열간 정수압 소결(HIP)에 의한 Y-Ba-Cu-O계rhdhs 초전도체의 제작 및 특성 (Properties of Y-Ba-Cu-O High Tc superconductor prepared by sintering, sintering+HIP encapsulation)

  • 김종문;백수현
    • 한국전기전자재료학회:학술대회논문집
    • /
    • 한국전기전자재료학회 1988년도 추계학술대회 논문집
    • /
    • pp.36-40
    • /
    • 1988
  • High TC Y-Ba-Cu-O Superconductors were fabricated by sintering, sinter+HIP encapsulation. Specimens were sintered at 920$^{\circ}C$∼960$^{\circ}C$. A part of sintered specimens were treated by HIP, and HIP conditions were 150 MPa, 880$^{\circ}C$, 30min under the Ar atmosphere. The relative density of HIP specimens was increased 5∼8% in comparison with sintered one(90∼93% relative density). X-ray analysis represented the orthorhobic-tetragonal phase transition with annealing condition. Tc measurements showed a sharp drp within 3$^{\circ}C$, 91K onset and 89K offset. Transport current density(Jc) of sintered specimens showed typically∼159A/㎤ but that of sinter+HIP encapsulation was decreased to∼89A/㎤ because of insufficient oxygen diffusion, Hardness(H) and Toughness(Kc) were increased to 38GPa; and 2.9 MPam$\^$$\frac{1}{2}$/, respectively.

  • PDF

고온 초전도체 $Y_{1-x}Sm_xBa_2Cu_3O_{7-y}$의 적외선 투과율과 자기적 성질에 관한 연구 (A study on the infrared transmittance and magnetic properties of high Tc superconductor $Y_{1-x}Sm_xBa_2Cu_3O_{7-y}$)

  • 김채옥;김재욱;김의훈
    • E2M - 전기 전자와 첨단 소재
    • /
    • 제5권2호
    • /
    • pp.189-197
    • /
    • 1992
  • 고온 초전도체 $Y_{1}$Ba$_{2}$Cu$_{3}$O$_{7-y}$에서 Y를 Sm으로 치환시켰을 때의 자기 임계 전류밀도와 저항은 각각 30K와 80-160K의 온도에서 측정되었다. 그리고 X-선 회절분석 및 적외선 투과율 측정은 실온에서 수행되었으며 시료들은 고상 반응법에 의해서 제조되었다. 93K근에의 값을 갖는 초전도 전이온도 T$_{c}$는 치환양에 따라 거의 변하지 않았다. 시료들의 결정구조는 X-선 회절무늬로 부터 모두 직방정계임이 판명되었다. 적외선 투과율 측정에서 날카로운 peak들은 472.78-618.53$cm^{-1}$ /범위에 있었다. 이것은 특이할 정도로의 low-lying plasmalike edge와 낮은 에너지의 전자적인 여기가 존재함을 나타내는 것이다. 자기 임계 전류밀도는 $10^{3}$~$10^{4}$A/$cm^{2}$범위에 있었다. 전이온도 T$_{c}$에 상자성 불순물의 영향이 거의 없는 것으로 보아 123phase에서 Y가 고온 초전도성에 주된 역할을 하지 않음을 알수 있었다.다.

  • PDF

Effects of artificial holes in very large single-grain Y1.5Ba2Cu3O7-y bulk superconductors

  • Park, S.D.;Park, H.W.;Jun, B.H.;Kim, CJ.
    • 한국초전도ㆍ저온공학회논문지
    • /
    • 제19권3호
    • /
    • pp.27-32
    • /
    • 2017
  • The effects of artificial holes on the trapped magnetic fields and magnetic levitation forces of very large single-grain $Y_{1.5}Ba_2Cu_3O_{7-y}$ (Y1.5) bulk superconductors were studied. Artificial holes were made for Y1.5 powder compacts by die pressing using cylindrical dies with a diameter of 30 mm or 40 m, or rectangular dies with a side length of 50 mm. The single grain Y1.5 bulk superconductors (25 mm, 33 mm in diameter and 42 mm in side length) with artificial holes were fabricated using a top-seeded melt growth (TSMG) process for the die-pressed Y1.5 powder compacts. The magnetic levitation forces at 77 K of the 25 mm single grain Y1.5 samples with one (diameters of 4.2 mm) or six artificial holes (diameters of 2.5 mm) were 10-17% higher than that of the Y1.5 sample without artificial holes. The trapped magnetic fields at 77 K of the Y1.5 samples with artificial holes were also 9.6-18% higher than that of the Y1.5 sample without artificial holes. The 33 mm and 42 mm single grain Y1.5 samples with artificial holes (2.5 mm and 4.2 mm in diameter) also showed trapped magnetic fields 10-13% higher than that of the Y1.5 samples without artificial holes in spite of the reduced superconducting volume fraction due to the presence of artificial holes. The property enhancement in the large single grain Y1.5 bulk superconductors appears to be attributed to the formation of the pore-free regions near the artificial holes and the homogeneous oxygen distribution in the large Y123 grains.

Low-Temperature Sintering of Barium Calcium Zirconium Titanate Lead-Free Piezoelectric Ceramics

  • Fisher, John G.;Lee, Dae-Gi;Oh, Jeong-Hyeon;Kim, Ha-Nul;Nguyen, Dieu;Kim, Jee-Hoon;Lee, Jong-Sook;Lee, Ho-Yong
    • 한국세라믹학회지
    • /
    • 제50권2호
    • /
    • pp.157-162
    • /
    • 2013
  • The need for lead-free piezoceramics has caused a renewal of interest in $BaTiO_3$-based systems. Recently, it was found that ceramics in the $(Ba,Ca)(Zr,Ti)O_3$ system have properties comparable to those of $Pb(Zr,Ti)O_3$. However, these ceramics require rather high sintering temperatures of $1450-1550^{\circ}C$. In this work, the effect of $TiO_2$ and CuO addition on the sintering behavior, microstructure, dielectric and piezoelectric properties of $(Ba_{0.85}Ca_{0.15})(Zr_{0.1}Ti_{0.9})O_3$ (BCTZ) ceramics will be discussed. BCTZ ceramics were prepared by the mixed oxide route and 1 mol % of $TiO_2$ or CuO was added. Undoped and doped ceramics were sintered at $1350^{\circ}C$ for 1-5 h. CuO was found to be a very effective sintering aid, with samples sintered for 1 h at $1350^{\circ}C$ having a bulk density of 95% theoretical density; however the piezoelectric properties were greatly reduced, probably due to the small grain size.

Effect of Metal Oxide on the Superconductivity of YBCO

  • Lee, Sang-Heon
    • 한국분말야금학회:학술대회논문집
    • /
    • 한국분말야금학회 2006년도 Extended Abstracts of 2006 POWDER METALLURGY World Congress Part2
    • /
    • pp.1241-1242
    • /
    • 2006
  • Electromagnetic properties of $CeO_2$ doped and undoped YBaCuO superconductors were evaluated to investigate the effect of pinning center on the magnetization and magnetic shielding. The variation $\DeltaM$ with doping was maximum for 3% doping and decrease with further doping. The magnetic shielding was evaluated by measuring the induced voltage in secondary coil and the voltage initially set to 0.5V, decreased to 0.17V and 0.28V respectively for the undoped and 3% $CeO_2$ doped sample. The much less change in the induced voltage for the 3% doped sample is attributed to the increased flux shielding by shielding vortex current. The $CeO_2$ was converted to fine $BaCeO_3$ particles which were trapped in YBaCuO superconductor during the reaction sintering. The trapped fine particles, $BaCeO_3$ may be acted as a flux pinning center.

  • PDF

용융침투성장법을 이용한 YBCO 단결정 제조 (A Fabrication of YBCO Single Crystal using Infiltration and Growth Method)

  • 한상철;정년호;한영희;성태현
    • 한국전기전자재료학회논문지
    • /
    • 제20권6호
    • /
    • pp.550-554
    • /
    • 2007
  • Large and single-grain Y-Ba-Cu-O(YBCO) bulk superconductors have been fabricated by using a seeded infiltration and growth method. $Y_2BaCuO_5$(Y211) precursor pellets and $YBa_2Cu_3O_x$(Y123) liquid source pellets were prepared using commercial powder and were processed by infiltration and growth method to achieve low pore and high trapped field property. The superconductor properties of the single crystal are measured and analyzed in relation with the density and size of the Y211 particle in the Y123 matrix. An optimum processing condition is suggested based on the analyzed results.

통가열도 TA26 해저산의 모암변질과 원소분산 (Element Dispersion and Wallrock Alteration of TA26 Seamount, Tonga Arc)

  • 유봉철;최헌수;고상모
    • 자원환경지질
    • /
    • 제44권5호
    • /
    • pp.359-372
    • /
    • 2011
  • 통가열도의 남단에 위치하는 TA26 해저산은 열수활동이 가장 활발한 것으로 알려진 해저산으로 열수플룸이 광범위하게 존재하며 열수광석 및 열수변질암이 채취된 지역이다. 이 지역에서 채취한 암석들은 현무암내지 현무암질 안산암이다. 열수용액에 의한 변질암석시료에서는 사장석, 휘석류, 황철석, 티탄철석, 비결정질 살리카, 중정석, 녹점토, iron sulfates, Fe-Si sulfates 및 Fe silicates 등이 산출된다. 모암변질시 열수작용에 의한 변질 암석의 주원소, 미량원소 및 희토류원소 이득 및 손실을 계산하면, $K_2O$(+0.04~+0.45 g), $SiO_2$(-6.52~+10.56 g), $H_2O$(-0.03~+6.04 g), $SO_4$(-0.46~+17.54 g), S(-0.46~+13.45 g) 및 총 S(-0.51~+16.93 g)들이 모암변질시 이득되었다. 또한 미량원소들 중 특히 Ba(-7.60~+185078.62 g), Sr(-36.18~+3033.08 g), Ag(+54.83 g), Au(+1467.49 g), As(-5.80~+1030.80 g), Cd(+249.78 g), Cu(-100.57~+1357.85 g), Pb(+4.91~+532.65 g), Sb(-0.32~+66.59 g), V(-113.58~+102.94 g), 및 Zn(-49.56~+14989.92 g)들이 모암변질시 이득되었다. 따라서 이득된 주원소 및 미량원소의 종류 및 함량($K_2O$, $H_2O$, $SO_4$, S, 총 S, Ba, Sr, Ag, Au, As, Cd, Cu, Pb, Sb, V, Zn) 등을 지시원소로서 활용하면 통가열도 심해저 열수광상 탐사시 유용하게 이용될 수 있다.

용융법에 의한 YBa2Cu3O7-y 초전도체 제작 (Preparation of YBa2Cu3O7-y Superconductor Using Melt Method)

  • 이상헌
    • 한국전기전자재료학회논문지
    • /
    • 제35권6호
    • /
    • pp.622-625
    • /
    • 2022
  • YBa2Cu3O7-y bulk as a high temperature oxide superconducting conductor has the high critical temperature of 92 K. YBa2Cu3O7-y bulk superconductors have been fabricated by a seeded melting growth. Magnetic properties were studied by using superconductor of melted YBa2Cu3O7-y oxides. It was demonstrated that Y2BaCuO5 particles acts as a pinning center which plays an important role on the magnetic properties. The thickness of the upper and lower pellets of the YBa2Cu3O7-y bulk was formed at 40 mm with 55 g of the composition, and the YBa2Cu3O7-y superconductor was manufactured through a heat treatment process. Manufacturing the superconducting bulk, it is possible to improve the pore density of the superconducting bulk by providing a path through which oxygen could be emitted.

BaSn(BO3)2세라믹스의 저온소결 및 유전특성 (Low-Temperature Sintering and Dielectric Properties of BaSn(BO3)2 Ceramics)

  • 남명화;김효태;황준철;남중희;여동훈;김종희;남산
    • 한국세라믹학회지
    • /
    • 제43권2호
    • /
    • pp.92-97
    • /
    • 2006
  • Dolomite type $BaSn(BO_3)_2$ ceramics with rhombohedral crystal structure has been synthesized via solid state reaction route. Dielectric properties were measured for the samples sintered at $1050\~1200^{\circ}C$ for 2 h in air. Dielectric constant, loss tangent, and temperature coefficient were increased with sintering temperature due to the evolution of $BaSnO_3$, secondary, phase. Optimum dielectric properties were obtained at the $BaSn(BO_3)_2$ ceramics sintered at $1100^{\circ}C.\;CuO/Bi_2O_3$ was added to $BaSn(BO_3)_2$ ceramics to lower the sintering temperature for LTCC application, then Co and Fe-based coloring agents were added for colorizing the LTCC tape. Typical dielectric properties of $BaSn(BO_3)_2$ ceramics with $5 wt\%\;CuO/Bi_2O_3\;and\;3wt\%$ Co-coloring agent that sintered at $900^{\circ}C$ were $\varepsilon_r=9.89,\;tan{\delta}=0.92\times10^{-3},\;and\;TCC=112ppm/^{\circ}C$. Thus obtained LTCC tape was co-fired with Ag paste for compatibility test and revealed no sign of Ag reaction with the ceramics.