Review on Flux Cored Wire Development for Welding Fume Reduction (용접 Fume 저감을 위한 용접재료의 개발 동향)

  • 한종만
    • Journal of Welding and Joining
    • /
    • v.16 no.1
    • /
    • pp.49-51
    • /
    • 1998
  • 최근 포항공단 내 철 구조물 용접작업자가 Mn에 의한 뇌병변이 국내 최초로 발견되어 CO$_{2}$ 용접시 발생하는 Mn Fume에 기인한 것으로 의심을 하고 있으며, 이 문제가 언론을 비롯한 관련기관에서 쟁점화 된 바가 있지만 확실한 결론이 도출된 것으로는 보이지 않는다. 본 고에서는 CO$_{2}$ 용접 시 Fume의 발생 기구 및 이의 영향에 대한 검토와 용접 Fume을 줄일 수 있는 용접재료 측면에서의 대책과 현황에 대해 검토하고자 한다.

  • PDF

Solidification Cracking Susceptibility of Al-Mg-Si Alloy Laser Welds

  • Yoon, J.W.
    • International Journal of Korean Welding Society
    • /
    • v.2 no.2
    • /
    • pp.42-46
    • /
    • 2002
  • The solidification cracking susceptibilities of Al-Mg-Si alloy laser welds were assessed using the self-restraint tapered specimen crack test. The cracking susceptibility of 6061 and 6082 Al-Mg-Si alloy laser welds was substantially reduced when the filler wire containing high Si such as Al-12 wt.% Si (4047A) was used. The amount of eutectic was observed to affect the solidification cracking of Al-Mg-Si alloy laser welds. Abundant eutectic seems to heal the cracking and reduces the cracking susceptibility, while an initial increase in eutectic liquid leads to the increased cracking tendency.

  • PDF

Development of Intelligent Filler Wire Feeding Device for Improvement of Weld quality (용접부 품질향상을 위한 지능형 용접 와이어 공급 장치 개발)

  • Lee J.S.;Sohn Y.I.;Park K.Y.;Lee K.D.
    • Proceedings of the Korean Society of Precision Engineering Conference
    • /
    • 2005.06a
    • /
    • pp.950-955
    • /
    • 2005
  • This paper describes an intelligent filler wire feeding device which can control 3- dimensional seam tracking and the filler wire speed by measuring the gap position and the joint gap width in laser welding. By means of visual sensor controlled filling the missing material into the joint gap and 3 dimensional seam tracking, lineup errors from manufacturing tolerances and the repeatability of lineup jigs and weld robot can be balanced and at an even seam quality which avoids weld defects. In this paper, we assessed weld quality in 2mm sheets of A16061 which had various gap width by using the intelligent filler wire feeding device.

  • PDF

Characteristics of copper wire wedge bonding

  • Tian, Y.;Zhou, Y.;Mayer, M.;Won, S.J.;Lee, S.M.;Cho, S.Y.;Jung, J.P.
    • Proceedings of the KWS Conference
    • /
    • 2005.06a
    • /
    • pp.34-36
    • /
    • 2005
  • Copper wire bonding is an alternative interconnection technology that serves as a viable and cost saving alternative to gold wire bonding. In this paper, ultrasonic wedge bonding with $25{\mu}m$ copper wire on Au/Ni/Cu metallization of a PCB substrate was performed at ambient temperature. The central composite design of experiment (DOE) approach was applied to optimize the copper wire wedge bonding process parameters. After that, pull test of the wedge bond was performed to study the bond strength and to find the optimum bonding parameters. SEM was used to observe the cross section of the wedge bond. The pull test results show good performance of the wedge bond. Additionally, DOE results gave the optimized parameter for both the first bond and the second bond. Cross section analysis shows a continuous interconnection between the copper wire and Au/Ni/Cu metallization. The diffusion of Cu into the Au layer was also observed.

  • PDF

Fatigue Damage Behavior in TIG Welded Joint of F82H Steel under Low Cycle Fatigue Loading (저주기 피로부하에서 F82H 강 TIG 용접 접합부의 피로손상거동)

  • Kim, Dong-Hyun;Park, Ki-Won
    • Journal of Welding and Joining
    • /
    • v.33 no.6
    • /
    • pp.42-48
    • /
    • 2015
  • Reduced activation ferritic/martensitic steels are recognized as the primary candidate structural materials for fusion blanket systems. Welding is an inevitable for breeding blanket for pressure tightness and radioisotope confinement. Especially, TIG welding was chosen for sealing because it has the largest gap allowance compared to the other welding methods, and its properties are controllable by feed wire and welding conditions. In this study, the low cycle fatigue test using two-type gage such as extensometer and strain gage was applied to the TIG welded joint of F82H steel, for evaluating fatigue damage accumulation behavior of the HAZs. As the result, the over-tempered HAZ have shown a higher fatigue damage accumulation compared with other materials at all the testing conditions.

Characteristics of Spatter Generation in the Short Circuit Transfer Region of $CO_2$ Arc Welding ($CO_2$ 용접의 단락이행영역에 있어서 스패터 발생특성)

  • 안영호;이종봉;최원규
    • Journal of Welding and Joining
    • /
    • v.19 no.6
    • /
    • pp.630-635
    • /
    • 2001
  • The characteristics of spatter generation in the short circuit transfer region of $CO_2$ welding was investigated. Spatteriing phenomena could be classified into three types : Type I generated due to the abrupt increase of arc voltage in arcing duration. Type II by the gas ejection from molten metal and Type III generated by the arc instability at the moment of arc re-ignition just after short circuiting. Main observed types were dependent on the chemical composition of welding wires. The case of YCW12 wires was mainly composed of spatters generated by Type l and Type II, while most, spatters in YCW11 wires were generated by Type II and Type III.

  • PDF

The Waveform Control and Blowhole Generation in the Wave Pulse MIG Welding for Galvanized Steel Sheets (아연도금강판에 대한 중첩펄스 MIG 용접에서의 파형제어와 기공 발생 특성)

  • Cho Sang-Myung;Kim Ki-Jung;Lee Byung-Woo
    • Journal of Welding and Joining
    • /
    • v.23 no.1
    • /
    • pp.69-76
    • /
    • 2005
  • Recently, application of arc welding to galvanized carbon steel sheet is on the increasing Ould in the fields of automobile and construction industries. In arc welding process, zinc is evaporated in weld pool, even under the appropriate welding condition and produce blowhole and/or pit. Zinc gas cause instability of arc and increase spatter and fume. This research is purposed to minimize the heat-input and the formation of porosities in the welded joint of the galvanized carbon steel sheet using variable polarity AC wave pulse MIG welding system. An appropriate welding condition which showed low spatter and good bead appearance was acquired by applying the AC pulse MIG welding machine to DC duplicated MIG welding with the solid wire. When oxygen gas was added to shield gas of MIG welding for galvanized steel sheet, arc length was increased and arc stability was improved. In the AC duplicated welding, the loss of galvanized layer was decreased as the amount of heat-input was decreased when the EN ratio was increased under the condition that average welding current was evenly set.

A Study on Adaptive Control to Fill Weld Groove by Using Multi-Torches in SAW (SAW 용접시 다중 토치를 이용한 용접부 적응제어에 관한 연구)

  • 문형순;정문영;배강열
    • Journal of Welding and Joining
    • /
    • v.17 no.6
    • /
    • pp.90-99
    • /
    • 1999
  • Significant portion of the total manufacturing time for a pipe fabrication process is spent on the welding following primary machining and fit-up processes. To achieve a reliable weld bead appearance, automatic seam tracking and adaptive control to fill the groove are urgently needed. For the seam tracking in welding processes, the vision sensors have been successfully applied. However, the adaptive filling control of the multi-torches system for the appropriate welded area has not been implemented in the area of SAW(submerged arc welding) by now. The term adaptive control is often used to describe recent advances in welding process control by strictly this only applies to a system which is able to cope with dynamic changes in system performance. In welding applications, the term adaptive control may not imply the conventional control theory definition but may be used in the more descriptive sense to explain the need for the process to adapt to the changing welding conditions. This paper proposed various types of methodologies for obtaining a good bead appearance based on multi-torches welding system with the vision system in SAW. The methodologies for adaptive filling control used welding current/voltage, arc voltage/welding current/wire feed speed combination and welding speed by using vision sensor. It was shown that the algorithm for welding current/voltage combination and welding speed revealed sound weld bead appearance compared with that of voltage/current combination.

  • PDF

Development of Low Frequency Pulse MIG Welding Process for AL and its alloy (AL 및 AL합금의 저주파 PULSE MIG 용접법의 개발)

  • 최병길;이사영;이승학;천성진
    • Proceedings of the KIPE Conference
    • /
    • 1997.07a
    • /
    • pp.45-48
    • /
    • 1997
  • The low frequency pulsed MIG welding process of new current waveform control to switch over unit pulse conditions (pulse current, pulse duration) in the fixed cycle was developed and its effect were investigated for aluminium and its alloy. By using this new welding process, the bead appearance having clear ripple pattern, such as TIG welding bead can be obtained and the gap tolerance of lap and butt welding joint can be expanded.

  • PDF

Finite Element Analysis of an Ultrasonic Horn for Wire Bonding (Wire Bonding Head Horn 설계 및 유한요소해석)

  • Kim, Won-Jong;Hwang, Eun-Ha
    • Journal of the Korean Society of Industry Convergence
    • /
    • v.15 no.4
    • /
    • pp.111-115
    • /
    • 2012
  • Ultrasonic meching technoloy has been developed over recent years for wire bonding.In this study, ultrasonic welding horn is analysed and designed with FEM, then manufactured based on it. The wire bonding mechine has been designed by conical horn model with very easy to come by and is readily accessible. The analysis is carried out by SoldEdge & Ansys software.