치과주조용 Ti-X%Cu(X=2,5,10)합금의 미세조직 및 경도 (Microstructure and Hardness of Ti-X%Cu(X=2,5,10) Alloys for Dental Castings)

  • 정종현
    • 대한치과기공학회지
    • /
    • 제31권3호
    • /
    • pp.9-14
    • /
    • 2009
  • This study evaluated the mechanical properties of Ti-Cu alloys with the hope of developing an alloy for dental casting with better mechanical properties than unalloyed titanium. Ti-Cu alloys with four concentrations of Cu(2,5,10wt%) were made in an argon-arc melting furnace. The microstructure and micro-Vickers hardness were determined. X-ray diffraction pattern test was performed on the polished specimens. The microstructure of 2%Cu and 5%Cu alloys are shown acicular ${\alpha}Ti$ phase formed on the surfaces of previously formed $\beta$grains. The 10%Cu alloys has essentially a eutectoid structure; this structure includes lamella of ${\alpha}Ti$ and $Ti_2Cu$ phase that transformed from ${\alpha}Ti$ at the eutectoid temperature. The micro-Vickers hardness of CP Ti specimens was significantly(p<0.05) lower than that of any of the other alloys. Among the Ti-Cu alloys, the 10%Cu alloys exhibited a significantly(p<0.05) higher hardness value. but lower than that of Ti-6%Al-4%V alloy. From these results, it was concluded that new alloys for dental castings should be designed as Ti-Cu based alloys if other properties necessary for dental castings were obtained.

  • PDF

Preparation of Fe-AC/$TiO_2$ composites and pH dependence of their Photocatalytic activity for methylene blue

  • Meng, Ze-Da;Zhang, Kan;Oh, Won-Chun
    • 한국결정성장학회지
    • /
    • 제19권5호
    • /
    • pp.268-276
    • /
    • 2009
  • In this study, activated carbon (AC) was treated with ferric ion by a sol-gel method. The compound (Fe-AC) was employed for the preparation of Fe-activated carbon/$TiO_2$, (Fe-AC/$TiO_2$) composites. The prepared Fe-AC/$TiO_2$ composites were characterized with surface properties, structural crystallinity, elemental identification and photocatalytic activity. The SEM results showed that ferric compounds and titanium dioxide were fixed onto the AC surfaces. The XRD results showed that Fe-AC/$TiO_2$ composites mostly contained anatase phase. EDX showed the presence of C, O, and Ti with Fe peaks in all samples. Its photocatalytic degradation effect was evaluated with the degradation behavior of the methylene blue (MB) solution. MB degradation could be attributed to the synergetic effects of adsorption, photo-degradation of $TiO_2$ and photo-Fenton of Fe component. The degradation rate for this photocatalysis was evaluated as a function of the concentration of the dye, the amount of $TiO_2$ and the pH. Photocataytic activity is good at activity pH.

Ti가 함유된 스테인리스강에서 Ti, Ti/cr코팅표면과 플라즈마질화표면의 부식특성 (Corrosion Characteristics of Ti, Ti/Cr Coated and Plasma-Nitrided Surface for Stainless Steel Containing Ti)

  • 최한철;이승훈;김관휴
    • 한국표면공학회지
    • /
    • 제35권6호
    • /
    • pp.391-400
    • /
    • 2002
  • Corrosion characteristics of Ti, Ti/Cr coated and plasma-nitrided surface for stainless steel containing Ti have been studied. Stainless steels containing 0.09-0.92wt% Ti were fabricated by using vacuum furnace and solutionized for 1hr at 105$0^{\circ}C$. Ti and Cr coatings were done on solutionized stainless steel surface by EB-PVD. The Ti coated specimen were coated by Cr and were nitrided by plasma at $450^{\circ}C$ for 5hr. Microstructure and phase analysis were performed using SEM, OM and EDX. Corrosion behavior of the coated specimen was investigated by electrochemical test. The coated surface was of fine columnar structure. The Ti/Cr coated surface was denser than the Ti coated and the Ti coated-nitrided surfaces. The corrosion and pitting potential increased in proportion to the Ti content, coating temperature, coating thickness and formation of stable oxide film. The current density in active and passive region decreased in the case of Ti/Cr coated sample and Ti coated-nitrided samples. Especially the plasma nitrided specimen after Ti coating have a good corrosion resistance compared with the Ti coated specimen. The number and size of pits decreased as Ti content of matrix increased.

전기방사를 이용한 Poly(vinyl alcohol)/TiO2 나노섬유 제조 (Electrospinning Fabrication of Poly(vinyl alcohol)/TiO2 Nanofibers)

  • 김영훈;도국배;최재영;;한상익;염정현
    • 한국염색가공학회지
    • /
    • 제25권2호
    • /
    • pp.118-125
    • /
    • 2013
  • Poly(vinyl alcohol) (PVA)/titanium dioxide ($TiO_2$) composite nanofibers were produced at different $TiO_2$ concentrations (0.5, 1 and 1.5 wt.%) using the electrospinning method. The parameters of electrospinning including polymer contents, voltage and tip-to-collector distance (TCD) were optimized for fabrication process. The study showed that 7.5 wt.% PVA, 15 kV applied voltage and 15 cm TCD are the best condition to obtain uniform PVA/$TiO_2$ nanofibers. $TiO_2$ nanoparticles give significant effect in fiber morphology. $TiO_2$ content increases the diameter of the fibers and roughen the fiber surfaces. The PVA/$TiO_2$ nanofibers were characterized by scanning electron microscope (SEM), transmission electron microscope (TEM) and X-ray diffraction (XRD).

화염 열복사의 파장별 선택적 반사를 위한 도료 코팅에 대한 수치적 연구 (Numerical study of a coating with pigment to selectively reflect the thermal radiation from fire)

  • 변도영;백승욱
    • 대한기계학회논문집B
    • /
    • 제22권3호
    • /
    • pp.399-407
    • /
    • 1998
  • The infrared reflection coatings with pigment can be used to protect the surfaces of combustible materials exposed to fire. To obtain high reflectivities in the infrared range (0.5-10.mu.m) important to fire, several dielectric pigments, such as titanium dioxide, iron oxide, and silicon, can be synthesized to polymer coatings. The theoretical analysis shows that the coating design with particles diameter in the 1.5 to 2.5.mu.m range and volume fraction in the 0.1 to 0.2 range is estimated to be optimal. In the analysis of the radiation, the dependent scattering, absorption by polymeric binder, and the internal interface reflection are considered. In addition, the temperature distribution in the semi-transparent coating layer and an opaque substrate (PMMA) is also presented.

Photocatalytic Oxidation for Organic Dye using Phenol Resin-based Carbon-titania Composites

  • Oh, Won-Chun;Na, Yu-Ri
    • 한국세라믹학회지
    • /
    • 제45권1호
    • /
    • pp.36-42
    • /
    • 2008
  • Carbon/$TiO_2$ composite photocatalysts were thermally synthesized with different mixing ratios of anatase to phenol resin through an ethanol solvent dissolving method. The XRD patterns revealed that only anatase phase can be identified for Carbon/$TiO_2$ composites. The diffraction peaks of carbon were not observed, however, due to the low carbon content on the $TiO_2$ surfaces and the low crystallinity of amorphous carbon. The results of chemical elemental analyses of the Carbon/$TiO_2$ composites showed that most of the spectra for these samples gave stronger peaks for carbon and Ti metal than that of any other elements. The BET surface area increases to the maximum value of $488\;m^2/g$ with the area depending on the amount of phenol resin. From the SEM images, small $TiO_2$ particles were homogeneously distributed to a composite cluster with the porosity of phenol resin-based carbon. From the photocatalytic results, the MB degradation should be attributed to the three kinds of synergetic effects, such as photocatalysis, adsorptivity, and electron transfer by light absorption between supporter $TiO_2$ and carbon.

Ti가 함유된 스테인리스강에서 Ti, Ti/Cr 코팅표면과 플라즈마질화표면의 부식특성 (Corrosion Characteristics of Ti, Ti/Cr Coated and Plasma-Nitrided Surface for Stainless Steel Containing Ti)

  • 최한철;이승훈;김관휴
    • 한국표면공학회지
    • /
    • 제36권1호
    • /
    • pp.89-98
    • /
    • 2003
  • Corrosion characteristics of Ti, Ti/Cr coated and plasma-nitrided surface for stainless steel containing Ti have been studied. Stainless steels containing 0.09-0.92wt% Ti were fabricated by using vacuum furnace and solutionized for 1hr at $1050^{\circ}C$. Ti and Cr coatings were done on solutionized stainless steel surface by EB-PVD. The Ti coated specimen were coated by Cr and were nitrided by plasma at $450^{\circ}C$ for 5hr Microstructure and phase analysis were performed using SEM, OM and EDX. Corrosion behavior of the coated specimen was investigated by electrochemical test. The coated surface was of fine columnar structure. The Ti/Cr coated surface was denser than the Ti coated and the Ti coated-nitrided surfaces. The corrosion and pitting potential increased in proportion to the Ti content, coating temperature, coating thickness and formation of stable oxide film. The current density in active and passive region decreased in the case of Ti/Cr coated sample and Ti coated-nitrided samples. Especially the plasma nitrided specimen after Ti coating have a good corrosion resistance compared with the Ti coated specimen. The number and size of pits decreased as Ti content of matrix increased.

Cu-TiB2 복합재료의 마모거동에 관한 연구 (A Study on the Wear Behavior of the Cu-TiB2 Composites)

  • 김정남;최종운;강계명
    • 한국재료학회지
    • /
    • 제15권1호
    • /
    • pp.61-65
    • /
    • 2005
  • The titanium $diboride(TiB_2)$ has high strength(750MPa), high melting point $(3225^{\circ}C)\;and\;10\%$ IACS electrical conductivity. On this account, the dispersion hardening $Cu-TiB_2$ composites(MMCs) are a promising candidate for applications as electrical contact materials. MMCs for electrical contact materials can reduce material cost and resource consumption caused by wear, due to its good mechanical and electrical property. In this study, we attempt to prepare MMCs with various volume fraction and particle size of $TiB_2$ by means of hot extruded and cold drawn process. Dry sliding wear tests were performed on a pin-on-disk type wear tester, sliding against SM45C under the different applied loads. After wear testing, the microstructures of the worn surfaces were observed by SEM and the microhardnesses of the subsurface zone were measured.

티타늄 합금(Ti-6A1-4V)의 밀링가공에서 L자형 얇은 벽 구조의 가공품질 향상 (Improving Machining Quality of L-Shaped Thin-Walled Structure in Milling Process of Ti-Alloy (Ti-6Al-4V))

  • 김종민;구준영;전차수
    • 한국기계가공학회지
    • /
    • 제20권11호
    • /
    • pp.52-59
    • /
    • 2021
  • Titanium alloy (Ti-alloy) is widely used as a material for core parts of aircraft structures and engines that require both lightweight and heat-resistant properties owing to their high specific stiffness. Most parts used in aircraft have I-, L-, and H-shaped thin-walled structures for weight reduction. It is difficult to machine thin-walled structures owing to vibrations and deformations during machining. In particular, cutting tool damage occurs in the corners of thin-walled structures owing to the rapid increase in cutting force and vibration, and machining quality deteriorates because of deep tool marks on machined surfaces. In this study, milling experiments were performed to derive an effective method for machining a L-shaped thin-walled structure with Ti-alloy (Ti-6Al-4V). Three types of machining experiment were performed. The surface quality, tool wear, cutting force, and vibration were analyzed comprehensively, and an effective machining method in terms of tool life and machining quality was derived.

Corrosion Characteristics of Cell-Covered Ternary Ti-Nb-Ta Alloy for Biomaterials

  • Kim, W.G.;Yu, J.W.;Choe, H.C.;Ko, Y.M.;Park, G.H.
    • Corrosion Science and Technology
    • /
    • 제8권2호
    • /
    • pp.62-67
    • /
    • 2009
  • Ti and Ti-alloys have good biocompatibility, appropriate mechanical properties and excellent corrosion resistance. However, the widely used Ti-6Al-4V is found to release toxic ions (Al and V) into the body, leading to undesirable long-term effects. Ti-6Al-4V has much higher elastic modulus (100 GPa) than cortical bone (20 GPa). Therefore, titanium alloys with low elastic modulus have been developed as biomaterials to minimize stress shielding. The electrochemical behavior of surface-modified and MC3T3-E1 cell-cultured Ti-30(Nb,Ta) alloys with low elastic modulus have been investigated using various electrochemical methods. Surfaces of test samples were treated as follows: $0.3{\mu}m$ polished; $25{\mu}m$, $50{\mu}m$ and $125{\mu}m$ sandblasted. Specimen surfaces were cultured with MC3T3-E1 cells for 2 days. Average surface roughness ($R_a$) and morphology of specimens were determined using a surface profilometer, OM, and FE-SEM. Corrosion behavior was investigated using a potentiostat(EG&G PARSTAT 2273), and electrochemical impedance spectroscopy was performed (10 mHz to 100 kHz) in 0.9% NaCl solution at $36.5{\pm}1^{\circ}C$. The microstructures of the Ti-30(Ta,Nb) alloys had a needle-like appearance. The $R_a$ of polished Ti-30Ta and Ti-30Nb alloys was lower than that of the sandblasted Ti alloy. Cultured cells displayed round shapes. For polished alloy samples, cells were well-cultured on all surfaces compared to sandblasted alloy samples. In sandblasted and cell-cultured Ti-30(Nb,Ta) alloy, the pitting potential decreased and passive current density increased as $R_a$ increased. Anodic polarization curves of cell-cultured Ti alloys showed unstable behavior in the passive region compared to non-cell-cultured alloys. From impedance tests of sandblasted and cell-cultured alloys, the polarization resistance decreased as $R_a$ increased, whereas, $R_a$ for cell-cultured Ti alloys increased compared to non-cell-cultured Ti alloys.