• Title/Summary/Keyword: conventional sintering

Search Result 427, Processing Time 0.024 seconds

A Study on the Phase Formation Process in Bi-system Superconductor with Heat Treatment Conditions (열처리 조건에 따른 Bi계 초전도체에서 상 생성 과정에 대한 연구)

  • 정진인;이준웅;박용필
    • Proceedings of the Korean Institute of Electrical and Electronic Material Engineers Conference
    • /
    • 1999.11a
    • /
    • pp.221-223
    • /
    • 1999
  • In this work, samples were manufactured variously by changing conventional calcining and sintering conditions and we tried the utilization by making the heat treatment time, which is demanded to high-Tc phase formation, much shorter. We found out optimal heat treatment conditions with the analysis on formation process at superconducting phase in term of the change of calcining and sintering time and then, examined X-ray diffraction(XRD) patterns, scanning electron microscope(SEM) measurement and energy dispersive X-ray spectrometer(EDX) of the samples manufactured under heat treatment conditions which we suggest here. As a result, 2223 high-$T_c$, phase of (Bi,Pb)SrCaCuO superconductor starting with ($Bi_l$ xPbx,)$_2$$Sr_2$$Ca_2$$Cu_3$$O_y$, composition was formed from 1 hr sintering sample at temperature nearby melting point and also the completed sample with calcining and sintering time of 9 hr was formed high-$T_c$.low-$T_c$ phase appearing in sight above the critical temperature of liquid $N_2$.

  • PDF

Sintering Behavior and Thermal Conductivity of Aluminum Nitride Ceramics with MgO-CaO-Al2O3-SiO2 Nano-glass Additive (나노 MgO-CaO-Al2O3-SiO2 glass 첨가제를 가진 AlN의 소결거동 및 열전도도)

  • Baik, Su-Hyun;Kim, Kyung Min;Ryu, Sung-Soo
    • Journal of Powder Materials
    • /
    • v.25 no.5
    • /
    • pp.426-434
    • /
    • 2018
  • In this study, $MgO-CaO-Al_2O_3-SiO_2$ (MCAS) nanocomposite glass powder having a mean particle size of 50 nm and a specific surface area of $40m^2/g$ is used as a sintering additive for AlN ceramics. Densification behaviors and thermal properties of AlN with 5 wt% MCAS nano-glass additive are investigated. Dilatometric analysis and isothermal sintering of AlN-5wt% MCAS compact demonstrates that the shrinkage of the AlN specimen increases significantly above $1,300^{\circ}C$ via liquid phase sintering of MCAS additive, and complete densification could be achieved after sintering at $1,600^{\circ}C$, which is a reduction in sintering temperature by $200^{\circ}C$ compared to conventional $AlN-Y_2O_3$ systems. The MCAS glass phase is satisfactorily distributed between AlN particles after sintering at $1,600^{\circ}C$, existing as an amorphous secondary phase. The AlN specimen attained a thermal conductivity of $82.6W/m{\cdot}K$ at $1,600^{\circ}C$.

Structure and Thermal Properties of a Ternary Al-Cr-Si Quenching Ribbon Manufactured by Single Roll Method (단일 롤 방법으로 제작한 3원계 Al-Cr-Si 급냉리본의 구조 및 열 특성)

  • Han, Chang-Suk;Kim, Ki-Woong;Kim, Woo-Suk
    • Korean Journal of Materials Research
    • /
    • v.31 no.5
    • /
    • pp.296-300
    • /
    • 2021
  • Al-Cr-Si ternary quench ribbons are fabricated using a single roll method and investigated for their structural and thermal properties. In particular, the sinterability is examined by pulse current sintering to obtain the following results. The Al74Cr20Si6 composition becomes a quasicrystalline single phase; by reducing the amount of Cr, it becomes a two-phase mixed structure of Al phase and quasicrystalline phase. As a result of sintering of Al74Cr20Si6, Al77Cr13Si10 and Al90Cr6Si4 compositions, the sintering density is increased with the large amount of Al phase; the sintering density is the highest in Al90Cr6Si4 composition. In addition, as a result of investigating the effects of sintering temperature and pressurization on the sintered density of Al90Cr6Si4, a sintered compact of 99% or more at 513 K and 500 MPa is produced. In particular, since the Al-Cr-Si ternary crystal is more thermally stable than the Al-Cr binary quaternary crystal, it is possible to increase the sintering temperature by about 100 K. Therefore, using an alloy of Al90Cr6Si4 composition, a sintered compact having a sintered density of 99 % or more at 613 K and 250 MPa can be manufactured. It is possible to increase the sintering temperature by using the alloy system as a ternary system. As a result, it is possible to produce a sintered body with higher density than that possible using the binary system, and at half the pressure compared with the conventional Al-Cr binary system.

Microstructural Feature of Full-densified W-Cu Nanocomposites Containing Low Cu Content

  • Lee, Jai-Sung;Jung, Sung-Soo;Choi, Joon-Phil;Lee, Geon-Yong
    • Journal of Powder Materials
    • /
    • v.20 no.2
    • /
    • pp.138-141
    • /
    • 2013
  • The microstructure evolution during sintering of the W-5 wt.%Cu nanocomposite powders was investigated for the purpose of developing a high density W-Cu alloy. The W-5 wt.%Cu nanopowder compact, fully-densified during sintering at 1623 K, revealed a homogeneous microstructure that consists of high contiguity structures of W-W grains and an interconnected Cu phase located along the edges of the W grains. The Vickers hardness of the sintered W-5 wt.%Cu specimen was $427{\pm}22$ Hv much higher than that ($276{\pm}19$ Hv) of the conventional heavy alloy. This result is mostly due to the higher contiguity microstructure of the W grains compared to the conventional W heavy alloy.

Rolling Contact Fatigue Property of Sintered and Carburized Compacts Made of Molybdenum Hybrid-alloyed Steel Powder

  • Unami, Shigeru;Ozaki, Yukiko;Uenosono, Satoshi
    • Proceedings of the Korean Powder Metallurgy Institute Conference
    • /
    • 2006.09a
    • /
    • pp.144-145
    • /
    • 2006
  • A developed molybdenum hybrid-alloyed steel powder is based on a molybdenum prealloyed steel powder to which molybdenum powder particles are diffusion bonded. The sintered compact made of this powder has a finer pore structure than that of the conventional molybdenum prealloyed steel powder, because the ferritic iron phase $({\alpha}-phase)$ with a high diffusion coefficient is formed in the sintering necks where molybdenum is concentrated resulting in enhanced sintering. The rolling contact fatigue strength of the sintered and carburized compacts made of this powder improved by a factor of 3.6 compared with that of the conventional powder due to the fine pore structures.

  • PDF

Unidirectional Sintering in LTCC Substrate (LTCC 기판의 일 방향 소결)

  • Sun Yong-Bin;Ahn Ju-Hwan;Kim Seuk-Buom
    • Journal of the Microelectronics and Packaging Society
    • /
    • v.11 no.4 s.33
    • /
    • pp.37-41
    • /
    • 2004
  • As mobile communication devices use wide bands for large data transmission, Low Temperature Co-fired Ceramic(LTCC) has been a candidate for module substrate, for it provides better electrical properties and enables various embedded passive devices compared to conventional PCB. The LTCC, however, has applied in limited area because of non-uniform shrinkage. Hybrid heating was developed to raise sample temperature uniformly in a short period of time This leads to unidirectional sintering which enables sample to be sintered layer by layer from the bottom, resulting in more stable shape of interconnection at the top surface of the sample than conventional electric furnace heating. When sintering properties of substrate and electrical/mechanical properties of interconnection were compared, hybrid heating showed possibility to be applicable to substrate miniaturization and interconnection densification superior to electric furnace heating.

  • PDF

Ag Sintering Die Attach Technology for Wide-bandgap Power Semiconductor Packaging (Wide-bandgap 전력반도체 패키징을 위한 Ag 소결 다이접합 기술)

  • Min-Su Kim;Dongjin Kim
    • Journal of the Microelectronics and Packaging Society
    • /
    • v.30 no.1
    • /
    • pp.1-16
    • /
    • 2023
  • Recently, the shift to next-generation wide-bandgap (WBG) power semiconductor for electric vehicle is accelerated due to the need to improve power conversion efficiency and to overcome the limitation of conventional Si power semiconductor. With the adoption of WBG semiconductor, it is also required that the packaging materials for power modules have high temperature durability. As an alternative to conventional high-temperature Pb-based solder, Ag sintering die attach, which is one of the power module packaging process, is receiving attention. In this study, we will introduce the recent research trends on the Ag sintering die attach process. The effects of sintering parameters on the bonding properties and methodology on the exact physical properties of Ag sintered layer by the realization 3D image are discussed. In addition, trends in thermal shock and power cycle reliability test results for power module are discussed.

Piezoelectric Properties of 0.98(Na0.5K0.5)NbO3-0.02Li(Sb0.17Ta0.83)O3+0.01wt%ZnO Ceramics with a Sintering Temperature (소결 온도에 따른 0.98(Na0.5K0.5)NbO3-0.02Li(Sb0.17Ta0.83)O3+0.01wt%ZnO 세라믹스의 압전 특성)

  • Lee, Dong-Hyun;Lee, Seung-Hwan;Lee, Sung-Gap;Lee, Ku-Tak;Lee, Young-Hie
    • Journal of the Korean Institute of Electrical and Electronic Material Engineers
    • /
    • v.24 no.7
    • /
    • pp.543-546
    • /
    • 2011
  • We studied sintering temperature to enhance the piezoelectric properties of $0.98(Na_{0.5}K_{0.5})NbO_3-0.02Li(Sb_{0.17}Ta_{0.83})O_3$+0.01wt%ZnO (hereafter NKN-LST+ZnO) lead free piezoelectric ceramics. The synthesis and sintering method were the conventional solid state reaction method and sintering was executed at $1,080\sim1,120^{\circ}C$. We found that NKN-LST+ZnO ceramics at optimal sintering temperature showed the improved piezoelectric properties at the optimal sintering temperature. The NKN-LST+ZnO ceramics show good performance with piezoelectric constant $d_{33}$= 153 pC/N sintered at $1,090^{\circ}C$. The results reveal that NKN-LST+ZnO ceramics are promising candidate materials for lead-free piezoelectric application.

Mechanical properties of $B_4C$ ceramics fabricated by a spark plasma sintering process (방전플라즈마 소결법을 이용한 고밀도 탄화 붕소 제조 및 기계적 특성)

  • Kim, Kyoung-Hun;Chae, Jae-Hong;Park, Joo-Seok;Kim, Dae-Keun;Shim, Kwang-Bo
    • Journal of the Korean Crystal Growth and Crystal Technology
    • /
    • v.17 no.3
    • /
    • pp.128-132
    • /
    • 2007
  • [ $B_4C$ ] ceramics were fabricated by spark plasma sintering process and their sintering behavior, microstructure and mechanical properties were evaluated. Relative density of $B_4C$ ceramics were obtained by spark plasma sintering method reached as high as 99% at lower temperature than conventional sintering method, in addition, without any sintering additives. The mechanical properties of $B_4C$ ceramics was improved by a methanol washing process which can be removed $B_2O_3$ phase from a $B_4C$ powder surface. This improvement results ken the formation of homogeneous microstructure because the grain coarsening was suppressed by the elimination of $B_2O_3$ phase. Particularly, fracture toughness of the sintered specimen using a methanol washed powder improved over 30% compared with the specimen using an as-received commercial powder.