Low-temperature Synthesis of (TiC+Al2O3) Reinforced Al Matrix Composite Based on Self-combustion Reaction (자발연소반응을 이용한 (TiC+Al2O3)/Al 복합재료의 저온합성)

  • Lee, Jung-Moo;Kim, Su-Hyeon;Cho, Young-Hee;Kim, Je-Woo;Lee, Jae-Chul
    • Korean Journal of Metals and Materials
    • /
    • v.49 no.12
    • /
    • pp.1001-1004
    • /
    • 2011
  • The formation of TiC and $Al_2O_3$ particles based on the self-combustion reaction of the $Al-TiO_2-C-CuO$ system in an Al alloy melt was investigated. With an adequate amount of CuO in the system, a spontaneous reaction occurred within the Al alloy melt at $850^{\circ}C$ and thereafter was self-maintained, producing an Al matrix composite reinforced with thermodynamically stable TiC and $Al_2O_3$ particles. TiC and $Al_2O_3$ particles contributed to a considerable increase in the strength and stiffness, demonstrating the feasibility of this method as a practical application for structural parts.

A Study of (Ba, Sr)$TiO_3$ Synthesis by Direct Wet Process ((Ba, Sr)$TiO_3$ 습식 직접 합성법)

  • 이경희;이병하;김준수
    • Journal of the Korean Ceramic Society
    • /
    • v.23 no.1
    • /
    • pp.27-32
    • /
    • 1986
  • This study is aimed at synthsizing high dielectric material (Ba, Sr)$TiO_3$ through direct wet process. Pure and ultra fine particle of (Ba, Sr)$TiO_3$ Powder was synthesized from $BaCl_2$ $SrCl_2$ and TiCl4 aqeous solution at KOH Solution in the $N_2$ gas atmosphere. $BaCl_2$ $SrCl_2$ and TiCl4 were Mixed with the mole ratio of 1:9, 3:7:10, 5:5:10, 7:3:10, 9:1:10 and sythesized at 4$0^{\circ}C$~9$0^{\circ}C$ for 10min~15hrs. The particle size particle shape crystallinity and synthesis condition of (Ba, Sr)$TiO_3$ powder with the variation of temperature and reaction time in the aqueous solution studied by the exprimental instruments of DTA. TGA, X-ray diffratometer SEM.

  • PDF

Synthesis of (Ti,Al)N Powder by the Direct Nitridation(II) (직접질화법에 의한 (Ti,Al)N계 복합질화물의 합성(II))

  • Cho, Young-Soo;Lee, Young-Ki;Sohn, Yong-Un;Park, Kyong-Ho;Kim, Seok-Yoon
    • Journal of the Korean Society for Heat Treatment
    • /
    • v.9 no.3
    • /
    • pp.219-227
    • /
    • 1996
  • The purpose of this research is to develop the technology for the synthesis of (Ti,Al)N powder, which shows simultaneously the excellent properties of TiN and AlN, from the Ti-Al intermetallic compounds by the direct nitriding method. The effects of variables such as temperature, Ti-Al intermetallic compounds ($TiAl_3$, TiAl and $Ti_3Al$) were investigated by TG, XRD and SEM. The (Ti,Al)N powder can be easily synthesized from the intermetallic compounds by the direct nitriding method. Among the intermetallic compounds, the nitriding behavior increased with TiAl> $Ti_3Al$ > $TiAl_3$, as the difference of diffusion coefficient for nitrogen in each materials. The ternary nitride such as $Ti_2AlN$ and $Ti_3Al_2N_2$ can be synthesized by the direct nitriding method, although the ternary nitride coexist with TiN and AlN. The ternary nitrides are stable below $1400^{\circ}C$, but these are gradually decomposed into TiN and AlN above $1400^{\circ}C$.

  • PDF

Fabrication of SiC-TiC Composites via Mechanochemical Synthesis

  • Park, Heon-Jin;Lee, Ki-Min;Kim, Hyung-Jong;Lee, June-Gunn
    • Journal of the Korean Ceramic Society
    • /
    • v.38 no.4
    • /
    • pp.314-318
    • /
    • 2001
  • SiC-TiC composites have been fabricated by using a mechanochemical processing of a mixture of Si, Ti, and C at room temperature and subsequent hot pressing. TiC powders have been obtained by the mechanochemical processing of a mixture of Ti and C whereas SiC powders has not been obtained from a mixture of Si and C. By using the exothermic reaction between Ti and C, SiC-TiC powder could be obtained from the mixture of Si, Ti, and C using the mechanochemical processing for more than 12h. The X-ray diffraction analysis has shown that the powder subjected to the mechanochemical processing consisted of the particles having crystallite size below 10nm. Fully densified SiC-TiC composites have been obtained by hot-pressing of the powder at 1850$\^{C}$ for 3h and it has shown comparable mechanical properties to those of the SiC-TiC composites prepared from the commercially available SiC and TiC powders. Flexural strength of 560 MPa and fracture toughness of 4.8 MP$.$am$\_$1/2/ have been shown for the SiC-TiC composites with composition corresponding to 0.75:0.25:1 mole ratio of Si:Ti:C.

  • PDF

Synthesis of TiC and TiC-Al Functionally Graded Materials by Electrothermal Combustion (ETC) (통전활성 연소에 의한 TiC와 TiC-Al 경사기능재료 합성)

  • 송인진
    • Journal of Powder Materials
    • /
    • v.4 no.4
    • /
    • pp.291-297
    • /
    • 1997
  • Titanium cabide, TiC-x mole% Al composites, and functionally-graded materials (FGMs) of TiC-x mole% Al were synthesized by an electrothermal combustion (ETC) method. TiC-70 mole% Al composite was not ignited by indirect tungsten coil heating, but can be synthesized by an electrothermal combustion. The velocity of the combustion wave decreased with increasing addition of Al and increased with an increase in the applied electric field. Functionally-graded TiC-Al materials were made from reactant layers with compositions of Ti+C+x moles Al with x ranging from zero to 70 by an electrothermal combustion. In the FGM products a nearly linear change in composition in the graded region was observed in samples with 0$\leq$ x $\leq$ 70 with x being the mole% Al.

  • PDF

Forming Mechanism of TiC Hollow Fibers during Self-Propagating High Temperature Synthesis (자전연소합성 반응중 속빈 TiC 섬유의 형성 기구)

  • 윤존도;방환철
    • Journal of the Korean Ceramic Society
    • /
    • v.37 no.4
    • /
    • pp.332-337
    • /
    • 2000
  • Forming mechanism of fibrous TiC during self-propagating high temperature synthetic reaction was analyzed and suggested. It was revealed that critical temperature for the stable fiber formation was not the melting point of TiC, but the eutectic reaction temperature of TiC and C. Minimum amount of TiC diluent addition required to form fibers was calculated to be 25.6%, which was consistent with the experimental result. Synthesized fibers were found hollow tube-like. The morphology was explained by the diffusion rates of C and Ti in TiC, and by the molar volume chnage of C during the reaction. Expanding shell model was suggested for the hollow fiber formation mechanism.

  • PDF

Synthesis of (Ti,Al)N Powder by Interdiffusion Nitriding Method (상호확산법에 의한 (Ti,Al)N계 복합질화물의 합성)

  • Lee, Young-Ki;Kim, Jung-Yeul;Kim, Dong-Kun;Sohn, Yong-Un
    • Journal of the Korean Society for Heat Treatment
    • /
    • v.10 no.2
    • /
    • pp.138-149
    • /
    • 1997
  • TiN and AlN are ceramic materials with extensive applications due to its excellent mechanical and chemical properties at elevated temperature. The purpose of this research is to develop the method for the synthesis of ternary nitride powder, titanium-aluminum-nitrogen system, which have an excellent property of both TiN and AlN. The ternary nitride such as $Ti_3AlN$, $Ti_2AlN$ and $Ti_3Al_2N_2$ can be synthesized by the interdiffusion nitriding method in Ar gas, however, the ternary nitride coexist with TiN, AlN, $Ti_3Al$ and ${\alpha}$-Ti. The ternary nitride are stable below $1400^{\circ}C$, but these are gradually decomposed into TiN, $Ti_3Al$ and AlN above $1400^{\circ}C$. The thermal oxidation characteristics of the Ti-Al-N compound synthesized by the interdiffusion nitriding method is superior to that of the TiN+AlN mixed powder, and the oxidation for both materials show the differential behaviors.

  • PDF