• Title/Summary/Keyword: a-C:F$C_{4}F_8$$Si_{2}H_{6}$

검색결과 24건 처리시간 0.032초

RF 스퍼터링으로 증착된 a-Si$_{1-x}$C$_{x}$: H 박막의 결합구조와 광학적 성질에 미치는 증착변수의 영향 (Effects of Deposition Parameters on the Bonding Structure and Optical Properties of rf Sputtered a-Si$_{1-x}$C$_{x}$: H films)

  • 한승전;권혁상;이혁모
    • 한국표면공학회지
    • /
    • 제25권5호
    • /
    • pp.271-281
    • /
    • 1992
  • Amorphous hydrogenated silicon carbide(a-Si1-xCx : H) films have been prepared by the rf sputtering using a silicon target in a gas mixture of Argon and methane with varying methane gas flow rate(fCH) in the range of 1.5 to 3.5 sccm at constant Argon flow rate of 30sccm and rf power in the range of 3 to 6 W/$\textrm{cm}^2$. The effects of methane flow rate and rf power on the structure and optical properties of a-Si1-xCx : H films have been analysed by measuring both the IR absorption spectrum and the UV transmittance for the films. With increasing the methane flow rate, the optical band gap(Eg) of a-Si1-xCx : H films increases gradually from 1.6eV to the maximum value of 2.42eV at rf power of 4 W/$\textrm{cm}^2$, which is due to an increases in C/Si ratio in the films by an significant increase in the number of C-Hn bonds. As the rf power increases, the number of Si-C and Si-Hn bonds increases rapidly with simultaneous reduction in the number of C-Hn bonds, which is associated with an increase in both degree of methane decomposition and sputtering of silicon. The effects of rf power on the Eg of films are considerably influenced by the methane flow rate. At low methane flow rate, the Eg of films decreased from 2.3eV to 1.8eV with the rf power. On the other hand, at high methane flow rate, that of films increased slowly to 2.4eV.

  • PDF

Isolation of Sphinin, an Inhibitor of Sphingomyelinase, from Streptomyces sp. F50970

  • LIM, SI-KYU;WAN PARK
    • Journal of Microbiology and Biotechnology
    • /
    • 제9권5호
    • /
    • pp.655-660
    • /
    • 1999
  • Sphingomyelinase (SMase EC:3.l.4.l2) has been suggested to play important roles in the cell cycle, differentiation, apoptosis, inflammation, and the regulation of eukaryotic stress responses. SMase inhibitors may be a powerful tool to elucidate and regulate these cellular responses in which SMase involves. We first isolated an SMase inhibitor, named sphinin, from a strain of soil actinomycetes, F50970. Sphinin inhibited Mg/sup 2+/ -dependent neutral SMase from chicken embryo at 1.2 ㎍/㎖ of IC/sub 50/ Sphinin also inhibited acidic SMase, but it had no inhibitory activity on PI-PLC and PC-PLC, suggesting that sphinin is a specific inhibitor of SMase. The strain F50970 was identified as a Streptomyces sp. by its spiral spore chain, LL-diaminopimelic acid, menaquinone patterns of MK-9 (H'6) and MK-9 (H'8), FA-2c type of fatty acid pattern, and other morphological, physiological, and cultural characteristics.

  • PDF

서낙동강 강수의 화학적${\cdot}$세균학적 수질 (Chemical and Bacteriological Water Qualify of the Sonakdong River)

  • 김용관
    • 한국수산과학회지
    • /
    • 제19권4호
    • /
    • pp.347-355
    • /
    • 1986
  • 서낙동강의 강수는 김해평야에 농업 용수의 공급원으로서 뿐만아니라 수산 용수로서도 중요한 수계이다. 김해시민들에 의하여 배출되는 생활 오수, 김해평야에 살포되는 농약 등의 유입과 양대 수문에 의한 강수의 완만한 유동으로 서낙동강의 수역을 급속도로 오탁시킬 우려성을 갖고 있는 실정이다. 이들 수질 관리에 대한 기초자료를 얻고자 1985년 7월부터 12월까지 7회에 걸쳐 8회 지점에서 총 시료 56개로서 강수 수질의 일반성상, 영양염류와 오염지표세균에 대한 조사 결과를 보고하는 바이다. 1. pH의 변화범위와 평균치는 $6.3{\sim}9.4$, 7.91이었으며, 중${\cdot}$하부 수역에서 높은 수치를 나타내었다. 수온은 $6.1{\sim}34.8^{\circ}C,\;23.88^{\circ}C$였고, 전기전도도(지점 $A{\sim}G$)는 $1.575{\times}10^2{\sim}30.50{\times}10^2{\mu}{\mho}/cm$로서 하구로 향할수록 증가하였으며 지점 F에서는 조만 강수의 영향으로 희석되어 낮은 값을 나타내었다. 또, 강우가 빈번하였던 8,9월은 갈수기 보다 월등히 낮은 값을 나타내었다. 염화이온 농도의 변화범위와 평균치는 $23.5{\sim}14,300mg/l$, 770.0mg/l로서 지점별로 큰 폭으로 변하였다. 이 농도의 변화범위 및 평균치는 수문이 없는 낙동강의 경우 귀포 지점에서 보다는 높은 값이었다. 2. 영양염류중의 아질산성 질소의 변화범위는 평균치는 $0.007{\sim}0.110mg/l$, 0.053mg/l, 질산성 질소는 $0.001{\sim}1.638mg/l$, 0.649mg/l, 암모니아성 질소는 $0.017{\sim}4.200mg/l$, 0.497mg/l, 인산성 인은 $0.011{\sim}0.281mg/l$, 0.086mg/l, 규산성 규소는 $2.4{\sim}6.5mg/l$, 4.43mg/l로 각각 나타났다. 3. 대장균군 최확수는 $36{\sim}110,000/100ml$, 분편계대장균은 $15{\sim}46,000/100ml$, 그리고 장구균은 $3.6{\sim}15,000/100ml$이었으며, 특히 지점 B와 C오염이 극심하였다. T.C/F.C값의 범위와 평균치는 $3.0{\sim}9.6,5.51$이었으며, 분편계대장균의 오염률이 $21.26\%$이었다. 또, F.C/F.S 값의 범위와 평균치는 $1.1{\sim}9.2$, 6.19이었으며, 4.0이상인 지점이 $75\%$로서 미처이된 분편에 의하여 오염되어 있음을 시사하여 준다. 대장균군의 조성은 E.coli군이 $52\%$로 제일 많이 분류되었고, Enterobacter aerogenes군이 $13\%$, Citrobacter freundii군 순이었다.

  • PDF

Boron doping with fiber laser and lamp furnace heat treatment for p-a-Si:H layer for n-type solar cells

  • Kim, S.C.;Yoon, K.C.;Yi, J.S.
    • 한국진공학회:학술대회논문집
    • /
    • 한국진공학회 2009년도 제38회 동계학술대회 초록집
    • /
    • pp.322-322
    • /
    • 2010
  • For boron doping on n-type silicon wafer, around $1,000^{\circ}C$ doping temperature is required, because of the relatively low solubility of boron in a crystalline silicon comparing to the phosphorus case. Boron doping by fiber laser annealing and lamp furnace heat treatment were carried out for the uniformly deposited p-a-Si:H layer. Since the uniformly deposited p-a-Si:H layer by cluster is highly needed to be doped with high temperature heat treatment. Amorphous silicon layer absorption range for fiber laser did not match well to be directly annealed. To improve the annealing effect, we introduce additional lamp furnace heat treatment. For p-a-Si:H layer with the ratio of $SiH_4:B_2H_6:H_2$=30:30:120, at $200^{\circ}C$, 50 W power, 0.2 Torr for 30 min. $20\;mm\;{\times}\;20\;mm$ size fiber laser cut wafers were activated by Q-switched fiber laser (1,064 nm) with different sets of power levels and periods, and for the lamp furnace annealing, $980^{\circ}C$ for 30 min heat treatment were implemented. To make the sheet resistance expectable and uniform as important processes for the $p^+$ layer on a polished n-type silicon wafer of (100) plane, the Q-switched fiber laser used. In consequence of comparing the results of lifetime measurement and sheet resistance relation, the fiber laser treatment showed the trade-offs between the lifetime and the sheet resistance as $100\;{\omega}/sq.$ and $11.8\;{\mu}s$ vs. $17\;{\omega}/sq.$ and $8.2\;{\mu}s$. Diode level device was made to confirm the electrical properties of these experimental results by measuring C-V(-F), I-V(-T) characteristics. Uniform and expectable boron heavy doped layers by fiber laser and lamp furnace are not only basic and essential conditions for the n-type crystalline silicon solar cell fabrication processes, but also the controllable doping concentration and depth can be established according to the deposition conditions of layers.

  • PDF

Effect of Crystallization Treatment on the Magnetic Properties of Amorphous Strips Based on Co-Fe-Ni-B-Si-Cr Containing Nitrogen

  • Cho H.J.;Kwon H.T.;Ryu H.H.;Sohn K.Y.;You B.S.;Park W.W.
    • 한국분말재료학회지
    • /
    • 제13권4호
    • /
    • pp.285-289
    • /
    • 2006
  • Co-Fe-Ni-B-Si-Cr based amorphous strips containing nitrogen were manufactured via melt spinning, and then devitrified by crystallization treatment at the various annealing temperatures of $300^{\circ}C{\sim}540^{\circ}C$ for up to 30 minutes in an inert gas $(N_2)$ atmosphere. The microstructures were examined by using XRD and TEM and the magnetic properties were measured by using VSM and B-H meter. Among the alloys, the amorphous ribbons of $Co_{72.6}Fe_{9.8}Ni_{5.5}B_{2.4}Si_{7.1}Cr_{2.6}$ containing 121 ppm of nitrogen showed relatively high saturation magnetization. The alloy ribbons crystallized at $540^{\circ}C$ showed that the grain size of $Co_{72.6}Fe_{9.8}Ni_{5.5}B_{2.4}Si_{7.1}Cr_{2.6}$ alloy containing 121 ppm of nitrogen was about f nm, which exhibited paramagnetic behavior. The formation of nano-grain structure was attributed to the finely dispersed Fe4N particles and the solid-solutionized nitrogen atoms in the matrix. Accordingly, it can be concluded that the nano-grain structure of 5nm in size could reduce the core loss within the normally applied magnetic field of 300A/m at 10kHz.

Lead-Borosilicate Glass계 LTCC용 유전체에 대한 고찰 (Investigation on Lead-Borosilicate Glass Based Dielectrics for LTCC)

  • 윤상옥;오창용;김관수;조태현;심상흥;박종국
    • 한국세라믹학회지
    • /
    • 제43권6호
    • /
    • pp.338-343
    • /
    • 2006
  • The effects of lead-borosilicate glass frits on the sintering behavior and microwave dielectric properties of ceramic-glass composites were investigated as functions of glass composition of glass addition ($10{\sim}50vol%$), softening point (Ts) of the glass, and sintering temperature of the composites ($500{\sim}900^{\circ}C$ for 2 h). The addition of 50 vol% glass ensured successful sintering below $900^{\circ}C$. Sintering characteristics of the composites were well described in terms of Ts. PbO addition in to the glass enhanced the reaction with $Al_{2}O_3$ to form liquid phase and $PbAl_{2}Si_{2}O_8$, which was responsible to lower Ts. Dielectric constant(${\epsilon}_r$), $Q{\times}f_0$ and temperature coefficient of resonant frequency (${\tau}_f$) of the composite with 50 vol% glass contents ($B_{2}O_{3}:PbO:SiO_{2}:CaO:Al_{2}O_3$ = 5:40:45:5:5) demonstrated 8.5, 6,000 GHz, $-70\;ppm/^{\circ}C$, respectively, which is applicable to substrate requiring a low dielectric constant. When the same glass composition was applied sinter $MgTiO_3\;and\;TiO_2,\;at\;900^{\circ}C$ (50 vol% glass in total), the properties were 23.8, 4,000 GHz, $-65ppm/^{\circ}C$ and 31.1, 2,500 GHz, $+80ppm/^{\circ}C$ respectively, which is applicable to filter requiring an intermidiate dielectric constant.

전이 및 중금속이온과 1,15-diaza-3,4 : 12,13-dibenzo-5,8,11-trioxa-cyclooctadecane과의 착물형성 (Complex Formation of Transition and Post-Transition Metal Ions with 1,15-Diaza-3,4 : 12,13-dibenzo-5,8,11-trioxacyclooctadecane)

  • 김시중;이명재;구창현;우경자
    • 대한화학회지
    • /
    • 제35권6호
    • /
    • pp.645-652
    • /
    • 1991
  • 몇 가지 전이금속이온(Co(Ⅱ), Ni(Ⅱ), Cu(Ⅱ), Zn(Ⅱ)) 및 후전이금속이온(Cd(Ⅱ), Hg(Ⅱ), Pb(Ⅱ))과 $N_2O_3$계 거대고리 리간드인 1,15-diaza-3,4 : 12,13-dibenzo-5,8,11-trioxacyclooctadecane 사이에 형성되는 착물의 안정도 상수를 수용액에서 전위차 적정법으로 결정하였다. 각 착물의 안정도 상수$(logK_f)$$25^{\circ}$C에서 Co(Ⅱ): 3.83, Ni(Ⅱ) : 4.56, Cu(Ⅱ) : 7.74, Zn(Ⅱ) : 4.98, Cd(Ⅱ) : 3.91, Hg(II) : 14.87, Pb(Ⅱ) : 6.65이었다. 전이금속착물의 안정도 순위는 Williams-Irving 서열인 Co(Ⅱ) < Ni(Ⅱ) < Cu(Ⅱ) < Zn(Ⅱ)와 일치하였고, 후전이금속착물의 안정도는 Cd(Ⅱ) < Pb(Ⅱ) < Hg(Ⅱ)이 순위이었다. 한편 메탄올 용액에서 자외-가시선이온과 리간드가 1:1인 조성을 가졌으나, Ni(Ⅱ), 착물은 1:1과 1:2 두 가지 조성을 가질 수 있음을 알았으며, 또 디메틸술폭시드 용액에서 $^1H-$$^{13}C-$핵자기공명스펙트럼을 분석하여 후전이금속이온 착물은 주로 리간드의 질소원자가 결합에 기여함을 알았다. Cu(Ⅱ)와 Zn(Ⅱ)이 고체착물은 원소분석, 전기전도도, 자화율 측정, 자외-가시선 및 적외선 스펙트럼분석 등으로 Cu(Ⅱ) 착물은 일그러진 팔면체, 그리고 Zn(Ⅱ) 착물은 사면체 구조를 이루고 있는 것으로 예측되었다.

  • PDF

Copolymerizations of Ethylene with 1-Hexene over ansa-Metallocene Diamide Complexes

  • Kim, Il;Kwak, Chang-Hun;Son, Gi-Wan;Kim, Jae-Sung;Sinoj Abraham;Bijal K. B.;Ha, Chang-Sik;Kim, Bu-Ung;Jo, Nam-Ju
    • Macromolecular Research
    • /
    • 제12권3호
    • /
    • pp.316-321
    • /
    • 2004
  • We have performed copolymerizations of ethylene with 1-hexene using various ansa-metallocene compounds in the presence of the non-coordinative [CPh$_3$][B(C$\_$6/F$\_$5/)$_4$ion pair as a cocatalyst. The metallocenes chosen for this study are isospecific metallocene diamide compounds, rac-(EBI)Zr(NMe$_2$)$_2$ [1, EBI = ethylene-l ,2-bis(1-indenyl)], rac-(EBI)Hf(NMe$_2$)$_2$ (2), rac-(EBI)Zr(NC$_4$H$\_$8/)$_2$ (3), and rac-(CH$_3$)$_3$Si(1-C$\_$5/H$_2$-2-CH$_3$-4-$\^$t/C$_4$H$\_$9/)2 Zr(NMe$_2$)$_2$ (4), and syndiospecific metallocene dimethyl compounds, ethylidene(cyclopentadienyl)(9-fluorenyl) ZrMe$_2$ [5, Et(Flu)(Cp )ZrMe$_2$] and isopropylidence (cyclopentadienyl)(9-fluorenyl)ZrMe$_2$ [6, iPr(Flu)(Cp)ZrMe$_2$]. The copolymerization rate decreased in the order 4 >1-3>2 >5>6. The reactivity of I -hexene decreased in the order 2 >6>1- 3-5> 4. We characterized the microstructure of the resulting poly(ethylene-co-l-hexene) by $\^$l3/C NMR spectroscopy and investigated various other properties of the copolymers in detail.

염화알미늄 증기의 부분가수분해를 통한 알파 알루미나 나노입자 제조 (Synthesis of ${\alpha}$-Alumina Nanoparticles Through Partial Hydrolysis of Aluminum Chloride Vapor)

  • 박회경;유연석;박균영;정경열
    • Korean Chemical Engineering Research
    • /
    • 제49권5호
    • /
    • pp.664-668
    • /
    • 2011
  • 500 mL 교반탱크반응기 내에서 $AlCl_3$ 증기를 $H_2O$ 증기에 의해 부분 가수분해시켜 30~200 nm 크기의 $AlO_xCl_y(OH)_z$로 표시되는 구형의 알루미나 전구체 입자를 제조하였다. 반응시간, 교반속도, 반응온도가 생성된 입자의 형상, 크기 등에 미치는 영향을 조사하였다. 반응시간을 20, 60, 300 s로 변화시킨 결과 생성 입자의 형상 및 크기에 별다른 차이가 없었으며, 교반속도를 0, 300, 800 rpm으로 변화시킨 결과 0 rpm에서 입자의 크기가 최대값을 보였고, 반응온도를 180, 190, 200, $240^{\circ}C$로 변화시킨 결과 $190^{\circ}C$에서 제조된 입자의 크기가 가장 작게 나타났다. 가수분해 생성물 입자를 $10^{\circ}C$/min의 속도로 $1,200^{\circ}C$까지 가열하고 6 시간동안 하소시켜 45 nm 크기의 ${\alpha}$ 알루미나 입자를 얻었다. 하소과정에서 인접입자 사이의 소결에 의해 입자 형상이 구형에서 벌레모양으로 변환되었다. 하소온도를 $1,400^{\circ}C$로, 승온속도를 $50^{\circ}C$/min 로 증가시키고, 유지시간을 0.5 시간으로 감소시켜 급속 하소시킴으로써 인접입자의 소결을 상당히 감소시킬 수 있었다. $AlCl_3$의 가수분해 과정에서 소량의 $SiCl_4$ 또는 TMCTS(2,4,6,8-tetramethylcylosiloxane) 첨가에 의해 인접입자의 소결 방지 효과가 나타났으나, ${\alpha}$ 결정 이외에 ${\gamma}$ 결정, mullite 결정 등이 함께 생성되었다. 하소과정에서 $AlF_3$를 첨가한 결과 육각형 디스크 형상의 ${\alpha}$ 알루미나 입자가 생성되었다.

Isoprenylated flavonoids from the root bark of Morus alba L. and their inhibition effect on NO production in LPS-induced RAW 264.7 cells

  • Jung, Jae-Woo;Ko, Jung-Hwan;Ko, Won-Min;Park, Ji-Hae;Baek, Yun-Su;Kim, Youn-Chul;Baek, Nam-In
    • Journal of Applied Biological Chemistry
    • /
    • 제60권2호
    • /
    • pp.109-111
    • /
    • 2017
  • The root bark of Morus alba L. were extracted with 80% aqueous MeOH, and the concentrated extract was partitioned with EtOAc, n-BuOH, and $H_2O$ fractions. The repeated silica gel ($SiO_2$), octadecyl $SiO_2$ (ODS), and Sephadex LH-20 column chromatographies of the EtOAc fraction led to isolation of 12 phenolic compounds. The chemical structures of the compounds were determined as sanggenol Q (1), sanggenol A (2), sanggenol L (3), kuwanon T (4), cyclomorusin (5), sanggenon F (6), sanggenol O (7), sanggenon N (8), sanggenon G (9), mulberrofuran G (10), mulberrofuran C (11), and moracin E (12). All isolated compounds were evaluated for inhibit lipopolysaccharide-induced nitric oxide production in RAW 264.7 macrophages.