Thermal Degradation Kinetics of Antimicrobial Agent, Poly(hexamethylene guanidine) Phosphate

  • Lee, Sang-Mook;Jin, Byung-Suk;Lee, Jae-Wook
    • Macromolecular Research
    • /
    • v.14 no.5
    • /
    • pp.491-498
    • /
    • 2006
  • The thermal degradation of poly(hexamethylene guanidine) phosphate (PHMG) was studied by dynamic thermogravimetric analysis (TGA) and pyrolysis-GC/MS (p-GC). Thermal degradation of PHMG occurs in three different processes, such as dephosphorylation, sublimation/vaporization of amine compounds and decomposition/ recombination of hydrocarbon residues. The kinetic parameters of each stage were calculated from the Kissinger, Friedman and Flynn-Wall-Ozawa methods. The Chang method was also used for comparison study. To investigate the degradation mechanisms of the three different stages, the Coats-Redfern and the Phadnis-Deshpande methods were employed. The probable degradation mechanism for the first stage was a nucleation and growth mechanism, $A_n$ type. However, a power law and a diffusion mechanism, $D_n$ type, were operated for the second degradation stage, whereas a nucleation and growth mechanism, $A_n$ type, were operated again for the third degradation stage of PHMG. The theoretical weight loss against temperature curves, calculated by the estimated kinetic parameters, well fit the experimental data, thereby confirming the validity of the analysis method used in this work. The life-time predicted from the kinetic equation is a valuable guide for the thermal processing of PHMG.

Synthesis and Swelling Kinetics of a Cross-Linked pH-Sensitive Ternary Copolymer Gel System (pH-민감성 삼성분계 공중합체 젤의 합성 및 팽윤 속도론)

  • Zafar, Zafar Iqbal;Malana, M.A.;Pervez, H.;Shad, M.A.;Momma, K.
    • Polymer(Korea)
    • /
    • v.32 no.3
    • /
    • pp.219-229
    • /
    • 2008
  • A pH sensitive ternary copolymer gel was synthesized in the presence of ethylene glycol dimethacrylate (EGDMA) as a crosslinking agent through radical polymerization of vinyl acetate (VA), acrylic acid (AA) and methyl acrylate(MA) with a weight ratio of 1 : 1.3 : 1. A number of experiments were carried out to determine the swelling behavior of the gel under a variety of pH conditions of the swelling medium. As the pH of the swelling medium was changed from 1.0 to 8.0 at $37^{\circ}C$, the gel showed a shift in the pH-dependent swelling behavior from Fickian (n=0.3447) to non-Fickian (n=0.9125). The resulting swelling parameters were analyzed using graphical and statistical methods. The results showed that the swelling of the gel was controlled by the pH of the medium, i.e. $n=n_o{\exp}(S_{C}pH)$, where n is the diffusion exponent, $n_o(=28.9645{\times}10^{-2})$ is the pre-exponential factor and $S_C$(=0.1417) is pH sensitivity coefficient. The swelling behavior of the gel was also examined in aliphatic alcohols. The results showed that the rate of swelling increased with increasing number of carbon atoms in the alcoholic molecular chain.

Development of Reduced Normal Dodecane Chemical Kinetics (축소 노멀 도데케인 화학반응 메커니즘 개발)

  • Lee, Sangyul;Kim, Gyujin;Min, Kyoungdoug
    • Transactions of the Korean Society of Automotive Engineers
    • /
    • v.21 no.2
    • /
    • pp.37-44
    • /
    • 2013
  • Generally, a reduced chemical mechanism of n-heptane is used as chemical fuel of a 3-D diesel engine simulation because diesel fuel consists of hundreds of chemical components and various chemical classes so that it is very complex and large to use for the calculation. However, the importance of fuel in a 3-D simulation increases because detailed fuel characteristics are the key factor in the recent engine research such as homogeneous charged compression ignition engine. In this study, normal paraffin, iso paraffin and aromatics were selected to represent diesel characteristics and n-dodecane was used as a representative normal paraffin to describe the heavy molecular weight of diesel oil (C10~C20). Reduced kinetics of iso-octane and toluene which are representative species of iso paraffin and aromatics respectively were developed in the previous study. Some species were selected based on the sensitivity analysis and a mechanism was developed based on the general oxidation scheme. The ignition delay times, maximum pressure and temperature of the new reduced n-dodecane chemical mechanisms were well matched to the detailed mechanism data.

Ordering Kinetics of Triblock Copolymer/Low Molecular Weight Homopolymer Mixtures (삼중블록공중합체와 저분자량 단일중합체 혼합물의 미세상분리 동력학)

  • 차국헌
    • The Korean Journal of Rheology
    • /
    • v.10 no.2
    • /
    • pp.65-73
    • /
    • 1998
  • 본연구에서는poystyrene-block-poly (ethlene-co-butylene)-block-polystyrene(SEBS) 삼중블록 공중합체와 저분자량 단일중합체인 Hercotac 1149 (H1149)의 70/30 (w/w) 혼합물 의 미세상분리와 그동력학을 유변물성 측정법과 SAXS 실험을 통하여 연구해 보았다. 먼저 혼합물의 미세상분리 온도를 유변물성 측정법과 SAXS 실험을 통해 각각구한 다음 샘플을 미세상분리 온도보다 높은 온도에서 그이하의 온도로 급냉시킨 후 유변물성과 산란강도의 사간에 따른 변화로부터 미세상분리 동력학에 대한 정보를 구하였다. 이렇게 얻어진 데이터 를 Avrami 형태의 핵생성 성장(NG) 메커니즘으로 해석해 보았는데 최대산란강도 Imax 뿐만 아니라 저장 점탄성계수 G'과 손실 점탄성계수 G"의 시간에 따른 변화를 잘 예측할수 있 었다. 한편 서로다른 두 time-resolved 실험으로부터 Avrami 플롯을 그려서 구해진 Avrami 변수들은 같은 급냉 깊이에서는 서로 잘 일치함을 확인하였다. 반감기는 급냉 깊이가 증가 함에 따라 점차 감소하는 경향을 보였는데 이는 급냉 깊이가 클수록 미세상분리가 더 빨리 진행되고 있음을 보여주는 것이다. 또한 Avrami 지수는 급냉 깊이가 증가함에 따라 3에서 4로 급격히 변했는데 이로부터 급냉 깊이가 작을 때에는 70/30 (w/w) SEBS/H1149 혼합물 의 미세상분리가 불균일 핵생성 성장 메커니즘에 따라 진행되고 급냉 깊이가 더 커지면 미 세상분리가 스피노달 상분리 메커니즘으로 변하고 있음을 예측할수 있었다.

  • PDF

A Study on Nitridation and Oxidation Reaction of Titanium Powder (금속티타늄분말의 질화반응과 산화반응에 관한 연구)

  • Lee, Young-Ki;Sohn, Yong-Un;Cho, Young-Soo;Kim, Yong Seog;Kim, Suk-Yoon
    • Journal of the Korean Society for Heat Treatment
    • /
    • v.8 no.2
    • /
    • pp.137-148
    • /
    • 1995
  • The nitridation kinetics of titanium powder were studied by isothermal and non-isothermal (dynamic) methods in high purity nitrogen under I atm pressure. For the comparison with nitridation, the oxidation kinetics of titanium powder were also studied in dry oxygen at I atm pressure. An automatic recording electrobalance was used to measure the weight gain as a function of time and temperature. For the reaction with nitrogen, the nitride was formed at over $700^{\circ}C$. The reaction with nitrogen followed the parabolic rate law, and the activation energy was calculated to be 31 kcal/mol in the isothermal method (above $900^{\circ}C$). The non-stoichiometric TiNx has been synthesized by the nitridation at a proper temperature and time, followed by the homogenizing treatment above $1100^{\circ}C$. In comparison with the stoichiometric $TiN_{1.0}$ and the non-stoichiometric TiNx ($TiN_{0.5}$ and $TiN_{0.65}$), the hot oxidation characteristics of the former is superior to that of the latter. However, both non-stoichiometric nitrides make little difference in the hot oxidation characteristics.

  • PDF

Effect of Methanethiol Administration on the Erythrocyte Damage in Rats (흰쥐에 Methanethiol 투여가 적혈구막 손상에 미치는 영향)

  • 정소웅;윤종국
    • Journal of Environmental Health Sciences
    • /
    • v.19 no.4
    • /
    • pp.83-89
    • /
    • 1993
  • To evaluate an effect of methanethiol on a cause of erythrocyte membrane damage in rats, methanethiol was given at 11.25 rag/100 g body weight, and after 4 hr, the animals were sacrifled, the activities of Na$^+$/K$^+$ ATPase, protein contents in partial purified erythrocyte membrane and erythrocyte indices were determined Concomitantly, in vitro, effect of methanethiol on the erythrocyte fragility, Na$^+$/K$^+$ ATPase activity and its kinetics in various concentration of substrate from the preincubated erythrocyte membrane with methanethiol were demonstrated. The spleen weight per body weight (%) and MCV of erythrocyte in methanethiol-treated rats were more increased than those in the control group. The Na$^+$/K$^+$ ATPase activities in erythrocyte membrane were more decreased in methanethiol-treated rats than those in the control group. The apply of 0.05 ng rat whole blood to the 0.24 mg/ng of methanethiol solution in isotonic condition showed the complete hemolysis. The Na$^+$/K$^+$ ATPase activity in preincubated erythrocyte membrane with methanethiol at 37$\circ$C showed the dual effect and the K$_m$ value of Na$^+$/K$^+$ ATPase was higher in the preincubated erythrocyte membrane with methanethiol than that in the preincubated erythrocyte membrane omitted the methanethiol. These results suggest that the methanethiol may induce the damage of rat's erythrocyte membrane due to a change in substrate binding affinity of Na$^+$/K$^+$ ATPase.

  • PDF

The Interlimb Coordination During Movement Initiation From a Quiet Stance: Manipulation of Swing Limb Kinetics and Kinematics -A Preliminary Study

  • Kim, Hyeong-Dong;Yoon, Bum-Chull
    • Physical Therapy Korea
    • /
    • v.13 no.4
    • /
    • pp.79-86
    • /
    • 2006
  • The purpose of the current experiment was to describe interlimb coordination when swing limb conditions are being manipulated by constraining step length or by adding a 5 or 10 pound weight to the swing limb distally. Subjects were asked to begin walking with the right limb to land on the primary target (normal step length) that is 10 cm in diameter. However, if, during movement, the light was illuminated, then the subject had to step on one of the secondary targets (long and short step length). These three step length conditions were repeated while wearing a 5 pound ankle weight and then when wearing a 10 pound ankle weight. Ground reaction force (GRF) data indicated that there were changes in the forces and slopes of the swing and stance Fx GRFs. Long stepping subjects had to increase the propulsive force required to increase step length. Consequently, swing and stance toe-off greatly increased in the long step length condition. Short step length subjects had to adequately adjust step length, which decreased the speed of gait initiation. Loading the swing limb decreased the force and slope of the swing limb. Swing and stance toe-off was longest for the long step length condition, but there was a small difference of temporal events between no weight and weight condition. It appears that subjects modulated GRFs and temporal events differently to achieve the peak acceleration force of the swing and stance limb in response to different tasks. The findings from the current study provide preliminary data, which can be used to further investigate how we modulate forces during voluntary movement from a quiet stance. This information may be important if we are to use this or a similar task to evaluate gait patterns of the elderly and patient populations.

  • PDF

Synthesis and Curing Behaviors of Polyisoimide Oligomers with Ethynyl End Groups (Ethynyl 말단기를 갖는 Polyisoimide 올리고머의 합성 및 이들의 경화거동에 관한 연구)

  • Choi, Seok Woo;Kim, Bo Ock;Kim, Ji-Heung;Nam, Sung Woo;Jeon, Boong Soo;Kim, Young Jun
    • Polymer(Korea)
    • /
    • v.38 no.6
    • /
    • pp.774-781
    • /
    • 2014
  • Acetylenic or phenylethynyl end-capped polyisoimide oligomers ($M_w$ 2500 g/mol, 5000 g/mol) based upon 4,4'-diamino diphenyl ether (4,4'-ODA)/4,4'-oxydiphthalic anhydride (ODPA) and 4,4'-ODA/3,3',4,4'-benzophenone tetracarboxylic acid dianhydride (BTDA) were synthesized by using 4-ethynylaniline (4-EA) or 4-phenylethynyl phthalic anhydride (4-PEPA) as an end capper. The incorporation of ethynyl groups were confirmed by FTIR spectroscopy. The isomerization temperature was influenced by molecular weight as well as the backbone structure of polyisoimides oligomers. Thus, polyisoimide oligomers with molecular weight of 2500 g/mol was found to be imidized at temperature $10^{\circ}C$ lower than that for the oligomers with molecular weight of 5000 g/mol. The crosslinking reaction of ethynyl groups occurred at a higher temperature than that for the isoimide/imide isomerization reaction. These two reactions were totally or partially overlapped on the DSC thermograms for the polyisoimide oligomer end-capped with 4-EA. Kinetics of thermal imidization and crosslinking reactions for the 4,4'-ODA/ODPA polyisoimide oligomers end-capped with 4-PEPA were investigated by performing dynamic DSC experiments at heating rate of $10^{\circ}C/min$. The activation energy and pre-exponential factors were 141 kJ/mol and $1.45{\times}10^{13}min^{-1}$ for the imidization reaction and 177 kJ/mol and $2.90{\times}10^{13}min^{-1}$ for the crosslinking reaction, respectively.

Degradation Behaviors of Poly(l-lactide) using Model Systems (모델 시스템을 이용한 Poly(l-lactide)의 분해거동)

  • Min Seong-Kee;Moon Myong-Jun;Lee Won-Ki
    • Journal of Environmental Science International
    • /
    • v.15 no.2
    • /
    • pp.177-183
    • /
    • 2006
  • The hydrolytic kinetics of biodegradable poly(l-lactide) (PLLA) have been studied by using two model systems, solution-grown single crystal (SC) and Langmuir monolayer techniques, for elucidating the mechanism for both alkaline and enzymatic degradations. The present study investigated the parameters such as degradation medium and time. The Langmuir mono layers of PLLA showed faster rates of hydrolysis when they were exposed to a basic subphase rather than they did when exposed to neutral subphase. Both degradation mediums had moderate concentrations to show a maximized activity, depending on their sizes. An alkaline degradation of SCs of PLLA showed the decrease of molecular weight of the remained crystals due to the erosion of chain-folding surface. However, the enzymatic degradation of SCs of PLLA occurred in the crystal edges thus the molecular weight of remained crystals was not changed. This behavior might be attributed to the size of enzymes which is much larger than that of alkaline ions; that is, the enzymes need larger contact area with monolayers to be activated.

A New Method to Measure the Conversion of Radiation Polymerization of Electrolyte Monomer Diallyldimethylammonium Chloride in Dilute Aqueous Solution

  • Zhang, Yalong;Yi, Min;Ren, Jing;Zhai, Maolin;Ha, Hongfei
    • Macromolecular Research
    • /
    • v.11 no.3
    • /
    • pp.146-151
    • /
    • 2003
  • The dependence of electrical conductivity on concentrations of diallyldimethylammonium chloride (DADMAC) monomer, linear poly(DADMAC) and their mixture monomer/poly(DADMAC) in dilute aqueous solution exhibits a linear relationship. It was possible to calculate conversion of DADMAC polymerization by measuring its electric conductivity. Although the electrical conductivity of the poly(DADMAC) solution decreased with increasing its molecular weight, in the process of UV or ionizing radiation polymerization the molecular weight of the polymers could be kept constant in the case of fixed temperature, UV-luminous intensity or dose rate. Based on the method mentioned above, the kinetics of UV induced polymerization of DADMAC in aqueous solution was studied; the overall activation energy of polymerization of DADMAC in the water phase was calculated to be 18.8 kJ mol$^{-1}$ . ${\gamma}$-Radiation-induced polymerization of DADMAC in aqueous solution as a function of absorbed dose was studied as well. The conversion of DADMAC increased quickly with dose before 30 kGy and then increased slowly. The experimental data of both UV- and ${\gamma}$-induced polymerization were verified to be reliable by inverted ultracentrifugation method.