650 ℃의 10%O2+10%CO2 가스 환경에서 2.25Cr-1Mo강의 산화특성에 미치는 KCl(s)과 K2SO4(s)의 영향 (Effect of KCl(s) and K2SO4(s) on Oxidation Characteristics of the 2.25Cr-1Mo Steel in 10%O2+10%CO2 Gas Environment at 650 ℃)

  • 정광후;김성종
    • Corrosion Science and Technology
    • /
    • 제19권1호
    • /
    • pp.43-50
    • /
    • 2020
  • In this study, the effects of KCl(s) and K2SO4(s) on the oxidation characteristics of 2.25Cr-1Mo steel were investigated for 500 h in 10O2 + 10CO2 (vol%) gas environmen at 650 ℃. Oxidation kinetics were characterized by weight gain, oxide layer thickness, and fitted models for the experiment data were proposed. The fitted models presented considerable agreement with the experimental data. The oxide layer was analyzed using the scanning electron microscope, optical microscope, and energy dispersive X-ray spectroscopy. The oxidation kinetics of 2.25Cr-1Mo steel with KCl and K2SO4 coatings showed significantly different oxidation kinetics. KCl accelerated the oxidation rate very much and had linear oxidation behavior. In contrast, K2SO4 had no significant effect, which had parabolic kinetics. The oxide layer was commonly composed of Fe2O3, Fe3O4, and FeCr2O4 spinel. KCl strongly accelerated the oxidation rates of 2.25Cr-1Mo steel in the high-temperature oxidation environment. Conversely, K2SO4 had little effect on the oxidation rates.

순티타늄판의 Nd:YAG 레이저 용접성에 관한 연구(I) - 실드 조건에 따른 용접특성 - (A Study of Weldability for Pure Titanium by Nd:YAG Laser(I) - Weld Properties with Shield Conditions -)

  • 김종도;곽명섭;김창수
    • Journal of Welding and Joining
    • /
    • 제27권5호
    • /
    • pp.55-61
    • /
    • 2009
  • Pure titanium and its alloys have good formability, excellent corrosion resistance and high strength to weight ratios. Therefore, it has been using to heat exchangers, offshore plants, sports equipments, and etc. As broad as its application fields, it also increases welding locations. Conventional GTAW and GMAW are very popular welding methods of titanium, but it has a high heat input and wide HAZ. It has a possibility of inducing Stress Corrosion Cracking. So, laser welding method has been using to get reliable welds by reducing heat input. Weld beads change its color to silver, gold, brown, blue, and gray by shied conditions. And the closer to gray, the more oxidize, nitride and embrittlement. The most effective atom to embrittlement was nitrogen. And shield gas flow was not so effective over the constant flow rates. In this study, weld properties of the pure titanium were investigated by pulsed & CW Nd:YAG lasers and evaluated by various shield conditions. And It is observed that nitrogen is more effective to oxidation and embrittlement of titanium compared with oxygen by oxygen and nitrogen quantitative analysis.

Etchant for Dissolving Thin Layer of Ag-Cu-Au Alloy

  • Utaka, Kojun;Komatsu, Toshio;Nagano, Hiroo
    • Corrosion Science and Technology
    • /
    • 제6권6호
    • /
    • pp.304-307
    • /
    • 2007
  • As to the reflection electrode of LCD (liquid crystal displays), silver-copper-gold alloy (hereafter, it is called as ACA (Ag98%, Cu1%, Au1%)) is an effective material of which weathering resistance can be improved more compared with pure silver. However, there is a problem that gold remains on the substrate as residues when ACA is etched in cerium ammonium nitrate solution or phosphoric acid. Gold can not be etched in these etchants as readily as the other two alloying elements. Gold residue has actually been removed physically by brushing etc. This procedure causes damage to the display elements. Another etchant of iodine/potassium iodide generally known as one of the gold etchants can not give precise etch pattern because of remarkable difference in etching rates among silver, copper and gold. The purpose of this research is to obtain a practical etchant for ACA alloy. The results are as follows. The cyanogen complex salt of gold generates when cyanide is used as the etchant, in which gold dissolves considerably. Oxygen reduction is important as the cathodic reaction in the dissolution of gold. A new etchant of sodium cyanide / potassium ferricyanide whose cathodic reduction is stronger than oxygen, can give precise etch patterns in ACA alloy swiftly at room temperature.

Zr 피복관의 ISCC 특성에 미치는 미세조직 및 첨가원소의 영향 (Effect of Microstructure and Alloying Element on the ISCC Characteristics of Zr Cladding)

  • 박상윤;최병권;이명호;김준환;정용환
    • 열처리공학회지
    • /
    • 제18권3호
    • /
    • pp.164-171
    • /
    • 2005
  • Iodine-Induced Stress Corrosion Cracking (ISCC) properties of Zircaloy-4 and HANA4 developed in KAERI for the high burn-up nuclear fuel cladding were evaluated. To confirm the effect of final heat treatment on ISCC resistance of Zr-alloy, stress relieved and recrystallized specimens were prepared and tested. With the pre-cracked specimen at internal surface, ISCC crack propagation rates and threshold stress intensity factor ($K_{ISCC}$) based on the fracture mechanics were measured by internal pressurization test at $350^{\circ}C$ in iodine environment. $K_{ISCC}$ of Zircaloy-4 and HANA4 cladding were $3.3MPa{\cdot}m^{1/2}$ and $4.4MPa{\cdot}m^{1/2}$, respectively. Pitting corrosion at the crack surface was observed and it seemed that TG crack propagation was derived from the pitting.

Investigation on Mechanical Property and Adhesion of Oxide Films Formed on Ni and Ni-Co Alloy in Room and High Temperature Environments

  • Oka, Yoshinori I.;Watanabe, Hisanobu
    • Corrosion Science and Technology
    • /
    • 제7권3호
    • /
    • pp.145-151
    • /
    • 2008
  • Material degradation such as high temperature oxidation of metallic material is a severe problem in energy generation systems or manufacturing industries. The metallic materials are oxidized to form oxide films in high temperature environments. The oxide films act as diffusion barriers of oxygen and metal ions and thereafter decrease oxidation rates of metals. The metal oxidation is, however, accelerated by mechanical fracture and spalling of the oxide films caused by thermal stresses by repetition of temperature change, vibration and by the impact of solid particles. It is therefore very important to investigate mechanical properties and adhesion of oxide films in high temperature environments, as well as the properties in a room temperature environment. The oxidation tests were conducted for Ni and Ni-Co alloy under high temperature corrosive environments. The hardness distributions against the indentation depth from the top surface were examined at room temperature. Dynamic indentation tests were performed on Ni oxide films formed on Ni surfaces at room and high temperature to observe fractures or cracks generated around impact craters. As a result, it was found that the mechanical property as hardness of the oxide films were different between Ni and Ni-Co alloy, and between room and high temperatures, and that the adhesion of Ni oxide films was relatively stronger than that of Co oxide films.

플랜트 하부의 강파일 인접 토양의 부식성 평가 (The Corrosivity Evaluations on Soil Surrounding the Buried Steel Piles under Manufacturing Plants)

  • 정성원;박경완;전재영
    • 플랜트 저널
    • /
    • 제12권1호
    • /
    • pp.37-43
    • /
    • 2016
  • 플랜트 하부 강파일 기초 주변 토양의 부식성을 평가하기 위해서 현장조사, 현장 보링작업을 통한 시료 채취 및 실험실 분석을 거친 결과를 검토하였다. 토양 분석 결과 강관파일이 타설된 토양은 여러 개의 특성이 다른 토양층으로 구성되어 있었으며, 각 지층의 화학적, 물리적 성질이 다르므로 강관파일의 타설깊이에 따른 부식성의 차이가 발생할 것을 예상할 수 있었다. 분석 결과를 토대로 정성적인 부식성 평가, 평균부식속도 및 최대부식속도를 예측한 결과, 일부 지층에서는 일반적으로 강관파일 설계시 적용되는 부식속도인 0.01-0.02mm/y 이상의 평균부식속도를 보이고 있었다 (0.33mm/y).

  • PDF

선원항 모델을 사용한 저준위 방사성폐기물 처분장의 보수적인 안전성고찰 (A Conservative Safety Study on Low-Level Radioactive Waste Repository Using Radionuclide Release Source Term Model)

  • Kim, Chang-Lak;Lee, Myung-Chan;Cho, Chan-Hee
    • Nuclear Engineering and Technology
    • /
    • 제25권1호
    • /
    • pp.63-70
    • /
    • 1993
  • 암반동굴 타입의 저준위방사성폐기물 처분장의 보수적인 안전성평가를 처분장 선원항 REPS 모델을 사용하여 수행하였다. 신뢰할만한 핵종별 침출율 예측을 위하여 REPS 모델에서 콘크리트 구조물의 열하시간, 부석의 형태와 부식율. 드럼표면의 부식면적 비, 그리고 핵종의 특성등이 고려되고 있다. 예비평가의 결과로 Cs-137, Ni-63, Sr-90등이 주요한 핵종임을 알 수 있다. 파라메타의 불확실성과 민감도분석을 위하여 라틴하이퍼큐브 샘플링과 Rank Correlation 기법이 사용되었다. 침입자 시나리오를 적용하였을 경우의 예상 피폭선량도 허용치 이하임과 처분장의 환경영향평가에 있어서 비교적 불확실성이 적은 Near Field의 중요성에 대한 인식이 새롭게 강조되어야 할 필요가 있음을 알 수 있었다.

  • PDF

Using Coffee-Derived Hard Carbon as a Cost-Effective and Eco-Friendly Anode Material for Li-Ion Batteries

  • Hong, Sung Joo;Kim, Seong Su;Nam, Seunghoon
    • Corrosion Science and Technology
    • /
    • 제20권1호
    • /
    • pp.15-21
    • /
    • 2021
  • Through a simple filtration process, followed by carbonization within a reductive environment, coffee waste grounds can be transformed into a non-porous hard carbon for use in multiple contexts. This resulting coffee-waste carbon has been evaluated as an eco-friendly and cost-effective replacement for conventional graphite. When compared with different types of carbon, our study found that the coffee-waste carbon fell into the category of hard carbon, as verified from the galvanostatic charge/discharge profiles. The coffee-waste carbon showed a superior rate capability when compared to that of graphite, while compromising smaller capacity at low C rates. During electrochemical reactions, it was also found that the coffee-waste carbon is well exposed to electrolytes, and its disordered characteristic is advantageous for ionic transport which leads to the low tortuosity of Li ions. Finally, the high irreversible capacity (low initial Coulombic efficiency) of the coffee-waste carbon, which if also often observed in amorphous carbon, can be adequately resolved through a solution-based prelithiation process, thereby proving that the coffee-waste carbon material is quite suitable for commercial use as an anode material for quickly-chargeable electrodes.

Fe-Cr합금의 공식저항성 평가를 위하여 다양한 규격(KS D 0238, ASTM G 61, ISO 17475)에 따라 실시한 동전위 분극 시험과 임계공식온도 측정시험 (Evaluation on Resistance to Pitting Corrosion of Fe-Cr Alloys via Measurement of the Critical Pitting Temperature (CPT) and Potentiodynamic Polarization According to KS D 0238 (wet, dry), ASTM G 61 and ISO 17475 Standards)

  • 강수연;이재봉;김영호
    • 대한금속재료학회지
    • /
    • 제47권10호
    • /
    • pp.635-643
    • /
    • 2009
  • The resistance to pitting corrosion of Fe-Cr alloys was evaluated by performing potentiodynamic polarization and critical pitting temperature (CPT) tests. For the potentiodynamic polarization tests, various standards were applied, i.e., KS D 0238 (wet, dry), ASTM G 61, and ISO 17475, showing different potentiodynamic polarization results including pitting potentials. ASTM G 61 and ISO 17475 standards presented relatively higher pitting potential while KS D 0238 (dry) indicated lower values than the others. Effects of surface roughness, scan rates, and exposure time to air before tests were also investigated. CPT tests were performed under two different applied potentials, 300 m$V_{SCE}$ and 200 m$V_{SCE}$ in deaerated 1 M NaCl aqueous solution. CPT values and the polarization test results showed a linear relationship.

Effect of Water Impingement Conditions on the Degradation of Epoxy Coatings in Tap Water

  • Kim, D.H.;Yoo, Y.R.;Kim, Y.S.
    • Corrosion Science and Technology
    • /
    • 제21권5호
    • /
    • pp.327-339
    • /
    • 2022
  • The water-jet technique started by Bridgman can cut metal and alloys without harmful gas and fume. However, while this technique is convenient to cut metals and alloys, in the case of coated pipe, water jet induces the degradation of coatings on the pipes, and may facilitate structural failure, leakage, and loss of products. While there are many reports on the effect of water jet on cut metals and the damage of metallic materials, research on the effect of water impingement on the epoxy coatings has been little studied. In this work, we therefore control the velocity of water jet, distance between nozzle and specimen, and water temperature, and discuss the effect of water impingement on the epoxy coatings. Increasing water velocity and water temperature and reducing nozzle distance increased the degradation rates of three epoxy coatings were increased. Among three test parameters - water velocity, nozzle distance and water temperature, water temperature was relatively effective to increase the degradation rate of epoxy coatings.