• Title/Summary/Keyword: dielectric losses

Search Result 83, Processing Time 0.021 seconds

Dielectric properties of ZrTiO4 thin films deposited by DC magnetron reactive sputtering

  • Kim, Taeseok;Park, Byungwoo;Hong, Kug-Sun
    • Journal of Korean Vacuum Science & Technology
    • /
    • v.3 no.2
    • /
    • pp.130-133
    • /
    • 1999
  • Paraelectric ZrTiO4 thin films were synthesized on a Si(100) substrate using DC magnetron reactive sputtering. Films deposited above-400$^{\circ}C$ exhibited crystalline characteristics. The dielectric constants ($\varepsilon$) and dielectric losses (tan$\delta$) of as-deposited and annealed films were measured in the 1 MHz range using a Pt upper electrode and a phosphorous-doped si bottom electrode. Preliminary data showed that as the deposition temperature increased, the dielectric losses decreased while the dielectric constants did not change significantly. similar trends for dielectric losses were observed when the as-deposited samples were annealed at 800$^{\circ}C$. The reduction of dielectric losses at high-deposition temperatures and post annealing correlated well with the x-ray diffraction peak widths.

  • PDF

Dielectric Properties Analysis in Paraelectric $ZrTiO_4$Thin Films (상유전 $ZrTiO_4$박막의 유전특성 분석에 관한 연구)

  • 허진희;김경해;이준신
    • Proceedings of the Korean Institute of Electrical and Electronic Material Engineers Conference
    • /
    • 2001.07a
    • /
    • pp.547-549
    • /
    • 2001
  • The dielectric constants and dielectric losses of ZrTiO$_4$thin films deposited by DC magnetron reactive sputtering were investigated. The paraelectric properties were measured in the 100kHz range. As the deposition temperature increased (up to 67$0^{\circ}C$), the dielectric losses (tan$\delta$) decreased (down to 0.017$\pm$0.007), while the dielectric constants ($\varepsilon$) were in the range of 35$\pm$7. Post annealing at 80$0^{\circ}C$ in oxygen for 2h reduced tan$\delta$ down to 0.005$\pm$0.001, higher than those of well-sintered bulk ZrTiO$_4$.

  • PDF

Dielectric Properties of Unsaturated Polyester Resin for Electric Safety (전기 안전에 관한 불포화폴리에스테르 수지의 유전특성)

  • 이성일;권호영
    • Journal of the Korean Society of Safety
    • /
    • v.6 no.3
    • /
    • pp.12-20
    • /
    • 1991
  • The dielectric properties that effect to electric safety for unsaturated Pelvester resin were studied over the temperature range of 30-40[$^{\circ}C$] and the frequency range of 110~3$\times$10$^{6}$ [Hz]. According to the results of the study, it has been observed that two kinds of dielectric losses in electric safety were existed by the molecular movement of C-H and OH group. When the ,adio of hardener was 1.5[%], the characteristics of specimens were excellent in view of the electrical materical. In the range of measuring frequency the dielectric constants and the dielectric losses were 3.5~5.5 and 10$^2$~10$^3$ respectly. The activation energy of loss spectrum in aspect of electric safety and the entropy appeared at the 30[$^{\circ}C$] were 33.4[Kacl/mole] and 54.9[cal/mole.deg] respectly.

  • PDF

Properties of Electric Sofety for Dielectric Loss of Aging Natural Rubber. (노화된 천연고무의 유전손실에 관한 전기안전특성)

  • 이성일;권호영
    • Journal of the Korean Society of Safety
    • /
    • v.6 no.4
    • /
    • pp.5-12
    • /
    • 1991
  • The dielectric properties of natural rubbers for electric safety are very important to investigate the molecular structure. The electric safety characteristics of the dielectric absorption in aging vulcanized natural rubber were studied in the range of frequency from 1$\times$10$^3$[Hz]to 3.2$\times$10$^3$[Hz]l at the temperature of 23[$^{\circ}C$]. As the results, it has been confirmed that in the case of aging natural rubber of above 2 phr the specimens exhibit two kinds of dielectric losses due to the dipole polarization by impurities and sulfurs, and of raw rubber exhibit the kind of losses due to the dipole polarization. Rurthermore, dielectric loss maximum tansspectrum in high freguency region for electric safety, which removed to the low freguency according to increasing sulfur, depends greatly on sulfur.

  • PDF

Influence of the Vulcanization on the Dielectric Properties of Natural Rubber (천연고무의 유전특성에 미치는 가황의 영향)

  • Lee, Joon-Ung;Yon, Dae-Heum
    • The Transactions of the Korean Institute of Electrical Engineers
    • /
    • v.33 no.3
    • /
    • pp.112-117
    • /
    • 1984
  • The dielectric propertries of polymers are very important to investigate the molecular structure of polymer. The characteristrics of the dielectric absorption in vulcanized natural rubber were studied in the range of frequency from 10[KHz] to 32[MHz] at the temperature of 25[$^{\circ}C$]. As the results. it has been confirmed that in the case of natural ruber vulcanized between 2 and 4phr the specimens exhibit two kind of dielectric losses due to the dipole polarization by impurites and sulfure, and of above 7phr was only a loss due to the dipole polarization by sulfure and of natural rubber exhibit two kind of losses due to the interfacial and the dipole polarization. Furthermore, dielectric loss maximun tan spectrum, which removed to the low frequency according to increasing sulfure, depends greatly on sulfure. The volume resistivity of $10^{7}$~$10^{11}$[$\Omega\cdot$cm], regardness whether the crosslinking of rubber are tired by sulfure or, was observed.

  • PDF

Influence of the Vulcanization on the Dielectric Proper ties of the Ageing Natural Nubber (노화된 천연고무의 유전특성에 미치는 가황의 영향)

  • Kim, Bong-Heup;Kim, Wang-Kon;Lee, Joon-Ung
    • Elastomers and Composites
    • /
    • v.21 no.3
    • /
    • pp.205-212
    • /
    • 1986
  • The dielectric properties of natural rubber are very important to investigate the molecular structure. The charcteristics of the dielectric absorption in aging natural rubber were studied in the range of frequency from $1{\times}10^3Hz\;to\;3.2{\times}10^7Hz$ at the temperature of $23^{\circ}C$. As the results, it has been confirmed that in the case of aged NR vulcanized specimen with contained sulfur 2 phr above the specimens exhibit two kind of dielectic losses due to the the dipole polarization by impurities and sulfurs, and of raw rubber exhibit the kind of losses due the to dipole polarization. Particularly, it has been affirmed that the dielectric loss spectrum of the aging natural rubber is larger than that the natural rubber, and the dielectric strength of the aging natural rubber drop depreciate respctively.

  • PDF

Some Problems of the Partial Discharge Burning Time

  • Kinsht Nikolay V.;Katz Marat A.
    • Transactions on Electrical and Electronic Materials
    • /
    • v.7 no.6
    • /
    • pp.319-323
    • /
    • 2006
  • The problem of the partial discharge (PD) extinction is investigated. The transient process takes place in a small spherical inclusion which is located in the dielectric. Both the losses caused by polarization and ohmic losses as the dielectric parameters are taken into account. From the inclusion standpoint the dielectric is considered as an active two-pole element (equivalent generator) and inclusion represents by own current-voltage curve. PD extinction voltage was shown to depend on the polarization loss tangent.

Loss Characteristics of Flexible Dielectric Tube Waveguides using Commercial Polymer Substances in Millimeter Wave Band

  • Kim, Ki-Young;Youngsik Ahn;Sohn, Jon-Ryul;Tae, Heung-Sik
    • Proceedings of the Korea Electromagnetic Engineering Society Conference
    • /
    • 2000.11a
    • /
    • pp.233-237
    • /
    • 2000
  • Propagation losses including bath transmission losses and bending losses of the flexible dielectric tube waveguide using commercial polymer substances for a short distance millimeter wave transmission are analytically predicted. The transmission loss and the bending loss are strongly dependent on the power flow distributions in each region. The obtained propagation tosses are compared with those of the commercial metal rigid and flexible waveguides.

  • PDF

Enhancement of Dielectric Properties of Polyamide Enamel Insulation in High Voltage Apparatuses Used in Medical Electronics by Adding Nano Composites of SiO2 and Al2O3 Fillers

  • Biju, A.C.;Victoire, T. Aruldoss Albert;Selvaraj, D. Edison
    • Journal of Electrical Engineering and Technology
    • /
    • v.10 no.4
    • /
    • pp.1712-1719
    • /
    • 2015
  • In recent days, there was a significant development on the electrical, thermal, mechanical, physical, chemical, magnetic and optical properties of the polyamide enamel, varnish and other insulating materials by the addition of nano fillers to it. Enamel was used in High Voltage Apparatuses used in Medical Electronics as insulation. Insulating materials determine the life time of the electrical apparatuses. The life time of the insulating materials was improved by the addition of nano fillers to it. Hence the life time of the electrical apparatuses was improved by the mixing of nano fillers to the enamel. In this research, the basic dielectric properties of the enamel and enamel mixed with nano composites of silica and alumina were analyzed and compared with each other. The addition of nano fillers has improved the quality factor and capacitance of the enamel. It was also observed that the addition of nano fillers has reduced the dissipation factor and dielectric losses of the enamel. Heat produced by the dielectric losses was also reduced by adding nano fillers to it.

Dielectric Properties of (Ba,Sr)$TiO_3$ Thin Films with Substrate Temperature (기판온도에 따른 (Ba,Sr)$TiO_3$ 박막의 유전특성)

  • Lee, Sang-Chul;Chung, Jang-Ho;Bae, Seon-Gi;Lee, Young-Hie
    • Proceedings of the KIEE Conference
    • /
    • 1999.07d
    • /
    • pp.1879-1881
    • /
    • 1999
  • (Ba,Sr)$TiO_3$[BST] thin films were fabricated on Pt/Ti/$SiO_2$/Si substrate by RF sputtering. We investigated the effects of substrate temperature on the structural and dielectric properties of BST thin films. Increasing the substrate temperature, barium multi titanate phases were decreased, and BST (100), (200) peaks were increased. The relative dielectric constant and dielectric loss of the BST thin films at the substrate temperature of $500^{\circ}C$ were 300 and 0.018, respectively at l[kHz]. In all films, the dielectric constants decreased. Dielectric losses increased as increasing the frequency. The switching voltage was 5V of the BST thin films at the substrate temperature of $500^{\circ}C$.

  • PDF