Improvement of Color for Iron Oxide from Waste Pickling Acid

산화철 안료의 색상개선 연구

  • 손진군 (포항산업과학연구원 자원활용연구팀) ;
  • 금대영 (포항산업과학연구원 자원활용연구팀) ;
  • 이재영 (포항산업과학연구원 자원활용연구팀) ;
  • 이훈하 (포항산업과학연구원 자원활용연구팀)
  • Published : 2002.10.01

Abstract

In this study, to improve the color of iron oxide from waste pickling acid at the cold rolling mill, the quality control technologies especially about color were investigated on the spray roaster and iron oxide powder. At the operation condition of the spray roaster, the charge amount of waste acid per hour, temperature, numbers of spray nozzle were investigated. At admixing process, titanium oxide, silica, goethite were tested. Color character of iron oxide can be improved by process control at spray roaster and by admixing process at a pigment factory Iron oxide from results of this study is enough to use as the colorant of concrete product.

철강압연공장에서 산세공정중 발생하는 산화철의 색상을 개선하기 위하여 배소로 조업과 색상혼합공정을 연구하였다. 배소로 조업에서는 조업온도, 폐산장입량, 폐산분사 노즐수에 대하여 검토하였으며, 색상혼합공정에서는 산화티탄, 실리카, 괴타이트를 색상혼합재로 검토하였다. 배소로 조업에서는 조업온도를 낮게 할수록 산화철의 명도가 개선되었으며, 색상혼합공정에서는 괴타이트 첨가 경우에 제일 많이 산화철의 적색 및 명도가 개선되었다.

Keywords

References

  1. Jin-Gun Sohn, T. B. Byeon : Bulletin of the Korean Inst.of Met. & Mat. 9(2), 190-198 (1996)
  2. M. H. Gutcho : 'Inorganic Pigment Manufacturing Process'Mayes Data Corp. Park Ridge, NJ: 110-128 (1988)
  3. Takao Kazama, Katsuo Koshizuka: J. of the Japan Society of Color Material, 57(6), 342-349 (1984) https://doi.org/10.4011/shikizai1937.57.342
  4. Jae-Keun Yu, K.I.Lee, S.S Lee : J. of Korean Inst. of Resources Recycling. 8(4) 45-56 (1999)
  5. V. Schwertmaim, R. M. Cornell : 'Iron Oxide in the Laboratory' VCH Publisher New York: 30-34 (1991)