• Title/Summary/Keyword: Uniform Temperature

Search Result 1,837, Processing Time 0.028 seconds

The Structural properties of PZT thick film with preparation condition states (제작조건에 따른 PZT후막의 구조적 특성)

  • Kang, Jung-Min;Cho, Hyun-Moo;Lee, Sung-Gap;Lee, Sang-Heon;Lee, Young-Hie;Bae, Seon-Gi
    • Proceedings of the Korean Institute of Electrical and Electronic Material Engineers Conference
    • /
    • 2004.07a
    • /
    • pp.142-145
    • /
    • 2004
  • [ $Pb(Zr_{0.8}Ti_{0.2})TiO_3$ ] powder were prepared by the sol-gel method using a solution of Pb-acetate, Zr n-propoxide and Ti iso-propoxide. PZT thick film were fabricated by the screen printing method. and then the structural properties as a function of the sintering temperature were studied. PZT film thickness, obtained by four screen printing, was approximately $70{\sim}90{\mu}m$. The PZT thick film, sintered at $1050^{\circ}C$, showed deuse and uniform grain stractures and percent porosity of the thick film was 25.43%.

  • PDF

An experimental study on the birefringence and extinction angle distribution in the injection/compression molded optical disk (사출/압축 성형된 광디스크 내의 복굴절 및 광축의 분포에 관한 연구)

  • Kim J. S.;Yoon K. H.
    • Proceedings of the Korean Society for Technology of Plasticity Conference
    • /
    • 2005.05a
    • /
    • pp.445-448
    • /
    • 2005
  • Recently, injection molding process became more popular than ever to produce large quantities of high precision products or optical products. Injection molding products can cause sensorial problems because of high birefringence or deformation from the residual stresses in the optical media. In the present study, we have focussed on the effect of holding and compression pressures on the optical anisotropy remaining in the MOD by examining the gapwise distribution of birefringence and extinction angle The effect of holding pressure was found to form the inner two birefringence peaks. But the effect of compression pressure on the birefringence distribution was found to make the uniform distribution near the center in the gap-wise direction. Finally, the value of the birefringence near the wall decreased as the mold temperature increased.

  • PDF

Fabrication of Al 6061 Foamable Precursor by Powder Metallurgical and Induction Heating Method (P/M법과 유도가열 공정을 이용한 발포용 6061 Al 합금 프리커서 제조)

  • 윤성원;강충길
    • Transactions of Materials Processing
    • /
    • v.12 no.5
    • /
    • pp.457-464
    • /
    • 2003
  • In the powder compact melting technique, proper precursor fabrication is very important because density distribution after foaming and foamability are determined during precursor fabrication process. The fabrication of the precursor has to be performed very carefully because any residual porosity or other defects will lead to poor results in further processing. In order to evaluate the effect of the compaction parameters on the kinetics of the foaming process, a series of experiments were performed. In this study, aluminium foams with a closed cell structure were fabricated by using both the powder compact method and the induction heating process. A proper induction coil was designed to obtain a uniform temperature distribution over the entire cross sectional area of precursor. To establish the foamable precursor fabrication conditions, effects of process parameters such as the titanium hydride content (0.3∼1.5 wt.%), pressing pressure of the foamable precursor (50∼150kN) on the pore morphology were investigated.

A Study on the Angular Distortion in Weldment6s using the Laminated Plate Theory (적층판 이론을 이용한 용접부 각 변형량 해석에 관한 연구)

  • 손광재;양영수;최병익
    • Journal of Welding and Joining
    • /
    • v.17 no.2
    • /
    • pp.91-96
    • /
    • 1999
  • The problems of welding distortion in a welded structures are major concern in heavy industry. Weld-induced angular distortion's formula, composed weld parameter such as heat input and plate thickness, is developed analytically by the use of an elliptic cylindrical inclusion with an eigenstrain in an infinite laminated plate theory. The source of angular distortion in weldments is the plastic strains, which are caused by non-uniform temperature gradient. The distributions of the plastic strain corresponding eigenstrain are assumed by the use of Rosenthal's solution expressing thermal history. Comparison of calculated results with experimental data shows the accuracy and validity of the proposed method.

  • PDF

Stress Intensity Factors and Kink Angle of a Crack Interacting with a Circular Inclusion Under Remote Mechanical and Thermal Loadings

  • Lee, Saebom;Park, Seung-Tae;Earmme, Youn-Young;Chung, Dae-Youl
    • Journal of Mechanical Science and Technology
    • /
    • v.17 no.8
    • /
    • pp.1120-1132
    • /
    • 2003
  • A problem of a circular elastic inhomogeneity interacting with a crack under uniform loadings (mechanical tension and heat flux at infinity) is solved. The singular. integral equations for edge and temperature dislocation distribution functions are constructed and solved numeric-ally, to obtain the stress intensity factors. The effects of the material property ratio on the stress intensity factor (SIF) are investigated. The computed SIFs are used to predict the kink angle of the crack when the crack grows.

Activation Effect on Palladium Electroless Plating of Porous Stainless Steel Support (팔라듐 무전해 도금을 위한 활성화 처리에 대한 연구)

  • 허장은;우상국;서동수;한성욱;한인섭;서두원
    • Proceedings of the Korea Society for Energy Engineering kosee Conference
    • /
    • 1999.05a
    • /
    • pp.165-170
    • /
    • 1999
  • Palladium membranes have high selectivity of separation and removal of hydrogen to chemical process at high temperature. For the development of hydrogen permeable membrane, palladium was deposited on porous stainless steel support by electroless plating method. In this work, the activation effect on the surface of stainless steel support has been investigated for the effective palladium plating. The morphology and microstructure were characterized by SEM and the composition was analyzed by EDX. It is found that the composition of deposited nuclei on the stainless steel support was changed in accordance with activation cycles. It is also observed that Sn-enriched nuclei has been changed to Pd-enriched nuclei over the fifteenth activation. The uniform deposition of the dense palladium layer on porous stainless steel support has been performing with Sn-enriched nuclei and comparing with Pd-enriched nuclei.

  • PDF

Behavior of Surface Oxide on the Cold Rolled Steel Sheet and its Phosphatability (강판의 산화막 거동 및 인산염처리성의 평가)

  • Kim, H. J.
    • Journal of Surface Science and Engineering
    • /
    • v.29 no.3
    • /
    • pp.203-210
    • /
    • 1996
  • The purpose of this study is to investigate behavior of surface oxide on the cold rolled sheet used for the drum material and its phosphatability. Phosphatability is dependent of the characteristics of surface oxide on the cold-rolled sheet and can be estimated by using the electrochemical method and measuring $\tau$ value which is the time to be exposed to substrate Fe. $\tau$ value is varied with the steel composition, width direction of the sheet and SPM length. The good phosphatability and uniform surface color can be obtained by increasing SPM elongation and decreasing FCS temperature.

  • PDF

A Study on the Pd-Ni Alloy Hydrogen Membrane Using the Sputter Deposition (스퍼터 증착 방식으로 제조된 Pd-Ni 합금 수소 분리막 연구)

  • Kim Dong-Won;Park Jeong-Won;Kim Sang-Ho;Park Jong-Su
    • Journal of Surface Science and Engineering
    • /
    • v.37 no.5
    • /
    • pp.243-248
    • /
    • 2004
  • A palladium-nikel(Pd-Ni) alloy composite membrane has been fabricated on microporous nickel support formed with nickel powder. Plasma surface treatment process is introduced as pre-treatment process instead of HCI activation. Pd coating layer was prepared by dc magnetron sputtering deposition after $H_2$ plasma surface treatment. Palladium-nickel alloy composite layer had a fairly uniform and dense surface morphology. The membrane was characterized by permeation experiments with hydrogen and nitrogen gases at temperature of 773 K and pressure of 2.2psi. The hydrogen permeance was 6 ml/minㆍ$\textrm{cm}^2$ㆍatm and the selectivity was 120 for hydrogen/nitrogen($H_2$/$N_2$) mixing gases at 773 K.

A Study on the Pd-Ni Alloy Hydrogen Membrane using the Porous Nickel Metal Support (다공성 Ni 금속 지지체를 사용한 Pd-Ni 합금 수소 분리막 연구)

  • Kim Dong-Won;Um Ki-Youn;Kim Sang-Ho;Park Jong-Su
    • Journal of Surface Science and Engineering
    • /
    • v.37 no.5
    • /
    • pp.289-295
    • /
    • 2004
  • A dense palladium-nikel (Pd-Ni) alloy composite membrane has been fabricated on microporous nickel support mixed with submicron/micron nickel powder instead of mesoporous stainless steel support. Plasma treatment process is introduced as pre-treatment process instead of HCI activation. Pd-Ni alloy composite membrane prepared by electro plating was fairly a uniform and dense surface morphology. The membrane was characterized by permeation experiments with hydrogen and nitrogen gases at temperature 773 K and pressure 2.2 psi. The results showed that hydrogen ($H_2$) permeance was 27 ml/$\textrm{cm}^2$ㆍatmㆍmin and hydrogen/ nitrogen ($_H2$$N_2$) selectivity was 8 at 773 K.

Stepwise Adsorption in Gas-Solid Adsorption System and Phase Transition in Adsorbed Phase

  • Lee Song Hee;Lee Jo Woong;Pak Hyungsuk;Chang Seihun
    • Bulletin of the Korean Chemical Society
    • /
    • v.3 no.2
    • /
    • pp.37-44
    • /
    • 1982
  • In this work we have studied the multilayer stepwise adsorption of gases on solid adsorbents based on the previously developed theory. It is shown that stepwise adsorption isotherms emerge from our theory if an ad hoc adsorption regarding the degree of occupation for each successive layer is abolished and the effect of lateral intermolecular interactions among adsorbate molecules is included. In addition to these the effect of vertical interactions has also been taken into consideration. It seems that the vertical interaction plays a role in deciding the shape and the position of steps in resulting isotherms. It is evident from this research that it is the lateral interaction that is responsible for stepwise adsorption as long as the adsorbent surface is uniform and temperature is sufficiently low.