산화아연-탄소나노튜브 복합체의 일산화질소 가스 감지 특성에 미치는 코발트 첨가 효과 (Effects of Co Doping on NO Gas Sensing Characteristics of ZnO-Carbon Nanotube Composites)

  • 정훈철;안은성;웬래훙;오동훈;김효진;김도진
    • 한국재료학회지
    • /
    • 제19권11호
    • /
    • pp.607-612
    • /
    • 2009
  • We investigated the effects of Co doping on the NO gas sensing characteristics of ZnO-carbon nanotube (ZnO-CNT) layered composites fabricated by coaxial coating of single-walled CNTs with ZnO using pulsed laser deposition. Structural examinations clearly confirmed a distinct nanostructure of the CNTs coated with ZnO nanoparticles of an average diameter as small as 10 nm and showed little influence of doping 1 at.% Co into ZnO on the morphology of the ZnO-CNT composites. It was found from the gas sensing measurements that 1 at.% Co doping into ZnO gave rise to a significant improvement in the response of the ZnO-CNT composite sensor to NO gas exposure. In particular, the Co-doped ZnO-CNT composite sensor shows a highly sensitive and fast response to NO gas at relatively low temperatures and even at low NO concentrations. The observed significant improvement of the NO gas sensing properties is attributed to an increase in the specific surface area and the role as a catalyst of the doped Co elements. These results suggest that Co-doped ZnOCNT composites are suitable for use as practical high-performance NO gas sensors.

청색 발광층에 의한 백색 OLED의 발광 특성 (Emission Properties of White Organic Light-Emitting Diodes with Blue Emitting Layer)

  • 천현동;나현석;주성후
    • 한국전기전자재료학회논문지
    • /
    • 제26권6호
    • /
    • pp.451-456
    • /
    • 2013
  • To study emission properties of white phosphorescent organic light emitting devices (PHOLEDs), we fabricated white PHOLEDs of ITO(150 nm) / NPB(30 nm) / TcTa(10 nm) / mCP(7.5 nm) / light-emitting layer(25 nm) / UGH3(5 nm) / Bphen(50 nm) / LiF(0.5 nm) / Al(200 nm) structure. The total thickness of light-emitting layer with co-doping and blue-doping/co-doping using a host-dopant system was 25 nm and the dopant of blue and red was FIrpic and $Bt_2Ir$(acac) in UGH3 as host, respectively. The OLED characteristics were changed with position and thickness of blue doping layer and co-doping layer as light-emitting layer and the best performance seemed in structure of blue-doping(5 nm)/co-doping(20 nm) layer. The white PHOLEDs showed the maximum current density of $34.5mA/cm^2$, maximum brightness of $5,731cd/m^2$, maximum current efficiency of 34.8 cd/A, maximum power efficiency of 21.6 lm/W, maximum quantum efficiency of 15.6%, and a Commission International de L'Eclairage (CIE) coordinate of (0.367, 0.436) at $1,000cd/m^2$.

Investigation of degradation mechanism of phosphorescent and thermally activated delayed fluorescent organic light-emitting diodes through doping concentration dependence of lifetime

  • Song, Wook;Kim, Taekyung;Lee, Jun Yeob;Lee, Yoonkyoo;Jeong, Hyein
    • Journal of Industrial and Engineering Chemistry
    • /
    • 제68권
    • /
    • pp.350-354
    • /
    • 2018
  • Lifetime study of blue phosphorescent and thermally activated delayed fluorescent organic light-emitting diodes was carried out to understand the dominant degradation process during electrical operation of the devices. Doping concentration dependence of the phosphorescent and thermally activated delayed fluorescent organic light-emitting diodes was studied, which demonstrated long lifetime at low doping concentration in the phosphorescent devices and at high doping concentration in the thermally activated delayed fluorescent devices. Detailed mechanism study of the two devices described that triplet-triplet annihilation is the main degradation process of phosphorescent organic light-emitting diodes, whereas triplet-polaron annihilation is the key degradation factor of the thermally activated delayed fluorescent devices.

$CaAl_2O_4:Eu^{2+}$ 청색(靑色) 형광체(螢光體)의 $Nd^{3+}$ 도핑 최적화(最適化)에 관한 연구(硏究) (Optimization of $Nd^{3+}$ ion co-doping in $CaAl_2O_4:\;Eu^{2+}$ blue phosphor)

  • ;류호진
    • 자원리싸이클링
    • /
    • 제16권5호
    • /
    • pp.46-50
    • /
    • 2007
  • [ $Eu^{2+},\;Nd^{3+}$ ]로 도핑된 $CaAl_2O_4$ 청색 형광체를 고상반응법으로 제조하였다. 1 mol% $Eu^{2+}$로 doping된 형광체에 다양한 조성의 $Nd^{3+}$를 co-doping함에 따라 고휘도, 장잔광 특성을 보였다. 제조한 형광체에 대하여 XRD, SEM, TEM, 빛발광 특성을 조사하였다. $CaAl_2O_4:Eu^{2+}:Nd^{3+}$의 넓은 밴드의 UV로 여기된 빛발광 특성이 $Eu^{2+}$$4f^65d^1$에서 $4f^7$ 상태로 천이에 의해 기인된 청색영역(${\lambda}_{max}=440\;nm$)에서 관찰되었다. $Nd^{3+}$로 co-doping한 형광체는 여기광을 차단하였을 때 장잔광 발광 특성을 나타내었다.

밀폐유도용해로 제조한 CoSb3-yTey의 열전특성 (Thermoelectric Properties of CoSb3-yTey Prepared by Encapsulated Induction Melting)

  • 김미정;심우섭;어순철;김일호
    • 한국재료학회지
    • /
    • 제16권7호
    • /
    • pp.412-415
    • /
    • 2006
  • Te-doped $CoSb_3$ was prepared by the encapsulated induction melting, and its doping effects on the thermoelectric properties were investigated. Single phase ${\delta}-CoSb_3$ was successfully obtained by the subsequent annealing at 773 K for 24 hrs. Tellurium atoms acted as electron donors by substituting antimony atoms. Thermoelectric properties were remarkably improved by the appropriate doping. Dimensionless figure of merit was obtained to be 0.83 at 700K for the $CoSb_{2.8}Te_{0.2}$ specimen.

Enhanced Visible Light Activity and Stability of TiO2 Nanopowder by co-doped with Mo and N

  • Hu, Shaozheng;Li, Fayun;Fan, Zhiping
    • Bulletin of the Korean Chemical Society
    • /
    • 제33권4호
    • /
    • pp.1269-1274
    • /
    • 2012
  • A visible light responsive N, Mo co-doped $TiO_2$ were prepared by sol-gel method. X-ray diffraction, TEM, $N_2$ adsorption, UV-vis spectroscopy, photoluminescence, and X-ray photoelectron spectroscopy were used to characterize the prepared $TiO_2$ samples. Doping restrained the phase transformation from anatase to rutile and reduced the particle sizes. The band gap was much narrowed after N, Mo co-doping. The photocatalytic activities were tested in the degradation of an aqueous solution of a reactive dyestuff, methylene blue, under visible light. The photocatalytic activities of doped $TiO_2$ were much higher than that of neat $TiO_2$. The photocatalytic stability of N, Mo co-doped $TiO_2$ was much better than that of N doped $TiO_2$.

희토류 원소의 복합첨가에 의한 fluride 유리에서의 청색 상향전이현상 (Co-doping Effects on the Blue Up-conversion Characteristics of Fluoride Glasses)

  • 류선윤
    • 한국세라믹학회지
    • /
    • 제37권1호
    • /
    • pp.33-43
    • /
    • 2000
  • Up-conversion of rare-earth element added glass is promising area for short wavelength laser source by utilizing high power semiconductor infra-red laser if the efficiency can be increased by proper method. In this study, relatively low phonon energy fluoride glasses were prepared by co-doping rare-earth elements to realize the high efficiency up-convertor. The physical, chemical, andoptical properties of co-doped fluoride glasses were measured. 10 combinations of 5 different rare-earth fluoride elements doped samples were prepared and their transition temperatures, chemical durability, density, hardness, refractive index, absorption, fluorescence, and fluorescence lifetime were measured. 480nm wavelengths blue up-conversion was found in the Yb3+/Tm3+ co-doped glass sample with 800nm laser source and the optimum composition for the most efficient blue up-conversion was found from the glass sample with 0.3 mol% TmF3 and 1 mol% YbF3.

  • PDF

In 코도핑 된 p-GaN의 광학적 특성 (In Co-Doping Effect on the Optical Properties of P-Type GaN Epilayers)

  • 안명환;정호용;정상조
    • 한국재료학회지
    • /
    • 제18권8호
    • /
    • pp.450-453
    • /
    • 2008
  • Mg-doped and In-Mg co-doped p-type GaN epilayers were grown in a low-pressure metal organic chemical vapor deposition technique. The effect of In doping on the p-GaN layer was studied through photoluminescence (PL), persistent photoconductivity (PPC), and transmission electron microscopy (TEM) at room temperature. For the In-doped p-GaN layer, the PL intensity increases significantly and the peak position shifts to 3.2 eV from 2.95 eV of conventional p-GaN. Additionally, In doping greatly reduces the PPC, which was very strong in conventional p-GaN. A reduction in the dislocation density is also evidenced upon In doping in p-GaN according to TEM images. The improved optical properties of the In-doped p-GaN layer are attributed to the high crystalline quality and to the active participation of incorporated Mg atoms.

Softener 및 Hardener 동시 첨가가 PZT 압전세라믹에 미치는 영향 (Effects of Softener and Hardener Co-doping on Properties of PZT Piezoelectric Ceramics)

  • 이언종;김윤해;이병우
    • 한국해양공학회지
    • /
    • 제24권6호
    • /
    • pp.81-85
    • /
    • 2010
  • The effects of co-doping with complex dopants of softeners, $La^{+3}$ and/or $Nb^{+5}$, and a hardener, $Fe^{+3}$, on the microstructural and piezoelectric properties of PZT ceramics with a composition of a rhombohedral-tetragonal morphotropic phase boundary, $PbZr_{0.53}Ti_{0.47}O_3$, were investigated. Unlike single-element doping, the complex doping of both the softener and hardener ions led to various compensation effects for the piezoelectric properties of the PZT ceramics. For 0.5 wt.% $La_2O_3$ softener and/or 0.5 wt.% $Nb_2O_5$ doped compositions, there were apparent hardener doping (compensation) effects for an addition of over 1.0 wt.% $Fe_2O_3$. For the $La_2O_3$ and/or $Nb_2O_5$ doped composition, the co-dopant $Fe_2O_3$ addition led to lower kp and $\varepsilon$r, and increased $Q_m$ values. The prepared PZT ceramics modified with complex soft dopants, $La^{+3}$ and $Nb^+$, as well as a hard dopant, $Fe^{+3}$, showed that the piezoelectric properties were stable with the compositional variations, which made it possible to establish piezoelectric performances with higher reliability and reproducibility. The most improved piezoelectric properties of enhanced $Q_m$ with $\varepsilon_r$ remaining higher $k_p$, were obtained in the PZT composition complexly doped with $La^{+3}$ and $Fe^{+3}$. From the results obtained in this study, the properties of compositionally modified PZT ceramics can also be tailored over a wider range by changing the dopant compositions to meet the specific requirements for underwater or other applications.