Search Result 51, Processing Time 0.025 seconds

High-temperature Oxidation of the TiAlCrSiN Film Deposited on the Cemented Hard Carbide

  • Lee, Dong Bok
    • Journal of the Korean institute of surface engineering
    • /
    • v.47 no.5
    • /
    • pp.252-256
    • /
    • 2014
  • The TiAlCrSiN film was deposited on the WC-20%TiC-10%Co carbide, and its oxidation behavior was examined at $700-1000^{\circ}C$. It displayed relatively good oxidation resistance owing to the formation of $TiO_2$, $Al_2O_3$, $Cr_2O_3$, and $SiO_2$ up to $900^{\circ}C$. However, at $1000^{\circ}C$, the fast oxidation rate and partial oxidation of WC in the substrate led to the formation of the thick, fragile oxide scale.

Enhanced Mechanical Properties and Thermal Stability of CrAlN Coatings by Interlayer Deposition (중간층 증착에 의한 CrAlN 코팅의 기계적 물성 및 내열성 향상에 관한 연구)

  • Kim, Hoe-Geun;Ra, Jeong-Hyeon;Song, Myeon-Gyu;Lee, Sang-Yul
    • Proceedings of the Korean Institute of Surface Engineering Conference
    • /
    • 2016.11a
    • /
    • pp.100-100
    • /
    • 2016
  • 물리기상증착방법 (Physical vapor deposition)에 의하여 합성된 천이금속 질화물 박막은 경도, 내마모성 등 절삭공구의 성능을 향상시키며, Ti-Al-N, Ti-Zr-N, Zr-Al-N, Cr-Si-N 등의 3원계 경질 박막에 대한 연구가 지속적으로 이루어지고 있다. 이중에서도 CrAlN 코팅은 높은 경도, 낮은 표면 조도 등의 우수한 기계적 특성 이외에 고온에서 안정한 합금상 형성으로 인하여 우수한 내열성을 보유하여 공구 코팅으로의 적용 가능성이 크다. 그러나 최근 공구사용 환경의 가혹화로 인하여 코팅의 내마모성 및 내열성 등의 물성 향상을 통한 공구의 수명 향상이 필요시 되고 있으며, 코팅에 적합한 중간층을 합성함으로써 공구 코팅으로의 적용 가능성을 높이는 연구들이 진행되고 있다. 본 연구에서는 CrAlN 코팅의 물성을 향상시키기 위해 CrAlN 코팅과 WC-Co 6wt.% 모재 사이에 CrN, CrZrN, CrN/CrZrSiN 등의 다양한 중간층을 합성하였으며, 중간층을 포함한 모든 코팅의 두께는 $3{\mu}m$ 로 제어하였다. 합성된 코팅의 미세조직, 경도 및 탄성계수, 내모성을 분석하기 위해 field emission scanning electron microscopy(FE-SEM), nano-indentation, ball-on-disk 마모시험기 및 ${\alpha}-step$을 사용하였다. 코팅의 내열성을 확인하기 위해 코팅을 furnace에 넣어 공기중에서 500, 600, 700, 800, 900, $1,000^{\circ}C$로 30분 동안 annealing 한 후에 nano-indentation을 사용하여 경도를 측정하였다. CrAlN 코팅을 나노 인덴테이션으로 분석한 결과, 모든 코팅의 경도(35.5-36.2 GPa)와 탄성계수(424.3-429.2 GPa)는 중간층의 종류에 상관없이 비슷한 값을 보인 것으로 확인됐다. 그러나, 코팅의 마찰계수는 중간층의 종류에 따라 다른 값을 보였으며, CrN/CrZrSiN 중간층을 증착한 CrAlN 코팅의 마찰계수는 0.34로 CrZrN 중간층을 증착한 CrAlN 코팅의 마찰계수(0.41)에 비해 낮은 값을 보였다. 또한, 코팅의 마모율 및 마모폭도 비슷한 경향을 보인 것으로 보아, CrN/CrZrSiN 중간층을 합성한 CrAlN 코팅의 내마모성이 상대적으로 우수한 것으로 판단된다. 이것은 중간층의 H/E ratio가 코팅의 내마모성에 미치는 영향에 의한 결과로 사료된다. H/E ratio는 파단시의 최대 탄성 변형율로써, 모재/중간층/코팅의 H/E ratio 구배에 따라 코팅 내의 응력의 완화 정도가 변하게 된다. WC 모재 (H/E=0.040)와 CrAlN 코팅(H/E=0.089) 사이에서 CrN, CrZrSiN 중간층의 H/E ratio 는 각각 0.076, 0.083 으로 모재/중간층/코팅의 H/E ratio 구배가 점차 증가함을 확인 할 수 있었고, 일정 응력이 지속적으로 가해지면서 진행되는 마모시험중에 CrN과 CrZrSiN 중간층이 WC와 CrAlN 코팅 사이에서 코팅 내부의 응력구배를 완화시키는 역할을 함으로써 CrAlN 코팅의 내마모성이 향상된 것으로 판단된다. 모든 코팅을 열처리 후 경도 분석결과, CrN/CrZrSiN 중간층을 증착한 CrAlN 코팅은 $1,000^{\circ}C$까지 약 28GPa의 높은 경도를 유지한 것으로 확인 되었고, 이는 CrZrSiN 중간층 내에 존재하는 $SiN_x$ 비정질상의 우수한 내산화성에 의한 결과로 판단된다.

  • PDF

Study on the Surface Properties of Arc Ion Plated Ti-Al-Cr-N Thin Layers (아크 이온 증착된 Ti-Al-Cr-N 도포층의 표면 물성 연구)

  • Gang, Bo-Gyeong;Choe, Yong;Gwon, Sik-Cheol;Zang, Shi-Hong
    • Proceedings of the Korean Institute of Surface Engineering Conference
    • /
    • 2015.05a
    • /
    • pp.125-125
    • /
    • 2015
  • Ti-Al-Cr-N thin layer was prepared on Fe-Si thin sheet by arc ion plating to improve corrosion and mechanical properties. The compositions ratios of Fe : Cr : Al : Ti : Si : N of the thin layers at $500^{\circ}C$ was 1.24 : 0.56 : 36.82 : 32.72 : 0.59 : 28.07 [wt.%], respectively. The higher arc ion plating temperature was, the higher corrosion resistance and nano-hardness were observed due to chromium content. Corrosion potential and corrosion rate in artificial sea water of the coating layer were in the range of $-39mV_{SHE}$ and $2mA/cm^2$, respectively. Passivity was not observed in the artificial sea water. Nano-hardnesses of the thin layers was increased by adding Cr from 23.6 to 25.8 [GPa]. The friction coefficients and fatigue limits of the layers were 0.388, 0.031, respectively.

  • PDF

Wear properties of (Ti$_{1-x}$Cr$_{x}$)N coatings deposited by ion-plating method (이온 플레이팅법으로 제조한 (Ti$_{1-x}$Cr$_{x}$)N 박막의 마모특성에 관한 연구)

  • 이광희;박찬홍;이정중
    • Journal of the Korean institute of surface engineering
    • /
    • v.34 no.2
    • /
    • pp.125-134
    • /
    • 2001
  • ($Ti_{1-x}$ $Cr_{x}$ )N coatings were deposited by an ion-plating method in a reactor with two separate metal sources, Ti and Cr. Ti was evaporated using an electron beam, while Cr evaporation was carried out by resistant heating. The Ti and Cr concentrations in the coatings were controlled by the Ti and Cr evaporation ratio. The coating hardness increased with increasing the Cr content(x) and showed a maximum value of 6,000 HK at around x=0.8. The critical load of the coatings, measured by the scratch test, was around 30 N. The wear resistance properties of the ($Ti_{1-x}$$Cr_{ x}$)N coatings were evaluated using a CSEM pin-on-disk type tribometer. A Cr-steel ball as well as a SiC ball, which had hardness values of 590 HK and 2,600 HK respectively, were used as the pin. After the wear test, the surface morphology, roughness and the concentration of the coatings were investigated, with the main focus being on the effect of wear debris and the transferred layer on the wear behavior.

  • PDF

Analysis of Electronic Materials Using Transmission Electron Microscopy (TEM) (전자현미경을 이용한 전자재료분석)

  • Kim, Ki-Bum
    • Applied Microscopy
    • /
    • v.24 no.4
    • /
    • pp.132-144
    • /
    • 1994
  • The application of TEM in investigating the evolution of microstructure during solid phase crystallization of the amorphous Si, $Si_{1-x}Ge_x,\;and\;Si_{1-x}Ge_x/Si$ films deposited on $SiO_2$ substrate, in identifying the failure mechanism of the TiN barrier layer in the Cu-metallization scheme, and in comparing the microstructure of the as-deposited Cu-Cr and Cu-Ti alloy films are discussed. First, it is identified that the evolution of microstructure in Si and $Si_{1-x}Ge_x$ alloy films strongly depends on the concentration of Ge in the film. Second, the failure mechanism of the TiN diffusion barrier in the Cu-metallization is the migration of the Cu into the Si substrate, which results in the formation of a dislocation along the Si {111} plane and precipitates (presumably $Cu_{3}Si$) around the dislocation. Finally, the microstructure of the as-deposited Cu-Cr and Cu-Ti alloy films is also quite different in these two cases. From these several cases, we demonstrate that the information which we obtained using TEM is critical in understanding the behavior of materials.

  • PDF

Analysis and Design of half-mirror coating for sunglasses (썬글라스용 반미러(Half-Mirror) 코팅의 분석과 설계)

  • Park, Moon-Chan;Jung, Boo-Young;Hwangbo, Chang-Kwon
    • Journal of Korean Ophthalmic Optics Society
    • /
    • v.8 no.2
    • /
    • pp.111-117
    • /
    • 2003
  • We collected the domestic and foreign half-mirror coating lens for sunglasses. Their reflectance is measured using Spectrophotometer in order to analysis their optical property and the result which is calculated using Macleod program was compared with measured reflectance. In addition, we designed the new half-mirror coating lens with gold color using TiN material and investigated the optical property of the new half-mirror coating lens. The results obtained from analysis of half-mirror coating lenses are as follow : Two-tone half-mirror coating with silver color is fabricated with [air|$SiO_2$(or $Al_2O_3$)|Cr|glass]. The role of $SiO_2$(or $Al_2O_3$) on Cr improve the hardness of the lens and the thickness of the $Al_2O_3$ with 10 nm is good to show the lens silver color. Incase of color half-mirror coating lens. Blue system is designed by [air|$SiO_2$(66.3)|$TiO_2$(129.0)|$SiO_2$(62.9)|$SiO_2$(26.0)|$TiO_2$(120.3)|$SiO_2$(9.1)|glass], gold system [air|$SiO_2$(60.6)|$TiO_2$(86.2)|$SiO_2$(13.5)|$TiO_2$(86.8)|$SiO_2$(214.38)|glass], green system[air|$SiO_2$(74.3)|$TiO_2$(75.8)|$SiO_2$(44.3)|$TiO_2$(11.6)|$SiO_2$(160.8)|$TiO_2$(12.9)|$SiO_2$(183.3)|$TiO_2$(143.8)|glass], silver system[air|$SiO_2$(21.2)|$TiO_2$(49.7)|$SiO_2$(149.3)|glass]. White half-mirror coating lens has [air|$SiO_2$(17 nm)|$TiO_2$(43 nm)(or $ZrO_2$)|$SiO_2$(87 nm)|polysiloxane($4.46{\mu}m$|glass or CR-19]. It has half-mirror coaling lens which has about 19% reflectance and about 80% transmittance in the range of visible light(400~700nm). we designed the new half-mirror coating lens with gold color, the (x, y) value of the CIE is almost similar to the CIE value of [air|$SiO_2$(170 nm)|TiN(15 nm)|glass].

  • PDF

Investigation of the TiCrN Coating Deposited by Inductively Coupled Plasma Assisted DC Magnetron Sputtering. (Inductively Coupled Plasma Assisted D.C. Magnetron Sputtering법으로 제작된 TiCrN 코팅층의 특성 분석)

  • Cha, B.C.;Kim, J.H.;Lee, B.S.;Kim, S.K.;Kim, D.W.;Kim, D.;You, Y.Z.
    • Journal of the Korean Society for Heat Treatment
    • /
    • v.22 no.5
    • /
    • pp.267-274
    • /
    • 2009
  • Titanium Chromium Nitrided (TiCrN) coatings were deposited on stainless steel 316 L and Si (100) wafer by inductively coupled plasma assisted D.C. magnetron sputtering at the various sputtering power on Cr target and $N_2/Ar$ gas ratio. Increasing the sputtering power of Cr target, XRD patterns were changed from TiCrN to nitride $Cr_2Ti$. The maximum hardness was $Hk_{3g}$ 3900 at $0.3\;N_2/Ar$ gas ratio. The thickness of the TiCrN films increased as the Cr target power increased, and it showed over $Hk_{5g}3100$ hardness at 100 W, 150 W. TiCrN films were deposited by the ICP assisted DC magnetron sputtering shown good wear resistance as the $N_2/Ar$ gas ratio was 0.1, 0.3.

Microstructure and Fracture Strength of Si3N4 Joint System (질화 규소 접합체의 미세구조와 파괴 강도에 관한 연구)

  • 차재철;강신후;박상환
    • Journal of the Korean Ceramic Society
    • /
    • v.36 no.8
    • /
    • pp.835-842
    • /
    • 1999
  • Si3N4 -Si3N4 joints were made using Ag-Cu-Ti and Ag-Cu-In-Ti via brazing method and the change in joint strength was investigated after heat treatment at $400^{\circ}C$ or $650^{\circ}C$ for up to 2000h. The initial strength of as-brazed joints with Ag-Cu-In-Ti was lower but the reduction of the strength was less dramatic than that with Ag-Cu-Ti. The joints made of a new brazing alloy Au-Ni-Cr-Mo-Fe which is developed for high temperature applications were heat-treated at $650^{\circ}C$ for 1000h. As the heat treatment time increased the bond strength increased. The results of the joining system with Mo or Cu interlayer showed that the strength of the joint with Mo interlayer was higher but the system incurred problems in joint production Also it was found from oxidation experiment that Ti and In affected the oxidation resistance of brazing alloy.

  • PDF

Characteristics of PECVD-W thin films deposited on $Si_3N_4$ ($Si_3N_4$상에 PECVD법으로 형성한 텅스텐 박막의 특성)

  • 이찬용;배성찬;최시영
    • Journal of the Korean Vacuum Society
    • /
    • v.7 no.2
    • /
    • pp.141-149
    • /
    • 1998
  • The W thin films were deposited on Si3N4 by a PECVD technique. The effects of substrate temperature and gas flow ratio on the properties of the W films were investigated. The deposition of W films were limited by surface reaction at the temperature range of 150>~$250^{\circ}C$, W films had the deposition rate of 150~530 $\AA$/min and stress of 0.85~$14.35\times10 ^9 \textrm {dynes/cm}^2}$ at various substrate temperatures and $SiH_4/WF_6$ flow ratios. $SiH_4/WF_6$ flow ratio affected the deposition rate and stress of the W films, expecially, excessive flow of SiH4 abruptly changed the structure, chemical bonding, and stress of the W films. Among the deposited W films on TiN, Ti, Mo, NiCr and Al adhesion layer, the one on the Al had the best adhesion property.

  • PDF

Effects of Alloying Elements on Hardening of 13Cr Stainless Steels Using Plasma Nitriding Process (플라즈마질화처리에 의한 13Cr 스테인리스강의 표면경화특성에 미치는 질화물형성원소첨가의 영향)

  • ;;;;中田一博
    • Journal of Welding and Joining
    • /
    • v.16 no.1
    • /
    • pp.88-97
    • /
    • 1998
  • The surface characteristics of 13Cr stainless steel systems by plasma nitriding were investigated. The plasma nitriding for the 13Cr steels, in which the nitriding forming elements such as Ti, V, W, Nb, Al, Zr and Si were added about 2~3wt.%, respectively, was performed. In all nitrided specimens, .epsilon.-F $e_{2-3}$N, UPSILON.'-F $e_{4}$N and CrN were detected as the nitrides with the a-Fe in the nitrided layer. VN and .betha.- $W_{2}$N were also detected in 13Cr-3V and 13Cr-3W alloys. The growth of the nitrided layer was controlled by the diffusion process. The thickness of the nitrided layer was similar in the 13Cr-2Nb and 3Zr specimens to that of 13Cr(BM) specimen, while the others exhibited the thinner layer. The activation energy for the growth of the nitrided layer in the temperature range of 773-873K was about 130kJ/mol in 13Cr(BM), 13Cr-2Ti, 3W, 3Al, 3Zr and 3Si alloys. The hardness of the nitrided specimens was significantly increased above Hv1000, comparing to the non-nitrided specimen. The specimens with the nitrided forming elements revealed much higher hardness values and, especially, 13Cr-3Al, 3V and 3Si specimens were significantly hardened up to Hv1300.v1300.0.