• Title/Summary/Keyword: butadiene rubber

Search Result 279, Processing Time 0.032 seconds

Surface Modification of Steel Tire Cords via Plasma Etching and Plasma Polymerization Coating : Part II. Characterization (플라즈마 고분자 코팅에 의한 강철 타이어 코드의 표면 개질 : 제2부. 타이어 코드의 분석)

  • Kang, H.M.;Chung, K.H.;Kaang, S.;Yoon, T.H.
    • Elastomers and Composites
    • /
    • v.35 no.1
    • /
    • pp.63-70
    • /
    • 2000
  • Zinc plated steel tire cords were subjected to RF plasma etching of argon, followed by plasma polymerization coating of acetylene or butadiene in order to enhance adhesion to rubber compounds. Plasma polymerization was carried out under optimized conditions of 10 W, 30 sec, 30 mTorr for acetylene and butadiene gas, while plasma etching was performed at 90W, 10min and 30mTorr. The adhesion of tire cords was evaluated via Tire Cords Adhesion Test (TCAT) and the failure surfaces of the tested samples were analyzed by SEM. Polymer coating by plasma polymerization was also characterized by FT-IR, Alpha-Step and dynamic contact angle analyzer in order to elucidate the adhesion mechanism.

  • PDF

Gold functionalized-graphene oxide-reinforced acrylonitrile butadiene rubber nanocomposites for piezoresistive and piezoelectric applications

  • Mensah, Bismark;Kumar, Dinesh;Lee, Gi-Bbeum;Won, Joohye;Gupta, Kailash Chandra;Nah, Changwoon
    • Carbon letters
    • /
    • v.25
    • /
    • pp.1-13
    • /
    • 2018
  • Gold functionalized graphene oxide (GOAu) nanoparticles were reinforced in acrylonitrile-butadiene rubbers (NBR) via solution and melt mixing methods. The synthesized NBR-GOAu nanocomposites have shown significant improvements in their rate of curing, mechanical strength, thermal stability and electrical properties. The homogeneous dispersion of GOAu nanoparticles in NBR has been considered responsible for the enhanced thermal conductivity, thermal stability, and mechanical properties of NBR nanocomposites. In addition, the NBR-GOAu nanocomposites were able to show a decreasing trend in their dielectric constant (${\varepsilon}^{\prime}$) and electrical resistance on straining within a range of 10-70%. The decreasing trend in ${\varepsilon}^{\prime}$ is attributed to the decrease in electrode and interfacial polarization on straining the nanocomposites. The decreasing trend in electrical resistance in the nanocomposites is likely due to the attachment of Au nanoparticles to the surface of GO sheets which act as electrical interconnects. The Au nanoparticles have been proposed to function as ball rollers in-between GO nanosheets to improve their sliding on each other and to improve contacts with neighboring GO nanosheets, especially on straining the nanocomposites. The NBR-GOAu nanocomposites have exhibited piezoelectric gauge factor (${GF_{\varepsilon}}^{\prime}$) of ~0.5, and piezo-resistive gauge factor ($GF_R$) of ~0.9 which clearly indicated that GOAu reinforced NBR nanocomposites are potentially useful in fabrication of structural, high temperature responsive, and stretchable strain-sensitive sensors.

Foaming Behavior, Structure, and Properties of Rubber Nanocomposites Foams Reinforced with Zinc Methacrylate (아연 메타아크릴레이트로 보강된 발포고무 나노복합체의 발포거동, 구조 및 특성)

  • Basuli, U.;Lee, G.B.;Jang, S.Y.;Oh, J.;Lee, J.H.;Kim, S.C.;Jeon, N.D.;Huh, Y.I.;Nah, C.
    • Elastomers and Composites
    • /
    • v.47 no.4
    • /
    • pp.297-309
    • /
    • 2012
  • Different amounts of foaming agents were employed in natural rubber(NR)/butadiene rubber(BR) blends to understand the foaming behavior in presence of nano-reinforcing agent, zinc methacrylate (ZMA). The ZMA greatly improved most of the mechanical properties of the rubber foams, however it did not show considerable effect on the cell morphology, such as cell size, density and porosity. It was also observed that the foaming agent concentration affected all the mechanical parameters. When the content of foaming agent was increased, the number of foams was increased leading to a decrease in density of the compounds. But the size and distribution of foams remained unchanged with increased foaming agent. The effect of high styrene-butadiene rubber (HSBR) was also studied. The size of cells became smaller and the cell uniformity was improved with increasing HSBR. The foam rubber compounds showed much efficient energy absorbing capability at higher strains.

Effect of Silane and Sulfur Variation on the Vulcanizate Structure of Silica-Filled Styrene-Butadiene Rubber Compounds

  • Han, Sangwook;Kim, Donghyuk;Kim, Seongrae;Kim, Jongmyoung;Mun, Dalyong;Morita, Koichi;Kim, Wonho
    • Elastomers and Composites
    • /
    • v.56 no.1
    • /
    • pp.32-42
    • /
    • 2021
  • The vulcanizate structure of silica-filled compounds is affected by the filler-rubber interaction (FRI) due to the silica-rubber coupling reaction and the chemical crosslink density (CCD) of the matrix rubber. In this study, the vulcanizate structure changes of silica-filled compounds according to the silane and sulfur variation were quantitatively analyzed using the Flory-Rehner and Kraus equations. In efficiency vulcanization (EV) conditions with low sulfur content, FRI increased when the bis-[3-(triethoxysilyl)propyl]tetrasulfide (TESPT) content increased, and the CCD clearly decreased. By contrast, in semi-EV conditions with high sulfur content, as TESPT content increased, the FRI increased the same way EV conditions, but the CCD was unchanged. Based on these results, it was confirmed that FRI of the silica-filled compounds increased as TESPT content increased, but CCD decreased or retained similar values according to the vulcanization system, indicating that the formation reaction of FRI was preferred over CCD.

Study on the noise reduction occurred to rotation in duct (덕트 회전체에서 발생하는 소음저감에 대한 연구)

  • Park, Hong-Ul;Kim, You-Jae;Park, Sung-Kwan
    • Proceedings of the Korean Society for Noise and Vibration Engineering Conference
    • /
    • 2006.11a
    • /
    • pp.875-879
    • /
    • 2006
  • Noise reduction has become a major issue of the duct air-conditioners. This paper describes the reduction of noise and vibration of rotational slim duct system. The design of slim duct system is the most important point of noise reduction in terms of the motor of 2f line noise, resonance noise between forced frequency and natural frequency of Sirocco fan, unbalance noise of motor axis and the noise induced refrigerant. The noise of duct system is mainly measured from diffuser and bottom of duct. The optimal design was implemented after measuring the effect of noise and vibration in each part which is composed of duct system. In this paper, experimental results show that the main elements in air-conditioner duct design. These elements are anti-vibration rubber of motor, axis length of motor, rubber coupler, materials of sirocco fan and control method of motor which are the most vital factors in reducing noise.

  • PDF

Effect of Environmental Factors on the Properties of Polymeric Material(II) : Temperature and Ozone Exposure Time (고분자재료의 물성에 미치는 환경인자의 영향(II) : 온도 및 오존 노출시간)

  • 박찬영;박성수;민성기
    • Journal of Environmental Science International
    • /
    • v.10 no.1
    • /
    • pp.73-77
    • /
    • 2001
  • This study examined blends of styrene butadiene rubber(SBR) and chloroprene rubber(CR) prepared from an open 2-roll mill following the conventional polymer blend method for a wide range of the blend composition. Rubber vulcanizates were manufactured by hot press and then mechanical properties, heat and ozone resistance of the specimens were examined. Due to the post cure during the aging test, hardness of vulcanizates was increased. It was found that the undesirable characteristics of heat and ozone resistance of pure SBR was significantly improved through the blending of SBR with CR.

  • PDF

Preparation of Cross-linked Asymmetric Membrane and Control of Its Morphology and Mechanical Property

  • Hong, Byung-Pyo;Ko, Moon-Young;Kwon, Byeong-Min;Byun, Hong-Sik
    • Korean Membrane Journal
    • /
    • v.10 no.1
    • /
    • pp.1-7
    • /
    • 2008
  • Polystyrene-co-divinylbenzene (PS-co-DVB) asymmetric membranes were prepared. In order to control their structure and mechanical properties the degree of cross-linking and the composition of casting solution were varied. The rubber added PS-DVB membranes was also prepared to overcome the mechanical limitation of cross-linked membrane, and their mechanical properties were investigated. It was revealed that the concentration of polymer in the casting solution affected the determination of skin formation. When the PS-co-DVB membrane consists of styrene-butadiene (SB) rubber or liquid polybutadiene (PBD), the structures formed showed that the PS content in the PS/DVB system played an important role in determining the porous sublayer structure.

Studies on the Physical Properties and Application of EPDM-Polymer Blends. Part 6. Physical Properties for EPDM-NR-SBR Blends (EPDM과 각종(各種) Polymer의 Blend에 의(依)한 성능변화(性能變化) 및 그 응용(應用)에 관(關)한 연구(硏究)(제6보(第6報)) EPDM과 Natural Rubber 및 Butadiene-Styrene Rubber의 Blend에 대(對)하여)

  • Kim, Joon-Soo
    • Elastomers and Composites
    • /
    • v.7 no.2
    • /
    • pp.183-192
    • /
    • 1972
  • As a series of tile studies of EPDM-Polymer blends, tile experiment are concentrated to the investigation of the physical properties of tile EPDM-NR-SBR blends. The results are shown as follows: 1. In blending, tensile strength decreased with increase in EPDM contents, especially the ratio of EPDM/NR-SBR is 75/25. 2. Elongation and tear strength were much influenced by blending, especially the ratio of EPDM/NR-SBR is 50/50. 3. Ozone resistance is much improved after blending. It was effective more than tile ratio of EPDM/NR-SBR is 25/75. 4. Aging resistance is much improved after blending. It was effective more than the ratio of EPDM/NR-SBR is 50/50. 5. Hardness increased with increase in EPDM contents and on the other hand, abrasion resistance decreased.

  • PDF

Zinc Surfactant Effects on Nr/Tespd/Silica and SBR/Tespd/Silica Compounds

  • Kim, Kwang-Jea;Vanderkooi, John
    • Elastomers and Composites
    • /
    • v.39 no.4
    • /
    • pp.263-273
    • /
    • 2004
  • The effects of zinc surfactant (ZB) on the bis(triethoxysilylpropyl)disulfide (TESPD)-silica mixture in natural rubber (NR) and solution butadiene-co-styrene rubber(S-SBR) were compared with respect to their rheological property, processability, physical properties, and silica dispersion. In the NR compound, addition of the ZB increased the reversion resistance time (T-2), the tensile modulus, and the BO time; however, lowered the viscosity, the HBU, and tans values. In the S-SBR copound, addition of the ZB increased the $tan{\delta}$ values while lowered the T-2, the tensile modulus the BO time, the viscosity, and the HBU of the compound. In the NR compounds, addition of the ZB significantly increased the processability and mechanical property. However, in the S-SBR compounds, it improved the processability the mechanical property was not improved.

Kinetic Study on the Thermal Degradation of Poly(Methyl Methacrylate) and Poly(Acrylonitrile Butadiene Styrene) Mixtures (Poly(methyl methacrylate)와 Poly(acrylonitrile butadiene styrene)와의 혼합에 의한 열분해속도에 관한 연구)

  • Moon, Deok-Ju;Kim, Dong-Keun;Seul, Soo-Duk
    • Elastomers and Composites
    • /
    • v.24 no.1
    • /
    • pp.11-18
    • /
    • 1989
  • The thermal degradation of Poly(methyl methacrylate) (PMMA) and poly(acrylonitrile butadiene styrene)(ABS) terpolymer as well as their mixtures were carried out using the thermogravimetry and differential scanning calorimetry(DSC) in the stream of nitrogen and air with 50 ml/min at the various heating rate from 4 to $20^{\circ}C/min$ and temperature from 200 to $300^{\circ}C$ The values of activation energies of thermal degradation determined by TG and DSC in the various PMMA/ABS mixtures were $34{\sim}58Kcal/mol,\;35{\sim}54Kcal/mol$ in the stream of nitrogen. The values of activation energy of ABS20% mixture was appeared high in camparison with addition rule. According to increasing the composition of ABS, the temperatures of glass transition and initial decomposition temperature were increased. PMMA/ABS mixtures by the analysis of infrared spectrophotometer were decomposed by main chain scission in the stream of nitrogen.

  • PDF