Proceedings of the Korean Society of Precision Engineering Conference
/
2002.10a
/
pp.155-159
/
2002
This paper has studied to obtain the grinding characteristics and optimal grinding conditions of ceramics in the grinding with diamond wheel by Taguchi method. Feed rate was most important factor to the surface roughness. In the case of 4{Si_3}{N_4}$ and ${A1_2}{O_3}$, surface roughness value were small at 3m/min of feed rate. In the case of $ZrO_2$. surface roughness value was small at 4m/min of feed rate. Surface roughness have much influenced by major load for the :ii3N4 and $ZrO_2$. On the other hand, ${A1_2}{O_3}$ have more influenced by grain shedding of brittle fracture phenomenon. The major factors affecting the surface roughness and the optimum grinding conditions were obtained with minimum experiment using Taguchi method.
In this study, $(n-BuCp)_2ZrCl_2$, was supported on $SiO_2/MgCl_2$ binary support. Before supporting the catalyst, the $SiO_2/MgCl_2$ binary support was surface treated with three different alkyl aluminum compound, namely trimethylaluminum, triethylaluminum, and ethylaluminum sesquichloride. The synthesized surface-treated $SiO_2/MgCl_2$ supported metallocene catalysts were used for the copolymerization of ethylene and 1-hexene. Their catalytic properties and performances were analyzed through BET, XPS analysis, ICP-AES analysis, and FE-SEM. While the resulting copolymers were analyzed through DSC analysis, GPC analysis, 13C-NMR analysis, and FE-SEM. The analysis of synthesized surface-treated $SiO_2/MgCl_2$ supported metallocene catalysts showed that the Zr content of these catalysts is relatively lower compared to that of the catalyst supported on $SiO_2$. This could be attributed to the reduction in the surface area of $SiO_2$ due to the presence of recrystallized $MgCl_2$ and alkyl aluminum. Furthermore, they exhibited a better copolymerization activity compared to that of $SiO_2$ supported catalyst, particularly the EASC-surface treated binary support, which has the highest activity of 1.9 kg PE/($mmol-Zr^*hr$) because EASC acts as a strong Lewis acid. It could also be observed that the larger the ligand of alkyl aluminum used, the rougher the particle surface of the resulting polymer.
The volume and toxicity of radioactive waste can be decreased by separating the components of high-level liquid waste according to their properties. An impregnated silica-based adsorbent was prepared in this study by combining N,N,N',N',N",N"-hexa-n-octylnitrilotriacetamide (HONTA) extractant, N',N'-di-n-hexyl-thiodiglycolamide (Crea) extractant, and macroporous silica polymer composite particles (SiO2-P). The performance of platinum-group metals adsorption and separation on prepared (HONTA + Crea)/SiO2-P adsorbent was then assessed together with that of co-existing metal ions by batch-adsorption and chromatographic separation studies. From the batch-adsorption experiment results, (HONTA + Crea)/SiO2-P adsorbent showed high adsorption performance of Pd(II) owing to an affinity between Pd(II) and Crea extractant based on the Hard and Soft Acids and Bases theory. Additionally, significant adsorption performance was observed toward Zr(IV) and Mo(VI). Compared with studies using the Crea extractant, the high adsorption performance of Zr(IV) and Mo(VI) is attributed to the HONTA extractant. As revealed from the chromatographic experiment results, most of Pd(II) was recovered from the feed solution using 0.2 M thiourea in 0.1 M HNO3. Additionally, the possibility of recovery of Zr(IV), Mo(VI), and Re(VII) was observed using the (HONTA + Crea)/SiO2-P adsorbent.
The hydrolysis and condensation reactions in the mixed alkoxide solutions of Si(OC2H5)4 and Zr(O-nC3H7)4 with various water contents (1, 2, 4, and 8 in molar ratio to alkoxide, r) and catalysts were examined by rheological measurements and the number average molecular weight in order to explain the shape of the polymer in the mixed alkoxide solutions. It was found that fibers could be drawn in the viscosity range of 1∼100P from the acid-catalyzed solutions with lower water contents of the mole ratio H2O/alkoxide, r 2. On the other hand, crack free bulk gel was formed from the acid-catalyzed solutions including a large amount of water (r 4), and the base-catalyzed solutions. The relation between the intrinsic viscosity [{{{{ eta }}] and the number average molecular weight n, namely [{{{{ eta }}]=Knα, has shown that the acid-catalyzed spinnable solutions (r=1 and 2) have linear polymers and the exponent α's are about 0.56 and 0.81, whereas non-spinnable solutions (r=4 and 8) have three dimensional network polymers or spherical particles and the exponent α's are 0.41∼0.51 and 0.35.
Transactions of the Korean Society of Machine Tool Engineers
/
v.12
no.5
/
pp.8-14
/
2003
The characteristics of grinding and wear behavior of diamond wheel for grinding ceramic materials was investigated in this study. In case of $Si_3N_4$, the wear of wheel was large, the finding force was relatively stable and the fluctuation of surface roughness n small. On the other hand in case of $Al_2O_3$ and $ZrO_2$, the wear of wheel and surface roughness were decreasing, the grinding force was increasing. During grinding with vitrified bond wheel, $Si_3N_4$ shows renewal of cutting edge while $Al_2O_3$ and $ZrO_2$ show glazing phenomenon of cutting grains. We have found that it possible to observe the behavior of grinding wheel by grinding ratio, grinding resistance, surface roughness and cutting edge ratio. Through the grinding experiments, it was found that grinding life of diamond wheel is 20 times for $Si_3N_4$, and 40 times fir $Al_2O_3$ and $ZrO_2$.
Zirconium oxide films have been synthesized by radio-frequency magnetron sputtering deposition on n-Si(001) substrate with metal zirconium target at variant $O_2$ partial pressures. The influences of $O_2$ partial pressures of the morphology, deposition rate, microstructure, and the dielectric constant of $ZrO_2$ have been discussed. The results show that deposition rate of $ZrO_2$ films decreases, the roughness, and the thickness of the native $SiO_2$ interlayer increases with the increase of $O_2$ partial pressure. $ZrO_2$ films synthesized at low $O_2$ partial pressure are amorphous and monoclinic polycrystalline in nanometer scale at low $O_2$ partial pressure. The relative dielectrics of $ZrO_2$ films are in the range of 12 to 25.
Journal of the Korean institute of surface engineering
/
v.47
no.5
/
pp.263-268
/
2014
Nanocrystalline diamond(NCD) coated SiC balls were applied in a ball-on-disk tribometer. After seeding in an ultrasonic bath containing nanometer diamond powders, $2.2{\mu}m$ thick NCD films were deposited on sintered 3 mm diameter SiC balls at $600^{\circ}C$ in a 2.45 GHz microwave plasma CVD system. Bare $ZrO_2$ and SiC balls were prepared for comparison as test balls. Tribology tests were performed in air with pairs of three different balls and mirror polished steel(SKH51) disk. The wear tracks on balls and disks were examined by optical microscope and alpha step profiler. Under the load of 3 N, the friction coefficients of steel against $ZrO_2$, SiC and NCD-coated balls were between 0.4 and 0.8. After a few thousands sliding laps, the friction coefficient of NCD-coated balls dropped from 0.45 to below 0.1 and maintained thereafter. Under a higher load of 10 N or 20 N with a long sliding distance of 2 km, $ZrO_2$ and SiC balls exhibited the similar friction coefficients as above. The friction coefficient of NCD-coated balls was less than 0.1 from the beginning and increased to above 0.1 steadily or with some fluctuations as sliding distance increased. NCD coating layers were found worn out after long duration and/or high load sliding test, which resulted in the friction coefficient higher than 0.1.
For copolymerization of ethylene and norbornene initiated by various metallocene catalysts such as $rac-Et(Ind)_2ZrCl_2,\;rac-Me_2Si(Ind)_2ZrCl_2,\;rac-Me_2Si(Cp)_2ZrCl_2,\;and\;(n-BuCp)_2ZrCl_2$ with modified methylaluminoxane(MMAO) cocatalyst, the ${\alpha}$-olefins such as 1-hexene(H), 1-octene and 1-decene were added as a 3rd monomer. In this situation, the effects of the polymerization condition, the catalyst structure as well as the structure and the amount of added ${\alpha}$-olefin on the catalyst activity as well as the properties and structure of polymer were examined. As results, it was found that the catalyst activity and thermal property of polymer depended on not only catalyst structure but also ${\alpha}$-olefin structure. For $rac-Et(Ind)_2ZrCl_2/MMAO$ catalyst system, it was possible to get high activity and controllable $T_g$ of polymer. Among ${\alpha}$-olefins, H as a 3rd monomer exhibited the maximum enhancement in catalyst activity.
Proceedings of the Korean Vacuum Society Conference
/
2010.02a
/
pp.381-381
/
2010
$(ZrO_2)_{0.66}(HfO_2)_{0.34}$ thin films as gate dielectrics have been proposed to overcome the problems of tunneling current and degradation mobility inachieving a thin equivalent oxide thickness. An extremely thin $SiO_2$ layer is used in order to separate the carrier in MOSFET channel from the dielectric field fluctuation caused by phonons in the dielectric which decreases the carrier mobility. The electronic and optical properties influenced the device performance to a great extent. $(ZrO_2)_{0.66}(HfO_2)_{0.34}$ dielectric films on p-Si (100) were grown by atomic layer deposition method, for which the conduction band offsets, valence band offsets and band gapswere obtained by using X-ray photoelectron spectroscopy and reflection electron energy loss spectroscopy. The band gap, valence and conduction band offset values for $(ZrO_2)_{0.66}(HfO_2)_{0.34}$ dielectric thin film, grown on Si substrate were about 5.34, 2.35 and 1.87 eV respectively. This band alignment was similar to that of $ZrO_2$. In addition, The dielectric function (k, $\omega$), index of refraction n and the extinction coefficient k for the $(ZrO_2)_{0.66}(HfO_2)_{0.34}$ thin films were obtained from a quantitative analysis of REELS data by comparison to detailed dielectric response model calculations using the QUEELS-$\varepsilon$(k, $\omega$)-REELS software package. These optical properties are similar with $ZrO_2$ dielectric thin films.
JSTS:Journal of Semiconductor Technology and Science
/
v.17
no.2
/
pp.245-251
/
2017
Niobium doped zirconium oxide (Nb-Zr-O:NZO) thin films were fabricated on Si substrates by a sol-gel technique with an annealing temperatures of $500{\sim}1000^{\circ}C$ in air ($N_2:O_2=3:1$) for 20 minutes. It was found that the NZO film is based on tetragonal $ZrO_2$ polycrystalline structure with the Nb 5+ ion state and there is almost no diffusion of Nb or Zr to Si substrate. The relative dielectric constant for the NZO film with the Nb composition of 30 mol% and annealed at $800^{\circ}C$ was around 40. The root mean roughness was 1.02 nm. In addition, the leakage current of NZO films was as low as $10^{-6}A/cm^2$ at 4.4 V.
본 웹사이트에 게시된 이메일 주소가 전자우편 수집 프로그램이나
그 밖의 기술적 장치를 이용하여 무단으로 수집되는 것을 거부하며,
이를 위반시 정보통신망법에 의해 형사 처벌됨을 유념하시기 바랍니다.
[게시일 2004년 10월 1일]
이용약관
제 1 장 총칙
제 1 조 (목적)
이 이용약관은 KoreaScience 홈페이지(이하 “당 사이트”)에서 제공하는 인터넷 서비스(이하 '서비스')의 가입조건 및 이용에 관한 제반 사항과 기타 필요한 사항을 구체적으로 규정함을 목적으로 합니다.
제 2 조 (용어의 정의)
① "이용자"라 함은 당 사이트에 접속하여 이 약관에 따라 당 사이트가 제공하는 서비스를 받는 회원 및 비회원을
말합니다.
② "회원"이라 함은 서비스를 이용하기 위하여 당 사이트에 개인정보를 제공하여 아이디(ID)와 비밀번호를 부여
받은 자를 말합니다.
③ "회원 아이디(ID)"라 함은 회원의 식별 및 서비스 이용을 위하여 자신이 선정한 문자 및 숫자의 조합을
말합니다.
④ "비밀번호(패스워드)"라 함은 회원이 자신의 비밀보호를 위하여 선정한 문자 및 숫자의 조합을 말합니다.
제 3 조 (이용약관의 효력 및 변경)
① 이 약관은 당 사이트에 게시하거나 기타의 방법으로 회원에게 공지함으로써 효력이 발생합니다.
② 당 사이트는 이 약관을 개정할 경우에 적용일자 및 개정사유를 명시하여 현행 약관과 함께 당 사이트의
초기화면에 그 적용일자 7일 이전부터 적용일자 전일까지 공지합니다. 다만, 회원에게 불리하게 약관내용을
변경하는 경우에는 최소한 30일 이상의 사전 유예기간을 두고 공지합니다. 이 경우 당 사이트는 개정 전
내용과 개정 후 내용을 명확하게 비교하여 이용자가 알기 쉽도록 표시합니다.
제 4 조(약관 외 준칙)
① 이 약관은 당 사이트가 제공하는 서비스에 관한 이용안내와 함께 적용됩니다.
② 이 약관에 명시되지 아니한 사항은 관계법령의 규정이 적용됩니다.
제 2 장 이용계약의 체결
제 5 조 (이용계약의 성립 등)
① 이용계약은 이용고객이 당 사이트가 정한 약관에 「동의합니다」를 선택하고, 당 사이트가 정한
온라인신청양식을 작성하여 서비스 이용을 신청한 후, 당 사이트가 이를 승낙함으로써 성립합니다.
② 제1항의 승낙은 당 사이트가 제공하는 과학기술정보검색, 맞춤정보, 서지정보 등 다른 서비스의 이용승낙을
포함합니다.
제 6 조 (회원가입)
서비스를 이용하고자 하는 고객은 당 사이트에서 정한 회원가입양식에 개인정보를 기재하여 가입을 하여야 합니다.
제 7 조 (개인정보의 보호 및 사용)
당 사이트는 관계법령이 정하는 바에 따라 회원 등록정보를 포함한 회원의 개인정보를 보호하기 위해 노력합니다. 회원 개인정보의 보호 및 사용에 대해서는 관련법령 및 당 사이트의 개인정보 보호정책이 적용됩니다.
제 8 조 (이용 신청의 승낙과 제한)
① 당 사이트는 제6조의 규정에 의한 이용신청고객에 대하여 서비스 이용을 승낙합니다.
② 당 사이트는 아래사항에 해당하는 경우에 대해서 승낙하지 아니 합니다.
- 이용계약 신청서의 내용을 허위로 기재한 경우
- 기타 규정한 제반사항을 위반하며 신청하는 경우
제 9 조 (회원 ID 부여 및 변경 등)
① 당 사이트는 이용고객에 대하여 약관에 정하는 바에 따라 자신이 선정한 회원 ID를 부여합니다.
② 회원 ID는 원칙적으로 변경이 불가하며 부득이한 사유로 인하여 변경 하고자 하는 경우에는 해당 ID를
해지하고 재가입해야 합니다.
③ 기타 회원 개인정보 관리 및 변경 등에 관한 사항은 서비스별 안내에 정하는 바에 의합니다.
제 3 장 계약 당사자의 의무
제 10 조 (KISTI의 의무)
① 당 사이트는 이용고객이 희망한 서비스 제공 개시일에 특별한 사정이 없는 한 서비스를 이용할 수 있도록
하여야 합니다.
② 당 사이트는 개인정보 보호를 위해 보안시스템을 구축하며 개인정보 보호정책을 공시하고 준수합니다.
③ 당 사이트는 회원으로부터 제기되는 의견이나 불만이 정당하다고 객관적으로 인정될 경우에는 적절한 절차를
거쳐 즉시 처리하여야 합니다. 다만, 즉시 처리가 곤란한 경우는 회원에게 그 사유와 처리일정을 통보하여야
합니다.
제 11 조 (회원의 의무)
① 이용자는 회원가입 신청 또는 회원정보 변경 시 실명으로 모든 사항을 사실에 근거하여 작성하여야 하며,
허위 또는 타인의 정보를 등록할 경우 일체의 권리를 주장할 수 없습니다.
② 당 사이트가 관계법령 및 개인정보 보호정책에 의거하여 그 책임을 지는 경우를 제외하고 회원에게 부여된
ID의 비밀번호 관리소홀, 부정사용에 의하여 발생하는 모든 결과에 대한 책임은 회원에게 있습니다.
③ 회원은 당 사이트 및 제 3자의 지적 재산권을 침해해서는 안 됩니다.
제 4 장 서비스의 이용
제 12 조 (서비스 이용 시간)
① 서비스 이용은 당 사이트의 업무상 또는 기술상 특별한 지장이 없는 한 연중무휴, 1일 24시간 운영을
원칙으로 합니다. 단, 당 사이트는 시스템 정기점검, 증설 및 교체를 위해 당 사이트가 정한 날이나 시간에
서비스를 일시 중단할 수 있으며, 예정되어 있는 작업으로 인한 서비스 일시중단은 당 사이트 홈페이지를
통해 사전에 공지합니다.
② 당 사이트는 서비스를 특정범위로 분할하여 각 범위별로 이용가능시간을 별도로 지정할 수 있습니다. 다만
이 경우 그 내용을 공지합니다.
제 13 조 (홈페이지 저작권)
① NDSL에서 제공하는 모든 저작물의 저작권은 원저작자에게 있으며, KISTI는 복제/배포/전송권을 확보하고
있습니다.
② NDSL에서 제공하는 콘텐츠를 상업적 및 기타 영리목적으로 복제/배포/전송할 경우 사전에 KISTI의 허락을
받아야 합니다.
③ NDSL에서 제공하는 콘텐츠를 보도, 비평, 교육, 연구 등을 위하여 정당한 범위 안에서 공정한 관행에
합치되게 인용할 수 있습니다.
④ NDSL에서 제공하는 콘텐츠를 무단 복제, 전송, 배포 기타 저작권법에 위반되는 방법으로 이용할 경우
저작권법 제136조에 따라 5년 이하의 징역 또는 5천만 원 이하의 벌금에 처해질 수 있습니다.
제 14 조 (유료서비스)
① 당 사이트 및 협력기관이 정한 유료서비스(원문복사 등)는 별도로 정해진 바에 따르며, 변경사항은 시행 전에
당 사이트 홈페이지를 통하여 회원에게 공지합니다.
② 유료서비스를 이용하려는 회원은 정해진 요금체계에 따라 요금을 납부해야 합니다.
제 5 장 계약 해지 및 이용 제한
제 15 조 (계약 해지)
회원이 이용계약을 해지하고자 하는 때에는 [가입해지] 메뉴를 이용해 직접 해지해야 합니다.
제 16 조 (서비스 이용제한)
① 당 사이트는 회원이 서비스 이용내용에 있어서 본 약관 제 11조 내용을 위반하거나, 다음 각 호에 해당하는
경우 서비스 이용을 제한할 수 있습니다.
- 2년 이상 서비스를 이용한 적이 없는 경우
- 기타 정상적인 서비스 운영에 방해가 될 경우
② 상기 이용제한 규정에 따라 서비스를 이용하는 회원에게 서비스 이용에 대하여 별도 공지 없이 서비스 이용의
일시정지, 이용계약 해지 할 수 있습니다.
제 17 조 (전자우편주소 수집 금지)
회원은 전자우편주소 추출기 등을 이용하여 전자우편주소를 수집 또는 제3자에게 제공할 수 없습니다.
제 6 장 손해배상 및 기타사항
제 18 조 (손해배상)
당 사이트는 무료로 제공되는 서비스와 관련하여 회원에게 어떠한 손해가 발생하더라도 당 사이트가 고의 또는 과실로 인한 손해발생을 제외하고는 이에 대하여 책임을 부담하지 아니합니다.
제 19 조 (관할 법원)
서비스 이용으로 발생한 분쟁에 대해 소송이 제기되는 경우 민사 소송법상의 관할 법원에 제기합니다.
[부 칙]
1. (시행일) 이 약관은 2016년 9월 5일부터 적용되며, 종전 약관은 본 약관으로 대체되며, 개정된 약관의 적용일 이전 가입자도 개정된 약관의 적용을 받습니다.