /
    • 2018
  • In this work, Fe-Pd alloy films have been electrodeposited on different substrates using an electrolyte containing $[Pd(NH_3)_4]^{2+}$ (0.02 M) and $[Fe-Citrate]^{2+}$ (0.2 M). The influences of substrate and overpotential on chemical composition, nucleation and growth kinetics as well as the electrodeposited films morphology have been investigated using energy dispersive X-ray spectroscopy (EDS), current-time transients, scanning electron microscopy (SEM), atomic force microscopy (AFM) and X-ray diffraction (XRD) patterns. In all substrates - brass, copper and sputtered fluorine doped tin oxide on glass (FTO/glass) - Fe content of the electrodeposited alloys increases by increasing the overpotential. Also the cathodic current efficiency is low due to high rate of $H_2$ co-reduction. Regarding the chronoamperometry current-time transients, it has been demonstrated that the nucleation mechanism is instantaneous with a typical three dimensional (3D) diffusion-controlled growth in the case of brass and copper substrates; while for FTO, the growth mode changes to 3D progressive. At a constant overpotential, the calculated number of active nucleation sites for metallic substrates is much higher than that of FTO/glass; however by increasing the overpotential, the number of active nucleation sites increases. The SEM micrographs as well as the XRD patterns reveal the formation of Fe-Pd alloy thin films with nanostructure arrangement and ultra-fine grains.

Characteristics and osteogenic effect of zirconia porous scaffold coated with ${\beta}$-TCP/HA

  • Song, Young-Gyun;Cho, In-Ho
    • The Journal of Advanced Prosthodontics
    • /
    • 제6권4호
    • /
    • pp.285-294
    • /
    • 2014
  • PURPOSE. The purpose of this study was to evaluate the properties of a porous zirconia scaffold coated with bioactive materials and compare the in vitro cellular behavior of MC3T3-E1 preosteoblastic cells to titanium and zirconia disks and porous zirconia scaffolds. MATERIALS AND METHODS. Titanium and zirconia disks were prepared. A porous zirconia scaffold was fabricated with an open cell polyurethane disk foam template. The porous zirconia scaffolds were coated with ${\beta}$-TCP, HA and a compound of ${\beta}$-TCP and HA (BCP). The characteristics of the specimens were evaluated using scanning electron microscopy (SEM), energy dispersive x-ray spectrometer (EDX), and x-ray diffractometry (XRD). The dissolution tests were analyzed by an inductively coupled plasma spectrometer (ICP). The osteogenic effect of MC3T3-E1 cells was assessed via cell counting and reverse transcriptase-polymerase chain reaction (RT-PCR). RESULTS. The EDX profiles showed the substrate of zirconia, which was surrounded by the Ca-P layer. In the dissolution test, dissolved $Ca^{2+}$ ions were observed in the following decreasing order; ${\beta}$-TCP > BCP > HA (P<.05). In the cellular experiments, the cell proliferation on titanium disks appeared significantly lower in comparison to the other groups after 5 days (P<.05). The zirconia scaffolds had greater values than the zirconia disks (P<.05). The mRNA level of osteocalcin was highest on the non-coated zirconia scaffolds after 7 days. CONCLUSION. Zirconia had greater osteoblast cell activity than titanium. The interconnecting pores of the zirconia scaffolds showed enhanced proliferation and cell differentiation. The activity of osteoblast was more affected by microstructure than by coating materials.