  • In this study, to improve the color of iron oxide from waste pickling acid at the cold rolling mill, quality control technologies to improve color were investigated. During operation of the spray roaster, the charge amount of waste acid per hour, temperature, and numbers of spray nozzles were investigated. At the admixing process, titanium oxide, silica, and goethite were tested. The color character of iron oxide can be improved by process control of the spray roaster and the admixing process at a pigment factory. Iron oxide from this study is appropriate for use as a colorant of a concrete product.

  • PDF

산화철 안료의 색상개선 연구 (Improvement of Color for Iron Oxide from Waste Pickling Acid)

  • 손진군;금대영;이재영;이훈하
    • 자원리싸이클링
    • /
    • 제11권5호
    • /
    • pp.24-29
    • /
    • 2002
  • 철강압연공장에서 산세공정중 발생하는 산화철의 색상을 개선하기 위하여 배소로 조업과 색상혼합공정을 연구하였다. 배소로 조업에서는 조업온도, 폐산장입량, 폐산분사 노즐수에 대하여 검토하였으며, 색상혼합공정에서는 산화티탄, 실리카, 괴타이트를 색상혼합재로 검토하였다. 배소로 조업에서는 조업온도를 낮게 할수록 산화철의 명도가 개선되었으며, 색상혼합공정에서는 괴타이트 첨가 경우에 제일 많이 산화철의 적색 및 명도가 개선되었다.

Purification of Iron Oxides and Application to Magnetic Hard Ferrite

  • Kim, Jeong-Seog;Chou, Kyoung-Ho;Kim, Jai-Young
    • The Korean Journal of Ceramics
    • /
    • 제2권3호
    • /
    • pp.125-130
    • /
    • 1996
  • Hematite iron ore and waste iron oxide sludge containing about 3-5 wt% $SiO_2$ were purified by three types of method developed on the basis of the Bayer process which is known as the purification process of bauxite ore. The basic principle of the developed methods lies in the fact that the impurities contained in the iron oxides, such as $SiO_2$ and $Al_2O_3$ are soluble in the alkaline reagents. Reaction of the raw materials with KOH was done in pressure vessel, at atmospheric pressure, and by both of these two. By the pressure vessel method $SiO_2$ content was reduced to below 0.5 wt% in the waste iron oxide sludge, while, in iron ore, $SiO_2$ remained at 2-3 wt%. The atmospheric pressure reaction rendered the waste iron oxide sludge $SiO_2$ content below 0.5wt% when the reaction temperature increased to above 90$0^{\circ}C$. The combined method of two previous methods was the most effective process and rendered the refined iron oxide about 300-400ppm of $SiO_2$. Using some refined iron oxides, Ba-ferrite was produced and magnetic properties were measured. The highest quality of magnetic properties obtained in this study were Br=2.09 G, bHc=1.99 KOe, iHc=4.54 KOe, $(BH)_{max}$=1.06 MGOe. Effect of sintering condition and chemical composition will be discussed.

  • PDF

산화철의 품질 안정화 (A Study on th Quality Stabilization of Iron Oxide)

  • 변태봉;한기현;김형석;배우현
    • 자원리싸이클링
    • /
    • 제7권4호
    • /
    • pp.55-63
    • /
    • 1998
  • 냉연공장의 산회수 설비로부터 제조되는 소프트 페라이트용 산화철의 품질편차를 감소시키기 위한 연구로서, 품질편차 원인분석, 산회수 조업조건 및 산화철 성분분석, 그리고 산화철의 품질변화를 조사하고 이로부터 도출된 산화철 품질편차 최소화를 위한 적정 조업 pattern을 확립하였다. 산화철의 품질편차를 감소시키기 위해서는 산화철의 원료가 되는 폐산의 발생, 즉 산세처리 대상재인 강종의 구분과 발생 폐산의 분리저장 및 분리운전이 필요하였다. 폐산의 분리, 운전조업 및 생성 산화철의 분리, 저장으로 $SiO_2$함량 약 80ppm, 편차 $\pm$ 10 ppm 이하의 산화철을 제조할 수 있었다. 추가필터 설치의 운영에 따라 산화철의 품질편차 감소뿐만 아니라 고순도 산화철의 생산도 가능할 것으로 예상되었다.

  • PDF

FASTMET$\circledR$ Process for Steel Mill Waste Recycling

  • Tanaka, Hidetoshi;Harada, Takao;Sugitatsu, Hiroshi
    • 대한전자공학회:학술대회논문집
    • /
    • 대한전자공학회 2001년도 The 6th International Symposium of East Asian Resources Recycling Technology
    • /
    • pp.387-392
    • /
    • 2001
  • Kobe Steel, LTD. and Midrex Technologies Inc. jointly developed the FASTMET$\circledR$ process as a steel mill waste recycle technology in which the DRI product meets BF feed material or BOF/EAF feed material requirements. FASTMET(R) process turns value-less wastes into valuable DRI and sellable zinc oxide, and gives the solution for the steel mill wastes recycling from both economical and environmental viewpoints. During the development of the process, Laboratory, Pilot Plant and Demonstration Plant tests were carried out from 1990 to 1998. The first FASTMET(R) commercial plant began operation in April, 2000 and the second commercial plant started in April, 2001 Both commercial plants have proceeded successfully preying that FASTMET$\circledR$ is a suitable process for recycling steel mill waste and for producing DRI as an iron source.

  • PDF

산화철 페촉매를 애용한 NiZn-페라이트의 합성 (Synthesis of NiZn-Ferrite from Waste Iron Oxide Catalyst)

  • 황연;이효숙;이우철
    • 한국결정학회지
    • /
    • 제12권1호
    • /
    • pp.20-24
    • /
    • 2001
  • NiZn-ferrite was synthesized usign waste iron oxide catalysts which were produced from styrene monomer process and buried underground as an industrial wastes. The spinel type ferrite was obtained by calcination and sintering of the mixture of finely ground waste catalysts, nickel oxide and zinc oxide powders. The sintered body of Ni/sub 0.5/Zn/sub 0.5/Fe₂O₄ composition at 1230℃ for 5 hours showed the density of 5.38g/㎤, and initial permeability of 59 at 1 kHz. Not only cerium oxide, which existed as a major component in the catalyst, but also unicorporated NiO and ZnO into spinel structure remained as second phases after sintering.

  • PDF

산화철계 형석대체제의 전로 정련특성 (BOF Refining of Fluorspar Substitute Using Iron Oxide Based By-product)

  • 금창훈;허보영
    • 한국재료학회지
    • /
    • 제16권5호
    • /
    • pp.336-340
    • /
    • 2006
  • Fluorspar has been essential flux in steelmaking process. The main effects of fluorspar addition are lowering of the viscosity and melting temperature of slag. In recent years, due to the increasing price and environmental problem of fluorspar, various types of fluorspar substitute have been investigated. In this study, iron oxide by-products such as sinter dust, basic oxygen furnace (BOF) sludge and mill scale were developed as a substitute in terms of waste recycling. Several plant trials were carried out by addition of briquetted substitutes of $4{\sim}6$ kg/ton to compare with the fluorspar of $0.7{\sim}1$ kg/ton. The substitutes showed a similar behavior of slag formation, phosphorus removal and MgO saturation content.

산화철 폐촉매로부터 합성된 NiZn- 페라이트의 자기적 특성 (Magnetic Properties of NiZn-ferrite Synthesized from Waste Iron Oxide Catalyst)

  • 황연;권순길;이효숙;제해준;박상일
    • 한국세라믹학회지
    • /
    • 제38권12호
    • /
    • pp.1162-1166
    • /
    • 2001
  • 석유화학 공정 중 Styrene(SM) 공정에서 발생되는 산화철 폐촉매는 산업 폐기물로서 전량 매립되고 있는데, 이를 출발 원료로 사용하여 NiZn-페라이트를 합성하였고 그 자기적 특성을 조사하였다. 산화철 폐축매 펠렛을 분쇄한 후 NiO 및 ZnO를 혼합하여 90$0^{\circ}C$에서 하소하고 123$0^{\circ}C$에서 5시간 소결하여 스핀넬형 페라이트 소결체를 얻었다. N $i_{x}$ Z $n_{1-x}$F $e_2$ $O_4$(x=0.36, 0.50, 0.66)조성에 대하여 초투자율을 측정하였고, S-parameter를 측정하여 반사 감쇄량을 계산하였다. 산화철 폐촉매를 이용하여 X-band 주파수 영역에서 높은 전자파 흡수능을 갖는 전파흡수체를 제조할 수 있음을 확인하였다.다.

  • PDF

수질오염 제염을 위한 세슘 선택성 상자성 코어 무기복합제염제 개발 (Development of Cesium-selective Paramagnetic Core Inorganic Composite Agent for Water Decontamination)

  • 홍성표;강보선
    • 방사선산업학회지
    • /
    • 제18권2호
    • /
    • pp.127-132
    • /
    • 2024
  • Large amounts of liquid radioactive waste or radioactive contaminated water could be produced during the treatment of radiation accidents or during the dismantling and decontamination process of nuclear power plants. Since most of the decontamination agents to date are difficult to recover after adsorption of radioactive isotopes, their use in open environments such as rivers, reservoirs, or oceans is limited. In this study, as a radioactive decontamination agent that can overcome the current limitations when used in an open environment, a paramagnetic core inorganic composite (PMCIC) decomposite agent with high selectivity to cesium ions was developed. PMCore was prepared by synthesizing paramagnetic iron oxide nanoparticles, and inorganic crystals such as metal-ferrocyanide were conjugated to the surface so that PMCore could be selective to cesium ions. The developed PMCIC could be easily recovered from the water by magnetism and could adsorb up to 94 μM of Cs atoms per 1 g of PMCIC.