Retrospective clinical and radiographic evaluation of restored endodontically treated teeth

  • Paula Pontes Garcia ;Aline Cappoani ;Ricardo Susin Schelbauer ;Gisele Maria Correr ;Carla Castiglia Gonzaga
    • Restorative Dentistry and Endodontics
    • /
    • v.45 no.4
    • /
    • pp.49.1-49.11
    • /
    • 2020
  • Objectives: The aim of this study was to perform a clinical and radiographic analysis of endodontically treated teeth (ETT) restored with cast metal posts (CMPs) or prefabricated glass fiber posts (GFPs) and crowns. Materials and Methods: Fifty ETT were restored with 25 CMPs and 25 GFPs at a private dental clinic between 2001 and 2016. The restorations consisted of 12 all-ceramic crowns, 31 metal-ceramic crowns, and 7 composite resin crowns. Demographic data, type of teeth, type of post-and-core system, time of placement, crown restorations, the number of proximal contacts, the type of antagonist, and reports of any complications after post-and-core placement were recorded for each patient. Assessments were performed at baseline (radiographic) and follow-up (radiographic and clinical). Data were analyzed by the McNemar test, the Pearson χ2 test, and Kaplan-Meier survival curves (α = 0.05). The mean follow-up was 67.6 months. Results: No significant difference was observed for any of the radiographic parameters when the baseline and final radiographs were compared. In the clinical evaluation, anatomical form (p = 0.009) and occlusion (p = 0.001) showed significant differences according to the type of crown restoration; specifically, metal-ceramic and all-ceramic crowns outperformed composite resin crowns. Conclusions: CMPs and GFPs showed favorable results for restoring ETT after 6 years of follow-up. All-ceramic and metal-ceramic crowns showed higher survival rates and better clinical outcomes.

FRACTURE STRENGTH OF THE IPS EMPRESS CROWN : THE EFFECTS OF INCISAL REDUCTION AND AXIAL INCLINATION ON UPPER CANINE (IPS Empress 도재관의 파절강도 : 상악 견치에서 절단연 삭제량과 축면 경사도에 따른 영향)

  • Shin Dong-Kuk;Kang Han-Joong;Park Yong-Suck;Park Kwang-Soo;Dong Jin-Keun
    • The Journal of Korean Academy of Prosthodontics
    • /
    • v.43 no.1
    • /
    • pp.30-40
    • /
    • 2005
  • Purpose. The purpose of this study was to compare the fracture strength of the IPS Empress ceramic crown according to the incisal reduction (2.0mm, 2.5mm, 3.0mm) and axial inclination ($4^{\circ}$, $8^{\circ}$, $12^{\circ}$) of the upper canine. Material and methods. After 10 metal dies were made for each group, the IPS Empress ceramic crowns were fabricated and each crown was cemented on each metal die with resin cement. The cemented crowns mounted on the testing jig were inclined 30 degrees and the universal testing machine was used to measure the fracture strength. Results. 1. The fracture strength of the ceramic crown with 3.0mm depth and $12^{\circ}$ inclination was the highest (839N) Crowns of 2.0mm depth and $12^{\circ}$ inclination had the lowest strength (559N). 2. There was no significant difference in the fracture strength by axial inclination in the same incisal reduction group. 3. The fracture mode of the crowns was similar. Most of fracture lines began at the loading area and extended through proximal surface perpendicular to the margin irrespective of incisal reduction.

Crown Duplication Technique of Upper Central Incisor using IPS-Empress system (IPS-Empress system을 이용한 상악 중절치의 치관복제술)

  • Oh, Sang-Chun;Shin, Young-Ho
    • Journal of Dental Rehabilitation and Applied Science
    • /
    • v.22 no.3
    • /
    • pp.243-250
    • /
    • 2006
  • Due to high esthetic demands from patients, we are driven to fabricate natural-looking(form and color) restorations. In the past decade, the glass-ceramic in dentistry has been used as a material with variable crystals that affects the appearance, characteristics, and mechanical properties of metal-free fixed restoration. The conventional IPS Empress glass-ceramic is a heat-pressed, leucite reinforced material using the "lost wax" principle. This glass-ceramic has been successfully used for esthetic restorations such as all-ceramic crowns, inlays/onlays, and veneers for about 15 years. This article presents that the form and surface texture of clinical crown are duplicated by IPS-Empress system using "lost-wax technique".

FRACTURE STRENGTH OF THE IPS EMPRESS CROWN: THE EFFECT OF OCCLUSAL DEPTH AND AXIAL INCLINATION ON UPPER FIRST MOLAR (IPS Empress 도재관의 파절강도 : 상악 제1대구치에서 교합면 두께와 축면경사도에 따른 영향)

  • Choi Teak-Rim;Lee Hae-Young;Dong Jin-Keun
    • The Journal of Korean Academy of Prosthodontics
    • /
    • v.39 no.2
    • /
    • pp.171-183
    • /
    • 2001
  • The purpose of this study was compare the fracture strength of the IPS Empress ceramic crown according to the occlusal depth (1.5mm, 2.0mm, 2.5mm) and axial inclination ($4^{\circ},\;8^{\circ},\;12^{\circ}$) of the upper first molar. After 10 metal dies were made for each group, the IPS Empress ceramic crowns were fabricated and were cemented with resin cement. The cemented crowns mounted on the testing jig were inclined 30 degrees and a universal testing machine was used to measure the fracture strength. The results of this study were as follows: 1. The fracture strength of the ceramic crown with 2.5mm depth and $8^{\circ}$ inclination was the highest (1393N). Crowns of 1.5mm depth and $4^{\circ}$ inclination had the lowest strength (1015N) 2. There were no significant differences of the fracture strength according to occlusal depth and axial inclination. 3. Most fracture lines began at the loading area and extended through proximal surface perpendicular to the margin, irrespective of occlusal depth. 4. There was positive correlation between the fracture strength and the fracture surface area of crowns.

  • PDF

Fracture Strength of IPS Empress Crown : The Effect of Incisal Reduction and Axial Inclination on Lower Canine (IPS Empress 도재관의 파절강도 : 하악 견치에서 절단연 삭제량과 축면 경사도에 따른 영향)

  • Jung, Young-Chan;Shin, Dong-Kuk;Park, Eun-Ju;Kim, Min-Jeong;Dong, Jin-Keun
    • Journal of Dental Rehabilitation and Applied Science
    • /
    • v.20 no.1
    • /
    • pp.19-29
    • /
    • 2004
  • The purpose of this study was to compare the fracture strength of the IPS Empress ceramic crown according to the incisal reduction(2.0mm, 2.5mm, 3.0mm) and axial inclination ($4^{\circ}$, $8^{\circ}$, $12^{\circ}$) of the lower canine. After 10 metal dies were made for each group, the IPS Empress ceramic crowns were fabricated and each crown was cemented on each metal die with resin cement. The cemented crowns mounted on the testing jig were inclined 30 degrees and a universal testing machine was used to measure the fracture strength. The results of this study were as follows : 1. The fracture strength of the ceramic crown with 3.0mm depth and $12^{\circ}$ inclination was the highest(1377N). Crowns of 2.0mm depth and $4^{\circ}$ inclination had the lowest strength (731 N). 2. There were no significant differences of the fracture strength by axial inclination in same incisal reduction group. 3. The fracture mode of the crowns was similar. Most of fracture lines began at the loading area and extended through proximal surface perpendicular to the margin irrespective of incisal reduction.

Fracture strength of the IPS Empress crown :The effect of incisal reduction and axial inclination on upper central incisor (IPS Empress 도재관의 파절강도 : 상악 중절치에서 절단연 삭제량과 축면 경사도에 따른 영향)

  • Song, Byung-Kwen;Lee, Hae-Hyoung;Dong, Jin-Keun
    • Journal of Dental Rehabilitation and Applied Science
    • /
    • v.16 no.3
    • /
    • pp.237-245
    • /
    • 2000
  • The purpose of this study was to compare the fracture strength of the IPS Empress ceramic crown according to the incisal depth(2.0mm, 2.5mm, 3.0mm) and axial inclination($4^{\circ}$, $8^{\circ}$, $12^{\circ}$) of the upper central incisor. After 10 metal dies were made for each group, the IPS Empress ceramic crowns were fabricated and each crown was cemented on each metal die with resin cement. The cemented crowns mounted on the testing jig were inclined 30 degrees and a universal testing machine was used to measure the fracture strength. The results were : 1. The fracture strength of the ceramic crown with 2.5mm depth and $8^{\circ}$ inclination was the highest(965N). Crowns of 2.0mm depth and $4^{\circ}$ inclination had the lowest strength(713N). There were no significant differences of the fracture strength by axial inclination in same incisal depth group. 2. The fracture mode of the crowns was similar. Most of fracture lines began at the loading area and extended through proximal surface perpendicular to the margin irrespective of incisal depth. There had correlation between fracture strength and fractured surface area.

  • PDF

Effect of the shades of background substructures on the overall color of zirconia-based all-ceramic crowns

  • Suputtamongkol, Kallaya;Tulapornchai, Chantana;Mamani, Jatuphol;Kamchatphai, Wannaporn;Thongpun, Noparat
    • The Journal of Advanced Prosthodontics
    • /
    • v.5 no.3
    • /
    • pp.319-325
    • /
    • 2013
  • PURPOSE. The objective of this study was to determine the effect of the color of a background substructure on the overall color of a zirconia-based all-ceramic crown. MATERIALS AND METHODS. Twenty one posterior zirconia crowns were made for twenty subjects. Seven premolar crowns and six molar crowns were cemented onto abutments with metal post and core in the first and second group. In the third group, eight molar crowns were cemented onto abutments with a prefabricated post and composite core build-up. The color measurements of all-ceramic crowns were made before try-in, before and after cementation. A repeated measure ANOVA was used for a statistical analysis of a color change of all-ceramic crowns at ${\alpha}$=.05. Twenty four zirconia specimens, with different core thicknesses (0.4-1 mm) were also prepared to obtain the contrast ratio of zirconia materials after veneering. RESULTS. $L^*$, $a^*$, and $b^*$ values of all-ceramic crowns cemented either on a metal cast post and core or on a prefabricated post did not show significant changes (P>.05). However, the slight color changes of zirconia crowns were detected and represented by ${\Delta}E{^*}_{ab}$ values, ranging from 1.2 to 3.1. The contrast ratios of zirconia specimens were 0.92-0.95 after veneering. CONCLUSION. No significant differences were observed between the $L^*$, $a^*$, and $b^*$ values of zirconia crowns cemented either on a metal cast post and core or a prefabricated post and composite core. However, the color of a background substructure could affect the overall color of posterior zirconia restorations with clinically recommended core thickness according to ${\Delta}E{^*}_{ab}$ values.

Six-year clinical performance of lithium disilicate glass-ceramic CAD-CAM versus metal-ceramic crowns

  • Ahmed Aziz;Omar El-Mowafy
    • The Journal of Advanced Prosthodontics
    • /
    • v.15 no.1
    • /
    • pp.44-54
    • /
    • 2023
  • PURPOSE. To assess the clinical performance of monolithic CAD-CAM lithium disilicate glass-ceramic (LDGC) crowns and metal-ceramic (MC) crowns provided by predoctoral students. This study also assessed the effects of patient and provider-related factors on their clinical performance as well as patient preference for these types of crowns. MATERIALS AND METHODS. Twenty-five patients who received 50 crowns (25 LDGC CAD-CAM and 25 MC) provided by predoctoral students were retrospectively examined. LDGC CAD-CAM crowns were milled in-house using the CEREC Bluecam system and cemented with either RelyX Unicem or Calibra Esthetic resin cements. MC crowns were cemented with RelyX Unicem cement. Clinical assessment of the crowns and the supporting periodontal structures were performed following the modified California Dental Association (CDA) criteria. Patients' preference was recorded using a visual analog scale (VAS). The results were statistically analyzed using log-rank test, Pearson Chi-squared test and Kaplan-Meier survival analysis. RESULTS. Twelve complications were observed in the MC crown group (9-esthetic, 2-technical and 1-biological). In comparison, 2 complications in the LDGC CAD-CAM crown group were observed (1-technical and 1-esthetic). The 6-year cumulative survival rates for MC crowns and LDGC CAD-CAM were 90.8% and 96%, respectively, whereas the success rates were 83.4% and 96%, respectively. Overall, patients preferred the esthetic outcomes of LDGC CAD-CAM crowns over MC crowns. CONCLUSION. The high survival and success rates, low number of complications, and the high level of patients' acceptance of monolithic LDGC CAD-CAM crowns lend them well as predictable and viable alternatives to the "gold standard" MC crowns.

Fracture Resistance and Stress Distribution of All Ceramic Crowns with Two Types of Finish Line on Maxillary Central Incisor (IPS Empress 도재관의 파절강도: 하악 중절치에서 절단연 삭제량과 축면 경사도에 따른 영향)

  • Nam, Young-Sung;Kim, Kyea-Soon;Jung, Young-Chan;Kim, Yu-Lee;Dong, Jin-Keun
    • Journal of Dental Rehabilitation and Applied Science
    • /
    • v.19 no.3
    • /
    • pp.207-217
    • /
    • 2003
  • The purpose of this study was to compare the fracture strength of the IPS Empress ceramic crown according to the incisal depth (1.5mm, 2.0mm, 2.5mm) and axial inclination ($4^{\circ}$, $8^{\circ}$, $12^{\circ}$) of the lower central ncisor. After 10 metal dies were made for each group, the IPS Empress ceramic crowns were fabricated and each crown was cemented on each metal die with resin cement. The cemented crowns mounted on the testing jig were inclined 30 degrees and a universal testing machine was used to measure the fracture strength. The results of this study were as follows : The fracture strength of the ceramic crown with 2.0mm depth and $12^{\circ}$ inclination was the highest (648 N). Crowns of 1.5mm depth and $4^{\circ}$ inclination had the lowest strength (482 N). There were no significant differences of the fracture strength by axial inclination in same incisal depth group. The fracture mode of the crowns was similar. Most of fracture lines began at the loading area and extended through proximal surface perpendicular to the margin irrespective of incisal depth. There had correlation between fracture strength and fractured surface area.

A STUDY ON MARGINAL FIDELITY OF CERAMIC METAL COPINGS TREATED BY VARIOUS METHODS (도재용 금속 코핑의 처리 방법에 따른 변연 적합도에 관한 연구)

  • Koo, Bum-Mo;Lim, Ju-Hwan;Cho, In-Ho
    • The Journal of Korean Academy of Prosthodontics
    • /
    • v.35 no.2
    • /
    • pp.265-276
    • /
    • 1997
  • The effect of thermocycling and surface finishing on the marginal fidelity of copings for a metal ceramic crown was examined. Methods for minimizing the loss of marginal fidelity were evaluated. The results were as follows ; 1. Thermocycling of ceramic metal copings resulted in increased marginal gap. 2. The greatest marginal gap occurred during the first thermocycling of the copings. 3. No additional distortion of marginal fidelity occurred when surface finishing and second thermocycling were completed after initial thermocycling. 4. The gap increases according to various treatment methods showed group 1 to be the highest values. 5. There was no significant difference between group 2 and group 3(p>0.05) 6. There was significant difference between group 1 and group 2, 3(p<0.05). 7. There was no significant difference among the measurement sites.

  • PDF