• 제목/요약/키워드: counter-ion

검색결과 166건 처리시간 0.03초

Crystal Structure of Dehydrated $Rb^{+}$-Exchanged Zeolite X, $Rb_{71}Na_{21}Si_{100}Al_{92}O_{384}$

  • 이석희;김양;김덕수;Karl Seff
    • Bulletin of the Korean Chemical Society
    • /
    • 제19권1호
    • /
    • pp.98-103
    • /
    • 1998
  • The crystal structure of dehydrated $Rb^+$-exchanged zeolite X, stoichiometry $Rb_{71}Na_{21}-X\; (Rb_{71}Na_{21}Si_{100}Al_{92}O_{384})$ per unit cell, has been determined from single-crystal X-ray diffraction date gathered by counter methods. The structure was solved and refined in the cubic space group Fd3, a=25.007(3) Å at 21(1) ℃. The crystal was prepared by ion exchange in a flowing stream using a 0.05 M aqueous RbOH solution (pH=12.7). The crystal was then dehydrated at 360 ℃ and $2{\times}10^{-6}$ torr for two days. The structure was refined to the final error indices, $R_1=0.047$ and $R_2=0.040$ with 239 reflections for which I> 3σ(I). In this structure, 71 $Rb^+$ ions per unit cell are found at six different crystallographic sites and 21 $Na^+$ ions per unit cell are found at two different crystallographic sites. Four and a half $Rb^+$ ions are located at site Ⅰ, the center of the hexagonal prism. Nine $Rb^+$ ions are found at site Ⅰ' in the sodalite cavity (Rb-O=2.910(15) Å and O-Rb-O=78.1(4)°). Eighteen $Rb^+$ ions are found at site Ⅱ in the supercage (Rb-O=2.789(9) Å and O-Rb-O=92.1(4)°). Two and a half $Rb^+$ ions, which lie at site Ⅱ', are recessed ca. 2.07 Å into the sodalite cavity from their three O(2) oxygen planes (Rb-O=3.105(37) Å and O-Rb-O=80.6(5)°). Thirty-two $Rb^+$ ions are found at site Ⅲ deep in the supercage (Rb-O=2.918(12) Å and O-Rb-O=71.9(4)°), and five $Rb^+$ ions are found at site Ⅲ'. Seven $Na^+$ ions also lie at site Ⅰ. Fourteen $Na^+$ ions are found at site Ⅱ in the supercage (Na-O=2.350(19) Å and O-Na-O=117.5(6)°).

온도 영향을 고려한 RC 구조의 반 전위 및 OCP의 상관성 분석 (Relationship Analysis between Half Cell Potential and Open Circuit Potential Considering Temperature Condition)

  • 윤용식;권성준
    • 한국건설순환자원학회논문집
    • /
    • 제10권1호
    • /
    • pp.124-132
    • /
    • 2022
  • 콘크리트 내의 부식전위는 노출환경 및 배합에 따라 크게 변화한다. 본 연구에서는 피복 두께, 염화물 농도, 물-시멘트 비를 변수로 하여 RC 시편을 제조하였으며, 철근과 표면과의 전위차를 평가하는 HCP 측정을 수행하였다. 또한 매립된 철근과 상대전극을 이용하여 OCP의 측정하였다. 한천과 NaOH 수용액을 이온교환물질로, Hg/HgO를 기준전극으로 사용하여 OCP를 측정하였는데, HCP에 비하여 온도에 더욱 민감하게 작용하였다. 영향 인자 중 존치 기간 및 염화물 농도는 피복 두께 및 물-시멘트 비보다 상대적으로 큰 영향을 가지고 있었다. 또한 전체 측정된 HCP 및 OCP는 피복 두께 및 물-시멘트와 뚜렷한 선형관계를 나타내었다. 다중회귀분석을 통하여 HCP와 OCP의 관계를 정량화하였으며 온도를 고려하여 개선된 상관성을 도출하였다.

환자에게 주입된 18F-FDG 의한 선량 평가에 대한 연구 (A Study on Dose Assessment by 18F-FDG injected into Patients)

  • 김창주;김장오;정근우;신지혜;이지은;전찬희;민병인
    • 한국방사선학회논문지
    • /
    • 제14권4호
    • /
    • pp.467-475
    • /
    • 2020
  • 본 연구는 PET 검사 중 방사성의약품인 18F-FDG에 대한 선량을 평가하여 환자와 보호자의 방사선에 대한 불안감을 완화하고, 의료기관 인력 및 공간 확보 문제, 건강검진으로 인한 무분별한 검사 진행을 최소화하는 데 그 목적이 있다. 선량평가는 방사선조직가중치 중 높은 조직 세 부위인 경부(갑상선), 흉부(심장), 하복부(생식선) 위치에 열형광선량계(TLD)와 전자개인선량계(EPD)를 이용하여 측정하였다. 또한, GM 계수기와 전리함을 이용하여 공간선량률과 소변에서의 방사능을 측정하였다. 그 결과는 다음과 같다. 첫째, 개인선량계인 TLD는 경부에서 0.0425±0.0277 mSv, 흉부에서 0.0485±0.0386 mSv, 하복부에서 0.0485±0.0436 mSv 측정되었고 방사선 민감도에 따른 심부선량 차이는 거의 없었다. EPD는 경부 위치에서 직후 0.942±0.141 mSv/h, 120분 후 0.192±0.031 mSv/h로 측정되었다. 흉부 위치에서 직후 0.516±0.085 mSv/h, 120분 후 0.128±0.040 mSv/h로 측정되었다. 하복부 위치에서 직후 0.468±0.091 mSv/h, 120분 후 0.105±0.021 mSv/h로 측정되었다. GM 계수기에서 공간선량률은 직후 0.041±0.005 mSv/h, 120분 후 0.014±0.002 mSv/h로 측정되었다. 전리함을 이용한 소변 내 방사능은 60분 후 0.113±0.24 MBq/cc, 120분 후 0.063±0.13 MBq/cc로 측정되었다. 이러한 결과로 볼 때 18F-FDG를 투여하고 PET 검사가 끝나는 2시간 후 선량 재평가를 하고 귀가 시점을 정하도록 해야 하며 보호자와의 접촉도 피해야 한다. 또한, 환자와 보호자에게 충분한 설명과 함께 피폭선량 예상 값을 제공하여 무분별한 검사를 지양해야 하도록 할 필요가 있을 것으로 판단된다. 본 연구에서 실측 실험한 데이터를 통해 환자와 가족들이 방사선에 대한 불안감을 해소하기를 바라며, 방사선 종사자의 피폭관리 시스템과 제도적 개선을 통해 의료방사선 발전에 힘이 되리라 기대한다.

중성자 모니터링을 위한 전도성 10B 박막 개발 (The development of conductive 10B thin film for neutron monitoring)

  • 임창휘;김종열;이수현;정용주;최영현;백철하;문명국
    • Journal of Radiation Protection and Research
    • /
    • 제39권4호
    • /
    • pp.199-205
    • /
    • 2014
  • 중성자 검출분야에서$^3He$는 높은 중성자 검출효율 때문에 아주 많이 사용되고 있다. 하지만 2009년 초반부터 발생하고 있는 전세계적인 $^3He$의 품귀현상으로 인하여 가격이 급등하고 수급이 어려워졌기 때문에 대체 중성자 검출물질에 대한 필요성이 높아졌다. 그러므로 중성자 검출물질로 사용될 수는 있지만 $^3He$에 비해 반응효율이 낮아 중성자 검출용으로 주로 사용되지 않던 물질들을 사용하여 검출기를 제작하는 연구가 다시 활발하게 진행되고 있다. $BF_3$, $^6Li$, $^{10}B$, $Gd_2O_2S$ 등과 같은 $^3He$ 대체 물질들 중 하나인 $^{10}B$은 손쉬운 감마선 구별, 무독성, 낮은 가격 등과 같은 여러 장점으로 인하여 여러 연구그룹에서 연구되고 있다. $^{10}B$ 박막을 이용한 중성자 검출은 중성자와 반응하여 발생되는 2차 방사선을 측정하여 간접적으로 중성자를 측정하는 검출기법이다. 반응을 통해 생성된 알파입자의 비정은 고체 내에서 아주 짧기 때문에 $^{10}B$ 층은 박막 형태로 얇게 제작해야 한다. 그러므로 중성자와 박막의 반응을 통해 발생되는 알파입자의 검출효율을 증가시키기 위해서는 $^{10}B$ 박막의 두께를 얇게 제작하는 것이 중요하다. 하지만 박막의 두께를 얇게 제작하는 것은 중성자와 반응하여 생성되는 알파입자의 수집효율을 증가시키는 장점이 있지만 또한 중성자와 반응할 단면적을 감소시키는 단점이 있다. 본 논문에서는 리튬이온전지에 사용되는 초박막 극판 제조 기술을 이용하여 중성자 검출을 위한 대략 $60{\mu}m$ 두께의 얇은 $^{10}B$ 박막을 제작하였다. 그리고 전도성, 분포, 점착력, 유연성와 같은 간단한 물리적 실험을 통해 제작된 $^{10}B$ 박막의 물성을 확인하였다. 또한, 제작된 $^{10}B$ 박막을 사용하여 중성자 모니터링을 위한 비례계수기 제작하고 이를 이용하여 한국원자력연구원의 중성자 조사시설의 중성자 파고 스펙트럼을 측정하였다. 또한, 중성자 검출효율을 증가시킬 수 있는 방법 중 하나인 다층 박막을 이용한 중성자 측정 방법을 이용하여 박막 층수에 따른 중성자 검출효율의 변화를 몬테칼로 전산모사 기법을 이용하여 계산하였고 실험을 통해 박막층의 증가에 따른 신호변화를 측정하였다.

혈중(血中) Thyroxine-결합(結合)-globulin(TBG)의 $T_4$ 결합능(結合能) 측정(測定)에 관한 고찰(考察) (Estimation of the $T_4$ Binding Capacity of Serum Thyroxine Binding Globulin)

  • 이경자;고창순;이문호
    • 대한핵의학회지
    • /
    • 제7권2호
    • /
    • pp.1-12
    • /
    • 1973
  • The most commonly used methods for determining thyroxine binding globulin(TBG) concentration as the total thyroxine-binding capacity utilize electrophoretic seperation of serum. Although technically simple, the electrophoretic method is time consuming and is limited in the number of samples which can be run in a single assay. The author presented a single $T_4$ load ion exchange resin method as an approach to simplify the technique as with clinical practicability and results were analyzed. For construction of the standard curves, serum mixtures were diluted with barbital buffer.which effectively blocked $T_4$-binding to TBPA. For each serum dilution, a constant amount of $T_4-^{125}I$ and increments of unlabelled $T_4$ were added. After incubation in water bath, resin beads were dispensed to the samples which binded all $T_4$ not bound to TBG. The radioactivity in the supernatant was counted in the gamma scintillation counter. Each standard curve was plotted from the percent counts in the supernatant and total $T_4$ in each tube. Unknown samples were diluted to 1:40 and ran at a single $T_4$ loading concentration, and the TBG capacity of the samples was able to be read on the standard isobars. The following results were obtained. 1) Mean and standard deviation for TBG capacity in normal population was $28.6{\pm}5.09{\mu}g\;T_4/100ml$. 2) $24.9{\pm}3.87{\mu}g\;T_4/100ml$ in hyperthyroidism showed low TBG capacity comparing to normal population.(p<0.025) 3) $31.0{\pm}2.40{\mu}g\;T_4/100ml$ in hypothyroidism showed high TBG capacity tendency comparing to normal population. 4) Reversed correlationship existed between TBG capacity and $T_3$ resin uptake(r=-0.624), TBG capacity and serum $T_4$ value (r=-0.859), and TBG capacity and free thyroxine index(r=-0.623). The author assumes that this method of assay is considerably simpler in instrumentation and technique than any other assays traditionally being used, and seems to be more practical for routine clinical laboratory use.

  • PDF

비정질 $WO_3$ 박막의 광특성 및 일렉트로크로미즘에 관한 연구 (A Study on the Optical Properties and Electrochromism of Amorphous $WO_3$ Thin Films)

  • 박승희;정주용;조봉희;김영호
    • 한국재료학회지
    • /
    • 제3권6호
    • /
    • pp.632-637
    • /
    • 1993
  • 3000$\AA$~6000$\AA$의 두께로 진공 증착한 $WO_3$ 박막의 광특성 및 일렉트로크로미즘에 대하여 연구하였다. 증착된 $WO_3$ 박막은 모두 무색 투명 하였으며 X-선회절 분석결과 비정질 상태로 밝혀졌으며, 비정질 $WO_3$ 박막의 굴절율은 가시광선 영격에서 1.9-2.1로, 광에너지 gap은 3.25eV로 나타났다. ITO투명전극/$WO_3$박막/$LiCIO_4$ ~propylene carbonate/백금 대향전극 구조를 갖는 일렉트로크로믹소자를 구성하여 일렉트로크로믹 특성을 조사하였다. $WO_3$ 박막의 coloration/과 bleaching현상은 $LiCIO_{4}$~propylene carbonate유기전해질과 ITO투명전극으로 부터 $Li^{+}$이온과 전자의 이중주입에 의하여 청색으로 나타났으며, 가역적으로 전기 화학적인 산화반응에 의하여 bleaching현상이 일어났다. Coloration과 bleaching현상, 광학밀도, 구동전압 및 응답속도 등의 일렉트로크로믹 특성은 $WO_3$ 박막의 증착조건, 전해액 농도, 투명전극의 sheet resistance 인가전압에 크게 의존하는 것으로 밝혀졌다.

  • PDF

순수 양이온성(DTAB, TTAB, CTAB), 비이온성(Tween-20, Tween-40, Tween-80) 및 이들 혼합 계면활성제의 미셀화에 대한 열역학적 연구 (Thermodynamics on the Micellization of Pure Cationic(DTAB, TTAB, CTAB), Nonionic(Tween-20, Tween-40, Tween-80), and Their Mixed Surfactant Systems)

  • 이남민;이병환
    • 한국응용과학기술학회지
    • /
    • 제30권4호
    • /
    • pp.679-687
    • /
    • 2013
  • 4-클로로벤조산의 가용화현상을 이용하여 순수양이온성 계면활성제(DTAB, TTAB, CTAB), 비이온성 계면활성제(Tween-20, Tween-40, Tween-80) 및 이들 혼합계면활성제(TTAB/Tween-20, TTAB/Tween-40, TTAB/Tween-80)의 임계미셀농도(CMC)값과 반대이온 결합상수값(B)를 온도 284 K에서 312 K까지 변화를 주면서 UV/Vis 분광광도법과 전도도법으로 측정하였다. 온도에 따른 CMC와 B값의 변화를 측정하여 미셀화현상에 대한 여러 가지 열역학 함수값(${\Delta}G^o{_m}$, ${\Delta}H^o{_m}$, 및 ${\Delta}S^o{_m}$)을 계산하고 분석 하였다. 그 결과 측정범위 내에서 ${\Delta}G^o{_m}$값은 모두 음의 값을 나타내었다. 그러나 ${\Delta}H^o{_m}$${\Delta}S^o{_m}$값은 계면활성제의 종류와 계면활성제분자에서 탄소사슬의 길이에 따라 양의 값 혹은 음의 값을 나타내었다.

리튬이차전지 음극재용 나노입자 Li4Ti5O12의 전기화학적 연구 (Electrochemical Study of Nanoparticle Li4Ti5O12 as Negative Electrode Material for Lithium Secondary Battery)

  • 오미현;김한주;김영재;손원근;임기조;박수길
    • 전기화학회지
    • /
    • 제9권1호
    • /
    • pp.1-5
    • /
    • 2006
  • 리튬이온전지용 음극 활물질로 스피넬 구조의 리튬 티탄산화물$(Li_4Ti_5O_{12})$이 졸겔법과 HEBM법으로 제조되었다. 제조된 $Li_4Ti_5O_{12}$의 입자크기 및 결정구조를 확인하기 위하여 X-선 회절분석(XRD), 주사전자현미경(SEM) 및 평균입자분석(PSA)을 수행한 결과 100nm의 균일한 크기의 입자를 확인하였다. 작업전극으로 $Li_4Ti_5O_{12}$를 사용하고 기준전극과 상대전극으로 lithium 호일을 사용하여 전기화학적인 삼상전극 셀을 구성하여 전기화학적인 특성 평가를 한 결과 $1.0\sim2.5V$의 전압 범위에서 고율 충 방전 성능과 0.2C에서 173mAh/g의 용량 특성을 나타내었다. $Li_4Ti_5O_{12}$은 리튬의 삽입과 탈리가 일어나는 동안 구조적인 안정성을 보여주고 있다.

수용액중(水溶液中)에서의 Kaolinite 입자(粒子)의 전기화학적(電氣化學的) 성질(性質) (Electrochemical Properties of Kaolinite in Aqueous Suspension)

  • 임형식
    • 한국토양비료학회지
    • /
    • 제16권4호
    • /
    • pp.318-324
    • /
    • 1983
  • 이온흡착, 전위차적정, 전기이동법 등을 이용 하여 kaolinite 현탄액의 전기 화학적 성질을 연구하였다. 0.001M 또는 0.1M NaCl 용액중에서 kaolinite로부터 용해되어 나온 알루미늄 이온이 $Na^+$$Cl^-$과 같이 지시이온으로서 kaolinite 표면에 흡착되는 것을 고려할 때 kaolinite는 pH independent + 및 -전하와 pH dependent + 및 -전하를 모두 가지고 있었다. 증류수와 0.001M NaCl 용액중에서 kaolinite 입자의 전기이동은 전기 이동셀(cell)에서 측정이 시작된 후 시간경과(전기이동 측정시간)에 관계없이 일정한 이동성을 나타냈으나 0.1M NaCl 용액중에서 kaolinite 입자는 등전점 (pH 4.7) 이상에서는 측정시간이 경과함에 따라 전하가 -에서 +로 변화하였다. 즉 최초 10초 동안에는 -전하를 가지며 그 후에는 +전하를 띠면서 전기이동 속도가 단계적으로 증가하게 되는데 약 10분 후에는 일정하게 되었다. 이것은 아마도 제일 바깥쪽 Octahedral layer 표면의 aluminol group의 부분들이 높은 이온 강도의 전해질 용액중에서 분해되어 복잡한 전기이중층(electric double layer)을 이루고 이것이 전기장 내에서 이동할 때 표면으로부터 counter이온들이 점차 떨어져 나가는 과정에서 전하(net charge)의 변화가 생기는 것으로 생각된다.

  • PDF

BF3LiMA기반 자기-도핑형 겔 고분자 전해질의 전기화학적 특성에 미치는 리튬이온 농도의 영향 (Effect of Lithium Ion Concentration on Electrochemical Properties of BF3LiMA-based Self-doping Gel Polymer Electrolytes)

  • 강완철;류상욱
    • 전기화학회지
    • /
    • 제13권3호
    • /
    • pp.211-216
    • /
    • 2010
  • 전해액 상용성의 boron trifluoride lithium methacrylate ($BF_3$LiMA)를 기본으로 하는 겔 고분자 전해질 (gel polymer electrolytes, GPE)에서 $BF_3$LiMA의 농도가 이온전도도, 전기화학적 안정성에 미치는 영향을 AC impedance 측정법과 linear sweep voltammetry (LSV)를 통하여 평가하였다. 그 결과 $BF_3$LiMA가 4wt% (고분자함량 21 wt%)일 때, 상온 이온전도도가 $5.3{\times}10^{-4}Scm^{-1}$로서 가장 높게 관찰되었으며 4 wt% 전후로 다시 감소하였다. $BF_3$LiMA 기반의 GPE는 음이온이 고정되어 있는 자기-도핑형 계열로서 우수한 전기화학적 안정성을 확인하였다. 한편 $BF_3$LiMA 기반 GPE는 리튬금속과 비교적 불안정한 계면반응성을 보여주었지만 흑연/GPE/흑연, LCO/GPE/LCO에서는 높은 계면안정성을 형성하였다. 따라서 $BF_3$LiMA 기반의 GPE를 통하여 높은 상온 이온전도도와 전기화학적 안정성 및 흑연과 LCO 양극산화물에 대한 우수한 계면특성을 확보할 수 있었다.