PIT method which is used at fabricating Bi-2223/Ag HTS wire includes a drawing process, conventional deformation method. Drawing of meta1(Ag) and ceramic (BiSrCaCuO) composite is also difficult and significant for uniform deformation. In this paper, parameters of uniform deformation was studied at Bi-2223/ Ag multifilamentary HTS wire. Powder and rod as a starting precursor was compared at 55 filament and 54 filament Bi-2223/Ag HTS wire, respectively. Micro-hardness and area COV of the filaments was also evaluated when the diameters were decreased through drawing operations.
Reflection properties, such as specular reflection and diffuse reflection, are very important optical properties for the reflector, which has high reflectance in the display and architecture industry. Calcite is lowcost, nontoxic, and stable over a wide temperature range. Therefore, it is one of the most widely using fillers in many industries and has some advantages over titania as a filler to improve reflectance. However, optical properties, especially those of ceramic-filled composites, have not been analyzed. We studied the reflectance of calcite composites with their surface roughness. The reflectance of the composites was determined using a UV-visible spectrometer. The surface morphology and the micro-structure of the composites were investigated by atomic force microscope. The reflectance of the composites was improved by increasing the content of calcite in the calcite-frit composite. The reflectance is related with the surface roughness in the composites. However, the reflectance depends on the calcite contents in materials with similar surface roughness.
The effects of the opaque porcelain firing temperature, the bonding agent and the degassing prior to the opaque firing On the bond strength were investigated by means of the tensile shear stIe$. The diffusional behaviours at the interface of the porcelain and the alloy, and .the microstructures of the ceramic and metal composite were studied for understanding the bonding mechanism. The results obtained in this experiment were summarizd as follow; 1. With no application of bonding agent, the tensile shear strength of the specimen firing at $1840^{\circ}F$ was higher than that of the specimen firing at $1760^{\circ}F$. 2. The highest bond strength was obtained by application of bonding agent without degassing prior to the opaque firing. 3. Application of bonding agent after the degassing showed the lowest bond strength. 4. The greater number of pores were observed at the firing temperature of $1840^{\circ}F$ than that of $1760^{\circ}F$ in the porcelain and the interface respectively.
MPB 조성영역인 Zr/Ti=52/48의 composite ceramic target을 사용하여 RF magnetron sputtering 방법으로 기판온도 약 30$0^{\circ}C$에서 RZT 박막을 Pt/Ti/Si 기판위에 증착시켰다. 안정상인 perovskite 구조를 형성시키기 위하여 PbO분위기에서 furnace annealing 과 Repid thermal annealing을 실시하여 열처리 방법에 따른 상형성 및 계면반응과 그에 따른 전기적 특성을 고찰 하였다. Pt 의 두께가 250$\AA$인 경우 furnace annealing 시 $650^{\circ}C$에서 perouskite 상이 형성되었으나 Pt층이 산소의 확산을 방지하지 못하여 상부의 Ti 층이 TiOx로 변태하였으며 하부의 Ti는 Si 과 반응하여 Ti-silicide 롤 변태하였다. 또한 75$0^{\circ}C$,60sec 인 경우 Pt 층의 응집화가 관찰되어 하부전극으로서 적용이 적절하지 못하다. 급속열처리를 실시한 경우에도 마찬가지로 Ti 층이 TiOx 와 silicide 층으로 변태되었다. Pt의 두께가 1000$\AA$인 경우에도 250$\AA$와는 달리 RTA 시 (III)방향으로 Furace annealing 시(001)방향으로 우선 성장하였다. 이는 Ti(001), P(111),PZT(111)면의 lattic mismatch 가 매우 작은데다 RTA 시 계면반응이 거의발생하지 않아 PZT 박막이 (111) 방향으로 우선 성장한 것으로 보인다. Furnace annealing 경우는 심한 계면반응이 발생하여 Pt층에 어느 정도 영향을 주었기 때문에 우선성장 방향이 바뀌었다구 생각한다.
The ultrasonic motor have recently begun to be used for certain unique practical utilizations in the fields of industrial medical consumer and automotive applications. Ultrasonic motor stimulated to ultrasonic oscillations by piezoelectrics to drive a rotor via friction contact. The metal and ceramic composite component was used as the stator element to generate ultrasonic vibrations. The ultrasonic motor used here was the windmill type ultrasonic motor operated by single-phase AC source. The windmill type ultrasonic motors has only three components; a stator element of two windmill shape slotted metal endcaps a rotor and a bearing. In this paper a prototype motor with 11.35 mm diameter was fabricated then relationship between the pressing force applied to a rotor and the rotation characteristic of windmill type ultrasonic motor are investigated when stator’s slots was changed from 4, 6, 8 and thickness changed from 0.15, 0.20 mm, respectively. Optimum pressing force applied to a rotor in the six stators was 1.2 mN.
The purpose of this study were to develop and validate a prototype slipmeter used on-site floor. The developed slipmeter was dreg sled type. It measured static coefficient of friction(SCOF). The developed slipmeter was evaluated with ASTM 2508-11 which use four different standard surfaces(polished granite, glazed porcelain, vinyl composite tile, and ceramic tile). The SCOF was then measured with developed slipmeter under the three different contaminants and seven different floors. The test results of slipmeter were also compared with those of BOT-3000, floor surface roughness, and human perception. The test results revealed that developed slipmeter successfully ranked all four standard surfaces and differentiated among standard surfaces with varying degrees of slipperiness. The developed slipmeter couldn't properly measure slipperiness under the two kind of floors(polished tile, ground steel plate) and one kind of contaminant(glycerol). The test results of developed slipmeter had stronger correlation with those of BOT-3000 and floor roughness under the water and detergent solution than under the glycerol. The test results of developed slipmeter also showed stronger correlation with those of BOT-3000 and surface roughness than those of human perception. The newly developed slipmeter had been found to give consistent results under the test conditions except for two kind of floors(polished tile, ground steel plate) and one kind of contaminant(glycerol).
Simple, small and portable oxygen sensors were fabricated by tape casting technique. Yttria stabilized zirconia containing cordierite ceramics (YSZC) were used as a porous diffused layer of oxygen in pumping cell. Yttria stabilized zirconia (YSZ) solid electrolyte, YSZC porous diffusion layer and heater-patterned ceramic sheets were prepared by co- firing method. Limit current characteristics and the linear relationship of current to oxygen concentration were observed. Viscosity variation of the slurries both YSZ and YSZC showed a similar behavior, but micro pores in the fired sheet were increased with increasing of the cordierite amount. Molecular diffusion was dominated due to the formation of large pores in porous diffusion layer. The plateau range of limit current in porous-type oxygen sensor was narrow than the one of aperture-type oxygen sensor. However limit current curve was appeared in porous-type oxygen sensor even at the lower applied voltage. The plateau range of limit-current was widen as increasing the thickness of porous diffusion layer of the YSZ containing cordierite. Measuring temperature of $600{\sim}650^{\circ}C$ was recommended for limit-current oxygen sensor. Porous diffusion layer-type oxygen sensor showed faster response than the aperture-type one and was stable up to 30 days running without any crack at interface between the layers.
Gyawali, Gobinda;Joshi, Bhupendra;Tripathi, Khagendra;Lee, Soo Wohn
한국표면공학회:학술대회논문집
/
한국표면공학회 2015년도 춘계학술대회 논문집
/
pp.43-44
/
2015
Electrodeposited Ni and Ni-SiC composite coatings were prepared on Cu substrates by using the Ni-Sulfamate electrolytic bath. Thus prepared samples were subjected for the two different types of post surface modification techniques; i.e. Laser Surface Texturing (LST) and Ultrasonic Nano Surface Modification (UNSM), respectively in order to investigate their effects on surface and interface related properties of the coatings. Hemispherical dimples, with 80 to 200 um dimple spacing, were created and examined on the surfaces of the materials studied. The results revealed that micro-surface texturing with 150 um dimple spacing considerably improved the coefficient of friction. Dimple spacing accuracy and incorporated second phase ceramic particles both contributed significantly to reduction in coefficient of friction. On the other hand, application of UNSM considerably modified the surface topography, led to increase the Vickers microhardness, and reduced the wear and coefficient of friction as compared to non UNSM treated Ni and Ni-SiC samples.
The effect of monoclinic $ZrO_2$(pure) and tetragonal $ZrO_2$ containing 5.35wt% $Y_2$$O_3$(Y-TZP) addition on the mechanical properties and thermal shock resistance of $Al_2$$O_3$ ceramic were investigated. The addition of $ZrO_2$(m) and Y-TZP increased sintering density of $Al_2$$O_3$. The vickers hardness increased with increasing the volume fraction of Y-TZP going through a maximum at 20wt%. The hardness of the specimens was found to be depend on the sintering density. With increasing the volume fraction of $ZrO_2$(m) and Y-TZP, the fracture toughness of the composite is increased. This result may be taken as evidence that toughening of ${Al_2}{O_3}$ can also be achieved by the transformation toughening and microcrack toughening of $ZrO_2$. The property of the& shock for ${Al_2}{O_3}$-$ZrO_2$ composites was improved by increasing the volume fraction of monoclinic $ZrO_2$(pure).Grain size increased with increasing the volume fraction of $ZrO_2$.
Spherical $CeO_2:Ho^{3+}/Yb^{3+}$ particles were synthesized using spray pyrolysis, and the upconversion (UC) properties were investigated with changing the preparation conditions and the infrared pumping power. The resulting particles had a size of about $1{\mu}m$ and hollow structure. The prepared $CeO_2:Ho^{3+}/Yb^{3+}$ particles exhibited intense green emission due to the $^5F_4/^5S_2{\rightarrow}^5I_8$ transition of $Ho^{3+}$ and showed weak red or near-IR peaks. In terms of achieving the highest UC emission, the optimal concentrations of $Ho^{3+}$ and $Yb^{3+}$ were 0.3% and 2.0%, respectively. The UC emission intensity of prepared $CeO_2:Ho^{3+}/Yb^{3+}$ particles had a linear relationship with crystallite size and concentration quenching was caused by dipole-dipole interaction between the same ions. Based on the dependency of UC emission on the pumping power, the observed green upconversion was achieved through a typical two-photon process and concluded that the main energy transfer from $Yb^{3+}$ to $Ho^{3+}$ was involved in the ground-state adsorption (GSA) process.
본 웹사이트에 게시된 이메일 주소가 전자우편 수집 프로그램이나
그 밖의 기술적 장치를 이용하여 무단으로 수집되는 것을 거부하며,
이를 위반시 정보통신망법에 의해 형사 처벌됨을 유념하시기 바랍니다.
[게시일 2004년 10월 1일]
이용약관
제 1 장 총칙
제 1 조 (목적)
이 이용약관은 KoreaScience 홈페이지(이하 “당 사이트”)에서 제공하는 인터넷 서비스(이하 '서비스')의 가입조건 및 이용에 관한 제반 사항과 기타 필요한 사항을 구체적으로 규정함을 목적으로 합니다.
제 2 조 (용어의 정의)
① "이용자"라 함은 당 사이트에 접속하여 이 약관에 따라 당 사이트가 제공하는 서비스를 받는 회원 및 비회원을
말합니다.
② "회원"이라 함은 서비스를 이용하기 위하여 당 사이트에 개인정보를 제공하여 아이디(ID)와 비밀번호를 부여
받은 자를 말합니다.
③ "회원 아이디(ID)"라 함은 회원의 식별 및 서비스 이용을 위하여 자신이 선정한 문자 및 숫자의 조합을
말합니다.
④ "비밀번호(패스워드)"라 함은 회원이 자신의 비밀보호를 위하여 선정한 문자 및 숫자의 조합을 말합니다.
제 3 조 (이용약관의 효력 및 변경)
① 이 약관은 당 사이트에 게시하거나 기타의 방법으로 회원에게 공지함으로써 효력이 발생합니다.
② 당 사이트는 이 약관을 개정할 경우에 적용일자 및 개정사유를 명시하여 현행 약관과 함께 당 사이트의
초기화면에 그 적용일자 7일 이전부터 적용일자 전일까지 공지합니다. 다만, 회원에게 불리하게 약관내용을
변경하는 경우에는 최소한 30일 이상의 사전 유예기간을 두고 공지합니다. 이 경우 당 사이트는 개정 전
내용과 개정 후 내용을 명확하게 비교하여 이용자가 알기 쉽도록 표시합니다.
제 4 조(약관 외 준칙)
① 이 약관은 당 사이트가 제공하는 서비스에 관한 이용안내와 함께 적용됩니다.
② 이 약관에 명시되지 아니한 사항은 관계법령의 규정이 적용됩니다.
제 2 장 이용계약의 체결
제 5 조 (이용계약의 성립 등)
① 이용계약은 이용고객이 당 사이트가 정한 약관에 「동의합니다」를 선택하고, 당 사이트가 정한
온라인신청양식을 작성하여 서비스 이용을 신청한 후, 당 사이트가 이를 승낙함으로써 성립합니다.
② 제1항의 승낙은 당 사이트가 제공하는 과학기술정보검색, 맞춤정보, 서지정보 등 다른 서비스의 이용승낙을
포함합니다.
제 6 조 (회원가입)
서비스를 이용하고자 하는 고객은 당 사이트에서 정한 회원가입양식에 개인정보를 기재하여 가입을 하여야 합니다.
제 7 조 (개인정보의 보호 및 사용)
당 사이트는 관계법령이 정하는 바에 따라 회원 등록정보를 포함한 회원의 개인정보를 보호하기 위해 노력합니다. 회원 개인정보의 보호 및 사용에 대해서는 관련법령 및 당 사이트의 개인정보 보호정책이 적용됩니다.
제 8 조 (이용 신청의 승낙과 제한)
① 당 사이트는 제6조의 규정에 의한 이용신청고객에 대하여 서비스 이용을 승낙합니다.
② 당 사이트는 아래사항에 해당하는 경우에 대해서 승낙하지 아니 합니다.
- 이용계약 신청서의 내용을 허위로 기재한 경우
- 기타 규정한 제반사항을 위반하며 신청하는 경우
제 9 조 (회원 ID 부여 및 변경 등)
① 당 사이트는 이용고객에 대하여 약관에 정하는 바에 따라 자신이 선정한 회원 ID를 부여합니다.
② 회원 ID는 원칙적으로 변경이 불가하며 부득이한 사유로 인하여 변경 하고자 하는 경우에는 해당 ID를
해지하고 재가입해야 합니다.
③ 기타 회원 개인정보 관리 및 변경 등에 관한 사항은 서비스별 안내에 정하는 바에 의합니다.
제 3 장 계약 당사자의 의무
제 10 조 (KISTI의 의무)
① 당 사이트는 이용고객이 희망한 서비스 제공 개시일에 특별한 사정이 없는 한 서비스를 이용할 수 있도록
하여야 합니다.
② 당 사이트는 개인정보 보호를 위해 보안시스템을 구축하며 개인정보 보호정책을 공시하고 준수합니다.
③ 당 사이트는 회원으로부터 제기되는 의견이나 불만이 정당하다고 객관적으로 인정될 경우에는 적절한 절차를
거쳐 즉시 처리하여야 합니다. 다만, 즉시 처리가 곤란한 경우는 회원에게 그 사유와 처리일정을 통보하여야
합니다.
제 11 조 (회원의 의무)
① 이용자는 회원가입 신청 또는 회원정보 변경 시 실명으로 모든 사항을 사실에 근거하여 작성하여야 하며,
허위 또는 타인의 정보를 등록할 경우 일체의 권리를 주장할 수 없습니다.
② 당 사이트가 관계법령 및 개인정보 보호정책에 의거하여 그 책임을 지는 경우를 제외하고 회원에게 부여된
ID의 비밀번호 관리소홀, 부정사용에 의하여 발생하는 모든 결과에 대한 책임은 회원에게 있습니다.
③ 회원은 당 사이트 및 제 3자의 지적 재산권을 침해해서는 안 됩니다.
제 4 장 서비스의 이용
제 12 조 (서비스 이용 시간)
① 서비스 이용은 당 사이트의 업무상 또는 기술상 특별한 지장이 없는 한 연중무휴, 1일 24시간 운영을
원칙으로 합니다. 단, 당 사이트는 시스템 정기점검, 증설 및 교체를 위해 당 사이트가 정한 날이나 시간에
서비스를 일시 중단할 수 있으며, 예정되어 있는 작업으로 인한 서비스 일시중단은 당 사이트 홈페이지를
통해 사전에 공지합니다.
② 당 사이트는 서비스를 특정범위로 분할하여 각 범위별로 이용가능시간을 별도로 지정할 수 있습니다. 다만
이 경우 그 내용을 공지합니다.
제 13 조 (홈페이지 저작권)
① NDSL에서 제공하는 모든 저작물의 저작권은 원저작자에게 있으며, KISTI는 복제/배포/전송권을 확보하고
있습니다.
② NDSL에서 제공하는 콘텐츠를 상업적 및 기타 영리목적으로 복제/배포/전송할 경우 사전에 KISTI의 허락을
받아야 합니다.
③ NDSL에서 제공하는 콘텐츠를 보도, 비평, 교육, 연구 등을 위하여 정당한 범위 안에서 공정한 관행에
합치되게 인용할 수 있습니다.
④ NDSL에서 제공하는 콘텐츠를 무단 복제, 전송, 배포 기타 저작권법에 위반되는 방법으로 이용할 경우
저작권법 제136조에 따라 5년 이하의 징역 또는 5천만 원 이하의 벌금에 처해질 수 있습니다.
제 14 조 (유료서비스)
① 당 사이트 및 협력기관이 정한 유료서비스(원문복사 등)는 별도로 정해진 바에 따르며, 변경사항은 시행 전에
당 사이트 홈페이지를 통하여 회원에게 공지합니다.
② 유료서비스를 이용하려는 회원은 정해진 요금체계에 따라 요금을 납부해야 합니다.
제 5 장 계약 해지 및 이용 제한
제 15 조 (계약 해지)
회원이 이용계약을 해지하고자 하는 때에는 [가입해지] 메뉴를 이용해 직접 해지해야 합니다.
제 16 조 (서비스 이용제한)
① 당 사이트는 회원이 서비스 이용내용에 있어서 본 약관 제 11조 내용을 위반하거나, 다음 각 호에 해당하는
경우 서비스 이용을 제한할 수 있습니다.
- 2년 이상 서비스를 이용한 적이 없는 경우
- 기타 정상적인 서비스 운영에 방해가 될 경우
② 상기 이용제한 규정에 따라 서비스를 이용하는 회원에게 서비스 이용에 대하여 별도 공지 없이 서비스 이용의
일시정지, 이용계약 해지 할 수 있습니다.
제 17 조 (전자우편주소 수집 금지)
회원은 전자우편주소 추출기 등을 이용하여 전자우편주소를 수집 또는 제3자에게 제공할 수 없습니다.
제 6 장 손해배상 및 기타사항
제 18 조 (손해배상)
당 사이트는 무료로 제공되는 서비스와 관련하여 회원에게 어떠한 손해가 발생하더라도 당 사이트가 고의 또는 과실로 인한 손해발생을 제외하고는 이에 대하여 책임을 부담하지 아니합니다.
제 19 조 (관할 법원)
서비스 이용으로 발생한 분쟁에 대해 소송이 제기되는 경우 민사 소송법상의 관할 법원에 제기합니다.
[부 칙]
1. (시행일) 이 약관은 2016년 9월 5일부터 적용되며, 종전 약관은 본 약관으로 대체되며, 개정된 약관의 적용일 이전 가입자도 개정된 약관의 적용을 받습니다.