• 제목/요약/키워드: different moduli

Search Result 151, Processing Time 0.025 seconds

A Study on Anisotropic Compression Behavior of Illite (일라이트의 비등방적 압축특성 연구)

  • Yun, Seohee;Lee, Yongjae
    • Korean Journal of Mineralogy and Petrology
    • /
    • v.33 no.1
    • /
    • pp.11-18
    • /
    • 2020
  • High-pressure synchrotron X-ray powder diffraction experiments were performed on natural illite (K0.65Al2(Al0.65Si3.35)O10(OH)2) using diamond anvil cell (DAC) under two different pressure transmitting media (PTM), i.e., water and ME41 (methanol:ethanol = 4:1 by volume). When using water as PTM, occasional heating was applied up to about 250℃ while reaching pressure up to 2.7 GPa in order to promote both hydrostatic conditions and intercalation of water molecules into the layer. When using ME41, pressure was reached up to 6.9 GPa at room temperature. Under these conditions, illite did not show any expansion of interlayer distance or phase transitions. Pressure-volume data were used to derive bulk moduli (K0) of 45(3) GPa under water and 51(3) GPa under ME41 PTM. indicating no difference in compressibility within the analytical error. Linear compressibilities were then calculated to be βa = 0.0025, βb = 0.0029, βc = 0.0144 under ME41 PTM showing the c-axis is ca. six times more compressible than a- and b-axes. These elastic behaviors of illite were compared to muscovite, one of its structural analogues.

Evaluation of Field Nonlinear Modulus of Subgrnde Soils Using Repetitive Static Plate Bearing Load Test (반복식 평판재하시험을 이용한 노상토의 현장 변형계수 평가)

  • Kim Dong-Soo;Seo Won-Seok;Kweon Gi-Chul
    • Journal of the Korean Geotechnical Society
    • /
    • v.21 no.6
    • /
    • pp.67-79
    • /
    • 2005
  • The field plate load test has a good potential for determining modulus since it measures both plate pressure and settlement. Conventionally the modulus has been assumed to be a constant secant value defined from the settlement of the plate at a given load intensity. A constant modulus (modulus of subgrade reaction, k), however, may not be a representative value of subgrade soil under working load. Field strain(o. stress)-dependent modulus characteristics of subgrade soils, at relatively low to intermediate strains, are important in the pavement design. In this study, the field strain dependent moduli of subgrade soils were obtained using cyclic plate load test. Testing procedure and data reduction method are proposed. The field crosshole and laboratory resonant column tests were also performed to determine field nonlinear modulus at $0.001\%\;to\;0.1\%$ strains, and the modulus values and nonlinear trends are compared to those obtained by cyclic plate load tests. Both modulus values match relatively well when the different state of stress between two tests was considered, and the applicability of field cyclic plate load test for determining nonlinear modulus values of subgrade soils is verified.

Effects of Initial Stress on the Deformation of Sand (초기응력상태(初期應力狀態)가 모래의 변형(變形)에 미치는 영향(影響))

  • Kang, Byung Hee;Chung, In Joon
    • KSCE Journal of Civil and Environmental Engineering Research
    • /
    • v.3 no.1
    • /
    • pp.65-72
    • /
    • 1983
  • Dry sand specimens for both normally consolidated and overconsolidated triaxial compression tests were prestressed on the path with five different coefficients of earth pressure 1.0, 3/4, 0.55, $K_0$ and 1/3. Deformation resistance of normally consolidated sand increased with increasing the initial stress for all coefficients of earth pressure during consolidation, and the deformation modulus at a certain initial stress showed a tendency to increase with increasing the coefficient of earth pressure. And deformation moduli($E_i$, $E_{50}$), were found to be proportional to the $n_{th}$ power of initial stresses[${\sigma}_{m0}{^{\prime}}$, ${\sigma}_{10}{^{\prime}}$, ${\sigma}_{30}{^{\prime}}$, $({\sigma}_1-{\sigma}_3)_0$] for both isotropically and anisotropically normally consolidated samples, where n varied from 0.37 to 0.92. Overconsolidated sand with the higher overconsolidation ratio showed the higher deformation modulus. It is concluded that the $K_0$-anisotropically consolidated triaxial compression test is necessary to obtain the more accurate value of in-situ deformation modulus.

  • PDF

Application of Seismic Tomography to the Inverstigation of Underground Structure in Gupo Train Accident Area (구포 기차 전복사고 지역의 지반상태 파악을 위한 탄성파 토모그래피 응용)

  • 김중열;장현삼;김유성;현혜자;김기석
    • The Journal of Engineering Geology
    • /
    • v.5 no.1
    • /
    • pp.1-20
    • /
    • 1995
  • A train overturn accident occurred on March 1993 in the Gupo area, northern part of Pusan, unfortunately had taken a heavy toll of lives and caused a great loss of property as well. The reasons for the subsidence of the basement under the railroads, which presumed to be the main cause of the accident, have been investigated from many different angles, including conventional geotechnical investigation methods. The deduced nuin reasons of the subsidence were: 1. blasting for tunnel excavation (NATM) at about 39 meter under the railroads, and 2. unexpected change of bedrock conditions along the direction of tunnel. But this accident was derived nrranlv from the lack of geological and geotechnical information under railroad area because it was impossible to drill beneath the railroads. This paper introduces a new geophysical survey techniqueseisrnic geotomography, and shows some results of the method applying to investigate the underground structure of the accident area. This method not only overcomes the unfavourable environment which many conventional investigation methods cannot face, but produces an image of underground structure with high resolution. Furthermore, the outputs from geotomogaphic analysis could provide very valuable in-situ basic parameters (like seismic velocities, elastic moduli, etc.) which is essential to the design and construction.

  • PDF

Synthesis of Multi-Walled Carbon Nanotube/Polystyrene (MWCNT/PS) Composites by Solution Process and Their Thermal Behavior (용액공정을 이용한 다중벽 탄소 나노튜브/폴리스티렌(MWCNT/PS) 복합체 합성 및 열적 거동)

  • Teng, Dayong;Shin, Young Hwan;Kwon, Younghwan
    • Applied Chemistry for Engineering
    • /
    • v.19 no.4
    • /
    • pp.421-426
    • /
    • 2008
  • Multi-walled carbon nanotube/polystyrene (MWCNT/PS) composites with various MWCNT contents were prepared by using a solution process with an aid of surfactant. Particularly, PS's with 3 different molecular weights (${\bar{M}}_n$ = 101500 g/mole for PS-1, ${\bar{M}}_n$ = 89900 g/mole for PS-2, and ${\bar{M}}_n$ = 85000 g/mole for PS-3) were used in this study. Thermal behavior of these composites was examined by using an oscillator rheometer at $210^{\circ}C$ and $180^{\circ}C$, of above and below the critical flow temperature ($T_{cf}{\sim}195^{\circ}C$) of PS matrix, respectively. The storage and loss modulus, and the complex viscosity of these composites increased with increasing MWCNT content at both temperatures. Largest increases in the frequency-dependent moduli and complex viscosity were observed between 2 wt% and 5 wt% of MWCNTs at $210^{\circ}C$ and $180^{\circ}C$. Only the composite at $210^{\circ}C$ showed the rheological phase transition from a viscous-dominant to an elastic-dominant behavior of the composites at a certain MWCNT content. The MWCNT content at the rheological phase transition of MWCNT/PS composites generally increased with decreasing molecular weight of PS, and was measured to be 3.5 wt% for MWCNT/PS-1, 3.2 wt% for MWCNT/PS-2, and 3.0 wt% for MWCNT/PS-3 composites.

Dynamic Deformation Characteristics of Joomunjin Standard Sand Using Cyclic Triaxial Test (반복삼축압축시험을 이용한 주문진 표준사의 동적변형특성 분석)

  • Kim, You-Seong;Ko, Hyoung-Woo;Kim, Jae-Hong;Lee, Jin-Gwang
    • Journal of the Korean Geotechnical Society
    • /
    • v.28 no.12
    • /
    • pp.53-64
    • /
    • 2012
  • In this study, the modified cyclic triaxial tests with Joomunjin standard sand are performed for dynamic deformation characteristics, such as Young's moduli and damping ratio. The cyclic triaxial test is equipped with Local Displacement Transducer (LDT) on the outside of a cell which has a range from $10^{-4}$ to $10^{-1}$ of shear strains, ${\gamma}$ (%), instead of conventional cyclic triaxial test which has linear variable displacement transducer (LVDT) with low precision. With the small strain control, tests were carried out at various loading rates, void ratios, and effective confining pressures. Based on the test results, such as dynamic deformation characteristics, shear modulus, and damping ratio, it is found that the test can measure more range of medium strains (0.02-0.2%) than results obtained from conventional test (resonant column test). For the medium strain range, dynamic deformation characteristics investigated by the cyclic triaxial test are also different from those predicted by nonlinear model in conventional test.

Numerical Analysis of Warpage and Stress for 4-layer Stacked FBGA Package (4개의 칩이 적층된 FBGA 패키지의 휨 현상 및 응력 특성에 관한 연구)

  • Kim, Kyoung-Ho;Lee, Hyouk;Jeong, Jin-Wook;Kim, Ju-Hyung;Choa, Sung-Hoon
    • Journal of the Microelectronics and Packaging Society
    • /
    • v.19 no.2
    • /
    • pp.7-15
    • /
    • 2012
  • Semiconductor packages are increasingly moving toward miniaturization, lighter and multi-functions for mobile application, which requires highly integrated multi-stack package. To meet the industrial demand, the package and silicon chip become thinner, and ultra-thin packages will show serious reliability problems such as warpage, crack and other failures. These problems are mainly caused by the mismatch of various package materials and geometric dimensions. In this study we perform the numerical analysis of the warpage deformation and thermal stress of 4-layer stacked FBGA package after EMC molding and reflow process, respectively. After EMC molding and reflow process, the package exhibits the different warpage characteristics due to the temperature-dependent material properties. Key material properties which affect the warpage of package are investigated such as the elastic moduli and CTEs of EMC and PCB. It is found that CTE of EMC material is the dominant factor which controls the warpage. The results of RSM optimization of the material properties demonstrate that warpage can be reduced by $28{\mu}m$. As the silicon die becomes thinner, the maximum stress of each die is increased. In particular, the stress of the top die is substantially increased at the outer edge of the die. This stress concentration will lead to the failure of the package. Therefore, proper selection of package material and structural design are essential for the ultra-thin die packages.

Rheological Properties of Sweet Potato Starch-sucrose Composite (고구마전분-sucrose 복합물의 레올로지 특성)

  • Cho, Sun-A;Yoo, Byoung-Seung
    • Korean Journal of Food Science and Technology
    • /
    • v.40 no.2
    • /
    • pp.184-189
    • /
    • 2008
  • Effects of sucrose at different concentrations (0, 10, 20, and 30%, w/w) on steady and dynamic shear rheological properties of sweet potato starch (SPS) paste (5%, w/w) were investigated. The steady shear rheological properties of SPS-sucrose composites were determined from rheological parameters based on power law and Casson flow models. At 25$^{\circ}C$ all the samples showed pseudoplastic and thixoropic behavior with high yield stress. Consistence index (K), apparent viscosity (${\eta}_{a,100}$), and yield stress (${\sigma}_{oc}$) values of SPS-sucrose composites decreased with increasing sucrose concentration from 10% to 30%. The decrease of swelling power was observed at higher sucrose concentration (>20%) and the low swelling power yielded a lower K, ${\eta}_{a,100}$, and ${\sigma}_{oc}$ values. In temperature range of 25-70$^{\circ}C$, Arrhenius equation adequately assessed variation with temperature. Oscillatory test data showed weak gel-like behavior. Magnitudes of storage (G') and loss (G") moduli increased with an increase in sucrose concentration and frequency. The SPS-sucrose composite at 30% concentration closely followed the Cox-Merz superposition rule.

Anisotropic Compression Behavior and Phase Transition of Sepiolite Under Moderate Pressure Conditions (천부지권 압력 하 해포석의 비등방적 압축 특성 및 상전이 연구)

  • Seohee, Yun;Yongjae, Lee
    • Korean Journal of Mineralogy and Petrology
    • /
    • v.35 no.4
    • /
    • pp.423-430
    • /
    • 2022
  • Pressure-dependent elastic behavior and chemical reaction of natural sepiolite (Mg8Si12O30(OH)4·12H2O) was studied under two different pressure-transmitting medium (PTM) conditions using synchrotron X-ray powder diffraction. Under non pore-penetrating silicone oil PTM, we observed that the b-axis length increases up to ca. 3.6 GPa, marking an anisotropic compression region with negative linear compressibility of βb= -0.0012 GPa-1, which then decreases at 7.7 GPa. Under pore-penetrating water PTM, the anisotropic compression behavior is enhanced with doubled negative linear compressibility of βb= -0.0025 GPa-1 up to 3.2 GPa, where transformation into stevensite is observed upon ex-situ temperature treatment at 280 ℃ as confirmed via XRD and SEM. Derived bulk moduli (K0) and linear compressibilities (β) were compared to other structurally and chemically related minerals.

Characteristics of Rigid-Soft Particle Mixtures with Size Ratio (입자크기비에 따른 강-연성 혼합재의 공학적 특성)

  • Lee, Chang-Ho;Yoon, Hyung-Koo;Kim, Rae-Hyun;Lee, Woo-Jin;Lee, Jong-Sub
    • Journal of the Korean Geotechnical Society
    • /
    • v.24 no.8
    • /
    • pp.125-135
    • /
    • 2008
  • Rigid-soft particle mixtures, which consist of sand and rubber, are investigated for the understanding of the stress-deformation and elastic moduli. Specimens are prepared with various size ratio sr between sand and rubber particles, and different volumetric sand fraction sf. Small strain shear waves are measured under $K_o$-loading condition incorporated with the stress-deformation test by using oedometer cell with bender elements. The stress-deformation and small strain shear wave characteristics of rigid-soft particle mixtures show the transition from a rigid particle behavior regime to a soft particle behavior regime under fixed size ratio. A sudden rise of $\Lambda$ factor and the maximum value of the $\zeta$ exponent in $G_{max}=\;{\Lambda}({\sigma}'_{o}/kPa)^{\zeta}$ are observed at $sf\;{\approx}\;0.4{\sim}0.6$ regardless of the size ratio sf. Transition mixture shows high sensitivity to confining stress. The volume fraction for the minimum porosity may depend on the applied stress level in the rigid-soft particle mixtures because the soft rubber particles easily distort under load. In this experimental study, the size ratio and volumetric sand fraction are the important factors which determine the behavior of rigid and soft particle mixtures.