Characteristics of Multilayer Coated $Si_3N_4-TiC$ Ceramic (다중 코팅된 $Si_3N_4-TiC$ 세라믹의 특성)

  • Kim, Dong-Won;Chun, Seong-Sun
    • Korean Journal of Materials Research
    • /
    • v.1 no.1
    • /
    • pp.9-17
    • /
    • 1991
  • TiC coating formed on $Si_3N_4-TiC$ composite ceramic by chemical vapor deposition (CVD) has an improved microstructures, better thermal shock resistance and interfacial bonding than TiN coating does. TiN coating formed by CVD, however, has lower friction coefficients against steels and better chemical stability. The experimental results indicate that the coated insert is superior to the uncoated one in flank and crater wear resistance. And the multilayer coating shows an improved wear resistance than the monolayer coating.

  • PDF

A Study for Cutting Resistance of TiN Coated Tools (TiN 코팅 공구의 절삭저항에 관한 연구)

  • 김광래
    • Journal of the Korean Society of Manufacturing Technology Engineers
    • /
    • v.9 no.2
    • /
    • pp.87-95
    • /
    • 2000
  • By using AIP(Arc Ion Plating) of a physical vapor deposition for the first time in Korea a ceramic tool whose surface is coated single layeredly with TiN is developed. In addition cutting resistance appearing in the process of finishing cut of hardened carbon tool steel STC3 is studied. The principal and radial components of cutting resistance in those cutting conditions appear to be the same or similar and the feed component is relatively small. The feed component is found to be in proportion to cutting width and the radial component in proportion to cutting thickness. Owing to coating the cutting resistance of a TiN coated ceramic tool increas-es compared with that of a general ceramic tool.

  • PDF

Presumption on Wear life of TiN Film (TiN 경질박막의 마모 수명 예측에 관한 연구)

  • 정기훈;이영제
    • Proceedings of the Korean Society of Tribologists and Lubrication Engineers Conference
    • /
    • 1997.04a
    • /
    • pp.41-46
    • /
    • 1997
  • TiN 코팅은 마모에 대한 저항성 및 고체 윤활 효과가 매우 우수하여 내마모성 및 저마찰이 요구되는 절삭공구나 피스톤 베어링 및 각종 축계의 코팅막으로 사용이 증가되고 있다. 일반적으로 재료의 경도와 인성은 서로 상반 관계를 갖고 있어 공학적으로 경도와 인성을 모두 요구하는 표면을 얻기 위해 연질 모재 위의 세라믹 코팅은 그 요구를 만족시킬 수 있는 가장 각광받는 표면처리 방법중의 하나이다. 그러나, TiN과 같은 경질 박막의 공학적 적용시 가장 요구되는 마모수명은 모재의 조도나 경도, 증착 방법, 접촉 상태, 코팅막의 두께 및 마모의 발생 기구 등에 따라 마찰 및 마모 메커니즘의 현저한 차이를 나타내기 때문에 예측이 거의 불가능한 실정이고, 아직까지 이러한 마모수명 비교 평가방법에 대한 기준 설정 및 정량적 정립이 이루어지지 않고 있다. 본 연구에서는 모재의 경도, 조도, 코팅 두께가 다른 TiN 경질 박막에 압입시험과 스크래치시험시 발생되는 균열 발생 메커니즘과 미끄럼 시험시 발생되는 마모 메커니즘의 연계성을 밝히고 압입 및 스크래치 시험시 코팅막이 손상되는 임계하중과 미끄럼 시험시 접촉하중 변화에 따른 마모수명의 정량적 연관성을 찾아보고자 한다.

  • PDF

A Study on the Coated Characteristics of Ceramic Tools (코팅공구의 절삭성능에 관한 연구)

  • 유봉환
    • Journal of the Korean Society of Manufacturing Technology Engineers
    • /
    • v.9 no.1
    • /
    • pp.96-101
    • /
    • 2000
  • Ceramic, PCD and CBN tools are available for the difficult-to-cut-materials such as hardened carbon tool steel, stainless steel, Inconel 718 and etc.. Ceramic toolsare likely to be chipped and abruptly broken before the appearance of normal wear in turning. Ther2efore ceramic tools are suitable for continuous cut in turning not for intermittent in milling. In this study, TiN/TiCN multi-layer coated ceramic tools were found to restrain the chipping, breaking and early fracture and to increase the critical cutting speed owing to TiN/TiCN multi-layer coating in Arc Ion Plating of PVD method.

  • PDF

Wear Behavior of TiN Coatings Deposited on High Speed Steel and Alloy Tool Steel (TiN 코팅된 고속도강과 합금공구강의 마멸거동)

  • 김석삼;서창민;박준목
    • Transactions of the Korean Society of Mechanical Engineers
    • /
    • v.19 no.3
    • /
    • pp.705-712
    • /
    • 1995
  • The wear characteristics and wear mechanisms in TiN coating deposited on high speed steel and alloy tool steel by ion plating were investigated. Pin on V-block wear tester was used for a wear test method. The specimen was composed of three kinds of high speed steel and alloy tool steel which had different hardness by changing the heat treating condition. Three kinds of coating thickness were also applied to each specimen. Microscopic observation of worn surfaces was made by SEM. The scratch test of coating surface by the ion plating showed that critical load to break the coating interface was greater than 50N. The critical load increased with both substrate hardness and coating thickness. The wear resistance of TiN coated high speed steel became 10 times greater than that of non-coated ones. SEM observation showed that leading edge of contact was compressive and trailing edge was under maximum tensile stress and then surface cracking broke out perpendicular to sliding direction.