Concentration of elemental ions released from non-precious dental casting alloys (치과주조용 비귀금속 합금의 금속 용출 수준)

  • Sakong, Joon;Park, Soo-Chul
    • Journal of Technologic Dentistry
    • /
    • v.35 no.1
    • /
    • pp.1-17
    • /
    • 2013
  • Purpose: This study was to assess the extents of the release of metals from the non-precious alloys used for dental casting by measuring the differences in the extents of the release of metals by types of alloys, pH level and elapsed time. Methods: Uniform-sized specimens(10 each) were prepared according to the Medical Device Standard of the Korea Food and Drug Administration(2010) and International Standard Organization(ISO22674, 2006), using four types of alloys(one type of Ni-Cr and one type of Co-Cr used for fixed prosthesis, and one type of Ni-Cr and one type of Co-Cr used for removable prosthesis). A total of 12 metal-release tests were performed at one-day, three-day, and two-week intervals, for up to 20 weeks. The metal ions were quantified using an Inductively Coupled Plasma-Atomic Emission Spectrometer. Results: The results showed that the extent of corrosion was higher in the ascending order of Jdium-$100^{(R)}$, Bellabond-$Plus^{(R)}$, Starloy-$C^{(R)}$, and Biosil-$F^{(R)}$. The lower the pH and the longer the elapsed time were, the greater the increase in metal corrosion. At pH 2.4, the release of Ni from Jdium-$100^{(R)}$, a Ni-Cr alloy, was up to 15 times greater than the release of Co from the Co-Cr alloy from two weeks over time, indicating that the Ni-Cr alloy is more susceptible to corrosion than the Co-Cr alloy. Conclusion: It is recommended that Co-Cr alloy, which is highly resistant to corrosion, be used for making dental prosthesis with a non-precious alloy for dental casting, and that non-precious alloy prosthesis be designed in such a way as to minimize the area of its oral exposure. For patients with non-precious alloy prostheses, a test of the presence or absence of periodontal tissue inflammation or allergic reaction around the prosthesis should be performed via regular examination, and education on the good management of the prosthesis is needed.

Anodic Polarization Characteristics in Ti-20%Zr(-5%Cr) Alloys for Dental Castings (치과주조용 Ti-20%Zr(-5%Cr)합금의 양극분극특성)

  • Jung, Jong-Hyun;Han, Sok-Yoon
    • Journal of Technologic Dentistry
    • /
    • v.26 no.1
    • /
    • pp.41-48
    • /
    • 2004
  • Ti-20%Zr(-5%Cr) alloys not containing harmful Al and V were newly designed in order to reveal their possibility for dental casting and melted in an arc melting and casting furnace under Ar atmosphere. The corrosion resistance was studied by anodic polarization test. From the observation of anodic polarization behavior, it was found that the corrosion resistance was markedly increased by the addition of Cr. The corrosion resistance of Ti-20%Zr-5%Cr alloy was superior to that in Ti-6%Al-4%V alloy but almost similar to that in CP Ti using in market place today.

  • PDF

A Study on the Toxicity of Several Dental Casting Alloys (수종(數種) 치과주조용(齒科鑄造用) 금속(金屬)의 독성(毒性)에 관(關)한 연구(硏究))

  • Kim, Gi-Jin;Park, Charn-Woon
    • The Journal of Korean Academy of Prosthodontics
    • /
    • v.25 no.1
    • /
    • pp.327-340
    • /
    • 1987
  • This study was performed to investigate the biocompatibility of several dental casting alloys (Gold, Dong Myung A-45, Dong Myung AP-35, Verabond, Rexillium, NPG) employing tissue culture. Fibroblast-like cells derived from the subcutaneous tissue of Sprague-Dawley rat were cultivated in DME medium with the addition of those alloys. Results were assessed by calculating the cell multiplication rate and relative growth rate and by observing the morphology of cells in the presence of the specimens. Gold was indicated to be most biocompatible with fibroblast-like cell. Dong Myung A-45 and Dong Myung AP-35 showed very similar effects on the cells as did Gold. Also there was a decrease in cytotoxicity of the alloys as the concentration of gold increased. Verabond and Rexillium showed a decreased in cell mutiplication rate as compared to low gold alloys. NPG exhibited the most severe cell toxicity among the tested alloys.

  • PDF

Effect of Two Variables on the Casting Ability of Some Nonpercious Alloys for Porcelain-Metal Restorations (납형의 직경 및 소환방법이 도재-금속 보철물용 비귀금속 합금의 주조성에 미치는 영향)

  • Kim, Uoong-Chul
    • Journal of Technologic Dentistry
    • /
    • v.6 no.1
    • /
    • pp.19-26
    • /
    • 1984
  • This Experimental study was performed to study the effect of the heat soaking and the diameter of pattern on the casting ability of three nonprecious alloys manufactured for porcelain-metal restorations, with respect to their ability to reproduce test pieces by casting over a selected range of uniform diameters. Samples of total 60 were constructed and divided into 6 groups according to the two variables, the diameter and the heat soaking. The completed cast samples were examined visually and measured with a caliper calibrated to 0.05mm. The results obtained were as follows: 1. Length cast was significantly related to the diameter to be cast, especially in the case of the marrowest diameter of 230m. 2. Length cast not significantly related to the heat soaking. 3. The completeness of casting was significantly related to the diameter to be cast, particularly in the case of the narrowest diameter of 230m. 4. The completeness of casting was not significantly related to the heat soaking. 5. All of the three nonprecious alloys used for this experiment were significantly different from an ideal alloy in the completeness of casting.

  • PDF

On Composition and HB of Dental Alloys (치과용합금(齒科用合金)type에 따른 조성(組成) 및 경도(硬度)에 관(關)한 연구(硏究))

  • Hyun, Joung-Gu;Lee, Byoung-Ki
    • Journal of Technologic Dentistry
    • /
    • v.7 no.1
    • /
    • pp.13-18
    • /
    • 1985
  • Casting alloys, both precious and non-precious, were by heat in order to observe the change in HB and the results were : 1. The hard treatment showed 1.4 - 1.5 times as high as the soft treatment in HB. 2. The experiment shows that Au-Pt should be contained more than 75% to prevent color change. 3. Cu by hard teatment played the greatect part in creasing the solidity of Ag-Cu alloy. 4. Casting Co-Cr alloys showed little difference of HB in heat treatment.

  • PDF

Wear Properties of Cast Titanium Alloys for Dental Use (치과용 Titanium 주조합금의 마멸특성)

  • Choi, Seok-Kyu;Kim, Hyung-Il;Park, Ik-Min
    • Journal of Korea Foundry Society
    • /
    • v.11 no.6
    • /
    • pp.482-490
    • /
    • 1991
  • This study presents the wear characteristics of Ti alloys (Pure Ti, Ti-6Al-4V, Ti-5Al-2.5Sn) fabricated by centrifugal precision casting in an Ohara dental titanium casting machine. It was found that the hardness of the surface region is higher than that of the interior region. It is considered that the oxygen adsorption in the surface region during casting, leads to the interstitial solid solution hardening. Wear resistance incerases in the order of pure Ti, Ti-6Al-4V, Ti-5Al-2.5Sn alloys. The interior hardness value increases in the same order. The specific wear rate increases with applied load and increases monotonously with sliding speed. The Fe transfer from the counterpart material was observed on the worn surface of the Ti-5Al-2.5Sn alloy. Oxidative wear occurs at low sliding speeds and mechanical fracture wear occurs at high sliding speeds.

  • PDF

Evaluation of a metal level in non-precious metal alloys dental casting having beryllium by lactic acid Solution (베릴륨함유 치과 주조용 비귀금속 합금의 젖산용액에 의한 금속 노출수준 평가)

  • Park, Soo-Chul;Jang, Eun-Jin;Han, Sok-Yoon
    • Journal of Technologic Dentistry
    • /
    • v.33 no.2
    • /
    • pp.121-128
    • /
    • 2011
  • Purpose: The purpose of this study is to investigate the level of each metal in non-precious metal alloys dental casting, still used even banned for use and trade by the law, for oral health. Methods: Two kinds of metal alloys were analyzed. One was Ticonium 100 for removable prosthesis and the other was Rexillium V for dental porcelain. Two samples of each metal alloy were made in 0.5g, 1.0g, and 1.5g. Total number of samples were 12. Two kinds of lactic acid Solution, pH7 and pH4.6, were injected into each samples. After injection, each samples had been for 21days ${\pm}$ 1 hour in the water tank of which temperature was $37^{\circ}C$. The level of metal was measured in each sample by inductively couplled plasma-atomic emission spectrometer. Results: In both metal alloys, metals, chrome, nickel, beryllium, and molybdenum, were founded. In Ticonium 1000, the highest level of nickel was 2.531ppm in 1.5g pH4.6 sample while the highest level of nickel was 4.062ppm in 1.5g pH4.6 sample of Rexillium V. In chemical composition of these methal alloys, chrome(14~17%) was much more than beryllium(1.95~1.99%) and molybdenum(5.0~9.0%) but berllium and molybdenum were founded more than chrome in samples. Therefore, chrome showed better anti-corrosion than other metal alloys. In both metal alloys, more metals were founded in higher pH level and more mass. Levels of chrome was significantly different in samples of both metal alloys in each pH level(p<0.05). Levels of nickels was significantly different in samples of both metal alloys in each pH level(p<0.05). Conclusion: For oral health, further studies are needed in nickel-chrome metal alloy and cobalt metal alloy of non-beryllium in addittion to beryllium metal alloy and also long-term studies needed in various period and other non-percious metal alloys for dental casting.

Comparison of the bond strength of ceramics to Co-Cr alloys made by casting and selective laser melting

  • Lawaf, Shirin;Nasermostofi, Shahbaz;Afradeh, Mahtasadat;Azizi, Arash
    • The Journal of Advanced Prosthodontics
    • /
    • v.9 no.1
    • /
    • pp.52-56
    • /
    • 2017
  • PURPOSE. Considering the importance of metal-ceramic bond, the present study aimed to compare the bond strength of ceramics to cobalt-chrome (Co-Cr) alloys made by casting and selective laser melting (SLM). MATERIALS AND METHODS. In this in-vitro experimental study, two sample groups were prepared, with one group comprising of 10 Co-Cr metal frameworks fabricated by SLM method and the other of 10 Co-Cr metal frameworks fabricated by lost wax cast method with the dimensions of $0.5{\times}3{\times}25\;mm$ (following ISO standard 9693). Porcelain with the thickness of 1.1 mm was applied on a $3{\times}8-mm$ central rectangular area of each sample. Afterwards, bond strengths of the samples were assessed with a Universal Testing Machine. Statistical analysis was performed with Kolmogorov-Smirnov test and T-test. RESULTS. Bond strength in the conventionally cast group equaled $74.94{\times}16.06\;MPa$, while in SLM group, it equaled $69.02{\times}5.77\;MPa$. The difference was not statistically significant ($P{\leq}.05$). CONCLUSION. The results indicated that the bond strengths between ceramic and Co-Cr alloys made by casting and SLM methods were not statistically different.