• 제목/요약/키워드: critical current($I_c$)

검색결과 163건 처리시간 0.017초

Influence of External Reinforcement on Strain Characteristics of Critical Current in BSCCO Superconducting Tapes

  • Shin, Hyung-Seop;Kazumune Katagiri
    • 한국초전도ㆍ저온공학회논문지
    • /
    • 제5권3호
    • /
    • pp.15-19
    • /
    • 2003
  • For the purpose of standardization of the critical current measurement, it is meaningful to describe how $I_{c}$ will behave as the stress/strain level changes. In this study, strain dependencies of the critical current $I_{c}$ in Ag-alloy sheathed multifilamentary Bi(2212) and Bi(2223) superconducting tapes were evaluated at 77K, 0T. The external reinforcement was accomplished by soldering AgMgNi alloy tapes onto single or both sides of the sample. With the external reinforcement to the Bi(2212) tape, the strength of the tapes increased but the critical current at the strain free state, $I_{c0}$ decreased in some cases. The strain for onset of the $I_{c}$ degradation, $\varepsilon$$_{\irr}$, increased with an increase of the reinforcing volume and then saturated to a certain value. The effect of external reinforcement on the degradation of $I_{c}$ due to the bending strain in the Bi(2223) tape was also examined. Contrary to the expectation, it showed a significant $I_{c}$ degradation even at a small strain of 0.4 %. The observations of damage morphologies gave a good explanation to the $I_{c}$ behavior.c/ behavior.r.

"Leak Current" correction for critical current measurement of no-insulation HTS coil

  • Song, Jung-Bin;Hahn, Seungyong
    • 한국초전도ㆍ저온공학회논문지
    • /
    • 제19권2호
    • /
    • pp.48-52
    • /
    • 2017
  • Discrepancy between a power supply current and an actual "spiral" coil current makes the conventional 4-probe measurement of a critical current ($I_c$) of a no-insulation (NI) high temperature superconductor (HTS) coil inaccurate and time-consuming. This paper presents a fast and accurate approach for $I_c$ measurement of NI HTS coils. With an NI HTS coil energized at a constant ramping rate, a complete analytic expression for the spiral coil current was obtained from a first-order partial differential equation that derived from an equivalent circuit model of the NI coil. From the analytic solution, both spiral coil current and radial leak current can be obtained simultaneously, which enables fast and accurate measurement of the NI coil $I_c$. To verify the proposed approach, an NI double-pancake (DP) coil, wound with GdBCO tapes of $6mm{\times}0.1mm$, was constructed and its $I_c$ was repeatedly measured with various ramping rates in a bath of liquid nitrogen at 77 K. The measured results agreed well with the calculated ones, which validates the proposed approach to measure $I_c$ of an NI HTS coil.

고온초전도체를 이용한 전류제한장치의 개발 (Development of superconducting current limiting device used high-$T_{c}$ superconductor)

  • 최명호;강형곤;유현수;박성진;한병성
    • 한국전기전자재료학회:학술대회논문집
    • /
    • 한국전기전자재료학회 1993년도 추계학술대회 논문집
    • /
    • pp.35-38
    • /
    • 1993
  • SCLD(supercondocting current 1imiting device) with YBaCuO superconductor was fabricated by the sol-gel and the doctor-blade method. Critical current density ($J_{c}$) and critical current ($I_{c}$) of the SCLD are 100.27 A/$cm^2$and 1A at 77K and the electrodes contact with SCLD by silver paste. The SCL was connected with test circuit in series. When apple iud current exceed critical current value of the SCLD in testing circuit, the SCLD ristricts the over current by generating resistance itself without delay. Resistance of SCLD increase lineary 0 to 1.6$\Omega$ in propotion to applied current above the critical current $I_{c}$.

  • PDF

250 m 급 Bi-2223/Ag 고온 초전도선재 제조 (Fabrication of 250 m class Bi-2223/Ag HTS Tapes)

  • 하홍수;오상수;하동우;장현만;김상철;송규정;박찬;권영길;류강식
    • Progress in Superconductivity
    • /
    • 제3권1호
    • /
    • pp.130-133
    • /
    • 2001
  • A multifilamentary Bi-2223 HTS tape for superconducting power applications was studied through the fabrication of 250-meter long tapes by the PIT(powder in tube) process. To fabricate continuous long wire, a drawing machine, a two-drum bull block and a rolled tape winding machine were developed. Especially, 250-meter long tapes were heat treated in the shape of pancake coil to reduce the heat affect zone and to achieve the high critical current. Engineering critical current density was improved through both the enhancements of critical current density by control of thermal process and the increase of filling factor by using thin Ag alloy sheath tubes less than 1.5 mm in thickness. We have made successfully 250-meter long 37 filamentary tapes with high filling factor up to 31 % employing the modified drawing and rolling technique. The critical current of 250-meter long tapes with pancake coil type was measured by transport method at self-field up to 250 gauss of center field. The measured values, based on the transport critical current at self-field, $I_{c}$ -B characteristics and magnetic field analysis, are 34 A of I$_{c}$ and 4.0 $kA/\textrm{cm}^2$ of $J_{e}$ at 250 m, 77 K, and 0 T. We also have achieved the 56 A of I$_{c}$ and 7.0 $0 kA/\textrm{cm}^2$ of$ J_{e}$ in short tapes at 77K, self-field, and 1$mutextrm{V}$/cm.

  • PDF

고온초전도 coated conductor의 임계전류 측정 표준화 연구 I (A study of standardizing Critical-Current Measurements for coated conductor I)

  • 오상수;이남진;김호섭;염도준
    • 한국전기전자재료학회:학술대회논문집
    • /
    • 한국전기전자재료학회 2009년도 하계학술대회 논문집
    • /
    • pp.363-364
    • /
    • 2009
  • 본 연구는 IEC/TC 90 규격을 참조하여 Cu stabilizer/Ag/$LaMnO_3$/IBAD-MgO/$Y_2O_3$/$Al_2O_3$/Hastelloy C276/Cu stabilizer의 구조를 가지는 coated conductor의 DC 임계 전류의 결정에 대한 사전 연구를 위해 (1) 시편의 냉각시간, (2) 전류 선의 용량을 변화하여 임계 전류의 변화를 관찰하여 다음과 같은 결과를 얻었다. (1) 5분 이상의 시편 냉각시간은 COV가 약 0.4% 정도로 거의 임계 전류 결정에 영향을 주지 않았으며, 냉각 시간이 길면 길수록 임께 전류 이하에서 전압의 기저면이 낮아지는 경향을 보였다. (2) 전류 선의 용량이 클수록 임계 전류 이하에 전압의 기저면이 낮아지는 경향을 보였다.

  • PDF

연속 연료공급식 MOCVD법으로 증착시킨 YBCO 박막의 증착조건 (Deposition condition of YBCO films by continuous source supplying MOCVD method)

  • 김호진;주진호;최준규;전병혁;김찬중
    • 한국초전도ㆍ저온공학회논문지
    • /
    • 제6권3호
    • /
    • pp.6-11
    • /
    • 2004
  • YBa$_2$Cu$_3$$O_{7-x}$ (YBCO) films were deposited on MgO(100) and SrTiO$_3$(100) single crystal substrates by cold-wall type MOCVD method using continuous source supplying system. Under the deposition temperature of 740∼76$0^{\circ}C$, c-axis oriented YBCO films were obtained. In case of the YBCO films deposited on MgO (100) single crystal substrate, the critical temperature (T$_{c}$) was under 81 K regardless of the deposition conditions, whereas T$_{c}$ of the YBCO films deposited on SrTiO$_3$(100) single crystal substrate was 83∼84 K. The critical current (I$_{c}$) of the YBCO film deposited on SrTiO$_3$(100) single crystal substrate for 30 min was 49 A/cm-width and the critical current density (J$_{c}$) was 0.82 MA/$\textrm{cm}^2$ to film thickness of 0.6 ${\mu}{\textrm}{m}$. I$_{c}$ increased to 84.4 A/cm-width as the deposition time increased to 50 min, but J$_{c}$ decreased to 0.53 MA/$\textrm{cm}^2$ to film thickness of 1.8 ${\mu}{\textrm}{m}$.rm}{m}$.

고온 초전도 tape의 임계전류 저하에 따른 교류손실 특성 (AC loss Characteristics under Critical Current Degradation of HTS Tapes)

  • 김해준;조전욱;김재호;심기덕;곽동순;배준한;김해종;성기철
    • 한국초전도ㆍ저온공학회논문지
    • /
    • 제7권3호
    • /
    • pp.29-33
    • /
    • 2005
  • Critical current$(I_c)$ degradation of High $T_c$ Superconducting(HTS) tapes and AC loss under mechanical load is one of the hottest issues in HTS development and application. Mechanical load reduces the critical current of superconducting wire, and the $I_c$ degradation affects the AC loss of the wire. We measured the $I_c$ degradation and AC loss under tension and bending of Bi-2223 tapes made by 'Powder-in-Tube' technique at 77K with self-field. Also, we have studied the frequency characteristics on self-field AC loss in multi-filamentary Bi-2223/Ag tape at 77K. The measurement results and discussions on the relationship between $I_c$ degradation and AC loss are presented.

Inter- and Intra-granular Critical Current in $Bi_{1.4}Pb_{0.6}Sr_2Ca_2Cu_{3.6}O_x$ Superconducting Oxide

  • Choy, Jin-Ho;Kim, Seung-Joo;Park, J.C.;Frohlich, K.;Dordor, P.;Grenier, J.C.
    • Bulletin of the Korean Chemical Society
    • /
    • 제11권6호
    • /
    • pp.560-563
    • /
    • 1990
  • A.c. susceptibility for $Bi_{1.4}Pb_{0.6}Sr_2Ca_2Cu_{3.6}O_x$ superconductor is measured as a function of temperature at different value of a.c. magnetic field amplitude. Two transition steps are attributed to the intergranular and intragranular properties. Based on Bean's critical state model, intergranular critical current density, $J_c^{gb}$ (11 $A/cm^2$ at 77 K) and intragranular critical current density, $J_c^g (7{\times}10^3\;A/cm^2$ at 100 K) are estimated. The low values of $J_c^{gb}$and $J_c^g$ reflect a poor nature of coupling between grains and the low pinning force density of intragrain in $Bi_{1.4}Pb_{0.6}Sr_2Ca_2Cu_{3.6}O_x$ superconductor.

급속응고법을 이용한 Bi 계 고온초전도체 전류도입선 제조 (Current Leads Fabrication of High $T_c$ Bi System Superconductor Using Rapid Cooling Method)

  • 박용민;한진만;류운선;류운선
    • 한국전기전자재료학회논문지
    • /
    • 제13권3호
    • /
    • pp.254-258
    • /
    • 2000
  • Current leads of high $T_{c}$ superconductor were fabricated with Bi excess B $i_{2.2}$/S $r_{1.8}$/C $a_{1}$/C $u_{2}$/ $O_{x}$ composition by rapid cooling method. The dimensions of final samples were fixed 3 mm and 8 mm diameter with 50 mm length each To control uniform density the samples were preformed by CIP(Cold Isostatic Press) process and followed by partial or full melting process after raising up to 90$0^{\circ}C$ for 30min. Plate shaped microstructure was clearly observed adjacent to the Ag tube wall and the size of plate was about 100$\mu$m. However the severe destruction of growth orientation was shown in the inner growth part. critical temperature ( $T_{c}$) was about 53~71K after directional growth while Tc was decreased about 77~80 K before directional growth. After directional growth critical current( $I_{c}$) and critical current density( $J_{c}$) in the specimen of 8 mm diameter at 50 K were about 110 A and 280 A/c $m^2$ respectively.pectively.ely.

  • PDF

외부보강된 밀봉 상태가 다른 Bi-2223테이프의 가압 LN2하에서 임계전류의 굽힘변형률 의존성 (Bending Strain Dependence of the Critical Current in Externally-reinforced Bi-2223 Tapes with Different Hermeticity under pressurized Liquid Nitrogen)

  • 신형섭;;박정수
    • 한국전기전자재료학회논문지
    • /
    • 제20권6호
    • /
    • pp.541-545
    • /
    • 2007
  • The critical current degradation behaviors of multifilamentary Bi-2223 superconducting tapes under pressurized liquid nitrogen were investigated using a r-shaped sample holder which gives a series of bending strains to tape. Three kinds of externally-reinforced Bi-2223 tapes with different hermeticity were used as samples. The tape with the thicker reinforcement layer had a better bending strain tolerance of $I_c$, but when the bending strain was calculated at the outermost filament, the $I_c$ degradation behavior became identical. For all samples, $I_{c0}$ decreased with the increase of applied pressure, but the $I_c$ degradation behavior with bending strain at each pressure level was similar. Furthermore, after depressurization from 1 MPa to atmospheric pressure, $I_c$ was completely recovered to its initial values. When the samples were warmed up to room temperature after pressurization tests, the ballooning damage occurred at lower bending strain regions. The region where ballooning was observed was identical to the one where the significant $I_c$ degradation occurred.