• Title/Summary/Keyword: ball milling processing

Search Result 63, Processing Time 0.028 seconds

Effect of Powder Morphology on the Deposition Quality for Direct Laser Melting (Direct Laser Melting 공정시 분말 형태가 적층 품질에 미치는 영향)

  • Lee, S.H.;Kil, T.D.;Han, S.W.;Moon, Y.H.
    • Transactions of Materials Processing
    • /
    • v.25 no.3
    • /
    • pp.195-202
    • /
    • 2016
  • Direct laser melting(DLM) is an additive manufacturing process that can produce parts by solidification of molten metallic powder layer by layer. The properties of the fabricated parts strongly depend on characteristics of the metallic powder. Atomized powders having spherical morphology have commonly been used for DLM. Mechanical ball-milling is a powder processing technique that can provide non-spherical solid powders without melting. The aim of the current study was to investigate the effect of powder morphologies on the deposition quality in DLM. To characterize the morphological effect, the performances of spherical and non-spherical powders were compared using both single- and multi-track DLM experiments. DLM experiments were performed with various laser process parameters such as laser power and scan rate, and the deposition quality was evaluated. The surface roughness, cross-section bead shape and process defects such as balling or non-filled area were compared and discussed in this study.

Wet preparation of calcium phosphates from aqueous solutions

  • Lee, Byeong Woo;Hong, Il Gok
    • Journal of Ceramic Processing Research
    • /
    • v.20 no.6
    • /
    • pp.655-659
    • /
    • 2019
  • Calcium phosphates such as HA (hydroxyapatite), β-TCP (tricalcium phosphate) and biphasic HA/β-TCP, were synthesized by wet chemical precipitation in aqueous solution combined with ball milling process. Nanosize powders of the calcium phosphates were synthesized using Ca(OH)2 and H3PO4. The effects of initial precursor Ca/P ratio (1.30, 1.50 and 1.67), ball milling process and post heat-treatment on the phase evolution behavior of the powders were investigated. The phase of resulting powder was controllable by adjusting the initial Ca/P ratio. HA was the only phase for as-prepared powders in both cases of Ca/P ratios of 1.50 and 1.67. The single HA phase without any noticeable second phase was obtained for the initial Ca/P ratio of 1.67 in the overall heat-treatment range. Pure β-TCP and biphasic calcium phosphate (HA/β-TCP) were synthesized from precursor solutions having Ca/P molar ratios of 1.30 and 1.50, respectively, after having been heat-treated above 700 ℃. The β-TCP phase has appeared on the pre-existing DCPD (dicalcium phosphate dihydrate) and/or HA phase. Dense ceramics having translucency were obtained at a considerably lower sintering temperature. The modified process offered a fast, convenient and economical route for the synthesis of calcium phosphates.

Thermal Stability of Amorphous Ti-Cu-Ni-Sn Prepared by Mechanical Alloying

  • Oanha, N.T.H.;Choi, P.P.;Kim, J.S.;Kim, J.C.;Kwone, Y.S.
    • Proceedings of the Korean Powder Metallurgy Institute Conference
    • /
    • 2006.09b
    • /
    • pp.953-954
    • /
    • 2006
  • Ti-Cu-Ni-Sn quaternary amorphous alloys of $Ti_{50}Cu_{32}Ni_{15}Sn_3$, $Ti_{50}Cu_{25}Ni_{20}Sn_5$, and $Ti_{50}Cu_{23}Ni_{20}Sn_7$ composition were prepared by mechanical alloying in a planetary high-energy ball-mill (AGO-2). The amorphization of all three alloys was found to set in after milling at 300rpm speed for 2h. A complete amorphization was observed for $Ti_{50}Cu_{32}Ni_{15}Sn_3$ and $Ti_{50}Cu_{25}Ni_{20}Sn_5$ after 30h and 20h of milling, respectively. Differential scanning calorimetry analyses revealed that the thermal stability increased in the order of $Ti_{50}Cu_{32}Ni_{15}Sn_3$, $Ti_{50}Cu_{25}Ni_{20}Sn_5$, and $Ti_{50}Cu_{23}Ni_{20}Sn_7$.

  • PDF

The Fabrication and Sinterability of $Al_2O_3/Cu$ Nanocomposite Powder ($Al_2O_3/Cu$ 나노복합분말의 제조 및 소결 특성)

  • 홍대희;오승탁;김지순;김영도;문인형
    • Journal of Powder Materials
    • /
    • v.6 no.4
    • /
    • pp.301-306
    • /
    • 1999
  • Mechanical properties of oxide based materials could be improved by nanocomposite processing. To investigate optimum route for fabrication of nanocomposite enabling mass production, high energy ball milling and Pulse Electric Current Sintering (PECS) were adopted. By high energy ball milling, the $Al_2O_3$-based composite powder with dispersed Cu grains below 20 nm in diameter was successfully synthesized. The PECS method as a new process for powder densification has merits of improved sinterability and short sintering time at lower temperature than conventional sintering process. The relative densities of the $Al_2O_3$-5vol%Cu composites sintered at $1250^{\circ}C$ and $1300^{\circ}C$ with holding temperature of $900^{\circ}C$ were 95.4% and 95.7% respectively. Microstructures revealed that the composite consisted of the homogeneous and very fine grains of $Al_2O_3$ and Cu with diameters less than 40 nm and 20 nm respectively The composite exhibited enhanced toughness compared with monolithic $Al_2O_3$. The influence of the Cu content upon fracture toughness was discussed in terms of microstructural characteristics.

  • PDF

A combination method of the theory and experiment in determination of cutting force coefficients in ball-end mill processes

  • Kao, Yung-Chou;Nguyen, Nhu-Tung;Chen, Mau-Sheng;Huang, Shyh-Chour
    • Journal of Computational Design and Engineering
    • /
    • v.2 no.4
    • /
    • pp.233-247
    • /
    • 2015
  • In this paper, the cutting force calculation of ball-end mill processing was modeled mathematically. All derivations of cutting forces were directly based on the tangential, radial, and axial cutting force components. In the developed mathematical model of cutting forces, the relationship of average cutting force and the feed per flute was characterized as a linear function. The cutting force coefficient model was formulated by a function of average cutting force and other parameters such as cutter geometry, cutting conditions, and so on. An experimental method was proposed based on the stable milling condition to estimate the cutting force coefficients for ball-end mill. This method could be applied for each pair of tool and workpiece. The developed cutting force model has been successfully verified experimentally with very promising results.

Highly Economic and High Quality Zinc-flake Manufacturing by High Kinetic Processing

  • Ren, H.;Benz, H.U.;Chimal V., O.;Corral G., M.S.;Zhang, Y.;Jaramillo V., D.;Zoz, H.
    • Proceedings of the Korean Powder Metallurgy Institute Conference
    • /
    • 2006.09b
    • /
    • pp.975-976
    • /
    • 2006
  • The present paper is a parameter study of zinc flake production using a Simoloyer CM01 horizontal high energy rotary ball mill. The manufactured flakes have a dimension in thickness (t) < $1{\mu}m$ and diameters (d) 5-100 ${\mu}m$, consequently a ratio d/t up to 200. The flake geometry is mainly controlled by the variation of process parameters such as rotary speed of the rotor, ratio of powder/ball charge, load ratio of the system, process temperature, operating model and the quantity of process control agent (PCA). The Zn flakes were characterized by SEM, tap densitometry, laser diffraction and water coverage measurement.

  • PDF

Development of Pre-treatment for Tin Recovery from Waste Resources (주석 함유 폐자원의 공정부산물 전처리 기술)

  • Jin, Y.H.;Jang, D.H.;Jung, H.C.;Lee, K.W.
    • Journal of Powder Materials
    • /
    • v.21 no.2
    • /
    • pp.142-146
    • /
    • 2014
  • Fundamental experiences have been studied for development of pre-treatment process of Sn by-products such as solders. Dry and wet separation/recovery processes were considered by the differences of physical properties. The by-products, which are analyzed by solder metal and oxides. The metal and oxide were simply separated by dry ball-milling process for 12 hours, after that recovery metal powder might be reusable as lead or lead-free solders. In terms of wet separation process, samples were dissolved in $HNO_3+H_2O_2$ and the precipitation were analyzed by $SnO_2$. Overall efficiency of recovery might be increasing via developing simple pre-treatment process.

Changes of Getter properties by Crystallization of Amorphous Zr-V-Ti alloy Powders (비정질 Zr-V-Ti 합금분말의 결정화에 따른 게터 특성 변화)

  • Park, Je-Shin;Kim, Won-Baek;Baek, Jin-Sun
    • Journal of Powder Materials
    • /
    • v.14 no.1 s.60
    • /
    • pp.50-55
    • /
    • 2007
  • The hydrogen sorption speeds of $Zr_{57}V_{36}Ti_7$ amorphous alloy and its crystallized alloys were evaluated at room temperature. $Zr_{57}V_{36}Ti_7$ amorphous alloy was prepared by ball milling. The hydrogen sorption rate of the partially crystallized alloy was higher than that of amorphous. The enhanced sorption rate of partially crystallized alloy was explained in terms of grain refinement that has been known to promote the diffusion into metallic bulk of the gases. The grain refinement could be obtained by crystallization of amorphous phase resulting in the observed increase in sorption property.

The Effect of Processing Conditions on the Gradient Pore Structure of Diatomite by Centrifugal Molding (경사 기공 구조를 가지는 규조토의 제조에 원심 분리 성형 공정 변수들이 미치는 영향)

  • Ha, Jang-Hoon;Oh, Eun-Ji;Ahmad, Rizwan;Song, In-Hyuck
    • Journal of Powder Materials
    • /
    • v.19 no.4
    • /
    • pp.304-309
    • /
    • 2012
  • The purpose of our study was to develop the fabrication method of porous diatomite ceramics with a porosity gradient by centrifugal molding. The processing variables of centrifugal molding were derived from Stoke's law of sedimentation, which were the radius of the particles, the acceleration due to centrifugal molding and the dynamic viscosity of the slurry. And these could be controlled by ball-milling conditions, centrifugal conditions, and the addition of methyl cellulose, respectively. The effects of processing conditions on the gradient pore structure of diatomite were investigated by particle size analysis, scanning electron microscope, and mercury porosimeter.

Effect of Grinding Method and Grinding Rate on the Dry Beneficiation of Kaolin Mineral (분쇄방식 및 분쇄율이 고령토 광물의 건식 정제에 미치는 영향)

  • Kim, Sang-Bae;Choi, Young-Yoon;Cho, Sung-Baek;Kim, Wan-Tae
    • Journal of the Mineralogical Society of Korea
    • /
    • v.21 no.2
    • /
    • pp.129-138
    • /
    • 2008
  • The characteristics of beneficiating kaolin mineral by liberation (selective grinding) and air classification have been investigated, comparing the grinding rates of ball mill and impact mill. The ore was ground using a ball mill and a impact mill to evaluate the grindability of the two grinding methods based on the constant production amount of fine particles in size less than 325 mesh. Then, the fine product was further separated into two fractions using an air-classifier and each fraction was chemically analyzed to compare the beneficiation efficiency of the two grinding methods. The chemical grade of kaolin mineral decreased as increasing the grinding rate of both the mills. particularly in the case of ball mill because of overgrinding impurities such as quartz and feldspar. In the case of the ball milling, the fine fraction less than 325 mesh was air-classified at a cutting point of $43\;{\mu}m$. The production rate of the air-classified concentrate was found to be 66.2 wt%, removing 5.3% of $Fe_2O_3$ and 34.6% of CaO. Under the same conditions mentioned above with the impact mill, the production rate of the air-classified concentrate was 64.4 wt%, removing 34.2% of $Fe_2O_3$, 67.6% of CaO and 25.0% of $TiO_2$. Therefore, our results indicate that impact mill is superior to ball mill in terms of impurity removal.