• 제목/요약/키워드: apatite formation

검색결과 68건 처리시간 0.028초

아파타이트의 형성에 미치는 티타늄의 표면처리 효과 (Effect of Surface Treatment of Titanium on the Formation of Apatite Crystal)

  • 정회웅;원대희;이민호;배태성
    • 대한의용생체공학회:학술대회논문집
    • /
    • 대한의용생체공학회 1998년도 추계학술대회
    • /
    • pp.231-232
    • /
    • 1998
  • The purpose of this study was to examine whether the precipitation of calcium phosphate on titanium surface was affected by surface modification. To improve the bone conductivity, of titanium, samples were devided into 4 groups. Group 1 was immersed in 5M-NaOH solution at $60^{\circ}C$ for 24 hours. Group 2 was immersed in 5M-NaOH solution at $60^{\circ}C $ for 24 hours and heat-treated at $600^{\circ}C$ for 1 hour. Group 3 was anodized in Hanks' solution at 1V, $25^{\circ}C$ for 1 hour. Group 4 was anodized in Hanks' solution at 5V, $80^{\circ}C$ for 5 minutes. And then, all specimens were immersed in the MEM Eagle's medium whose composition was similar to that of extracellular fluid for 30 days. The precipitation of the calcium phosphate on implant surface was increased by the immersion in the NaOH solution, and more highly accelerated by heat treatment at $600^{\circ}C$. The precipitation of the calcium phosphate on titanium implant was increased with the treatment of the anodic oxidation in Hanks' solution at 5V, $80^{\circ}C$.

  • PDF

밀양 납석광상에서 산출되는 단괴의 광물조성 (Mineralogy of Nodules in the Milyang Pyrophyllite Deposit, Gyeongsangnamdo, South Korea)

  • 문희수;이강원;송윤구
    • 자원환경지질
    • /
    • 제26권4호
    • /
    • pp.455-464
    • /
    • 1993
  • Some nodules occur in the Milyang pyrophyllite deposit which are hydrothermal alteration products by Late Cretaceous andesitic tuff. These nodules are divided into two types on the basis of mineral assemblages; diaspore and pyrophyllite nodules. The diaspore nodules consist mainly of diaspore, kaolinite, pyrophyllite and pyrite with a small amounts of wavellite and tourmaline. They are light purplish grey in color, ellipsoid in shape and range 1 cm to 15 cm in size. A small or large diffuse band exists in some nodules. The platy coarse-grained diaspore is intergrown with the fine-aggregated kaolinite in the central part of the nodule. It appears that the grain size become fine from center to margin. The pyrophyllite nodules, which have the same shape with diaspore nodules, consist dominantly of pyrophyllite accompanied by small amounts of quartz, kaolinite, svanbergite, wavellite, tourmaline and apatite. Chemical compositions of alteration zones and nodules show that the wall rock alteration involved mainly the removal of large quantities of silica and alkalies and small quantities of Ca, Mg and Fe. The sharp increase in the Al content of the nodules is the result of residual concentration of alumina by the leaching of the mobile components. The pyrophyllite nodules were formed in the fluid saturated with quartz as ${\mu}_{HK_{-1}}$ and ${\mu}_{H_{2}O}$ increase. Under this condition, the pyrophyllite-kaolinite-quartz assemblage was stable. Diaspores formed from pyrophyllites in the fluid undersaturated with quartz as ${\mu}_{H_{2}O}$ increases (decreasing temperature). Under this condition, diaspore-pyrophyllite-kaolinite assemblage become stable. The formation temperature of the nodules on the basis of mineral assemblage is estimated as $275{\sim}340^{\circ}C$.

  • PDF

골결손부 재건을 위한 금속 이온 치환 이상인산칼슘 합성 및 생체 활성 평가 (Synthesis and bioactivity evaluation of metal ion-substitution biphasic calcium phosphate for bone defect reconstruction)

  • 김태완;김동현;진형호;이승호;박홍채;윤석영
    • 한국결정성장학회지
    • /
    • 제22권6호
    • /
    • pp.279-285
    • /
    • 2012
  • BCP, Mg-BCP, Si-BCP 분말을 공침법(co-precipitation process)을 이용하여 합성하였다. 제조된 분말을 X-선 회절 분석(XRD), 적외선분광분석(FTIR)을 이용하여 특성을 분석하였다. Ca/P 몰 비율이 1.602인 칼슘 결손 아파타이트 공침물을 제조하여 $1000^{\circ}C$ 열처리 과정을 통하여 HAp와 ${\beta}$-TCP 상이 혼재된 BCP, Mg-BCP, Si-BCP을 합성할 수 있었다. 제조된 분말의 생체활성 거동을 평가하기 위하여 Hanks' Balanced Salt Solution(HBSS)에 침적시켜 시간에 따라 형상의 변화 및 결정상을 분석한 결과, BCP 분말에 비하여 금속 이온이 치환된 BCP 분말에서 빠른 생체활성을 관찰할 수 있었다. MTT assay를 통한 세포 성장률 평가에서모든 분말에서 시간 경과에 따라 독성을 나타내지 않았으며, 세포의 활성이 증가하였다.

삼덕 Mo 광상에서 산출되는 백색운모 및 화학조성 (White Mica and Chemical Composition of Samdeok Mo Deposit, Republic of Korea)

  • 유봉철
    • 한국광물학회지
    • /
    • 제32권3호
    • /
    • pp.223-234
    • /
    • 2019
  • 삼덕 Mo 광상 주변지질은 고생대 화전리층, 고운리층, 서창리층, 이원리층, 황강리층, 백악기 우백질 반상화강암 및 화강반암으로 구성된다. 이 광상은 서창리층 내에 발달된 NS 방향의 열극대를 따라 충진한 3개조의 석영맥으로 구성된 광상으로 석영맥의 맥폭은 0.05~0.3 m 정도로 팽축이 심하고 석영맥의 연장성은 약 400 m 정도이다. 석영맥은 괴상, 각력상 및 정동조직들이 관찰되며 모암변질로는 규화작용, 견운모화작용, 점토화작용 및 녹니석화작용 등이 관찰된다. 산출광물은 석영, 형석, 백색운모, 흑운모, 인회석, 모나자이트, 금홍석, 티탄철석, 휘수연석, 황동석, Fe-Mg-Mn 산화물 및 철 산화물 등이다. 이 광상의 백색운모는 석영맥과 모암에서 세립질에서 조립질로 산출되며 4가지 산출유형(I 유형: 석영, 휘수연석, 철 산화물 및 Fe-Mg-Mn 산화물과 함께 산출되는 것, II 유형: 석영, 철 산화물 및 Fe-Mg-Mn 산화물과 함께 산출되는 것, III 유형: 석영 및 흑운모와 함께 산출되는 것 및 IV 유형: 석영과 함께 산출되는 것)을 갖는다. 석영맥에서 산출되는 백색운모의 화학조성은$(K_{0.89-0.60}Na_{0.05-0.00}Ca_{0.01-0.00}Sr_{0.02-0.00})_{0.94-0.62}(Al_{1.54-1.12}Mg_{0.36-0.18}Fe_{0.26-0.09}Mn_{0.04-0.00}Ti_{0.02-0.00}Cr_{0.02-0.00}Zn_{0.01-0.00})_{1.91-1.72}(Si_{3.40-3.11}Al_{0.92-0.60})_{4.00}O_{10}(OH_{1.68-1.42}F_{0.58-0.32})_{2.00}$이나 I 유형의 백색운모는 나머지 유형의 백색운모보다 $SiO_2$ 및 MgO 함량은 낮고 FeO 함량은 높게 나타난다. 또한 이 광상의 백색운모의 화학조성 변화는 팬자이틱 또는 Tschermark 치환($(Al^{3+})^{VI}+(Al^{3+})^{IV}{\leftrightarrow}(Fe^{2+}$ 또는 $Mg^{2+})^{VI}+(Si^{4+})^{IV}$) 및 직접적인 $(Fe^{3+})^{VI}{\leftrightarrow}(Al^{3+})^{VI}$ 치환에 의해 일어났음을 알 수 있다.

장군 연-아연 광상의 모암변질대에서 산출되는 백색운모의 산상 및 화학조성 (Occurrence and Chemical Composition of White Mica from Wallrock Alteration Zone of Janggun Pb-Zn Deposit)

  • 유봉철
    • 광물과 암석
    • /
    • 제35권4호
    • /
    • pp.469-484
    • /
    • 2022
  • 장군 연-아연 광상은 남한의 4대(연화 광상, 신예미 광상, 울진 광상) 연-아연 광상중의 하나이었다. 이 광상 지질은 선캠브리아기의 원남층, 율리층군, 캠브리안기내지 오도비스기의 장산규암층, 두음리층, 장군 석회암층, 석탄기내지 이엽기의 동수곡층, 재산층, 쥐라기의 동화지층 및 이들을 관입한 중생대의 춘양화강암류로 구성된다. 이 연-아연 광상은 고생대 캠브리안기내지 오도비스기의 장군석회암층에 배태되는 열수교대형 광상에 해당된다. 이 광상의 연-아연 광화작용과 관련된 모암변질작용은 주로 능망간석화작용과 돌로마이트화 작용이 관찰되나 황철석화작용, 견운모화작용 및 녹니석화작용 등도 관찰된다. 모암변질작용은 연-아연 광체 에서 모암으로 감에 따라 연-아연 광체 -> 능망간석대 -> 돌로마이트대 -> 돌로마이트질 석회암대 -> 석회암 및 돌로마이트 대리암 변화된다. 백색운모는 모암변질대(능망간석화작용과 돌로마이트화작용)에서 Ca-돌로마이트, Ferroan ankerite, sideroplesite, 금홍석, 인회석, 유비철석, 황철석, 섬아연석, 방연석, 석영, 녹니석 및 방해석 등과 함께 중립내지 세립질 입단으로 산출된다. 이 백색운모의 화학조성은(K0.77-0.62Na0.03-0.00Ca0.03-0.00Ba0.00Sr0.01)0.82-0.64(Al1.72-1.48Mg0.48-0.20Fe0.04-0.01Mn0.03-0.00Ti0.01-0.00Cr0.00As0.01-0.00Co0.03-0.00Zn0.03-0.00Pb0.05-0.00Ni0.01-0.00)2.07-1.92 (Si3.43-3.33Al0.67-0.57)4.00O10(OH1.94-1.80F0.20-0.06)2.00로써 이론적인 이중팔면체형 운모류 값보다 Si가 높고 K, Na, Ca는 낮다. 또한 장군 연-아연 광상, 연화1 연-아연 광상 및 백전 금-은 광상의 모암변질대와 구문소일대 석회암에서 산출되는 백색운모는 백운모와 팬자이트에 해당되나 둔전 금-은 광상의 모암변질대에서 산출되는 백색운모는 백운모에 해당된다. 더불어 이들 광상의 모암변질대 및 구문소일대 석회암에서 산출되는 백색운모의 화학조성 변화는 주로 팬자이틱 또는 Tschermark 치환 메카니즘(장군 연-아연 광상), 주로 팬자이틱 또는 Tschermark 치환과 일부 illitic 치환 메카니즘(연화1 연-아연 광상, 둔전 금-은 광상, 백전 금-은 광상) 및 주로 팬자이틱 또는 Tschermark 치환과 일부 illitic 치환 및 Na+ <-> K+ 치환 메카니즘(구문소일대)에 의해 일어났음을 알 수 있다.

양극산화에 의한 티타늄 산화막의 표면 특성 및 생체 활성에 관한 연구 (SURFACE CHARACTERISTICS AND BIOACTIVITY OF ANODICALLY OXIDIZED TITANIUM SURFACES)

  • 이상한;조인호
    • 대한치과보철학회지
    • /
    • 제45권1호
    • /
    • pp.85-97
    • /
    • 2007
  • Statement of problem: Recently, anodic oxidation of cp-titanium is a popular method for treatment of titanium implant surfaces. It is a relatively easy process, and the thickness, structure, composition, and the microstructure of the oxide layer can be variably modified. Moreover the biological properties of the oxide layer can be controlled. Purpose: In this study, the roughness, microstructure, crystal structure of the variously treated groups (current, voltage, frequency, electrolyte, thermal treatment) were evaluated. And the specimens were soaked in simulated body fluid (SBF) to evaluate the effects of the surface characteristics and the oxide layers on the bioactivity of the specimens which were directly related to bone formation and integration. Materials and methods: Surface treatments consisted of either anodization or anodization followed thermal treatment. Specimens were divided into seven groups, depending on their anodizing treatment conditions: constant current mode (350V for group 2), constant voltage mode (155V for group 3), 60 Hz pulse series (230V for group 4, 300V for group 5), and 1000 Hz pulse series (400V for group 6, 460V for group 7). Non-treated native surfaces were used as controls (group 1). In addition, for the purpose of evaluating the effects of thermal treatment, each group was heat treated by elevating the temperature by $5^{\circ}C$ per minute until $600^{\circ}C$ for 1 hour, and then bench cured. Using scanning electron microscope (SEM), porous oxide layers were observed on treated surfaces. The crystal structures and phases of titania were identified by thin-film x-ray diffractmeter (TF-XRD). Atomic force microscope (AFM) was used for roughness measurement (Sa, Sq). To evaluate bioactivity of modified titanium surfaces, each group was soaked in SBF for 168 hours (1 week), and then changed surface characteristics were analyzed by SEM and TF-XRD. Results: On basis of our findings, we concluded the following results. 1. Most groups showed morphologically porous structures. Except group 2, all groups showed fine to coarse convex structures, and the groups with superior quantity of oxide products showed superior morphology. 2. As a result of combined anodization and thermal treatment, there were no effects on composition of crystalline structure. But, heat treatment influenced the quantity of formation of the oxide products (rutile / anatase). 3. Roughness decreased in the order of groups 7,5,2,3,6,4,1 and there was statistical difference between group 7 and the others (p<0.05), but group 7 did not show any bioactivity within a week. 4. In groups that implanted ions (Ca/P) on the oxide layer through current and voltage control, showed superior morphology, and oxide products, but did not express any bioactivity within a week. 5. In group 3, the oxide layer was uniformly organized with rutile, with almost no titanium peak. And there were abnormally more [101] orientations of rutile crystalline structure, and bonelike apatite formation could be seen around these crystalline structures. Conclusion: As a result of control of various factors in anodization (current, voltage, frequency, electrolytes, thermal treatment), the surface morphology, micro-porosity, the 2nd phase formation, crystalline structure, thickness of the oxide layer could be modified. And even more, the bioactivity of the specimens in vitro could be induced. Thus anodic oxidation can be considered as an excellent surface treatment method that will able to not only control the physical properties but enhance the biological characteristics of the oxide layer. Furthermore, it is recommended in near future animal research to prove these results.

Ti-6Al-4V 합금의 알칼리 및 열처리가 인산칼슘 침착에 미치는 영향 (Effect of Alkali and Heat Treatments of Ti-6Al-4V Alloy on the Precipitation of Calcium Phosphate)

  • 박재한;임기정;김상목;김병옥;한경윤
    • Journal of Periodontal and Implant Science
    • /
    • 제30권1호
    • /
    • pp.187-203
    • /
    • 2000
  • The precipitation of calcium phosphate on implant surface has been known to accelerate osseointegration and to enhance osseous adaptation. The present study was performed to examine whether the precipitation of calcium phosphate on Ti-6Al-4V alloy could be affected by the immersion in NaOH solution and heat treatment. Ti-6Al-4V alloy plates of $15{\times}3.5{\times}1mm$ in dimension were polished sequentially from #240 to #2,000 emery paper and one surface of each specimen was additionally polished with $0.1{\mu}m$ alumina paste. Polished specimens were soaked in various concentrations of NaOH solution(0.1, 1.0, 3.0, 5.0, 7.0, 10.0 M) at $60^{\circ}C$ for 24 hours for alkali treatment, and 5.0 M NaOH treated specimens were heated for 1 hour at each temperature of 400, 500, 600, 700, $800^{\circ}C$. After the alkali and heat treatments, specimens were soaked in the Hank's solution with pH 7.4 at $36.5^{\circ}C$ for 30days.The surface ingredient change of Ti-6Al-4V alloy was evaluated by thin-film X-ray diffractometer(TF-XRD) and the surface microstructure was observed by scanning electron microscope(SEM), and the elements of surface were analyzed by X-ray photoelectron spectroscopy(XPS). The results were obtained as follows ; 1. The precipitation of calcium phosphate on Ti-6Al-4V alloy was accelerated by the immersion in NaOH solution and heat treatment. 2. In Alkali treatment for the precipitation of calcium phosphate on Ti-6Al-4V alloy, the optimal concentration of NaOH solution was 5.0 M. 3. In heat treatment after alkali treatment in 5.0 M NaOH solution, the crystal formation on alloy surface was enhanced by increasing temperature. In heat treated alloys at $600^{\circ}C$, latticed structure and prominences of calcium phosphate layer were most dense. On heat treated alloy surface at the higher temperature(${\geq}700^{\circ}C$), main crystal form was titanium oxide rather than apatite. The above results suggested that the precipitation of calcium phosphate on the surface of Ti-6Al-4V alloy could be induced by alkali treatment in 5.0 M-NaOH solution and by heat treatment at $600^{\circ}C$.

충주 어래산 일대에서 산출하는 희토류 광물의 광물학적 및 광물화학적 특성 (Mineralogy and Mineral-chemistry of REE Minerals Occurring at Mountain Eorae, Chungju)

  • 유병운;이길재;고상모
    • 자원환경지질
    • /
    • 제45권6호
    • /
    • pp.643-659
    • /
    • 2012
  • 충주 지역은 소위 옥천층군에 해당되는 계명산층이 분포하며, 계명산층내에는 변성화산암 모암과 페그마타이트 모암의 희토류 광체가 배태한다. 변성화산암 모암의 희토류 광체를 구성하는 희토류광물은 갈렴석, 저어콘, 인회석, 스핀이 산출하나 갈렴석이 가장 우세하게 산출한다. 페그마타이트 모암의 희토류 광체를 구성하는 희토류 광물은 퍼구소나이트, 카르나수르타이트, 저어콘, 토륨석이 산출하나 퍼구소나이트가 가장 우세하다. 변성화산암에서 산출하는 갈렴석의 화학식은 (Ca, Y, REE, Th)$_{2.095}$(Mg, Al, Ti, Mn, $Fe^{3+})_{2.770}(SiO_4)_{2.975}(OH)$로서 TREO 23.89-29.12 wt%, $La_2O_3$ 4.71-9.92 wt%, $Ce_2O_3$ 11.30-14.33 wt%, $Y_2O_3$ 0.11-0.29 wt%, $ThO_2$ 0.12-0.94 wt% 이다. A(2) 사이트 에서 $Ca^{2+}$$REE^{3+}$, M(2) 사이트에서 $Al^{3+}$$Fe^{2+}$의 치환이 일어나는데 이는 갈렴석의 화학조성에 밀접한 관련을 갖는 특징이고, Fe의 함량이 일반 갈렴석보다 높은 Ce 계열의 Ferriallanite에 해당된다. 이는 모암인 계명산층을 주로 구성하는 변성화산암(변성조면암)의 원암이 Fe이 풍부한 함철층이기 때문인 것으로 판단된다. 페그마타이트 모암에서 가장 우세하게 산출하는 퍼구소나이트의 화학조성은 A 사이트에서 Y-REE, Y-Th 치환이 우세하게 일어났으며, B 사이트에서는 Nb-Ta-Ti의 치환이 주로 초래되었으며, 계산된 화학식은 $YNbO_4$ 이다. 또한 $Y_2O_3$$Nb_2O_5$만의 비율로 상관도를 확인 한 결과 연구지역에서 산출되는 퍼구소나이트는 Y과 Nb의 이상적인 비율인 1:1 비율과 달리 1:1.5의 비율을 나타내고 있으며, Nb의 함량이 Y 함량보다 높으며, Y 사이트 즉, A 사이트에서 희토류 원소의 치환이 활발하게 초래되었다. 페그마타이트에서 산출하는 카르나수르타이트는 REE 및 Th를 치환하는 조성은 각각 $Ce_2O_3$ 9.16-22.88 wt%, $La_2O_3$ 2.15-9.16 wt%, $ThO_2$ 0.44-10.8 wt%, 화학조성으로 계산된 구조식은 (Y, REE, Th, K, Na, Ca)$_{1.478}$(Ti, Nb)$_{1.304}$(Mg, Al, Mn, $Fe^{+3})_{0.988}$(Si, P)$_{1.431}O_7(OH)_4{\cdot}3H_2O$이다. 870-860 Ma 인 초기 원생대에 로디니아 대륙의 분열기로서 한반도에서 A-1형 화산활동이 초래되어 철, 희토류원소 및 고장력원소(Nb, Zr, Y 등)가 풍부한 변성화산암으로 주로 구성되는 계명산층을 형성 시켰다면 갈렴석은 모암이 형성될 당시 알카리 화산암에서 정출되었거나 변성작용이 초래된 고생대 말(300-280 Ma, Cho et al., 2002) 광역변성작용에 의해 형성 되었을 가능성이 높다. 희토류를 함유하는 페그마타이트에서 산출하는 저어콘 연대가 190 Ma 인 것은 쥬라기에 충주지역에서 광범위하게 초래된 화강암 정치활동과 관련된 가능성이 크다. 따라서 충주지역 계명산층 내 배태된 희토류 광체는 인접한 지역에 배태되어 있지만 매우 차별적 희토류 광화작용이 초래 되어 희토류광물조성과 광체의 산상이 차별적으로 나타나는 것으로 해석된다.

Myriococcum albomyces가 생산하는 Cellulase에 관한 연구 (Studies on the Cellulase produced by Myriococcum of albomyces)

  • 정동효
    • Applied Biological Chemistry
    • /
    • 제14권1호
    • /
    • pp.59-97
    • /
    • 1971
  • Myriococcum albomycesf가 생산하는 섬유소 분해효소군에 관한 연구로서 호소생산배지 및 조효소의 성질을 규명하고 몇 가지 효소군으로 정제한바 다음과 같은 결과를 얻었다. 1. 밀기울 고채해양의 각 효소 활성은 쌀겨고체배양 및 탈지대두박고체배양의 그것보다 강하였다. 2. 밀기울진탕, 쌀겨진탕배양 및 대두박진탕배양등은 상기의 고체배양보다 각 효소의 활성이 우수하였다. 3. $45^{\circ}C$에서 배양한 것이 배양기의 종류에 관계없이 $37^{\circ}C$$50^{\circ}C$에서 배양한 것보다 각 효소의 활성이 강하였다. 4. CMCase는 무기 질소원보다 유기 질소원을 첨가하므로서 더욱 생성이 촉진되었다. 5. 기본밀기울진탕배양기에 CMC, Avicel, 여지분말 등의 indncer를 첨가 하므로서 각 효소활성은 $1.5{\sim}3$배나 증가되었다. 6. CMC와 Avicel을 inducer로 하여 jar formentor에서 배양할 때 작 효소의 활성은 대개 5일째에 최고에 달하였다. 7. Cellulae 조효소의 최적 pH는 $4.0{\sim}4.5$, pH안정성은 $3.5{\sim}8.0$이였다. 그리고 최적온도는 $65^{\circ}C$ 부근으로 다른 사상균의 cellulase에 비하여 높으며 온도안정성도 $60^{\circ}C$에서 120분으로 거의 실활되지 않았다. 8. 조효소의 활성은 $Ca^{++}$, $Mg^{++}$으로 부활되며, $Hg^{++}$, $Cu^{++}$, $Ag^{+}$는 강한 저해체였다. 그리고 투석으로 약간 그 활성이 저하되었다. 9. 배양액을 여과하고 황산암모니움 분획, DEA-E-sephadex A-25, Amberlite CG-50 및 hydroxy-apatite column chromatography로 Avicel, CMC, 여지 분말에 대하여 활성이 다른 4개의 fraction을 분리 하고 이를 cellulase fraction I, fraction II-a, fraction II-b 및 fraction III라고 명명하였다. 10. 이들 4개의 fraction은 전기 영동, 초원심상 및 자외선흡수 등으로 보아서 단일의 단백질로 생각되었다. 11. Fraction I은 Avicelase활성이 강하고, fraction II-a는 cellobiase 활성이 강하였다. 그리고 fraction II는 CMCase 활성이 강하였으며, fraction III는 CMC 점도감소 활성이 강하였다. 12. 섬유소질을 각 fraction으로 가수분해한 최종산물은 cellobiose 및 glucose였다. 그리고 fraction I과 fraction II-a는 Avicel을 협동적으로 분해하였다. 13. Fraction I의 최적 pH 5.5, fraction II-a는 pH 5.0, fraction II-b는 pH 4.0, fractionIII는 pH $4.0{\sim}4.5$이며, 각 fraction의 pH 안정성은 pH $3.0{\sim}7.0$이였다. 14. Fraction I의 최적온도는 $50^{\circ}C$, fractionII-a는 $55{\sim}60^{\circ}C$, fraction II-b 는 $60^{\circ}C$, fraction III는 $55^{\circ}C$이며 각 fraction의 열안정성은 $55^{\circ}C$ 부근에서 120분으로 거의 실활되지 않고 fraction II-a는 $60^{\circ}C$에서도 특별히 안정하였다. 15. Fraction I과 fraction II-b 활성은 $Ag^{++}$, $Hg^{++}$에 의하여 저해되며 $Ca^{++}$, $Mg^{++}$으로는 부활되었다.

  • PDF

영남(소백산)육괴 북동부 평해지역 화강편마암류의 SHRIMP U-Pb 저콘 연대 (SHRIMP V-Pb Zircon Ages of the Granite Gneisses from the Pyeonghae Area of the northeastern Yeongnam Massif (Sobaeksan Massif))

  • 김남훈;송용선;박계헌;이호선
    • 암석학회지
    • /
    • 제18권1호
    • /
    • pp.31-47
    • /
    • 2009
  • 영남(소백산)육괴 북동부의 고원생대 변성퇴적암류(평해층과 원남층)를 관입한 평해 화강편마암과 하다 우백질화강편마암에 대해 암석기재적, 지구화학적 및 지구연대학적 연구를 수행하였다. 평해 화강편마암은 하다 우백질화강편마암에 비해 대체로 흑운모 등 유색광물의 함량이 약간 높으며, 화학조성에서 $SiO_2$$K_2O$ 함량은 낮고 ${Fe_2}{O_3}^t$, MgO, CaO, $TiO_2$, $P_{2}O_{5}$ 등의 함량은 높다 하다 우백질화강편마암이 음(-)의 Eu 이상치가 다소 크지만 전체적인 희토류원소의 함량과 패턴은 평해 화강편마암과 매우 유사하다. 성분분화도에서 두 암체는 대체로 흑운모와 사장석, 인회석 또는 스핀의 정출에 의한 분화경향을 보인다. 두 화장편마암 모두 과알루미나질의 칼크-알칼리계열로 섭입대와 관련된 대륙화산호 조구조환경을 지시한다. 저어콘 U-Pb SHRIMP 연대측정의 결과를 보면 평해 화강편마암과 하다 우백질화강편마암의 상부교점연대는 각각 $1990{\pm}23\;Ma$ ($2{\sigma}$)와 $1939{\pm}41\;Ma$ ($2{\sigma}$)이고 $^{207}Pb/^{206}Pb$ 가중평균연령은 각각 $1982{\pm}6.3\;Ma$ ($2{\sigma}$)와 $1959{\pm}28\;Ma$ ($2{\sigma}$)로 오차범위에서 서로 겹치는 연대를 보인다. 따라서 이 지역에서의 선캠브리아기 화강암류의 관입시기는 분천화강편마암의 관입과 동시대이며, 태백산지역에서의 화강암질마그마작용은 대부분 이 시기에 대륙화산호 환경에서 있었던 것으로 해석된다.