• 제목/요약/키워드: chemical mechanical planarization (CMP)

검색결과 218건 처리시간 0.025초

산화막 CMP에서 패드 두께가 연마율과 연마 불균일도에 미치는 영향 (Effect of Pad Thickness on Removal Rate and Within Wafer Non-Uniformity in Oxide CMP)

  • 배재현;이현섭;박재홍;니시자와 히데키;키노시타 마사하루;정해도
    • 한국전기전자재료학회논문지
    • /
    • 제23권5호
    • /
    • pp.358-363
    • /
    • 2010
  • The polishing pad is important element for polishing characteristic such as material removal rate(MRR) and within wafer non-uniformity(WIWNU) in the chemical mechanical planarization(CMP). The result of the viscoelasticity measurement shows that 1st elastic modulus is increased and 2nd elastic modulus is decreased when the top pad is thickened. The finite element analysis(FEA) was conducted to predict characteristic of polishing behavior according to the pad thickness. The result of polishing experiment was similar with the FEA, and it shows that the 1st elastic modulus affects instantaneous deformation of pad related to MRR. And the 2nd elastic modulus has an effect on WIWNU due to the viscoelasticity deformation of pad.

고유전율막의 CMP 특성 (Chemical Mechanical Polishing Characteristics of High-k Thin Film)

  • 박성우;서용진;이우선
    • 한국전기전자재료학회:학술대회논문집
    • /
    • 한국전기전자재료학회 2006년도 하계학술대회 논문집 Vol.7
    • /
    • pp.55-56
    • /
    • 2006
  • In this paper, we first applied the chemical mechanical polishing (CMP) process to the planarization of ferroelectric film in order to obtain a good planarity of electrode/ferroelectric film interface. BST ($Ba_{0.6}Sr_{0.4}TiO_3$), PZT ($Pb_{1.1}(Zr_{0.52}TiO_{0.48})O_3$) and BTO ($BaTiO_3$) ferroelectric film are fabricated by the sol-gel method. And then, we compared the structural characteristics before and after CMP process of BST, PZT, BTO films. Their dependence on slurry composition was also investigated. We expect that our results will be useful promise of global planarization for ferroelectric random access memories (FRAM) application in the near future.

  • PDF

Alternative Optimization Techniques for Shallow Trench Isolation and Replacement Gate Technology Chemical Mechanical Planarization

  • Stefanova, Y.;Cilek, F.;Endres, R.;Schwalke, U.
    • Transactions on Electrical and Electronic Materials
    • /
    • 제8권1호
    • /
    • pp.1-4
    • /
    • 2007
  • This paper discusses two approaches for pre-polishing optimization of oxide chemical mechanical planarization (CMP) that can be used as alternatives to the commonly applied dummy structure insertion in shallow trench isolation (STI) and replacement gate (RG) technologies: reverse nitride masking (RNM) and oxide etchback (OEB). Wafers have been produced using each optimization technique and CMP tests have been performed. Dishing, erosion and global planarity have been investigated with the help of conductive atomic force microscopy (C-AFM). The results demonstrate the effectiveness of both techniques which yield excellent planarity without dummy structure related performance degradation due to capacitive coupling.

CMP 공정에서 마찰에너지가 연마결과에 미치는 영향 (Effects of Friction Energy on Polishing Results in CMP Process)

  • 이현섭;박범영;김구연;김형재;서헌덕;정해도
    • 대한기계학회논문집A
    • /
    • 제28권11호
    • /
    • pp.1807-1812
    • /
    • 2004
  • The application of chemical mechanical polishing(CMP) has a long history. Recently, CMP has been used in the planarization of the interlayer dielectric(ILD) and metal used to form the multilevel interconnections between each layers. Therefore, much research has been conducted to understand the basic mechanism of the CMP process. CMP performed by the down force and the relative speed between pad and wafer with slurry is typical tribo-system. In general, studies have indicated that removal rate is relative to energy. Accordingly, in this study, CMP results will be analyzed by a viewpoint of the friction energy using friction force measurement. The results show that energy would not constant in the same removal rate conditions

전해 이온화와 자외선광을 이용한 사파이어 화학기계적 연마의 재료제거 효율 향상에 관한 기초 연구 (Basic Study on the Improvement of Material Removal Efficiency of Sapphire CMP Using Electrolytic Ionization and Ultraviolet Light)

  • 박성현;이현섭
    • Tribology and Lubricants
    • /
    • 제37권6호
    • /
    • pp.208-212
    • /
    • 2021
  • Chemical mechanical polishing (CMP) is a key technology used for the global planarization of thin films in semiconductor production and smoothing the surface of substrate materials. CMP is a type of hybrid process using a material removal mechanism that forms a chemically reacted layer on the surface of a material owing to chemical elements included in a slurry and mechanically removes the chemically reacted layer using abrasive particles. Sapphire is known as a material that requires considerable time to remove materials through CMP owing to its high hardness and chemical stability. This study introduces a technology using electrolytic ionization and ultraviolet (UV) light in sapphire CMP and compares it with the existing CMP method from the perspective of the material removal rate (MRR). The technology proposed in the study experimentally confirms that the MRR of sapphire CMP can be increased by approximately 29.9, which is judged as a result of the generation of hydroxyl radicals (·OH) in the slurry. In the future, studies from various perspectives, such as the material removal mechanism and surface chemical reaction analysis of CMP technology using electrolytic ionization and UV, are required, and a tribological approach is also required to understand the mechanical removal of chemically reacted layers.

0.13μm Cu/Low-k 공정 Setup과 수율 향상에 관한 연구 (A Study on 0.13μm Cu/Low-k Process Setup and Yield Improvement)

  • 이현기;장의구
    • 한국전기전자재료학회논문지
    • /
    • 제20권4호
    • /
    • pp.325-331
    • /
    • 2007
  • In this study, the inter-metal dielectric material of FSG was changed by low-k material in $0.13{\mu}m$ foundry-compatible technology (FCT) device process based on fluorinated silicate glass (FSG). Black diamond (BD) was used as a low-k material with a dielectric constant of 2.95 for optimization and yield-improvement of the low-k based device process. For yield-improvement in low-k based device process, some problems such as photoresist (PR) poisoning, damage of low-k in etch/ash/cleaning process, and chemical mechanical planarization (CMP) delamination must be solved. The PR poisoning was not observed in BD based device. The pressure in CMP process decreased to 2.8 psi to remove the CMP delamination for Cu-CMP and USG-CMP. $H_2O$ ashing process was selected instead of $O_2$ ashing process due to the lowest condition of low-k damage. NE14 cleaning after ashing process lot the removal of organic residues in vias and trenches was employed for wet process instead of dilute HF (DHF) process. The similar-state of SRAM yield was obtained in Cu/low-k process compared with the conventional $0.13{\mu}m$ FCT device by the optimization of these process conditions.

구리 CMP 후 연마입자 제거에 버프 세정의 효과 (Effect of buffing on particle removal in post-Cu CMP cleaning)

  • 김영민;조한철;정해도
    • 대한기계학회:학술대회논문집
    • /
    • 대한기계학회 2008년도 추계학술대회A
    • /
    • pp.1880-1884
    • /
    • 2008
  • Cleaning is required following CMP (chemical mechanical planarization) to remove particles. The minimization of particle residue is required with each successive technology generation, and the cleaning of wafers becomes more complicated. In copper damascene process for interconnection structure, it utilizes 2-steop CMP consists of Cu CMP and barrier CMP. Such a 2-steps CMP process leaves a lot of abrasive particles on the wafer surface, cleaning is required to remove abrasive particles. In this study, the buffing is performed various conditions as a cleaning process. The buffing process combined mechanical cleaning by friction between a wafer and a buffing pad and chemical cleaning by buffing solution consists of tetramethyl ammonium hydroxide (TMAH)/benzotriazole(BTA).

  • PDF

고정입자 패드를 이용한 층간 절연막 CMP에 관한 연구 (The Study of ILD CMP Using Abrasive Embedded Pad)

  • 박재홍;김호윤;정해도
    • 한국정밀공학회:학술대회논문집
    • /
    • 한국정밀공학회 2001년도 춘계학술대회 논문집
    • /
    • pp.1117-1120
    • /
    • 2001
  • Chemical mechanical planarization(CMP) has emerged as the planarization technique of choice in both front-end and back-end integrated circuit manufacturing. Conventional CMP process utilize a polyurethane polishing pad and liquid chemical slurry containing abrasive particles. There have been serious problems in CMP in terms of repeatability and defects in patterned wafers. Since IBM's official announcement on Copper Dual Damascene(Cu2D) technology, the semiconductor world has been engaged in a Cu2D race. Today, even after~3years of extensive R&D work, the End-of-Line(EOL) yields are still too low to allow the transition of technology to manufacturing. One of the reasons behind this is the myriad of defects associated with Cu technology. Especially, dishing and erosion defects increase the resistance because they decrease the interconnection section area, and ultimately reduce the lifetime of the semiconductor. Methods to reduce dishing & erosion have recently been interface hardness of the pad, optimization of the pattern structure as dummy patterns. Dishing & erosion are initially generated an uneven pressure distribution in the materials. These defects are accelerated by free abrasive and chemical etching. Therefore, it is known that dishing & erosion can be reduced by minimizing the abrasive concentration. Minimizing the abrasive concentration by using Ce$O_2$ is the best solution for reducing dishing & erosion and for removal rate. This paper introduce dishing & erosion generating mechanism and a method for developing a semi-rigid abrasive pad to minimize dishing & erosion during CMP.

  • PDF

Ru CMP Slurry의 개발 및 특성평가 (Development and Characterization of Ru CMP Slurry)

  • 김인권;권태영;박진구;박형순
    • 한국전기전자재료학회:학술대회논문집
    • /
    • 한국전기전자재료학회 2006년도 추계학술대회 논문집 Vol.19
    • /
    • pp.57-58
    • /
    • 2006
  • In MIM (metal insulator metal) capacitor, Ru (ruthenium) has been suggested as new bottom electrode due to its excellent electrical performance, a low leakage of current and compatibility to the high dielectric constant materials. In this case of Ru bottom electrode, CMP (chemical mechanical planarization) process was needed m order to planarize and isolate the bottom electrode. In this study, the effect of chemical A on polishing and etching behavior was investigated as functions of chemical A concentration, abrasive particle and pressure. Chemical A was used as oxidant and etchant. The thickness of passivation layer on the treated Ru surface increased with the increase of chemical A concentration. The etch rate and removal rate of Ru were increased by the addition of chemical A. The removal rate was highest m slurry of pH 9 with the addition of 0.1 M chemical A and 2 wt% alumina at 4 psi. The maximum removal rate is about 80 nm/min.

  • PDF