티타늄 합금(Ti-6Al-4V)의 조직변화에 따른 기계적 특성 평가 (The Evaluation of Mechanical properties on the Changes of Microstructure for Titanium Alloy (Ti-6Al-4V))

  • 권재도;배용탁;최성종
    • 대한기계학회:학술대회논문집
    • /
    • 대한기계학회 2000년도 추계학술대회논문집A
    • /
    • pp.135-140
    • /
    • 2000
  • The characteristics of mechanical behavior were estimated for Ti-6Al-4V alloy with four kinds of microstructure prepared with heat treatments. For this study, impact test, tensile test and fatigue crack growth test were performed, and then compared mechanical properties on the four microstructures. Furthermore, for quantitative evaluation, fractal dimensions of crack pass were obtained using the box counting method. The main results obtained are summarized as follows. (1) The microstructures exhibited equiaxed microstructure, bimodal-microstructure and lamellar microstructure by heat treatment. (2) The impact absorbed energy and elongation is superior in the bimodal-microstructure, and the hardness and tensile strength are superior in the lamellar microstructure. (3) The fatigue crack growth rate is similar to all microstructures in the low ${\Delta}K$ region. The fatigue crack growth rate of equiaxed microstructure is fastest, and that of lamellar microstructure is lowest in the high ${\Delta}K$ region. (4) The fractal dimension D of lamellar microstructure is higher then that of the equiaxed microstructure and bimodal microstructure.

  • PDF

Ti-6Al-4V 합금의 알칼리 및 열처리가 인산칼슘 침착에 미치는 영향 (Effect of Alkali and Heat Treatments of Ti-6Al-4V Alloy on the Precipitation of Calcium Phosphate)

  • 박재한;임기정;김상목;김병옥;한경윤
    • Journal of Periodontal and Implant Science
    • /
    • 제30권1호
    • /
    • pp.187-203
    • /
    • 2000
  • The precipitation of calcium phosphate on implant surface has been known to accelerate osseointegration and to enhance osseous adaptation. The present study was performed to examine whether the precipitation of calcium phosphate on Ti-6Al-4V alloy could be affected by the immersion in NaOH solution and heat treatment. Ti-6Al-4V alloy plates of $15{\times}3.5{\times}1mm$ in dimension were polished sequentially from #240 to #2,000 emery paper and one surface of each specimen was additionally polished with $0.1{\mu}m$ alumina paste. Polished specimens were soaked in various concentrations of NaOH solution(0.1, 1.0, 3.0, 5.0, 7.0, 10.0 M) at $60^{\circ}C$ for 24 hours for alkali treatment, and 5.0 M NaOH treated specimens were heated for 1 hour at each temperature of 400, 500, 600, 700, $800^{\circ}C$. After the alkali and heat treatments, specimens were soaked in the Hank's solution with pH 7.4 at $36.5^{\circ}C$ for 30days.The surface ingredient change of Ti-6Al-4V alloy was evaluated by thin-film X-ray diffractometer(TF-XRD) and the surface microstructure was observed by scanning electron microscope(SEM), and the elements of surface were analyzed by X-ray photoelectron spectroscopy(XPS). The results were obtained as follows ; 1. The precipitation of calcium phosphate on Ti-6Al-4V alloy was accelerated by the immersion in NaOH solution and heat treatment. 2. In Alkali treatment for the precipitation of calcium phosphate on Ti-6Al-4V alloy, the optimal concentration of NaOH solution was 5.0 M. 3. In heat treatment after alkali treatment in 5.0 M NaOH solution, the crystal formation on alloy surface was enhanced by increasing temperature. In heat treated alloys at $600^{\circ}C$, latticed structure and prominences of calcium phosphate layer were most dense. On heat treated alloy surface at the higher temperature(${\geq}700^{\circ}C$), main crystal form was titanium oxide rather than apatite. The above results suggested that the precipitation of calcium phosphate on the surface of Ti-6Al-4V alloy could be induced by alkali treatment in 5.0 M-NaOH solution and by heat treatment at $600^{\circ}C$.

티타늄과 그 합금의 마찰교반용접기술 현황 (Recent R&D status on friction stir welding of Ti and its alloys)

  • 강덕수;이광진
    • Journal of Welding and Joining
    • /
    • 제33권2호
    • /
    • pp.1-7
    • /
    • 2015
  • This article describes the basic technical concepts for applying the friction stir welding (FSW) process to titanium and its alloys. Titanium and its alloys are demanding applications of FSW. During FSW, a protective atmosphere is needed at the welding region to prevent the joints from oxidation due to the absorption of interstitial elements (O, N, and H) at high temperature. The process parameters for FSW have great influence on the microstructure and properties of the joints. No phase transformation occurred in CP Ti because FSW was achieved below the ${\beta}$-transus temperature. Therefore, the mechanical properties of the joints with CP Ti were governed by recrystallization and grain refinement. Furthermore, the strong crystallographic texture indicating <0001>//ND formed in the stir zone. On the other hands, the phase transformation occurred in Ti-6Al-4V alloy because the process temperature reached above ${\beta}$-transus temperature. For this reason, the mechanical properties of the joints with Ti-6Al-4V alloy were altered by not only recry stallization and grain refinement but also phase transformation during FSW. Engineers who want to get sound FSW joints with Ti-6Al-4V alloy have to pay attention to the control about process conditions.

분말 3D 프린팅된 Ti-6Al-4V 합금의 피로특성에 미치는 후열처리의 영향 (Effect of post heat treatment on fatigue properties of EBM 3D-printed Ti-6Al-4V alloy)

  • 최영신;장지훈;김건희;이창우;김휘준;이동근
    • 한국분말재료학회지
    • /
    • 제25권4호
    • /
    • pp.340-345
    • /
    • 2018
  • Additive manufacturing by electron beam melting is an affordable process for fabricating near net shaped parts of titanium and its alloys. 3D additive-manufactured parts have various kinds of voids, lack of fusion, etc., and they may affect crack initiation and propagation. Post process is necessary to eliminate or minimize these defects. Hot isostatic pressing (HIP) is the main method, which is expensive. The objective of this paper is to achieve an optimum and simple post heat treatment process without the HIP process. Various post heat treatments are conducted for the 3D-printed Ti-6Al-4V specimen below and above the beta transus temperature ($996^{\circ}C$). The as-fabricated EBM Ti-6Al-4V alloy has an ${\alpha}^{\prime}$-martensite structure and transforms into the ${\alpha}+{\beta}$ duplex phase during the post heat treatment. The fatigue strength of the as-fabricated specimen is 400 MPa. The post heat treatment at $1000^{\circ}C/30min/AC$ increases the fatigue strength to 420 MPa. By post heat treatment, the interior pore size and the pore volume fraction are reduced and this can increase the fatigue limit.

생체용 Ti-Zr-Pd계 합금의 양극분극특성 (Anodic Polarization Properties of Ti-Zr-Pd Based Alloys for Biomedical Applications)

  • 정종현
    • 대한치과기공학회지
    • /
    • 제23권1호
    • /
    • pp.21-30
    • /
    • 2001
  • For biomedical applications. Ti-X%Zr-Y%Pd(X: $10{\sim}20$, Y:0.2 or 0.4) based alloys not containing harmful Al and V were newly designed, and polarization curves for their alloys were measured at $37^{\circ}C$ in 5% HCl solution in order to understand effects of Zr on the corrosion. From the results of anodic polarization behavior, it was found that the corrosion resistance increased with increasing Zr content. The results show their potential to develope Ti-based alloys for biomedical materials. The Ti-20%Zr-0.2%Pd alloy shows excellent corrosion resistance and was superior to those of the Ti. Ti-6%Al-4%V ELI alloy, Co-30%Cr-6%Mo alloy and STS 316L stainless steel.

  • PDF

Ti-Ta-Nb계 합금의 세포독성과 생체적합성의 평가 (THE EVALUATION OF CYTOTOXICITY AND BIOCOMPATIBILITY OF TI-TA-NB-BASE ALLOY)

  • 최득철;방몽숙;윤택림
    • 대한치과보철학회지
    • /
    • 제44권2호
    • /
    • pp.250-263
    • /
    • 2006
  • Statement of problem: Ti-alloy has been used widely since it was produced in the United States in 1947 because it has high biocompatibility and anticorrosive characteristics. Purpose: The pure titanium, however, was used limitedly due to insufficient mechanical charateristics and difficult manufacturing process. Our previous study was focused on the development of a new titanium alloy. In the previous study we found that the Ti-Ta-Nb alloy had better mechanical characteristics and similar anticorrosive characteristics to Ti-6Al-4V Material and methods: In this study, the cytotoxicity of the Ti-Ta-Nb alloy was evaluated by MTT assay using MSCs(Mesenchaimal stem cells) and L929 cells(fibroblast cell line). The biocompatibility of the Ti-Ta-Nb alloy was performed by inserting the alloy into the femur of the rabbits and observing the radiological and histological changes surrounding the alloy implant. Results: 1. In the cytotoxicity test using MSCs, the 60% survival rate was observed in pure titanium, 84% in Ti-6Al-4V alloy and 95% in Ti-10Ta-10Nb alloy. 2. In the animal study, the serial follow-up of the radiographs showed no separation or migration revealing gradual bone ingrowth surrounding the implants. Similar radiographic results were obtained among three implant groups pure titanium, Ti-6Al-4V alloy and Ti-10Ta-10Nb alloy. 3. In the histologic examination of the bone block containing the implants. the bone ingrowth was prominent around the implants with the lapse of time. There was no signs of any tissue rejection, degeneration, or inflammation. Active bone ingrowth was observed around the implants. In the comparison of the three groups, the rate of bone ingrowth was better in the Ti-10Ta-10Nb alloy group than those in pure titanium group or Ti-6Al-4V alloy group. In conclusion, Ti-10Ta-10Nb alloy revealed better biocompatibility in survival rate of the cells and bone ingrowth around the implants. Therefore we believe a newly developed Ti-10Ta-10Nb alloy can replace currently used Ti-6Al-4V alloy to increase biocompatibility and to decrease side effects. Conclusion: In conclusion, Ti-10Ta-10Nb alloy revealed better biocompatibility in survival rate of the cells and bone ingrowth around the implants. Therefore we believe a newly developed Ti-10Ta-10Nb alloy can replace currently used Ti-6Al-4V alloy to increase biocompatibility and to decrease side effects.

중엔트로피 합금 기지 위에 적층조형된 스테인리스강과 타이타늄 합금의 접합특성 분석 (Joint Properties of Stainless Steel and Titanium Alloys Additive Manufactured on Medium Entropy Alloys)

  • 박찬웅;;이민규;김정한
    • 한국분말재료학회지
    • /
    • 제26권4호
    • /
    • pp.319-326
    • /
    • 2019
  • Additive manufacturing (AM) is a highly innovative method for joining dissimilar materials for industrial applications. In the present work, AM of STS630 and Ti-6Al-4V powder alloys on medium entropy alloys (MEAs) NiCrCo and NiCrCoMn is studied. The STS630 and Ti64 powders are deposited on the MEAs. Joint delamination and cracks are observed after the deposition of Ti64 on the MEAs, whereas the deposition of STS630 on the MEAs is successful, without any cracks and joint delamination. The microstructure around the fusion zone interface is characterized by scanning electron microscopy and X-ray diffraction. Intermetallic compounds are formed at the interfacial regions of MEA-Ti64 samples. In addition, Vicker's hardness value increased dramatically at the joint interface between MEAs and Ti-6Al-4V compared to that between MEAs and STS630. This result is attributed to the brittle nature of the joint, which can lead to a decrease in the joint strength.

전자기 연속 주조법을 이용한 의료용 타이타늄 합금 제작에 관한 연구 (Fabrication of Titanium alloy by Electromagnetic Continuous Casting (EMCC) Method for Medical Applications)

  • 최수지;이현재;백수현;현승균;정현도;문병문
    • 한국주조공학회지
    • /
    • 제38권1호
    • /
    • pp.9-15
    • /
    • 2018
  • Electromagnetic continuous casting (EMCC) was used to fabricate Ti-6Al-4V alloys with properties suitable for medical applications. Ti-6Al-4V alloy ingots fabricated by EMCC were subjected to heat treatment, such as residual stress removing (RRS), furnace cooling after solution treatment (ST-FC) and water-cooling after solution treatment (ST-WC), in order to obtain characteristics suitable for the standard. After component analysis, the microstructure and mechanical properties (tensile strength and elongation) were evaluated by ICP, gas analysis, OM, SEM, a Rockwell hardness tester and universal testing machine. The Ti-6Al-4V alloy ingot fabricated by EMCC was fabricated without segregation, and the lamellar structure was observed in the RRS and ST-FC specimens. The ST-WC specimen showed only martensite structure. As a result of evaluating the mechanical properties based on the microstructure results, we found that the water-cooled heat treatment condition after the solution treatment was most suitable for the Ti-6Al-4V ELI standard.

Laser Powder Bed Fusion 공정으로 제조된 Ti-6Al-4V 합금의 형상 차이에 따른 기계적 특성 변화 (Effect of Bulk Shape on Mechanical Properties of Ti-6Al-4V Alloy Manufactured by Laser Powder Bed Fusion)

  • 박하음;김연우;이승연;최중호;유지훈;김정기;박정민
    • 한국분말재료학회지
    • /
    • 제30권2호
    • /
    • pp.140-145
    • /
    • 2023
  • Although the Ti-6Al-4V alloy has been used in the aircraft industry owing to its excellent mechanical properties and low density, the low formability of the alloy hinders broadening its applications. Recently, laser-powder bed fusion (L-PBF) has become a novel process for overcoming the limitations of the alloy (i.e., low formability), owing to the high degree of design freedom for the geometry of products having outstanding performance used in high-tech applications. In this study, to investigate the effect of bulk shape on the microstructure and mechanical properties of L-PBFed Ti-6Al-4V alloys, two types of samples are fabricated using L-PBF: thick and thin samples. The thick sample exhibits lower strength and higher ductility than the thin sample owing to the larger grain size and lower residual dislocation density of the thick sample because of the heat input during the L-PBF process.

미세조직적 인자가 밀소둔된 Ti-6Al-4V 합금의 피로 및 피로균열전파 거동에 미치는 영향 (Effect of Microstructural Factors on Fatigue and Fatigue Crack Propagation Behaviors of Mill-Annealed Ti-6Al-4V Alloy)

  • 박상후;김수민;이다은;안수진;김상식
    • 대한금속재료학회지
    • /
    • 제56권12호
    • /
    • pp.845-853
    • /
    • 2018
  • To understand the effect of microstructural factors (i.e., the size of ${\alpha}$ phase, equiaxed vs bimodal structure) on high cycle fatigue (HCF) and fatigue crack propagation (FCP) behaviors of mill-annealed Ti-6Al-4V (Ti64) alloy, three specimens of EQ (equiaxed)-8 (8 indicates the size of ${\alpha}$ grain), BM (bimodal)-8, and BM-16 were studied. The uniaxial HCF and FCP tests were conducted at an R ratio of 0.1 under sinusoidal fatigue loading. The microstructural influence (i.e., EQ vs BM) was not significant on the tensile properties of mill-annealed Ti64 alloy, and showed an increase in tensile strength and elongation with decreasing gauge thickness from 50 mm to 1.3 mm. The microstructure, on the other hand, affected the resistance to HCF substantially. It was found that the EQ structure in mill-annealed Ti64 has better resistance to HCF than the BM structure, as a result of different crack initiation mechanism. Unlike HCF behavior, the effect of microstructural features on the FCP behavior of mill-annealed Ti64 was not significant. Among the three specimens, BM-16 specimen showed the highest near-threshold ΔK value, probably because it had the greatest slip reversibility with large ${\alpha}$ grains. The effect of microstructural factors on the HCF and FCP behaviors of mill-annealed Ti64 alloy are discussed based on fractographic and micrographic observations.