• Title/Summary/Keyword: Wood drying

Search Result 319, Processing Time 0.028 seconds

A Devolatilization Model of Woody Biomass Particle in a Fluidized Bed Reactor (유동층 반응기에서의 목질계 바이오매스 입자의 탈휘발 예측 모델)

  • Kim, Kwang-Su;Leckner, Bo;Lee, Jeong-Woo;Lee, Uen-Do;Choi, Young-Tai
    • Korean Chemical Engineering Research
    • /
    • v.50 no.5
    • /
    • pp.850-859
    • /
    • 2012
  • Devolatilization is an important mechanism in the gasification and pyrolysis of woody biomass, and has to be accordingly considered in designing a gasifier. In order to describe the devolatilization process of wood particle, there have been proposed a number of empirical correlations based on experimental data. However, the correlations are limited to apply for various reaction conditions due to the complex nature of wood devolatilization. In this study, a simple model was developed for predicting the devolatilization of a wood particle in a fluidized bed reactor. The model considered the drying, shrinkage and heat generation of intra-particle for a spherical biomass. The influence of various parameters such as size, initial moisture content, heat transfer coefficient, kinetic model and temperature, was investigated. The devolatilization time linearly increased with increasing initial moisture content and size of a wood particle, whereas decreases with reaction temperature. There is no significant change of results when the external heat transfer coefficient is over 300 $W/m^2K$, and smaller particles are more sensitive to the outer heat transfer coefficient. Predicted results from the model show a similar tendency with the experimental data from literatures within a deviation of 10%.

Characteristics of Flame Retardent and Mothproof Conservation of Microwave Heated wood (마이크로파 가열 목재의 방염·방충 복합 보존처리 특성)

  • Kim, Chong-Gun;Park, Cheul-Woo;Yoon, Tae-Ho;Lim, Nam-Gi
    • Journal of the Korean Wood Science and Technology
    • /
    • v.41 no.3
    • /
    • pp.234-246
    • /
    • 2013
  • It was found that test piece heated rapidly by 3 kW microwave for 5 minutes satisfies the targeted temperature and the percentage of moisture content, and the highest rate of weight increase is obtained in case of 120 minute immersion in the mixture of phosphates and heterocyclic compounds, from the result of such analysis as: kiln drying schedule, flame retardent by flammability test, insect resistance by termites, and permeability of combined penetrant for the wood after assigning multifunctional finish by immersing conifer structural frame, which is used for the frame work of wooden house and indoor/outdoor finishing in flame retardant and insect repellent materials mixture with the remaining heat of microwave. In addition, after a test of flame retardent treated item, it was identified that every mixture of phosphates corresponds with the standards of flame retardent, and upon investigation of moritality of 7 days after putting termites, it was showed that test piece immersed in the mixture of phosphates and heterocyclic compounds has the best characteristics, showing over 96% of high moritality. From the analysis of inward permeability of combined penetrant for the wood, it was decided that excellent performance in the flame retardent and insect resistance of the wood revealed due to full penetration of combined penetrant as it was found that combined penetrant penetrated through the whole inner cells of the wood.

Effects of Adhesion Conditions on Bonding Strength of Pitch Pine Woods for Glued-Laminated Wood (리기다소나무 판재(板材)의 접착조건(接着條件)이 집성재(集成材)의 접착성능(接着性能)에 미치는 영향(影響))

  • Park, Sang-Bum;Kong, Young-To;Jo, Jae-Myeong
    • Journal of the Korean Wood Science and Technology
    • /
    • v.16 no.4
    • /
    • pp.48-53
    • /
    • 1988
  • This study was carried out to investigate the effects of pressing time and spreading amount, moisture content, gap-distance with butt to butt joint and adhesives on bonding strength in manufacturing the laminated wood with Pitch pine (Pinus rigida). The results obtained were as follows: 1) The pressing time of 12 hours, 10 kilogram per square centimeter of pressure and 200 gram per square meter of spreading amount were required to reach over 50 kilogram per square centimeter (block shear strength) in manufacturing the laminated wood by aqueous vinyl urethane adhesive. 2) The bonding strength decreased with the increase of moisture content of wood. The block shear strength, however, showed over 100 kilogram per square centimeter when the strength test was carried out after air-drying the laminated wood in high moisture content (30-70%). 3) Regardless of direction of load, every flexural property decreased with the increase of gap-distance with butt to butt joint. However, little of every flexural property was changed at 0.5 millimeter of joint-gap distance. The flexural property of vertically laminated wood (perpendicular to glue line to load direction: 1) showed more than that of horizontally laminated wood (parallel to glue line to load direction: //). 4) Among five adhesives used at this experiment, the bonding strength of aqueous vinyl urethane adhesive was the highest in dry bond and wet tests.

  • PDF

A Study on the RDF making Process of Heat-dried Sludge from Cheonan by using Oil-drying Method (유중건조를 이용한 천안시 열건조물의 고형연료화 공정 연구)

  • Park, So-yeon;Kim, Sang-bin;Ha, Jin-wook
    • Journal of the Korea Academia-Industrial cooperation Society
    • /
    • v.19 no.2
    • /
    • pp.660-667
    • /
    • 2018
  • This study examined the optimal manufacturing conditions of RDF using heat-dried sludge from sewage treatment plant in Cheonan with the oil-drying method. The amounts of oil evaporation and oil drying of the heat-dried sludge were measured at different temperatures to evaluate the value of the product. The performance of the product was then measured using a calorimeter and TGA. In addition, the concentration of odor, NH3, H2S, and TVOC during drying was determined using a portable odor-meter. Ingredient analysis was performed by EDS. Considering mass-production, the oil to heat-dried sludge weight ratio was fixed to 4:1. At $130^{\circ}C$, only physical mixing occurred after the instantaneous drying of internal water. Considering the eco-friendly aspects, there was no significant difference in the drying efficiency between $160^{\circ}C$ and $190^{\circ}C$. Therefore, the optimal conditions were a drying temperature of $160^{\circ}C$ within 5 minutes. Finally, the RDF manufactured in this study and fuel used in the thermal power plants were compared. The calorific value was 4,449kcal/kg, the water content was 2% and the ash content was 34%, which is higher than the fuel of thermal power plants. Therefore, it is believed that coal energy as well as wood pellets can be replaced.

Development of New Powdered Additive and Its Application for Improving the Paperboard Bulk and Reducing Drying Energy (II) - Surface Modification of Brewers Grain(BG) and Oil Palm Frond(OPF) Powders with Cationic and Oxidized Starches - (산업용지의 벌크 향상 및 건조에너지 절감을 위한 분말상 첨가제 제조기술 개발(II) - 맥주박과 팜잎 분말상 첨가제의 표면개질에 대한 연구 -)

  • Lee, Ji-Young;Kim, Chul-Hwan;Kim, Sun-Young;Kim, Byeong-Ho;Lim, Gi-Baek;Kim, Jun-Sik
    • Journal of Korea Technical Association of The Pulp and Paper Industry
    • /
    • v.45 no.2
    • /
    • pp.33-40
    • /
    • 2013
  • Powdered additive or organic filler is used to improve paperboard thickness and to reduce drying energy consumption in the Korean paperboard industry. In a previous study, we identified alternative non-lignocellulosic resources to wood powder, specifically brewers grain and oil palm frond powders, and verified that these materials had the same functionality as wood powder. The main drawback of the use of such additives, including both lignocellulosic and non-lignocellulosic resources, is the deterioration in paperboard strengths. Therefore, we carried out a basic study on the surface modification of brewers grain and oil palm frond powders to improve the strengths of paperboard. Surface modification was performed using various types of cationic and oxidized starches. The streaming current and zeta-potential of the two non-lignocellulosic powders were measured and CLSM images were taken to assess the surface modification.

Fire Retardant Treatment to the Plywood with Di-ammonium Phosphate [(NH4)2HPO4] (II) - Effect of Platen Temperature on Bending Strength of Treated Plywoods - (제2인산(第二燐酸) 암모늄에 의(依)한 합판(合板)의 내화처리(耐火處理)(II) - 열판온도(熱板溫度)가 처리합판(處理合板)의 곡강도(曲强度)에 미치는 영향(影響) -)

  • Chung, Woo-Yang;Lee, Phil-Woo
    • Journal of the Korean Wood Science and Technology
    • /
    • v.12 no.2
    • /
    • pp.3-9
    • /
    • 1984
  • This study was carried out to examine the practicality of DAP[$(NH_4)_2HPO_4$] as fire retardant for plywood by static bending test the redried plywoods which had been soaked in 20% $(NH_4)_2HPO_4$ solution. Being hot/cold soaked in the solution for 3/3, 6/3, 9/3 and 12/3 hours and redried by cyclic press-drying method at the platen temp. of 130, 145, 100 and $175^{\circ}C$, the treated plywoods were tested to offer the mechanical data, that is, $S_{pl}$(stress at proportional limit), MOE(modulus of elasticity), MOR(modulus of rupture) and $W_{pl}$(work per unit volume to proportional limit ) in flexure. The results obtained were summarized as follows. 1. $S_{pl}$ of fire retardant treated plywoods ("FRP" would be used hereinafter) decreased as the platen temperature increased, but it was superior to that of non-treated plywoods(Control) at $160^{\circ}C$ or higher. 2. MOE of FRP decreased roughly with the increase of temperature, hut this tendency was not constant. And the value of FRP was higher than that of Control even at $175^{\circ}C$. 3. MOR of FRP showed same temperature-dependent tendency as MOE, but it was influenced more sensitively at the higher temperature. 4. $W_{pl}$ of FRP also decreased gradually with the increase of platen temperature and the value in DAP 9/3 treatment was Jess than 70% of control plywoods. 5. In view of redrying time and mechanical properties, the most reasonable platen temperature for DAP treated FRP was $160^{\circ}C$ in this study.

  • PDF

Studies on the Technical Development of the Traditional Korean Golden Varnish(Hwangchil) (III) - Main Component Analysis of Korea Golden Varnishes Traditonally Refined from the Exudates of Dendropanax morbifera Lev. - (전통 황칠 도료 개발에 관한 연구(III) - 전통 황칠 도료의 주성분 분석 -)

  • Lim, Kie-Pye;Jung, Woo-Yang;Hong, Dong-Hwa
    • Journal of the Korean Wood Science and Technology
    • /
    • v.26 no.3
    • /
    • pp.73-80
    • /
    • 1998
  • In order to reconstruct the traditional technology of Korean golden varnish coatings, this study was carried out to separate and determine some main coloring components of the exudates of D. morbifera and its traditionally refined golden varnishes using a process of solvent extractions, chromatographies and spectrometries. The results obtained are as follows: 1. The exudate and its traditional-refined golden varnishes appear to have a kind of natural polyacetylenes because it has some triple bond peaks in FT-IR spectrometry. 2. Some yellowing spots of the polar-solvent extrats from the exudates and refined varnishes separated on TLC appeared under natural drying condition, but those of non-polar solvent extract such as hexane did not. 3. A traditional refining method for reconstructing a Korea golden varnishes was thought to be better than solvent separation because the former had higher triple-bond peaks than the latter in FT-IR spectrometry. 4. One of main conponents in the hexane-extracts of the traditional-refined varnishes and the exudates had the same molcular weighr of 204, but the fragmentation patterns was a little different between the exudate and the refined. in LC-MS soectrometry.

  • PDF

Warpinging and Budding Prediction Model of Wooden Hollow Core Flush Door due to Moisture Content Change (II) : Simple Method of LMC and MOE, and Monte Carlo Simulation for Calculating Reject (목제(木製) 프러쉬 문의 함수율 변동에 따른 틀어짐과 좌굴 예측모델 (II) : 치수변동과 탄성계수의 간이측정법과 불량율 예측 Monte Carlo 시뮬레이션)

  • Kang, Wook;Jung, Hee-Suk
    • Journal of the Korean Wood Science and Technology
    • /
    • v.28 no.1
    • /
    • pp.18-27
    • /
    • 2000
  • Even the same materials are assembled in flush door skin panel, warping is not simply prevented under the changes of environmental conditions since wood and wood-based material have large variations in their physical and mechanical properties. The parameters such as linear movement coefficient(LMC), modulus of elasticity (MOE), required to predict warping could be estimated by oven drying method and dynamic method instead of American Society for Testing Materials(ASTM) procedure. The relationship between warping and LMC was curvilinear, while it between warping and MOE was linear. LMC had a larger effect on warping than MOE. Material propensity of skin panel such as hardboard and plywood showed normal distributions. The variation of material properties, however, was much larger in plywood than in hardboard. Monte Carlo simulation also indicated that rejection ratio of flush door due to the occurrence of warping could be predicted with consideration of the relationship of warping and parameters of probability distribution of MOE, LMC, and moisture content.

  • PDF

Extractives of the Wood of Black Locust and the Bark of Poplar as Decay-Resistant Hardwood Tree Species (내후성 활엽수종인 아까시나무 목질부와 현사시나무 수피의 추출성분)

  • Bae, Young-Soo;Ham, Yeon-Ho
    • Journal of the Korean Wood Science and Technology
    • /
    • v.28 no.3
    • /
    • pp.52-61
    • /
    • 2000
  • Black locust(Robinia pseudoacacia) and poplar(Populus alba ${\times}$ glandulosa) trees were collected, extracted with acetone-$H_2O$(7:3, v/v) after drying, fractionated with hexane, chloroform and ethylacetate, and freeze dried to get some brown powder. Each fraction of the powder was chromatographed on a Sephadex LH-20 column using a series of aqueous methanol and ethanol-hexane mixture as eluting solvents. The wood extractives of black locust contained (+)-leucorobinetinidin as flavan, robtin as flavanone and dihydrorobinetin as flavanonol, and robinetin as flavonol. The poplar bark extractives contained various kinds of phenolic compounds : (+)-catechin as flavan, naringeoin, eriodictyol, sakuranetin, aromadendrin and taxifolin as flavanonol, salireposide as salicin derivative, and minor compounds such as aesculin and p-coumaric acid. However, aesculin has not been reported as a constituent of the poplar bark in Korea yet. NMR and FAB-MS analyses were done to elucidate the structures of isolated phenolic constituents.

  • PDF

Evaluation of Pretreatment Moisture Content and Fixation Characteristics of Treated Wood for Pressure Treatment of Japanese Red Pine and Japanese Larch Skin Timber with ACQ, CUAZ and CuHDO (소나무와 낙엽송 스킨팀버의 ACQ, CUAZ, CuHDO 가압처리를 위한 처리용 목재의 적정 함수율 및 처리목재의 정착 특성 평가)

  • Choi, Yong-Seok;Oh, Se-Min;Kim, Gyu-Hyeok
    • Journal of the Korean Wood Science and Technology
    • /
    • v.39 no.6
    • /
    • pp.481-489
    • /
    • 2011
  • This study was conducted to evaluate the pressure treatment characteristics of Japanese red pine and Japanese larch skin timber with ACQ-2, CUAZ-2 and CuHDO-1. The effect of moisture content (MC) on preservative treatability was investigated for Japanese red pine sapwood and Japanese larch heartwood, and fixation characteristics of CCA alternatives was also evaluated. Japanese red pine sapwood, which was dried below 30 percent MC, was fully penetrated with preservatives, and minimum requirement of preservative retention for the hazard class H3 was achieved. Through measuring preservative retention gradient in Japanese red pine sapwood, it was confirmed that the retention gradient of CuHDO-1 was steeper than that of both ACQ-2 and CUAZ-2. In particular, it was intensified at a higher MCs of wood samples (25∼30%). Japanese larch heartwood did not meet the minimum requirement of penetration and retention for the hazard class H3 over the range of pretreatment MCs tested. With presteaming under $121^{\circ}C$ for 12 hours, the treatability of Japanese larch heartwood was enhanced to meet the minimum requirement for the hazard class H3. The fixation rate of copper was much more faster under drying condition compared with nondrying condition; more than 95% of copper were fixed in 3~6 days and 1 day under drying conditions in Japanese red pine sapwood and Japanese larch heartwood, respectively. After 3-week fixation period at ambient temperature, the amount of mobile copper in treated wood sample that remains available for leaching from treated wood was the highest in the wood samples treated with ACQ-2, followed by CuHDO-1 and CUAZ-2. It was proportional to the amount of copper in treating solution.