Proceedings of the Korean Institute of Electrical and Electronic Material Engineers Conference
/
2002.07b
/
pp.589-592
/
2002
The $Sr_{0.7}Bi_{2.3}Ta_2O_9$(SBT) thin films are deposited on Pt-coated electrode(Pt/TiO2/SiO2/Si) using RF magnetron sputtering method. The structural and electric properties of SBT capacitors were influenced with annealing atmosphere. In the XRD pattern, the SBT thin films in all annealing atmosphere had (105) orientation. In the SEM images, Bi-layered perovskite phase was crystallized in all annealing atmosphere and grains largely grew in oxygen annealing atmosphere. The maximum remanent polarization and the coercive electric field in oxygen annealing atmosphere are $12.40{\mu}C/cm^2$ and 48kV/cm respectively. The dielectric constant and leakage current density annealing in oxygen atmosphere are 340 and $6.81{\times}10^{-10}A/cm^2$ respectively. The fatigue characteristics of SBT capacitors did not change up to $10^{10}$ switching cycles.
Proceedings of the Korean Institute of Electrical and Electronic Material Engineers Conference
/
2003.05d
/
pp.77-81
/
2003
The $Sr_{0.7}Bi_{2.6}Ta_2O_9$(SBT) thin films are deposited on Pt-coated electrode(Pt/$TiO_2/SiO_2$/Si) using RF magnetron sputtering method. The structural and electrical properties of SBT capacitors were influenced with annealing atmosphere. In the XRD pattern, the SBT thin films in all annealed atmosphere had (105) orientation. In the SEM images, Bi-layered perovskite phase was crystallized in all annealing atmosphere and grains largely grew in oxygen annealing atmosphere. The dielectric constant and leakage current density of capacitors annealed oxygen atmosphere are 340 and $2.13{\times}10^{-9}[A/cm^2]$ respectively.
Journal of the Korean Institute of Electrical and Electronic Material Engineers
/
v.16
no.3
/
pp.207-213
/
2003
The Sr$\_$0.7/Bi$\_$2.6/Ta$_2$O$\_$9/(SBT) thin films are deposited on Pt-coated electrode(Pt/TiO$_2$/SiO$_2$/Si) using RF magnetron sputtering method. The structural and electrical properties of SBT capacitors were influenced with annealing atmosphere. In the XRD pattern, the SBT thin films in all annealed atmosphere had (105) orientation. In the SEM images, Bi-layered perovskite phase was crystallized in all annealing atmosphere and grain largely grew in oxygen annealing atmosphere. The maximum remnant polarization and the coercive electric field in oxygen annealing atmosphere are 12.40[${\mu}$C/cm$^2$] and 30[kV/cm] respectively. The dielectric constant and leakage current density of capacitors annealed oxygen atmosphere are 340 and 2.13${\times}$10$\^$-9/ [A/cm$^2$] respectively. The fatigue characteristics of SBT capacitors did not change up to 10$\^$10/ switching cycles.
Proceedings of the Korean Institute of Electrical and Electronic Material Engineers Conference
/
2003.05d
/
pp.72-76
/
2003
The $Sr_{0.7}Bi_{2.6}Ta_2O_9$(SBT) thin films are deposited on Pt-coated electrode(Pt/$TiO_2/SiO_2$/Si) using RF magnetron sputtering method. The structural and electrical properties of SBT capacitors were influenced with annealing atmosphere. In the XRD pattern, the SBT thin films in all annealed atmosphere had (105) orientation. In the SEM images, Bi-layered perovskite phase was crystallized in all annealing atmosphere and grains largely grew in oxygen annealing atmosphere. The maximum remanent polarization and the coercive electric field in oxygen annealing atmosphere are $12.40[{\mu}C/cm^2]$ and 30[kV/cm] respectively. The fatigue characteristics of SBT capacitors did not change up to $10^{10}$ switching cycles.
The sliding wear behavior of the plasma-sprayed zirconia containing 3 mol% yttria was investigated after the annealing at room temperature to 80$0^{\circ}C$ in various concentrations of humid atmosphere as laboratory, humid, dry argon atmosphere. Both of the friction coefficient and the wear loss increased with increasing temperature up to 80$0^{\circ}C$. Surface morphology of the worn samples changed with annealing temperature. The change of monoclinic/tetragonal (m/t) x-ray peak intensity ratio effected the wear behavior. The m/t ratio had maximum value at 20$0^{\circ}C$ and decreased with increased temperature in laboratory and humid atmosphere. In argon atmosphere the m/t ratio had no maximum value and decreased with increasing temperature. At all the annealing temperature humid atmosphere had more the m/t ratio value than any other atmosphere. The change of toughness was showed the inversed result of m/t ratio change. The results indicated that the resudial stress which was induced by the different amount of phase transformation takes a detrimental role in wear behavior.
Journal of the Korean Society for Precision Engineering
/
v.18
no.1
/
pp.129-138
/
2001
This study examined the effects of the annealing heat treatments on the mechanical properties of the Invar(Fe-36%Ni Alloy) materials. Invar materials were annealed at various temperatures range 900~120$0^{\circ}C$ in vacuum(10-4Torr) and hydrogen atmospheres. And annealing conditions were changed by cooling rate and holding time at 110$0^{\circ}C$. The grain size of rolled Invar materials was very fine but those of annealed Invar materials at 900~120$0^{\circ}C$ in vacuum and hydrogen atmosphere increased with increasing annealing temperature. The micro-vickers hardness values of annealed Invar materials were decreased about 15% that of the rolled Invar materials, regardless of the various of annealing temperatures, atmosphere(vacuum, hydrogen) and annealing conditions. The tensile strength and yield strength of annealed Invar materials at 900~120$0^{\circ}C$ in vacuum and hydrogen atmosphere were decreased 10.0~14.4% and 34.6~39.1% those of the rolled Invar materials, respectively. The strength ratio(tensile strength/ yield strength) of annealed Invar materials was improved to 1.7~1.8 from the value of 1.2~1.3 of rolled Invar materials. The degree of spring back of annealed Invar materials was about 50% of the rolled Invar materials, regardless of the various of annealing temperatures, atmosphere(vacuum, hydrogen) and annealing conditions.
(Ba, Sr) TiO$_3$(BST) thin films were prepared on RuO$_2$/Si substrates by rf magnetron sputtering and annealing was followed at temperatures ranging from 550 to 80$0^{\circ}C$ in $N_2$or $O_2$atmosphere. The effects of annealing conditions on the properties of BST film deposited on RuO$_2$bottom electrodes were investigated. It was found that the crystallinity. surface roughness, and grain size of BST films vary with the annealing temperature but they are not dependent upon the annealing atmosphere. The flat region in the current-voltage (I-V) curves of BST capacitors shortened with increasing annealing temperature under both atmospheres. This is believed to be due to the lowering of potential barrier caused by unstable interface and the increase of charge The shortening of the flat region by $O_2$annealing was more severe than that by $N_2$-annealing. As a result, there was no flat region when the films were annealed at 700 and 80$0^{\circ}C$ in $O_2$atmosphere. The dielectric properties of BST films were improved by annealing in either atmosphere. however, a degradation with frequency was observed when the films were annealed at relatively high temperature under $O_2$atmosphere.
It was the electrical properties of IGZO prepared by the annealing in a vaccum and an atmosphere conditions to research the current-voltage characteristics. The IGZO film annealed in a vaccum became an amorphous structure but films annealed in an atmosphere condition had a crystal structure. Because of the content of oxygen vacancies during the annealing processes was changed, and the annealing in an atmosphere condition increased the oxygen vacancy in IGZO. Oxygen vacancy in IGZO increased the current and then it was observed the Ohmic contact at IGZO annealed in an atmosphere conditions. However, the IGZO prepared in a vaccum showed the Schottky contact.
Effects of annealing temperature, time, and atmospehre on the flow characteristics of Atmospheric Pressure Chemical Vapor Deposition-borophosphosilicate glass were investigated. Stable step coverage can be obtained by annealing the BPSG film at 90$0^{\circ}C$ for 30 minutes in N2 atmosphere, but further heat treatment isnot effective. Flow characteristics of the BPSG film was better in steam atmosphere than in N2 atmosphere, and the factors which cause it were analyzed. The concentration of boron in the BPSG film was measured pretty accurately by FTIR spectrum. Boron content in the BPSG film was reduced by annealing treatment. The decrement of boron was greater in steam atmosphere than in the N2 atmosphere. Also it was found from the FTIR spectroscopic analysis that PH3 inhibited the oxidation of B2H6.
YMnO3 thin films were prepared on Pt/Ti/SiO2/Si substrate by chemical solution deposition method. The films were crystallized by heat-treatment at 85$0^{\circ}C$ for 1 hour. Effects of an annealing atmosphere(O2, Ar, vacuum) on the crystallization behavior and electridcal properties were investigated. YMnO3 thin films annealed under Ar atmosphere showed a superior crystallinity and a very strong c-aix preferred-orientation which was a polar axis. Leakage current density of the films decreased with lowering oxygen partial pressure of the annealing atmosphere. C-V and P-E ferroelectric hysteresis were observed only in the thin film heat-treated under Ar atmosphere.In order to prepare YMnO3 thin films having both low leakage current and ferroelectricity, the annealing atmsphere should be kept under a proper oxygen partial pressure which was about 1 Pa in this work. Leakage current density at 1 volt, dielectric constant($\varepsilon$r), remanent polarization(Pr), and coercive field(Ec) were 1.7$\times$10-8 A/$\textrm{cm}^2$, 25, 1.08$\mu$C/$\textrm{cm}^2$, and 100 kV/cm, respectively.
본 웹사이트에 게시된 이메일 주소가 전자우편 수집 프로그램이나
그 밖의 기술적 장치를 이용하여 무단으로 수집되는 것을 거부하며,
이를 위반시 정보통신망법에 의해 형사 처벌됨을 유념하시기 바랍니다.
[게시일 2004년 10월 1일]
이용약관
제 1 장 총칙
제 1 조 (목적)
이 이용약관은 KoreaScience 홈페이지(이하 “당 사이트”)에서 제공하는 인터넷 서비스(이하 '서비스')의 가입조건 및 이용에 관한 제반 사항과 기타 필요한 사항을 구체적으로 규정함을 목적으로 합니다.
제 2 조 (용어의 정의)
① "이용자"라 함은 당 사이트에 접속하여 이 약관에 따라 당 사이트가 제공하는 서비스를 받는 회원 및 비회원을
말합니다.
② "회원"이라 함은 서비스를 이용하기 위하여 당 사이트에 개인정보를 제공하여 아이디(ID)와 비밀번호를 부여
받은 자를 말합니다.
③ "회원 아이디(ID)"라 함은 회원의 식별 및 서비스 이용을 위하여 자신이 선정한 문자 및 숫자의 조합을
말합니다.
④ "비밀번호(패스워드)"라 함은 회원이 자신의 비밀보호를 위하여 선정한 문자 및 숫자의 조합을 말합니다.
제 3 조 (이용약관의 효력 및 변경)
① 이 약관은 당 사이트에 게시하거나 기타의 방법으로 회원에게 공지함으로써 효력이 발생합니다.
② 당 사이트는 이 약관을 개정할 경우에 적용일자 및 개정사유를 명시하여 현행 약관과 함께 당 사이트의
초기화면에 그 적용일자 7일 이전부터 적용일자 전일까지 공지합니다. 다만, 회원에게 불리하게 약관내용을
변경하는 경우에는 최소한 30일 이상의 사전 유예기간을 두고 공지합니다. 이 경우 당 사이트는 개정 전
내용과 개정 후 내용을 명확하게 비교하여 이용자가 알기 쉽도록 표시합니다.
제 4 조(약관 외 준칙)
① 이 약관은 당 사이트가 제공하는 서비스에 관한 이용안내와 함께 적용됩니다.
② 이 약관에 명시되지 아니한 사항은 관계법령의 규정이 적용됩니다.
제 2 장 이용계약의 체결
제 5 조 (이용계약의 성립 등)
① 이용계약은 이용고객이 당 사이트가 정한 약관에 「동의합니다」를 선택하고, 당 사이트가 정한
온라인신청양식을 작성하여 서비스 이용을 신청한 후, 당 사이트가 이를 승낙함으로써 성립합니다.
② 제1항의 승낙은 당 사이트가 제공하는 과학기술정보검색, 맞춤정보, 서지정보 등 다른 서비스의 이용승낙을
포함합니다.
제 6 조 (회원가입)
서비스를 이용하고자 하는 고객은 당 사이트에서 정한 회원가입양식에 개인정보를 기재하여 가입을 하여야 합니다.
제 7 조 (개인정보의 보호 및 사용)
당 사이트는 관계법령이 정하는 바에 따라 회원 등록정보를 포함한 회원의 개인정보를 보호하기 위해 노력합니다. 회원 개인정보의 보호 및 사용에 대해서는 관련법령 및 당 사이트의 개인정보 보호정책이 적용됩니다.
제 8 조 (이용 신청의 승낙과 제한)
① 당 사이트는 제6조의 규정에 의한 이용신청고객에 대하여 서비스 이용을 승낙합니다.
② 당 사이트는 아래사항에 해당하는 경우에 대해서 승낙하지 아니 합니다.
- 이용계약 신청서의 내용을 허위로 기재한 경우
- 기타 규정한 제반사항을 위반하며 신청하는 경우
제 9 조 (회원 ID 부여 및 변경 등)
① 당 사이트는 이용고객에 대하여 약관에 정하는 바에 따라 자신이 선정한 회원 ID를 부여합니다.
② 회원 ID는 원칙적으로 변경이 불가하며 부득이한 사유로 인하여 변경 하고자 하는 경우에는 해당 ID를
해지하고 재가입해야 합니다.
③ 기타 회원 개인정보 관리 및 변경 등에 관한 사항은 서비스별 안내에 정하는 바에 의합니다.
제 3 장 계약 당사자의 의무
제 10 조 (KISTI의 의무)
① 당 사이트는 이용고객이 희망한 서비스 제공 개시일에 특별한 사정이 없는 한 서비스를 이용할 수 있도록
하여야 합니다.
② 당 사이트는 개인정보 보호를 위해 보안시스템을 구축하며 개인정보 보호정책을 공시하고 준수합니다.
③ 당 사이트는 회원으로부터 제기되는 의견이나 불만이 정당하다고 객관적으로 인정될 경우에는 적절한 절차를
거쳐 즉시 처리하여야 합니다. 다만, 즉시 처리가 곤란한 경우는 회원에게 그 사유와 처리일정을 통보하여야
합니다.
제 11 조 (회원의 의무)
① 이용자는 회원가입 신청 또는 회원정보 변경 시 실명으로 모든 사항을 사실에 근거하여 작성하여야 하며,
허위 또는 타인의 정보를 등록할 경우 일체의 권리를 주장할 수 없습니다.
② 당 사이트가 관계법령 및 개인정보 보호정책에 의거하여 그 책임을 지는 경우를 제외하고 회원에게 부여된
ID의 비밀번호 관리소홀, 부정사용에 의하여 발생하는 모든 결과에 대한 책임은 회원에게 있습니다.
③ 회원은 당 사이트 및 제 3자의 지적 재산권을 침해해서는 안 됩니다.
제 4 장 서비스의 이용
제 12 조 (서비스 이용 시간)
① 서비스 이용은 당 사이트의 업무상 또는 기술상 특별한 지장이 없는 한 연중무휴, 1일 24시간 운영을
원칙으로 합니다. 단, 당 사이트는 시스템 정기점검, 증설 및 교체를 위해 당 사이트가 정한 날이나 시간에
서비스를 일시 중단할 수 있으며, 예정되어 있는 작업으로 인한 서비스 일시중단은 당 사이트 홈페이지를
통해 사전에 공지합니다.
② 당 사이트는 서비스를 특정범위로 분할하여 각 범위별로 이용가능시간을 별도로 지정할 수 있습니다. 다만
이 경우 그 내용을 공지합니다.
제 13 조 (홈페이지 저작권)
① NDSL에서 제공하는 모든 저작물의 저작권은 원저작자에게 있으며, KISTI는 복제/배포/전송권을 확보하고
있습니다.
② NDSL에서 제공하는 콘텐츠를 상업적 및 기타 영리목적으로 복제/배포/전송할 경우 사전에 KISTI의 허락을
받아야 합니다.
③ NDSL에서 제공하는 콘텐츠를 보도, 비평, 교육, 연구 등을 위하여 정당한 범위 안에서 공정한 관행에
합치되게 인용할 수 있습니다.
④ NDSL에서 제공하는 콘텐츠를 무단 복제, 전송, 배포 기타 저작권법에 위반되는 방법으로 이용할 경우
저작권법 제136조에 따라 5년 이하의 징역 또는 5천만 원 이하의 벌금에 처해질 수 있습니다.
제 14 조 (유료서비스)
① 당 사이트 및 협력기관이 정한 유료서비스(원문복사 등)는 별도로 정해진 바에 따르며, 변경사항은 시행 전에
당 사이트 홈페이지를 통하여 회원에게 공지합니다.
② 유료서비스를 이용하려는 회원은 정해진 요금체계에 따라 요금을 납부해야 합니다.
제 5 장 계약 해지 및 이용 제한
제 15 조 (계약 해지)
회원이 이용계약을 해지하고자 하는 때에는 [가입해지] 메뉴를 이용해 직접 해지해야 합니다.
제 16 조 (서비스 이용제한)
① 당 사이트는 회원이 서비스 이용내용에 있어서 본 약관 제 11조 내용을 위반하거나, 다음 각 호에 해당하는
경우 서비스 이용을 제한할 수 있습니다.
- 2년 이상 서비스를 이용한 적이 없는 경우
- 기타 정상적인 서비스 운영에 방해가 될 경우
② 상기 이용제한 규정에 따라 서비스를 이용하는 회원에게 서비스 이용에 대하여 별도 공지 없이 서비스 이용의
일시정지, 이용계약 해지 할 수 있습니다.
제 17 조 (전자우편주소 수집 금지)
회원은 전자우편주소 추출기 등을 이용하여 전자우편주소를 수집 또는 제3자에게 제공할 수 없습니다.
제 6 장 손해배상 및 기타사항
제 18 조 (손해배상)
당 사이트는 무료로 제공되는 서비스와 관련하여 회원에게 어떠한 손해가 발생하더라도 당 사이트가 고의 또는 과실로 인한 손해발생을 제외하고는 이에 대하여 책임을 부담하지 아니합니다.
제 19 조 (관할 법원)
서비스 이용으로 발생한 분쟁에 대해 소송이 제기되는 경우 민사 소송법상의 관할 법원에 제기합니다.
[부 칙]
1. (시행일) 이 약관은 2016년 9월 5일부터 적용되며, 종전 약관은 본 약관으로 대체되며, 개정된 약관의 적용일 이전 가입자도 개정된 약관의 적용을 받습니다.