PURPOSES: This study is to estimate nondestructive strength equation based on probability for bridges using field test data. METHODS : In this study, a series of the field inspection and the test have been performed on 297 existing bridges, in order to evaluate the bridges, based on the test results of the in-depth inspection, and the estimated strengths by means of the nondestructive strength equations are analyzed and compared with results of the core specimen strengths. RESULTS : According to results of analyses, In case of standard design compressive strength of concrete is 18MPa, 21MPa, similar reliability of RILEM equation were 0.89~0.90, but in case of standard design compressive strength of concrete is 35MPa, 40MPa were 0.4~0.56. According to standard design compressive strength of concrete is 40MPa, similar reliability of ultrasonic pulse velocity method equation were 0.56. CONCLUSIONS :RILEM equation had high similar reliability than other equation in case of standard design compressive strength of concrete is 18MPa, 21MPa, but had low similar reliability than other equation in case of standard design compressive strength of concrete is 35MPa, 40MPa. and ultrasonic pulse velocity method equation had low similar reliability than other equation in case of standard design compressive strength of concrete is 40MPa.
This study was carried out to research the strength drop of concrete in dry environment. The mixing ratio of cement-fine aggregate was 1: 1, 1 : 2, 1: 3 and 1 : 4. The curing was compared standard curing with dry curing immediately after casting. It is analysis of strength change by water-proof mixing. The curing age of cement mortar was 3days, 7days, l4days and 28days. The result obtained from this study are summarized as follows. 1. The compressive and bending strength change by increasing the curing age, dry curing mortar the increasing rate of strength was decreased than standard curing mortar. 2. The compressive and bending strength change in early curing, strength difference between standard curing mortar and dry curing motar was gradually closed by increasing the W/C. 3. The dry curing mortar was decreased than standard curing mortar in decreasing rate of compressive and bending strength by increasing the W/C. 4. The compressive strength of water-proof mortar in early curing, liquid water-proof mortar was shown high strength in dry curing than standard curing. The powder and liquid water-proof mortar have a small effect in dry environment. The liquid water-proof mortar was high strength without relation change of curing age in dry environment than standard curing. 5. The compressive strength of liquid water-proof mortar in poverty mix, dry curing was shown high strength than standard curing. 6. The bending strength was increased than compressive strength by decreasing the volume of cement in early curing. The increasing rate of bending strength was decreased to compressive stength by increasing the curing age.
An artificial neural network is applied to the prediction of compressive strength, slump value of concrete. Standard mixed tables arc trained and estimated, and the results are compared with those of experiments. To consider the varieties of material properties, the standard mixed tables of two companies of Ready Mixed Concrete are used. And they are trained with the neural network. In this paper, standard back propagation network is used. For the arrangement on the approval of prediction of compressive strength and slump value, the standard compressive strength of 210, $240kgf/cm^2$ and target slump value of 12, 15cm are used because the amount of production of that range arc the most at ordinary companies. In results, in the prediction of compressive strength and slump value, the predicted values are converged well to those of standard mixed tables at the target error of 0.10, 0.05, 0.001 regardless of two companies.
The compressive strength of concrete varies depending on various factors. Among them, based on the curing temperature, the KCS 14 20 10 Standard Specification for General Concrete calculates the nominal strength by applying the temperature correction value (Tn) based on the compressive strength of the standard cured concrete at 20±2℃ when designing the formulation strength. However, Tn is a correction value that considers only the temperature, and the correction of strength difference due to heat of hydration is not applied. Therefore, in this study, one-component and two-component concrete are mixed in the summer, structural concrete are manufactured, standard concrete specimen are manufactured, and coring is performed on the central and boundary parts of the structural concrete to calculate the correction value applied to the nominal strength by comparing the compressive strength of standard cured concrete on the 28th day of curing and the compressive strength of structural concrete on the 91st day of curing.
In order to assure the quality of concrete structure in construction process, the odor strength measured by using odor sensor was used to evaluate curing effect. Then, the compressive strength and odor strength in ordinary concrete N were shown in water curing(=standard curing), indoor and outdoor atmospheric curing condition. The difference between odor strength in the standard curing and that in each curing condition was defined as the difference in the odor strength. And the difference in odor strength in slag powder concrete BP cured in water curing(=standard curing) for different period before exposing in outdoor atmosphere in winter season were evaluated at the age of 14 days. A necessity to prolong the moisture curing for the slag powder concrete BP compared with the ordinary concrete N to obtain a required curing effect was shown by measuring the odor strength and long term compressive strength.
Because of the high unit cement content in the concrete mix, major concrete temperature rises are observed in the initial stages of hardening in structural members with large cross-sections made of high-strength concrete. While this temperature rise in the initial stages of hardening contributes to the initial development of the concrete strength, it also causes thermal cracking and obstructs medium to long-term increases of the concrete strength. In the study reports below, investigations were made on the effects of the concrete temperature rise in the initial stages of hardening on the medium to long-term development of the strength of structural concrete between the ages of 28 and 91 days. In the study, comparisons were made, for example, between the compressive strength of a control specimen subjected to standard curing at 28 days and the compressive strength of core specimens taken from structural members, and observations were made on the methods of evaluating the concrete strength in structure, defined here as the compressive strength of core specimens at 91 days. The results obtained indicate that, when the maximum temperature of the concrete is the structure does not exceed $60^{\circ}C$, the concrete strength in structure at the age of long-term will generally be greater than the compressive strength of the standard-curing specimens at 28 days, allowing one to evaluate the strength of the structural concrete in terms of the compressive strength of the 28-days standard-curing specimens. When, on the other hand, the maximum temperature of the concrete in the structure exceeds $60^{\circ}C$, the strength in concrete structure may be smaller than the compressive strength of the 28-days standard-curing specimens, creating risks in the evaluation of the concrete strength in structure by latter.
One of the causes of recent construction site collapses was that the compressive strength of concrete was less than half of the allowable design standard strength range. In the safety diagnosis of structures, the compressive strength of concrete is a factor that determines the durability of a building. Therefore, in this study, we aim to examine the characteristics of compressive strength according to the particle size distribution of coarse aggregate among the compressive strength factors using small-diameter cores. To avoid problems when collecting cores, core specimens with diameters of 100×200, 50×100, and 25×50 (mm) were manufactured directly. As a result of measuring the compressive strength of concrete for each diameter, the larger the core diameter, the higher the compressive strength. has increased.
This study is intended to analyze the relationship between the rebound value of P type schmidt hammer and the compressive strength for a quality control of concrete. According to the results, the compressive strength of standard curing specimen increases in proportion to age, but that of air curing specimen hardly increases after 28 days. The rebound value of P type schmidt hammer, however, increases due to carbonation of concrete in air curing specimen. The correlativity between the rebound value and the compressive strength is very favorable in the case of standard curing specimen, but drops remarkably in the case of air curing specimen. Thus, as application of age coefficient is required for exact estimation of the compressive strength, the age coefficient is derived from this study. The age coefficient of P type schmidt hammer is higher at the age of 3 and 7days, and drops significantly, compared with the age of 28days. And it is lower before 28days than that of N type schmidt hammer suggested in Japan, and shows the similar tendency after 28days.
Kim, Doo-Kie;Kim, Hee-Joong;Chang, Sang-Kil;Chang, Seong-Kyu
International Journal of Concrete Structures and Materials
/
제19권1E호
/
pp.11-16
/
2007
Recently, probabilistic neural network (PNN) has been proposed to predict the compressive strength of concrete for the known effect of improvement on PNN by the iteration method. However, an empirical method has been incorporated in the PNN technique to specify its smoothing parameter, which causes significant uncertainty in predicting the compressive strength of concrete. In this study, a modified probabilistic neural network (MPNN) approach is hence proposed. The global probability density function (PDF) of variables is reflected by summing the heterogeneous local PDFs which are automatically determined by the individual standard deviation of each variable. The proposed MPNN is applied to predict the compressive strength of concrete using actual test data from a concrete company. The estimated results of MPNN are compared with those of the conventional PNN. MPNN showed better results than the conventional PNN in predicting the compressive strength of concrete and provided promising results for the probabilistic approach to predict the concrete strength by using the individual standard deviation of a variable.
일반적으로 플라이애시의 입도, 화학성분, 비정질양, 비정질 Si, Al 양등 매우 다양한 요인이 시멘트와의 반응에 영향을 미치고 있다. 본 연구에서는 플라이애시의 입자 특성이 압축강도에 미치는 영향을 확인하고자 한다. 표준사를 플라이애시와 유사한 입도로 분쇄하여 플라이애시와 동일하게 시멘트와 배합하여 압축강도를 측정하였다. 측정된 압축강도 결과 값을 사용하여 시멘트 수화반응에 의한 강도와 입자 충진 효과에 의한 강도 증진을 확인하였다. 표준사 분말을 치환한 모르타르의 압축강도 결과를 활용하여 플라이애시의 포졸란 반응에 의한 강도 증가분을 계산하였다. 이러한 결과 값과 플라이애시의 입자 특성을 비교한 결과, 분말도는 압축강도와 약한 상관성을 보이고 있으며, PI(Pozzolanic Index)는 10% 통과직경(D10)과 50% 통과직경(D50)과 좋은 상관관계를 나타내었다. 따라서 향후 PI와 D10과의 상관성은 플라이애시의 화학적 특성과 함께 플라이애시 특성을 파악하는 좋은 수단이 될 것으로 판단된다.
본 웹사이트에 게시된 이메일 주소가 전자우편 수집 프로그램이나
그 밖의 기술적 장치를 이용하여 무단으로 수집되는 것을 거부하며,
이를 위반시 정보통신망법에 의해 형사 처벌됨을 유념하시기 바랍니다.
[게시일 2004년 10월 1일]
이용약관
제 1 장 총칙
제 1 조 (목적)
이 이용약관은 KoreaScience 홈페이지(이하 “당 사이트”)에서 제공하는 인터넷 서비스(이하 '서비스')의 가입조건 및 이용에 관한 제반 사항과 기타 필요한 사항을 구체적으로 규정함을 목적으로 합니다.
제 2 조 (용어의 정의)
① "이용자"라 함은 당 사이트에 접속하여 이 약관에 따라 당 사이트가 제공하는 서비스를 받는 회원 및 비회원을
말합니다.
② "회원"이라 함은 서비스를 이용하기 위하여 당 사이트에 개인정보를 제공하여 아이디(ID)와 비밀번호를 부여
받은 자를 말합니다.
③ "회원 아이디(ID)"라 함은 회원의 식별 및 서비스 이용을 위하여 자신이 선정한 문자 및 숫자의 조합을
말합니다.
④ "비밀번호(패스워드)"라 함은 회원이 자신의 비밀보호를 위하여 선정한 문자 및 숫자의 조합을 말합니다.
제 3 조 (이용약관의 효력 및 변경)
① 이 약관은 당 사이트에 게시하거나 기타의 방법으로 회원에게 공지함으로써 효력이 발생합니다.
② 당 사이트는 이 약관을 개정할 경우에 적용일자 및 개정사유를 명시하여 현행 약관과 함께 당 사이트의
초기화면에 그 적용일자 7일 이전부터 적용일자 전일까지 공지합니다. 다만, 회원에게 불리하게 약관내용을
변경하는 경우에는 최소한 30일 이상의 사전 유예기간을 두고 공지합니다. 이 경우 당 사이트는 개정 전
내용과 개정 후 내용을 명확하게 비교하여 이용자가 알기 쉽도록 표시합니다.
제 4 조(약관 외 준칙)
① 이 약관은 당 사이트가 제공하는 서비스에 관한 이용안내와 함께 적용됩니다.
② 이 약관에 명시되지 아니한 사항은 관계법령의 규정이 적용됩니다.
제 2 장 이용계약의 체결
제 5 조 (이용계약의 성립 등)
① 이용계약은 이용고객이 당 사이트가 정한 약관에 「동의합니다」를 선택하고, 당 사이트가 정한
온라인신청양식을 작성하여 서비스 이용을 신청한 후, 당 사이트가 이를 승낙함으로써 성립합니다.
② 제1항의 승낙은 당 사이트가 제공하는 과학기술정보검색, 맞춤정보, 서지정보 등 다른 서비스의 이용승낙을
포함합니다.
제 6 조 (회원가입)
서비스를 이용하고자 하는 고객은 당 사이트에서 정한 회원가입양식에 개인정보를 기재하여 가입을 하여야 합니다.
제 7 조 (개인정보의 보호 및 사용)
당 사이트는 관계법령이 정하는 바에 따라 회원 등록정보를 포함한 회원의 개인정보를 보호하기 위해 노력합니다. 회원 개인정보의 보호 및 사용에 대해서는 관련법령 및 당 사이트의 개인정보 보호정책이 적용됩니다.
제 8 조 (이용 신청의 승낙과 제한)
① 당 사이트는 제6조의 규정에 의한 이용신청고객에 대하여 서비스 이용을 승낙합니다.
② 당 사이트는 아래사항에 해당하는 경우에 대해서 승낙하지 아니 합니다.
- 이용계약 신청서의 내용을 허위로 기재한 경우
- 기타 규정한 제반사항을 위반하며 신청하는 경우
제 9 조 (회원 ID 부여 및 변경 등)
① 당 사이트는 이용고객에 대하여 약관에 정하는 바에 따라 자신이 선정한 회원 ID를 부여합니다.
② 회원 ID는 원칙적으로 변경이 불가하며 부득이한 사유로 인하여 변경 하고자 하는 경우에는 해당 ID를
해지하고 재가입해야 합니다.
③ 기타 회원 개인정보 관리 및 변경 등에 관한 사항은 서비스별 안내에 정하는 바에 의합니다.
제 3 장 계약 당사자의 의무
제 10 조 (KISTI의 의무)
① 당 사이트는 이용고객이 희망한 서비스 제공 개시일에 특별한 사정이 없는 한 서비스를 이용할 수 있도록
하여야 합니다.
② 당 사이트는 개인정보 보호를 위해 보안시스템을 구축하며 개인정보 보호정책을 공시하고 준수합니다.
③ 당 사이트는 회원으로부터 제기되는 의견이나 불만이 정당하다고 객관적으로 인정될 경우에는 적절한 절차를
거쳐 즉시 처리하여야 합니다. 다만, 즉시 처리가 곤란한 경우는 회원에게 그 사유와 처리일정을 통보하여야
합니다.
제 11 조 (회원의 의무)
① 이용자는 회원가입 신청 또는 회원정보 변경 시 실명으로 모든 사항을 사실에 근거하여 작성하여야 하며,
허위 또는 타인의 정보를 등록할 경우 일체의 권리를 주장할 수 없습니다.
② 당 사이트가 관계법령 및 개인정보 보호정책에 의거하여 그 책임을 지는 경우를 제외하고 회원에게 부여된
ID의 비밀번호 관리소홀, 부정사용에 의하여 발생하는 모든 결과에 대한 책임은 회원에게 있습니다.
③ 회원은 당 사이트 및 제 3자의 지적 재산권을 침해해서는 안 됩니다.
제 4 장 서비스의 이용
제 12 조 (서비스 이용 시간)
① 서비스 이용은 당 사이트의 업무상 또는 기술상 특별한 지장이 없는 한 연중무휴, 1일 24시간 운영을
원칙으로 합니다. 단, 당 사이트는 시스템 정기점검, 증설 및 교체를 위해 당 사이트가 정한 날이나 시간에
서비스를 일시 중단할 수 있으며, 예정되어 있는 작업으로 인한 서비스 일시중단은 당 사이트 홈페이지를
통해 사전에 공지합니다.
② 당 사이트는 서비스를 특정범위로 분할하여 각 범위별로 이용가능시간을 별도로 지정할 수 있습니다. 다만
이 경우 그 내용을 공지합니다.
제 13 조 (홈페이지 저작권)
① NDSL에서 제공하는 모든 저작물의 저작권은 원저작자에게 있으며, KISTI는 복제/배포/전송권을 확보하고
있습니다.
② NDSL에서 제공하는 콘텐츠를 상업적 및 기타 영리목적으로 복제/배포/전송할 경우 사전에 KISTI의 허락을
받아야 합니다.
③ NDSL에서 제공하는 콘텐츠를 보도, 비평, 교육, 연구 등을 위하여 정당한 범위 안에서 공정한 관행에
합치되게 인용할 수 있습니다.
④ NDSL에서 제공하는 콘텐츠를 무단 복제, 전송, 배포 기타 저작권법에 위반되는 방법으로 이용할 경우
저작권법 제136조에 따라 5년 이하의 징역 또는 5천만 원 이하의 벌금에 처해질 수 있습니다.
제 14 조 (유료서비스)
① 당 사이트 및 협력기관이 정한 유료서비스(원문복사 등)는 별도로 정해진 바에 따르며, 변경사항은 시행 전에
당 사이트 홈페이지를 통하여 회원에게 공지합니다.
② 유료서비스를 이용하려는 회원은 정해진 요금체계에 따라 요금을 납부해야 합니다.
제 5 장 계약 해지 및 이용 제한
제 15 조 (계약 해지)
회원이 이용계약을 해지하고자 하는 때에는 [가입해지] 메뉴를 이용해 직접 해지해야 합니다.
제 16 조 (서비스 이용제한)
① 당 사이트는 회원이 서비스 이용내용에 있어서 본 약관 제 11조 내용을 위반하거나, 다음 각 호에 해당하는
경우 서비스 이용을 제한할 수 있습니다.
- 2년 이상 서비스를 이용한 적이 없는 경우
- 기타 정상적인 서비스 운영에 방해가 될 경우
② 상기 이용제한 규정에 따라 서비스를 이용하는 회원에게 서비스 이용에 대하여 별도 공지 없이 서비스 이용의
일시정지, 이용계약 해지 할 수 있습니다.
제 17 조 (전자우편주소 수집 금지)
회원은 전자우편주소 추출기 등을 이용하여 전자우편주소를 수집 또는 제3자에게 제공할 수 없습니다.
제 6 장 손해배상 및 기타사항
제 18 조 (손해배상)
당 사이트는 무료로 제공되는 서비스와 관련하여 회원에게 어떠한 손해가 발생하더라도 당 사이트가 고의 또는 과실로 인한 손해발생을 제외하고는 이에 대하여 책임을 부담하지 아니합니다.
제 19 조 (관할 법원)
서비스 이용으로 발생한 분쟁에 대해 소송이 제기되는 경우 민사 소송법상의 관할 법원에 제기합니다.
[부 칙]
1. (시행일) 이 약관은 2016년 9월 5일부터 적용되며, 종전 약관은 본 약관으로 대체되며, 개정된 약관의 적용일 이전 가입자도 개정된 약관의 적용을 받습니다.