  • The effect of the treatment with CCFZ, FR-4, and PEG400 from butt end on the dimensional stability and bending properties was examined. Three softwood species such as red pine, Korean white pine and Japanese larch and three hardwood species such as poplar, alder and oak were investigated in this research. Shrinkage of red pine, Korean white pine, poplar, and alder treated with PEG400 decreased. However, there was no significant decrease of shrinkage in Japanese larch and oak. The decrease of shrinkage when moisture content changed from about 20% to 10% was larger than that at any other phase. In regard to the effect of treatment on bending properties, bending MOE and MOR of all specimens treated with PEG400 decreased significantly. Especially in the case of red pine, poplar, and alder treated with PEG400, bending MOR reduced 9%, 14%, and 12%, respectively. Reductions of MOR of the hardwood was also much larger than that of the softwood. However, in all species, treatment with CCFZ and FR-4 did not affect the change of bending MOE and MOR significantly. Comparing the large specimen which also included heartwood with the small specimen which included only treated sapwood, there was a difference in the change of bending MOE and MOR between them. The large specimens of Korean white pine, alder and Poplar, which had a relatively low proportion of sapwood(18~22%), showed the decrease of MOR by 11~13% more than that of small specimens, while red pine, Japanese larch and oak, which had a relatively high proportion of sapwood(35~40%), showed little decrease. It means that bending MOE and MOR of structural wood treated from butt end should be considered in terms of sapwood proportion as well as effect of treated chemicals.

  • PDF

Applicability of the induction bending process to the P91 pipe of the PGSFR

  • Kim, Nak Hyun;Kim, Jong Bum;Kim, Sung Kyun
    • Nuclear Engineering and Technology
    • /
    • 제53권5호
    • /
    • pp.1580-1586
    • /
    • 2021
  • The application of induction bending processes to industrial pipe production is increasing. The induction bending process has the effect of reducing the number of inspections and preventing leaks by reducing the weld of the pipe. For these reasons, efforts have been made to apply an induction bending process to the pipe of the PGSFR under development in Korea and this is the first attempt in the SFR design. Since the PGSFR pipe has a relatively large diameter-to-thickness ratio, it is difficult to fabricate an induction bending pipe that meets the requirements. In addition, the material properties may change because the pipe heats to a very high temperature during the induction bending process. In this study, P91 pipes were fabricated by induction bending, and the results from analyzing the induction bending process' applicability to the P91 pipe of the PGSFR are examined. The various dimensional measurements of the pipes fabricated by the induction bending process were surveyed to determine whether the requirements of the ASME Code were met. The minimum thickness, ovality, and wall buckling measured in the fabricated pipe met all the requirements. Tensile, impact, and hardness tests at various locations of the fabricated pipe also satisfied the requirements.

Evaluation of Physical and Mechanical Properties of Non-certificated Laminated Veneer Lumber (LVL) Circulated in Domestic Lumber Market

  • Oh, Sei-Chang
    • Journal of the Korean Wood Science and Technology
    • /
    • 제39권5호
    • /
    • pp.429-436
    • /
    • 2011
  • The selected physical and mechanical properties of non-certificated LVL circulated in domestic lumber market were investigated and compared to relevant standards. The tested LVL passed the moisture content and the soaking delamination rate limit as per domestic (KS) and Japanese standard (JAS). The evaluated mechanical properties were flatwise/edgewise bending strength, modulus of elasticity (MOE), horizontal shear and compressive strength. The 30 mm-thick LVL showed significantly higher bending strength than that of the 25 mm-thick LVL. The modulus of elasticity (MOE) showed same tendency in the results of bending strength. The edgewise bending strength and MOE were higher than that of flatwise bending strength and MOE. The horizontal shear strength values were also showed similar results to bending strength values. The tested results were compared each other and each products were graded according to JAS 701 grade specification. The failure mode of LVL in bending test showed the similar failure mode of solidwood that failed in a simple tension manner (splintery tension). The glue line failure was severe in 25 mm-thick specimens due to concentration of shear stress in layer discontinuity containing small voids and starved glue lines. In horizontal shear strength test, failure mode of LVL showed the typical horizontal shear failure. Compressive specimens failed with fiber crushing in company with apparent delamination that splitted along the length of the specimens. From the results, the complete bonding between lamination and consistency in thin veneer layer were considered as a critical factor in the mechanical properties of LVL. Moreover, the standard test procedure and specification for non-certificated LVL should be required to check the performance of uncertificated materials.

Effect of Induction Heat Bending Process on the Properties of ASME SA106 Gr. C Carbon Steel Pipes

  • Kim, Ki Tae;Kim, Young Sik;Chang, Hyun Young;Oh, Young Jin;Sung, Gi Ho
    • Corrosion Science and Technology
    • /
    • 제14권2호
    • /
    • pp.47-53
    • /
    • 2015
  • Recently, the bending process is greatly applied to fabricate the pipe line. Bending process can reduce welding joints and then decrease the number of inspection. Thus, the maintenance cost will be reduced. Induction heat bending process is composed of bending deformation by repeated local heat and cooling. By this thermal process, corrosion properties and microstructure can be affected. This work focused on the effect of induction heating bending process on the properties of ASME SA106 Gr. C low carbon steel pipes. Microstructure analysis, hardness measurements, and immersion corrosion test were performed for base metal and bended area including extrados, intrados, crown up, and down parts. Microstructure was analyzed using an optical microscope and SEM. Hardness was measured using a Rockwell B scale. Induction heat bending process has influenced upon the size and distribution of ferrite and pearlite phases which were transformed into finer structure than those of base metal. Even though the fine microstructure, every bent area showed a little lower hardness than that of base metal. It is considered that softening by the bending process may be arisen. Except of I2, intrados area, the others showed a similar corrosion rate to that of base metal. But even relatively high rate of intrados area was very low and acceptable. Therefore, it is judged that induction heat bending process didn't affect boric acid corrosion behaviour of carbon steel.

고강도 강선의 인장 및 회전굽힘 피로특성 (Characteristic of Fatigue Properties with Tension and Bending Loading Using High Strength Steel Wire)

  • 우병철;김상수;김병걸;서창민
    • 대한기계학회논문집A
    • /
    • 제25권1호
    • /
    • pp.161-167
    • /
    • 2001
  • The overhead transmission wires operating both at warm temperature and tighten state for a long period of time in a power transmission plant are degraded by air pollution, wind, creep and slip between steel wire and aluminium conductor. The objective of this study is to investigate to investigate the characteristics of fatigue properties with tension and bending loading of a high carbon steel wire. The fatigue behaviors have been carried out by tension-tension, 4 points bending and 3 points bending loading. In the present study, a conventional fatigue strengths between 4 points bending and tension-tension fatigue were determined by Gerber, Sorderberg and Goodmans theory and we investigated S-N diagram for bending and tensile loading.

알루미늄 사각관의 굽힘붕괴특성에 관한 실험적 고찰 (Experimental Study on The Bending Collapse Characteristics of Al Rectangular Tubes)

  • 강신유;김창수;정태은
    • 한국소성가공학회:학술대회논문집
    • /
    • 한국소성가공학회 1997년도 춘계학술대회논문집
    • /
    • pp.265-272
    • /
    • 1997
  • In this paper the bending collapse characteristics of 60 series Al rectangular tubes were studied with a pure bending collapse test rig which could apply the pure bending moment, there occured three kinds of bending collapse modes - local buckling, delayed buckling, tensile failure - depending on the b/t(width/thickness) ratio and material properties. Experiment results are compared with the results of finite element method.

  • PDF

알루미늄 합금박판 비등온 성형공정 스프링백 해석용 유한요소 프로그램 개발 ( 1부 : 실험 ) (Development of Finite Element Program for Analyzing Springback Phenomena of Non-isothermal Forming Processes for Aluminum Alloy Sheets(Part 1 : Experiment))

  • 금영탁;유동열;한병엽
    • 소성∙가공
    • /
    • 제12권3호
    • /
    • pp.202-207
    • /
    • 2003
  • In order to examine the springback amount and material properties of aluminum alloy sheets (AL1050 and AL5052) in the warm forming which forms the sheet above the room temperature, the stretch bending and draw bending tests and tensile test in various high temperatures are carried out. The warm forming temperature 15$0^{\circ}C$ is a transition in terms of the material properties: over the forming temperature 15$0^{\circ}C$, them $\sigma$$_{YS}$ , $\sigma$$_{TS}$ , E, K, n, etc. are bigger but $\varepsilon$ and plastic strain ratio are smaller. Below the forming temperature 15$0^{\circ}C$, there are no big differences in material properties as the forming temperature changes. AL5052 sheet has more springback effect than AL1050 sheet. While the springbacks of AL5052 and AL1050 sheets show a big reduction over the warm forming temperature 15$0^{\circ}C$ in the stretch bending test, the springback rapidly reduces in the warm forming temperature 15$0^{\circ}C$-20$0^{\circ}C$ for AL5052 sheet and 20$0^{\circ}C$-25$0^{\circ}C$ for AL1050 sheet in the draw bending test.

옻나무 경사핑거접합재의 휨강도와 AE 특성 (The Bending Strength and Acoustic Emissions Properties of Sloped Finger-Jointed Rhus Verniciflua)

  • 변희섭;김사익
    • 한국가구학회지
    • /
    • 제10권2호
    • /
    • pp.73-78
    • /
    • 1999
  • This paper describes the relationship between the bending strength properties of sloped finger-jointed woods and the acoustic emissions(AEs) generated during the test. Rhus verniciflua pieces were cut in sloped-finger types and glued with three kinds of adhesives(polyvinyl acetate, polyvinyl-acryl acetate and oilic urethane resin). The slope ratios of finger joints were 0, 1.0, 1.5, and 2.0. The AE cumulative event count and cumulative count were measured during the bending test. The results were as follows: The lower the bending strength(load) was, the generation time of AE event count got and the higher the increasing rate of AE event count became in the sloped finger-jointed specimens bonded with polyvinyl acetate, polyvinyl-acryl acetate oilic urethane resin adhesives. Therefore, the slope from load-AE cumulative event count was very steep. The patterns of AE event count and count were very similar. The relationship between the MOR and the AE parameter from load and AE cumulatve event count in the early stage of the sloped finger-jointed specimens bonded with polyvinyl acetate, polyvinyl-acryl and oilic urethane resin adhesives was much greater than that between the MOE and the MOR. Therefore, the AE signals obtained during bending test are useful for estimating the strength of sloped finger-jointed Rhus verniciflua specimens.

  • PDF

양버즘나무의 소재(素材) 및 집성곡목제조(集成曲木製造)에 관(關)한 연구(硏究)(I) - 증자(蒸煮)에 의한 소재(素材)휨가공성(加工性) - (Study on the Solid and Laminated Wood Bending of Platanus occidentalis L.(I) - Solid Wood-bending Properties by Steaming -)

  • 소원택;정희석
    • Journal of the Korean Wood Science and Technology
    • /
    • 제18권4호
    • /
    • pp.26-40
    • /
    • 1990
  • The plane trees(Platanus occidentalis L.) have been grown in Korea very widely as ornamental garden or street trees but they have not been used as manufacturing materials The proportion of imported wood has been now over 85% of raw materials needed in the wood industry, and therefore, many of studies on the substitution of domestic wood for imported wood and on the increasing the utilization rate of domestic species have been attempted and considered as very important projects to solve. From a this point of view, this study was carried out to investigate solid wood bending properties of plane trees and then to develop their end-uses, and the size of specimens tested was $15\times15\times350mm$ for steaming treatment and they were dried to $15\pm1%$ before bending. The results obtained were as follows: 1. The optimum conditions for solid wood bending processing of Platanus occidentalis are showed in Table 7. 2. The minimum solid-bending radii of Platanus occidentalis were 40mm in steaming treatment. 3. The effect of knots, diagonal grain and decay on the degradation of bending processing properties were very severe. 4. The bending stress was setted successfully through $80^{\circ}C$-15hrs drying after bending and the spring back for 24hr-exposing time was only about 1%.

  • PDF

파티클보드에 보강된 유리섬유의 layer 수가 기계적 성질에 미치는 영향 (The effect of mechanical properties on the particleboard reinforced with fiberglass layer number)

  • 차재경
    • 한국가구학회지
    • /
    • 제21권5호
    • /
    • pp.347-353
    • /
    • 2010
  • This research examined the technical feasibility of composite that had 2- and 3- layers of fiberglass reinforcement to enhance the load carrying capacity of particleboard. Specimens were prepared from commercial particleboard. Results indicated that bending properties, hardness and impact bending energy increased as the number of layers of fiberglass reinforcement increased. The wood screw withdrawal load only decreased at the 3-layer of fiberglass reinforcement. The technique developed by this study may increase an opportunity to use particleboard for structural purposes.