섬유쉬트 보강부위의 부착성능 평가에 관한 기초연구 (A Foundamental Study on Evaluation of Adhesive Strength in Reinforced Position Concrete Structure Used Fiber Sheet)

  • 안상철;곽규성;이성혁;오상근;박국배;안상덕
    • 한국콘크리트학회:학술대회논문집
    • /
    • 한국콘크리트학회 1998년도 봄 학술발표회논문집(II)
    • /
    • pp.613-617
    • /
    • 1998
  • This study deals with the effect on adhesive strength properties of fiber sheet layer and maintenance position of coccrete structure reinforced using epoxy resin carbon and aramit fiber sheet. Properties of epoxy resin adhesive strength of the concrete bridge slab, tunnel and wall etc. reinforced using fiber sheet under many different environment change according to condition of concrete substrate, temperature, moisture, curing, cleaning, and chemical effects and so on. The purpose of this study is that it makes the estimation value of adhesive strength of concrete substrate and fiber sheet reinforcing layer penetrated epoxy resin under high temperature(9$0^{\circ}C$), chemical attack and condition of curing.

  • PDF

비소성 황토 결합재를 혼합한 콘크리트의 강도 발현 평가를 위한 초음파 속도법의 검토 (A Study on Evaluating the Compressive Strength Development of Concrete Mixed with Non-sintered Hwangto Admixture by an Ultrasonic Method)

  • 김정욱;김원창;김규용;이태규
    • 한국건축시공학회지
    • /
    • 제23권1호
    • /
    • pp.35-43
    • /
    • 2023
  • 본 연구에서는 시멘트 대체 재료로서 비소성 황토(NHT)를 혼합한 콘크리트의 역학적 특성을 평가하였으며, 초음파 속도 분석을 통한 콘크리트의 강도 예측식을 제안하였다. 혼합된 NHT의 시멘트 치환율을 0, 15 및 30%로 설정하였으며, 시멘트 및 NHT의 분체량에 대한 영향을 평가하기 위해 목표 강도를 30 및 45MPa로 설정하였다. 평가한 항목은 압축 강도, 초음파 속도 및 탄성계수로 설정하였으며, 재령 1, 3, 7 및 28일마다 설정한 항목을 측정하였다. 실험 결과, NHT 치환율이 증가함에 따라 역학적 특성은 감소하는 경향을 보였으며. 또한, 압축 강도와 초음파 속도의 상관관계 분석 결과 상관계수(R2)는 NHT를 혼합한 콘크리트의 경우 약 0.95로 높은 관계성을 보였다.