LPMOCVD 법으로 증착된 TiO$_2$ 박막의 특성 (Properties of TiO$_2$ Thin Film Deposited by LPMOCVD)

  • 이하용;박용환;고경현;박정훈;홍국선
    • 한국세라믹학회지
    • /
    • 제36권9호
    • /
    • pp.901-908
    • /
    • 1999
  • Effects of LPMOCVD process parameters on the properties of TiO2 thin film were investigated. Depositions were made in the range of temperature 300-67$0^{\circ}C$ with various TTIP(Titanium Tetraisopropoxide) concentrations by contrlling bubbler temperature(40-8$0^{\circ}C$) and/or flow rate(30-90 sccm). Post annealing treatments were carried out at 500-80$0^{\circ}C$ range in the air. Films deposited at 40$0^{\circ}C$ have denser morphology than those of films deposited at 50$0^{\circ}C$ and $600^{\circ}C$ due to slower deposition rate. Bubbler temperature can affect on the deposition rate in mass transfer controlled regime such as 50$0^{\circ}C$ or higher but not below 50$0^{\circ}C$ where surface reaction rate becomes important. On the contrary for films deposited above 50$0^{\circ}C$ flow rate can raise deposition rate but eventually saturate it at the 50 sccm and above due to retarded adhesion of decomposed species. But for films deposited at 40$0^{\circ}C$ deposition rate increases stadily with flow rate. As the film becomes more porous A(200) texture can not be developed and AnataselongrightarrowRutile transition kinetics increases.

  • PDF

Temperature-dependent Structural and Magnetic Properties of Diamagnetic $HgI_2$

  • Park, C.I.;Jin, Zhenlan;Hwang, I.H.;Yeo, S.M.;Han, S.W.
    • 한국진공학회:학술대회논문집
    • /
    • 한국진공학회 2013년도 제45회 하계 정기학술대회 초록집
    • /
    • pp.291.1-291.1
    • /
    • 2013
  • We examined the temperature-dependent structural and magnetic properties of HgI2 in the temperature range of 300~400 K. HgI2 is a diamagnetic material and can be used for X-ray or γ-ray detectors. DCmagnetization measurements on HgI2 showed that there is a small but distinguishable change in its diamagnetic properties near 375 K. The magnetic property change is not expected because Hg and I are known as nonmagnetic elements. X-ray diffraction (XRD) measurements revealed a structural transition in the temperature of 350~400 K. Temperature-dependent x-ray absorption fine structure (XAFS) demonstrated that the chemical valence states of both Hg and I did not changed in the temperature range of 300~400 K. However, XAFS revealed that the bond-length disorder was slightly increased in the temperature range, particularly, near Hg atoms. The structural changes of HgI2 are likely related to its diamagnetic property change. We will discuss the relation between the diamagnetic properties and local structural properties of HgI2 in detail.

  • PDF

TPR/TPO 실험기법을 이용한 전이금속산화물의 산화-환원 특성 연구 (Redox Property of Transition Metal Oxides in Catalytic Oxidation)

  • 김영호;이호인
    • 공업화학
    • /
    • 제10권8호
    • /
    • pp.1161-1168
    • /
    • 1999
  • 3주기 전이금속(Cr~Zn)의 산화물 및 V, Mo, W의 산화물에 대하여 temperature-programmed reduction/trmperature-programmed oxidation(TPR/TPO) 실험을 통하여 그 산화-환원 특성을 조사하였다. TPO 곡선의 산화피크는 TPR 곡선의 환원피크와 비슷하거나 약간 낮은 온도에서 나타났으며, 환원피크에 비하여 온도 폭이 넓었다. 3주기 전이금속한화물의 산화 및 환원 과정의 활성화에너지는 33~149 kJ/mol 범위에 있는 반면, V, Mo, W 산화물에서는 더 컸다. 금속산화물의 산화 및 환원 과정의 활성화에너지 변화는 금속-산소 결합세기에 비례하였다. 환원(TPR) 및 산화(TPO) 과정에 대한 활성화에너지 차이(${\Delta}E_a$)가 작을수록 o-자일렌 산화반응에서 금속산화물 촉매의 활성화에너지도 작았다. 금속한화물 촉매에서 o-자일렌 산화반응은 금속산화물 표면의 산화-환원 과정을 반복하는 Mars-van Krevelen 반응 메카니즘으로 설명될 수 있음을 확인하였다.

  • PDF

Flexural analysis of thermally actuated fiber reinforced shape memory polymer composite

  • Tiwari, Nilesh;Shaikh, A.A.
    • Advances in materials Research
    • /
    • 제8권4호
    • /
    • pp.337-359
    • /
    • 2019
  • Shape Memory Polymer Composites (SMPC) have gained popularity over the last few decades due to its flexible shape memory behaviour over wide range of strains and temperatures. In this paper, non-linear bending analysis has been carried out for SMPC beam under the application of uniformly distributed transverse load (UDL). Simplified C0 continuity Finite Element Method (FEM) based on Higher Order Shear Deformation Theory (HSDT) has been adopted for flexural analysis of SMPC. The numerical solutions are obtained by iterative Newton Raphson method. Material properties of SMPC with Shape Memory Polymer (SMP) as matrix and carbon fibre as reinforcements, have been calculated by theory of volume averaging. Effect of temperature on SMPC has been evaluated for numerous parameters for instance number of layers, aspect ratio, boundary conditions, volume fraction of carbon fiber and laminate stacking orientation. Moreover, deflection profile over unit length and behavior of stresses across thickness are also presented to elaborate the effect of glass transition temperature (Tg). Present study provides detailed explanation on effect of different parameters on the bending of SMPC beam for large strain over a broad span of temperature from 273-373K, which encompasses glass transition region of SMPC.

Velocity Oscillations in the Chromosphere and the Transition Region above Plage Regions

  • Kwak, Hannah;Chae, Jongchul
    • 천문학회보
    • /
    • 제42권2호
    • /
    • pp.81.4-82
    • /
    • 2017
  • We investigate velocity oscillations in the active region plage by using the high-spatial, high-spectral and high-temporal resolution spectral data acquired by the Interface Region Imaging Spectrograph (IRIS). From the Mn I $2801.907{\AA}$ (lower chromosphere), C II (lower transition region) and Si IV (middle transition region) lines, we measure the line of sight Doppler velocity at different atmospheric layers, and present results of wavelet analysis of the plage region with a range of periods from 2 to 8 minutes. In addition, we present correlations of the oscillations from the lower chromosphere to the middle transition region. Finally, we will discuss the regional dependence of the oscillation properties on physical properties such as temperature and magnetic field inclination.

  • PDF

열처리조건에 따른 VO2 후막 급변온도센서의 특성연구 (Characterization of VO2 thick-film critical temperature sensors by heat treatment conditions)

  • 송건화;유광수
    • 센서학회지
    • /
    • 제16권6호
    • /
    • pp.407-412
    • /
    • 2007
  • For $VO_{2}$ sensors applicable to temperature measurement by using the nature of semiconductor to metal transition, the crystallinity, microstructure, and temperature vs. resistance characteristics were investigated systematically as a function of the annealing condition. The starting materials, vanadium pentoxide ($V_{2}O_{5}$) powders, were mixed with vehicle to form paste. This paste was screen-printed on $Al_{2}O_{3}$ substrates and then $VO_{2}$ thick films were heat-treated at $450^{\circ}C$ to $600^{\circ}C$, respectively, for 1 hr in $N_{2}$ gas atmosphere for the reduction. As results of the temperature vs. resistance property measurements, the electrical resistance of the $V_{2}O_{5}$ sensor in phase transition range was decreased by $10^{3.9}$ order. The presented critical temperature sensor could be used in fire-protection and control systems.

온도 변화에 의한 열전도성 실리콘 고무의 절연 열화 특성 (A Study on Insulation Degradation Properties of Thermal Conductive Silicone Rubber due to Temperature Transition)

  • 이성일
    • 한국전기전자재료학회논문지
    • /
    • 제28권7호
    • /
    • pp.456-461
    • /
    • 2015
  • In this study, the frequency properties of electrostatic capacity and dielectric loss for the samples with different types of filler has been measured in through the applied frequency range of 7 kHz ~3,000 kHz at temperature of $80^{\circ}C$, $110^{\circ}C$, $140^{\circ}C$, $170^{\circ}C$. The results of this study are as follows. When the sample is degradated at the temperature of $80^{\circ}C$, $110^{\circ}C$, $140^{\circ}C$, $170^{\circ}C$ and the frequency range of 7 kHz ~3,000 kHz is applied, It found that the electrostatic capacity of the sample with Polyimide film is larger than the sample with Grass fiber. It found that the dielectric loss for the sample with Polyimide film is larger than the sample with Grass fiber with increasing frequency and temperature in the $80^{\circ}C$, $110^{\circ}C$, $140^{\circ}C$, $170^{\circ}C$ range. Also, the dielectric loss decreased with increasing frequency. In case of the sample with Polyimide film, It found that the electrostatic capacity decreased with increasing temperature, and the dielectric loss gradually decreased with increasing frequency.

Reaction temperature dependence of MgB2 superconducting bulks using the different sizes of Mg raw powders

  • K.C., Chung
    • 한국초전도ㆍ저온공학회논문지
    • /
    • 제24권4호
    • /
    • pp.36-39
    • /
    • 2022
  • Since the MgB2 superconductor is simply composed of two constituents of Mg and B, its performance can be monitored easily with the change of one ingredient compared to the other. With the powder size of B less than 100 nm, two different sizes of Mg powders are used to investigate the reaction temperature dependence of MgB2 bulk samples. In the range of 630-700℃ for the duration of 30 min., the un-reacted Mg is seen only at 630℃ with Mg powder size of <5 ㎛, whereas Mg traces are detected at all the temperature range with Mg powder size of <45 ㎛. The reaction temperature dependence of MgB2 superconducting transition temperature, Tc, shows little difference whether Mg powder size is large or small in this range except for the 630℃. It is worthy of notice that the critical current densities of MgB2 show higher performance with the small size of Mg compared to the large one at all field ranges. With the Mg powder size of <45 ㎛, flux pinning is enhanced with decreasing the reaction temperature, whereas flux pinning properties is quite similar in the Mg powder size of <5 ㎛ except for the 630℃, where Mg is left behind after the reaction.

$\textrm{0.9Pb}\textrm({Mg}_{1/3}\textrm{Nb}_{2/3})\textrm{O}_3$-$\textrm{0.1PbTiO}_3$계 강유전체에서 전계인가에 따른 분극 및 변위의 상관관계 (Correlations between the Polarization and Strain Induced by Electric field in $\textrm{0.9Pb}\textrm({Mg}_{1/3}\textrm{Nb}_{2/3})\textrm{O}_3$-$\textrm{0.1PbTiO}_3$ Relaxor Ferroelectrics)

  • 박재환;박재관;박순자
    • 한국재료학회지
    • /
    • 제9권1호
    • /
    • pp.81-85
    • /
    • 1999
  • Polarization and strain induced by unipolar electric field (P\ulcorner, S\ulcorner), those induced by bipolar electric field (P, S) and remanent polarization (P\ulcorner) were investigated in 0.9Pb(Mg\ulcornerNb\ulcorner)O$_3$-$0.1PbTiO_3$relaxor ferroelectric ceramics in the temperature range of $-50^{\circ}C$~$90^{\circ}C$. From the temperature dependence of polarization and strain, the transition from predominantly paraelectric (electrostrictive) to partially ferroelectric (piezoelectric) is visualized. Under the given temperature, the P\ulcorner/P\ulcorner is always larger than the S\ulcorner/S\ulcorner and the difference between them becomes larger ass the temperature decrease. The S\ulcorner/P\ulcorner increases as the temperature decreased below phase transition temperature. It was suggested that these experimental results might be explained with a simple rigid ion model concentrating on BO\ulcorner octahedron.

  • PDF

Poly(n-Butyl Methacrylate)에 의한 메탄가스의 용해도 (Solubility of Methane in Poly(n-Butyl Methacrylate) at Elevated Pressures)

  • 김진환;이우태;한능원
    • 멤브레인
    • /
    • 제2권2호
    • /
    • pp.129-134
    • /
    • 1992
  • Poly(n-butyl methacrylate)(PnBMA)에 의한 메탄가스의 용해도를 35atm의 압력까지 측정하였다. 용해도의 측정은 -$10^{\circ}$C 에서 30$^{\circ}$C까지의 온도범위에서 용적법에 의하여 실시하였다. PnBMA에 의한 메탄가스의 용해도는 유리 전이온도 이하에서 측정압력에 대하여 비선형으로 나타났으며, dual-mode sorption model로 만족스럽게 해석할 수 있었다. Langmuri capacity constant는 온도가 증가할수록 감소하였으며 유리전이온도 근처에서 영이 되며, 용해도 등온선은 유리 전이온도 이상에서는 직선으로 나타났다. Dual-mode sorption parameter의 온도 의존성도 고찰하였다.

  • PDF