Wear Debris Analysis using the Color Pattern Recognition

  • Chang, Rae-Hyuk;Grigoriev, A.Y.;Yoon, Eui-Sung;Kong, Hosung;Kang, Ki-Hong
    • KSTLE International Journal
    • /
    • 제1권1호
    • /
    • pp.34-42
    • /
    • 2000
  • A method and results of classification of four different metallic wear debris were presented by using their color features. The color image of wear debris was used far the initial data, and the color properties of the debris were specified by HSI color model. Particles were characterized by a set of statistical features derived from the distribution of HSI color model components. The initial feature set was optimized by a principal component analysis, and multidimensional scaling procedure was used fer the definition of a classification plane. It was found that five features, which include mean values of H and S, median S, skewness of distribution of S and I, allow to distinguish copper based alloys, red and dark iron oxides and steel particles. In this work, a method of probabilistic decision-making of class label assignment was proposed, which was based on the analysis of debris-coordinates distribution in the classification plane. The obtained results demonstrated a good availability for the automated wear particle analysis.

  • PDF

부적합한 금관이 치아주위조직에 미치는 영향에 관한 실험적 연구 (Effects of Improper Metal Crown to Period Onium in Experimental the Dogs)

  • 조근옥
    • 대한치과의사협회지
    • /
    • 제11권5호
    • /
    • pp.353-358
    • /
    • 1973
  • The purpose of this study was to determine the gingival response to the various restorations for 3 weeks, 5 weeks and 8 weeks respectively after they had been inserted in 42 tooth of 5dogs. The histopathological observation was also performed to evaluate the effect of the variuos restorations on gingival tissue. They inclued gold, copper and nickel-chrome alloy. The following findings were obtained. 1. The gingivae adjacent to the well adapted and polished restorations and their margins with a level of gingival crest were grossly and histopathologically found no specific changes. 2. The gingive adjacent to the ill fitting and unpolished restorations and their margins with subgingival extension of 1 to 1.5mm were not grossly found any changes but hitopathologically, the inflammatory changes. 3. Thee wee no obvious difference in gingival response among the various alloys in histopathological observation.

  • PDF

Yield function of the orthotropic material considering the crystallographic texture

  • Erisov, Yaroslav A.;Grechnikov, Fedor V.;Surudin, Sergei V.
    • Structural Engineering and Mechanics
    • /
    • 제58권4호
    • /
    • pp.677-687
    • /
    • 2016
  • On the basis of the energy approach it is reported a development of the yield function and the constitutive equations for the orthotropic material with consideration of the crystal lattice constants and parameters of the crystallographic texture for the general stress state. For practical use in sheet metal forming analysis it is considered different loading scenarios: plane stress and plane strain states. Using the proposed yield function, the influence of single ideal components on the shape of yield surface was analyzed. The six texture components investigated here were cube, Goss, copper, brass, S and rotated cube, as these components are typically observed in rolled sheets from FCC alloys.

Taguchi법에 의한 방전가공의 공정변수 최적화 (Optimization of Process Parameters for EDM using Taguchi Design)

  • 최만성
    • 반도체디스플레이기술학회지
    • /
    • 제14권4호
    • /
    • pp.78-83
    • /
    • 2015
  • The method of electrical discharge machining (EDM), one of the processing methods based on non-traditional manufacturing procedures, is gaining increased popularity, since it does not require cutting tools and allows machining involving hard, brittle, thin and complex geometry. Modern ED machinery is capable of machining geometrically complex or hard material components, that are precise and difficult-to-machine such as heat treated tool steels, composites, super alloys, ceramics, etc. This paper reports the results of an experimental investigation by Taguchi method carried out to study the effects of machining parameters on material surface roughness in electric discharge machining of SM45C. The work material was ED machined with graphite and copper electrodes by varying the pulsed current, voltage and pulse time. Investigations indicate that the surface roughness is strongly depend on pulsed current.

순간접전기전력법에 의한 용융 Cd중의 Zn과 Cu, Ag, In, Bi, Pb 및 Sn와의 상위작용 파라미터 (Thermodynamic interaction parameter between Zn and Cu, Ag, In, Bi, Pb, Sn in Dilute cadmium alloy by Touch Instant electro-motive force method)

  • 김대룡;윤겸하
    • 한국표면공학회지
    • /
    • 제15권4호
    • /
    • pp.192-207
    • /
    • 1982
  • A study has been made of the interaction parameters of Zn other elements in dilute solutesd solution of molten cadmium alloys over the temperature range of 450 to 570$^{\circ}C$. The experi-mental measurementss were made in a touch instant cell using a fusedd Licl-KCl electrolyte. The activity of zinc in binary and ternary solutions sexhibiteds a strong positive deviation from Raoult's law. The addition of silver, indium or lead increased the activity of zinc whereas addition of copper, bismuth or tin decreased the zinc activity slightly. The results for all the metallic solutions showed a linear dependence of reciprocal of ab-solute temperature over the experimental range. The interaction parameters obtained are as follows.

  • PDF

Ag925의 전기화학적 특성에 미치는 네오디뮴 함량의 영향 (Effect of Neodymium concentration on electrochemical properties of 925 silver)

  • 신병현;정승진;정원섭
    • 한국표면공학회지
    • /
    • 제54권2호
    • /
    • pp.71-76
    • /
    • 2021
  • Ag925, silver with added copper, is popular alloy due to its low price. However, it has a difficult to use because of the low corrosion resistance. In various alloys, neodymium (Nd) works as an element to improve corrosion resistance by reacting with interstitial elements in the alloy. When 1.5 wt. % Neodymium was added to Ag925, the potential on the activated polarization in a potentiodynamic polarization test was increased from -0.15 V to -0.05 V. Ag925 with added neodymium showed the passivation after activation polarization. But When the potential increased around 50 mV, the current density is increased to 3 × 10-3. Ag925 with the 1.5 wt. % Nd had the low corrosion rate.

Titanium Ions Released from Oral Casting Alloys May Contribute to the Symptom of Burning Mouth Syndrome

  • Park, Yang Mi;Kim, Kyung-Hee;Lee, Sunhee;Jeon, Hye-Mi;Heo, Jun-Young;Ahn, Yong-Woo;Ok, Soo-Min;Jeong, Sung-Hee
    • Journal of Oral Medicine and Pain
    • /
    • 제42권4호
    • /
    • pp.102-108
    • /
    • 2017
  • Purpose: Many metal ions released from dental casting alloys have been reported to influence the intraoral symptoms of oral lichen planus (OLP) and burning mouth syndrome (BMS). The aim of this study was to investigate the relationship between salivary metal ion levels and the prosthetic duration as well as to evaluate the time-dependent morbid effects of metal ions in OLP and BMS patients. Methods: Three study groups consist of the following subjects respectively: 17 OLP patients, 12 BMS patients, and 12 patients without oral symptoms. The salivary concentrations of 13 metal ions (copper, cobalt, zinc, chromium, nickel, aluminum, silver, iron, titanium [Ti], platinum, tin, palladium, and gold) were measured by Laser Ablation Microprobe Inductively coupled Plasma Mass Spectrometry. Results: The Ti ions had statistically significant differences among the groups with a prosthetic duration of less than 5 years. There were no significant differences between all ion levels among the groups wearing dental cast alloys for over 5 years. In the BMS group, the level of Ti ions in patients with prosthetic restorations less than 5 years old were significantly high (p<0.05). Conclusions: In the BMS group, 3-60 months during which salivary Ti levels were higher were matched with the duration of burning symptoms ($15.6{\pm}17.1months$). Furthermore, Ti ions were statistically high in the oral cavity of BMS patients fitted with dental casting alloys for 5 years. These results suggest that Ti ions released from dental implants and oral prostheses could attribute to burning sensation of BMS.

수소저항합금을 이용한 150ℓ급 수소저장용기의 제작과 특성에 관한 연구 (Fabrication and Characteristics of 150ℓ Class Hydrogen Tank Using Hydrogen Storage Alloy)

  • 강길구;강세선;권호영;이임렬
    • 한국수소및신에너지학회논문집
    • /
    • 제13권2호
    • /
    • pp.110-118
    • /
    • 2002
  • The hydrogen storage vessel having a good heat conductivity along with a simple structure and a low cost for these alloys was designed and manufactured, and then its characteristic properties were studied in this study. The various parts in hydrogen storage vessel consisted of copper pipes and stainless steel of 250 mesh reached the setting temperature after 4~5 minutes, which indicated that storage vessel had a good heat conductivity that was required in application. And also the storage vessel had a good property of hydrogen transport considering that the reaction time between hydrogen and rare-earth metal alloys in storage vessel was found to be within 10 min at $18^{\circ}C$ under 10 atmospheric pressure. It showed that the average capacity of discharged hydrogen volume was found to be $120{\ell}$ for $MmNi_{4.5}Mn_{0.5}$ under discharging conditions of $40^{\circ}C{\sim}80^{\circ}C$ at a constant flow rate of $5{\ell}$/min. It was found that the optimum discharging temperature for obtaining an appropriate pressure of 3atm was determined to be $60^{\circ}C$ for $MmNi_{4.5}Mn_{0.5}$ hydrogen storage alloy.

Effects of the Atmosphere on the Comparative Solderability of Lead-Tin and Lead-Free Solders

  • Bin, Jeong-Uk;S.M.Adams;P.F.Stratton
    • 한국마이크로전자및패키징학회:학술대회논문집
    • /
    • 한국마이크로전자및패키징학회 2001년도 Proceedings of 6th International Joint Symposium on Microeletronics and Packaging
    • /
    • pp.45-47
    • /
    • 2001
  • Due to pressure from threatened legislation in Europe, consumer and governmental pressure in Japan, and glob머 market considerations in the US, there is a rapidly growing interest in lead-free solderinger, Although the move to lead free soldering seems inevitable, many problems will arise in production assembly. It is generally acknowledged that the lead-free solders available offer a much s smaller process window than lead/tin, related mainly to the higher soldering temperatures which naturally result from increases of liquidus temperatures of at least 300 C. However, raising reflow temperatures from the current 220-2300 C to 250 2600 C will lead to problems with the boards and components as well as i increasing oxidation effects. There is a need to keep reflow temperatures low without reducing solderablity. Some results on benefits of inert atmospheres are discussed in this paper. For example, testing in a nitrogen atmosphere, with 300 ppm oxygen, by the N National Physical Laboratory (NPU has revealed clear benefits for ine$\pi$mg lead-free alloys, by restoring the solderability to lead/tin levels, by enabling lower soldering temperatures. However, there has been little testing over a range of oxygen levels in nitrogen and this is an important issue in determining n nitrogen supply and oven costs. Some results are reported here from work by NPL conducted for BOC in w which solderability was evaluated for tin기ead and tin/silver/copper eutectic a alloys in a wetting balance over a range of oxygen levels form 10 ppm to 21% ( (air). The studies confirm that acceptable wetting times occur in inert atmospheres a at soldering temperatures 20 to 300 C lower than are possible in air.

  • PDF

알루미늄의 Sb 첨가에 따른 미세조직, 전기전도도 및 기계적 특성 변화 (Influence of Sb Addition on Microstructure, Mechanical Properties and Electric Conductivity of Aluminum)

  • 유효상;김용호;이병권;고은찬;이성희;이상찬;손현택
    • 한국재료학회지
    • /
    • 제32권11호
    • /
    • pp.489-495
    • /
    • 2022
  • This research investigated how adding Sb (0.75, 1.0, 2.0 and 5.0 wt%) to as-extruded aluminum alloys affected their microstructure, mechanical properties, electric and thermal conductivity. The addition of Sb resulted in the formation of AlSb intermetallic compounds. It was observed that intermetallic compounds in the alloys were distributed homogenously in the Al matrix. As the content of Sb increased, the area fraction of intermetallic compounds increased. It can be clearly seen that the intermetallic compounds were crushed into fine particles and homogenously arrayed during the extrusion process. As the Sb content increased, the average grain size decreased remarkably from 282.6 ㎛ (0.75 wt%) to 109.2 ㎛ (5.0 wt%) due to dynamic recrystallization by the dispersed intermetallic compounds in the aluminum matrix during the hot extrusion. As the Sb content increased from 0.75 to 2.0 wt%, the electrical conductivity decreased from 61.0 to 59.8 % of the International Annealed Copper Standard. Also, as the Sb content increased from 0.75 to 2.0 wt%, the ultimate tensile strength did not significantly change, from 67.3 to 67.8 MPa.