• Title/Summary/Keyword: Three-point Bending

Search Result 492, Processing Time 0.031 seconds

A Study on the Weight-Reduction Design of High-Speed Maglev Carbody made of Aluminum Extrusion and Sandwich Composite Roof (알루미늄 압출재와 샌드위치 복합재 루프를 적용한 초고속 자기부상 열차의 차체 경량화 설계 연구)

  • Kang, SeungGu;Shin, KwangBok;Park, KeeJun;Lee, EunKyu;Yoon, IllRo
    • Transactions of the Korean Society of Mechanical Engineers A
    • /
    • v.38 no.10
    • /
    • pp.1093-1100
    • /
    • 2014
  • The purpose of this paper is to suggest a weight-reduction design method for the hybrid carbody of a high-speed maglev train that uses aluminum extrusion profiles and sandwich composites. A sandwich composite was used on the roof as a secondary member to minimize the weight. In order to assemble the sandwich composite roof and aluminum extrusion side frame of the carbody using welding, a guide aluminum frame located at the four sides of the sandwich composite roof was introduced in this study. The clamping force of this guide aluminum frame was verified by three-point bending test. The structural integrity and crashworthiness of the hybrid carbody of a high-speed maglev train were evaluated and verified according to the Korean Railway Safety Law using a commercial finite element analysis program. The results showed that the hybrid carbody composed of aluminum extrusion frames and a sandwich composite roof was lighter in weight than a carbody made only of aluminum extrusion profiles and had better structural performance.

The Effect of Fiber Volume Fraction on the Tension Softening Behavior of Steel Fiber-Reinforced Ultra High Strength Concrete (섬유혼입률이 강섬유보강 초고강도 콘크리트의 인장연화거동에 미치는 영향)

  • Kang, Su-Tae;Hong, Ki-Nam;Han, Sang-Hoon;Kim, Sung-Wook
    • Journal of the Korea Concrete Institute
    • /
    • v.21 no.1
    • /
    • pp.13-20
    • /
    • 2009
  • The influence of steel fiber volume on the tension softening behavior in steel fiber-reinforced ultra high strength concrete was investigated. Three-point bending test (TPBT) with notched beams was performed and inverse analysis method by Uchida et al. was adopted to obtain the tension softening behaviors from the results of TPBT. It could be found that the intial stiffness was constant regardless of steel fiber volume, the increase of steel fiber volume fraction made the tensile strength higher, but all of the curves converged on an asymptote with a crack width. It was proposed the equation of softening curve expressed by combination of plastic behavior part and exponential descending behavior part considering the steel fiber volume fraction and $\omega_0$, which is corresponding to the maximum crack width of plastic area. Thereafter, the crack propagation analysis using finite element method with smeared crack model was also carried out and it was confirmed that the proposed equation had a good agreement with the experimental results.

Effects of incorporation of 2.5 and 5 wt% TiO2 nanotubes on fracture toughness, flexural strength, and microhardness of denture base poly methyl methacrylate (PMMA)

  • Naji, Sahar Abdulrazzaq;Behroozibakhsh, Marjan;Kashi, Tahereh Sadat Jafarzadeh;Eslami, Hossein;Masaeli, Reza;Mahgoli, Hosseinali;Tahriri, Mohammadreza;Lahiji, Mehrsima Ghavvami;Rakhshan, Vahid
    • The Journal of Advanced Prosthodontics
    • /
    • v.10 no.2
    • /
    • pp.113-121
    • /
    • 2018
  • PURPOSE. The aim of this preliminary study was to investigate, for the first time, the effects of addition of titania nanotubes ($n-TiO_2$) to poly methyl methacrylate (PMMA) on mechanical properties of PMMA denture base. MATERIALS AND METHODS. $TiO_2$ nanotubes were prepared using alkaline hydrothermal process. Obtained nanotubes were assessed using FESEM-EDX, XRD, and FT-IR. For 3 experiments of this study (fracture toughness, three-point bending flexural strength, and Vickers microhardness), 135 specimens were prepared according to ISO 20795-1:2013 (n of each experiment=45). For each experiment, PMMA was mixed with 0% (control), 2.5 wt%, and 5 wt% nanotubes. From each $TiO_2$:PMMA ratio, 15 specimens were fabricated for each experiment. Effects of $n-TiO_2$ addition on 3 mechanical properties were assessed using Pearson, ANOVA, and Tukey tests. RESULTS. SEM images of $n-TiO_2$ exhibited the presence of elongated tubular structures. The XRD pattern of synthesized $n-TiO_2$ represented the anatase crystal phase of $TiO_2$. Moderate to very strong significant positive correlations were observed between the concentration of $n-TiO_2$ and each of the 3 physicomechanical properties of PMMA (Pearson's P value ${\leq}.001$, correlation coefficient ranging between 0.5 and 0.9). Flexural strength and hardness values of specimens modified with both 2.5 and 5 wt% $n-TiO_2$ were significantly higher than those of control ($P{\leq}.001$). Fracture toughness of samples reinforced with 5 wt% $n-TiO_2$ (but not those of 2.5% $n-TiO_2$) was higher than control (P=.002). CONCLUSION. Titania nanotubes were successfully introduced for the first time as a means of enhancing the hardness, flexural strength, and fracture toughness of denture base PMMA.

COMPARISON OF MECHANICAL PROPERTIES IN 4 INDIRECT COMPOSITE RESIN (4종의 간접법용 복합 레진의 기계적 특성 비교)

  • Kim, Kil-Soo;Yoon, Tae-Ho;Song, Kwang-Yeob;Ahn, Seung-Geun
    • The Journal of Korean Academy of Prosthodontics
    • /
    • v.45 no.1
    • /
    • pp.21-33
    • /
    • 2007
  • Statement of problem: The esthetic component of dental care has become increasingly more important, while new tooth-colored materials are continually marketed. Various new indirect composite materials have been developed with required advantages. The most recent development in the indirect composites has been the introduction of the second-generation laboratory composite or poly-glass materials. They are processed by different laboratory techniques based on combinations of heat, pressure, vacuum and light polymerization. Although, second generation products became available in 1995, their characteristics and clinical performance have not been adequately investigated. Purpose: The aim of this study was to measure the mechanical properties of the second generation indirect resin system and compare these with an existing universal direct composite resin. Material and method: In this study four indirect composite material (Adoro LC, BelleGlass HP, Tescera, Synfony) were tested for flexural strength, wear resistance, hardness and their degree of conversion against Z250, a light cure direct composite. Results: Within the limitations of this study, the following conclusions were drawn: 1. From the abrasion wear result, Adoro showed the least volume loss while Synfony showed the greatest volume loss. Z250 and BelleGlass HP didn't show significant difference (p>0.05), but they showed significant difference with other groups (p<0.05). From the attrition wear, BelleGlass HP showed the least volume loss and it didn’t show significant difference with Tescera (p>0.05). While Synfony showed the greatest volume loss that it showed significant difference with other groups (p>0.05). 2. Mean values of flexural strength by means of three point bending test was in the order of Z250, Adoro, Belleglass HP, Tescera and Synfony. Mean elastic modulus was in the order of Z250, BelleGlass HP, Tescera, Adoro and Synfony. 3. The result of Vicker‘s microhardness value showed that significantly higher value in Z250 (p<0.05), and is in the order of BelleGlass HP, Tescera, Adoro and Synfony. 4. The degree of conversion measured by FT-IR showed significantly higher value in BelleGlass HP (p<0.05), and is in the order of Adoro, Synfony, Tescera and Z250. Conclusion: Significant differences were found in the flexural strength, wear resistance, hardness and their degree of conversion.

THE THREE DIMENSIONAL FINITE ELEMENT ANALYSIS OF THE BONE ANCHORED FIXED PROSTHESIS ACCORDING TO THE LOAD CONDITION (골유착 고정성 보철물 하에서 하중조건에 따른 삼차원 유한요소법적 분석)

  • Yang, Soon-Ik;Chung, Chae-Heon
    • The Journal of Korean Academy of Prosthodontics
    • /
    • v.33 no.4
    • /
    • pp.780-806
    • /
    • 1995
  • The purpose of this study was to describe the application of 3D finite element analysis to determine resultant stresses on the bone anchored fixed prosthesis, implants and supporting bone of the mandible according to fixture numbers and load conditions. 4 or 6 fixtures and the bone anchored fixed prosthesis were placed in 3D finite element mandibular arch model which represents an actual mandibular skull. A $45^{\circ}$ diagonal load of 10㎏ was labiolingually applied in the center of the prosthesis(P1). A $45^{\circ}$ diagonal load of 20㎏ was buccolingually applied at the location of the 10mm or 20mm cantilever posterior to the most distal implant(P2 or P3). The vertical distribution loads were applied to the superior surfaces of both the right and the left 20mm cantilevers(P4). In order that the boundary conditions of the structure were located to the mandibular ramus and angle, the distal bone plane was to totally fixed to prevent rigid body motion of the entire model. 3D finite element analysis was perfomed for stress distribution and deflection on implants and supporting bone using commercial software(ABAQUS program. for Sun-SPARC Workstation. The results were as follows : 1. In all conditions of load, the hightest tensile stresses were observed at the metal lates of prostheses. 2. The higher tensile stresses were observed at the diagonal loads rather than the vertical loads 3. 6-implants cases were more stable than 4-implants cases for decreasing bending and torque under diagonal load on the anterior of prosthesis. 4. From a biomechanical perspective, high stress developed at the metal plate of cantilever-to-the most distal implant junctions as a consequence of loads applied to the cantilever extension. 5. Under diagonal load on cantilever extension, the 6-implants cases had a tendency to reduce displacement and to increase the reaction force of supporting point due to increasing the bendign stiffness of the prosthesis than 4-implants cases. 6. Under diagonal load on cantilever extension, the case of 10mm long cantilever was more stable than that of 20mm long cnatilever in respect of stress distribution and displacement. 7. When the ends of 10mm or 20mm long cantilever were loaded, the higher tensile stress was observed at the second most distal implant rather than the first most distal implant. 8. The 6-implants cases were more favorable about prevention of screw loosening under repeated loadings because 6-implants cases had smaller deformation and 4-implants cases had larger deformation.

  • PDF

Fatigue Strength Evaluation of Steel-Concrete Composite Bridge Deck with Corrugated Steel Plate (절곡강판을 이용한 교량용 강-콘크리트 합성 바닥판의 피로 성능평가)

  • Ahn, Jin Hee;Sim, Jung Wook;Jeong, Youn Joo;Kim, Sang Hyo
    • Journal of Korean Society of Steel Construction
    • /
    • v.20 no.6
    • /
    • pp.731-740
    • /
    • 2008
  • This paper deals with the fatigue behavior and strength of a new-type of steel-concrete composite bridge deck. The new-type composite bridge deck consists of corrugated steel plate, welded T-beams, stud-type shear connectors and reinforced concrete filler. A total of eight composite bridge deck specimens were fabricated, the fatigue tests were conducted under four-point bending test with three different stress ranges in constant amplitude. According to the test results, the fatigue crack generated at the welding part of the corrugated steel plate, progressed down to the bottom of the steel plate and encountered the crack, which came out from the opposite side at the same position. After the two cracks were connected at the bottom of the steel plate, the lower flange was cut off and the fatigue crack developed up to the T-beam. And the displacements and strains of fatigue test specimens were increasing with cyclic loading number, these were changed sharply at the fatigue failure. The fatigue results are compared with the design S-N curves specified in the Korea Highway Bridge Design Specifications and data in NCHRP 102 and NCHRP 147 report. The new-type composite bridge deck has a stress category of C, which means that new-type composite bridge deck can be designed by the current fatigue design specifications provided for steel members.

Effect of Fiber Type and Combination on the Reinforcement of Heat Polymerized Denture Base Resin (섬유의 종류와 조합이 열중합 의치상 레진의 강화에 미치는 영향)

  • Yu, Sang-Hui;Kim, Young-Im
    • Journal of dental hygiene science
    • /
    • v.10 no.6
    • /
    • pp.445-450
    • /
    • 2010
  • The aim of this study was to evaluate the effect according to the fiber type and combination on the reinforcement of heat-polymerized denture base resin. The heat-polymerized resin(Vertex RS, Dentimax, Netherlands) was used in this study. Glass fiber(GL; ER 270FW, Hankuk Fiber Glass, Korea), polyaromatic polyamide fiber(PA; aramid; Kevlar-49, Dupont, U.S.A.) and ultra high molecular weight polyethylene fiber(PE, polyethylene; P.E, Dong Yang Rope, Korea) were used to reinforce the denture base resin specimens. The final size of test specimen was $64mm{\times}10mm{\times}3.3mm$. The specimens of each group were stored in distilled water at $37^{\circ}C$ for 50 hours before measurement. The flexural strength and flexural modulus were measured by an universal testing machine(Z020, Zwick, Germany) at a crosshead speed of 5 mm/min in a three-point bending mode. In this study, all fibers showed reinforcing effects on denture base resin(p<0.05). In terms of flexural strength and flexural modulus, glass fiber 5.3 vol.% showed most effective reinforcing effect on heat polymerized denture base resin. For flexural modulus, PA/GL was the highest in denture base resin specimen for hybrid FRC using two combination (p<0.05). Glass fiber 5.3 vol.% and PA/GL are considered to be applied effectively in reinforcing the heat polymerized denture base resin.

Thermal Shock Properties of 316 Stainless Steel (316 스테인레스강의 열충격 특성)

  • Lee, Sang-Pill;Kim, Young-Man;Min, Byung-Hyun;Kim, Chang-Ho;Son, In-Soo;Lee, Jin-Kyung
    • Journal of Ocean Engineering and Technology
    • /
    • v.27 no.5
    • /
    • pp.22-27
    • /
    • 2013
  • The present work dealt with the high temperature thermal shock properties of 316 stainless steels, in conjunction with a detailed analysis of their microstructures. In particular, the effects of the thermal shock temperature difference and thermal shock cycle number on the properties of 316 stainless steels were investigated. A thermal shock test for 316 stainless steel was carried out at thermal shock temperature differences from $300^{\circ}C$ to $1000^{\circ}C$. The cyclic thermal shock test for the 316 stainless steel was performed at a thermal shock temperature difference of $700^{\circ}C$ up to 100 cycles. The characterization of 316 stainless steels was evaluated using an optical microscope and a three-point bending test. Both the microstructure and flexural strength of 316 stainless steels were affected by the high-temperature thermal shock. The flexural strength of 316 stainless steels gradually increased with an increase in the thermal shock temperature difference, accompanied by a growth in the grain size of the microstructure. However, a thermal shock temperature difference of $800^{\circ}C$ produced a decrease in the flexural strength of the 316 stainless steel because of damage to the material surface. The properties of 316 stainless steels greatly depended on the thermal shock cycle number. In other words, the flexural strength of 316 stainless steels decreased with an increase in the thermal shock cycle number, accompanied by a linear growth in the grain size of the microstructure. In particular, the 316 stainless steel had a flexural strength of about 500 MPa at 100 thermal-shock cycles, which corresponded to about 80% of the strength of the as-received materials.

Fracture toughness of high performance concrete subjected to elevated temperatures Part 2 The effects of heating rate, exposure time and cooling rate

  • Zhang, Binsheng;Cullen, Martin;Kilpatrick, Tony
    • Advances in concrete construction
    • /
    • v.5 no.5
    • /
    • pp.513-537
    • /
    • 2017
  • In this study, the fracture toughness $K_{IC}$ of high performance concrete (HPC) was investigated by conducting three-point bending tests on a total of 240 notched beams of $500mm{\times}100mm{\times}100mm$ subjected to heating temperatures up to $450^{\circ}C$ with exposure times up to 16 hours and various heating and cooling rates. For a heating rate of $3^{\circ}C/min$, $K_{IC}$ for the hot concrete sustained a monotonic decrease trend with the increasing heating temperature and exposure time, from $1.389MN/m^{1.5}$ at room temperature to $0.942MN/m^{1.5}$ at $450^{\circ}C$ for 4-hour exposure time, $0.906MN/m^{1.5}$ for 8-hour exposure time and $0.866MN/m^{1.5}$ for 16-hour exposure time. For the cold concrete, $K_{IC}$ sustained a two-stage decrease trend, dropping slowly with the heating temperature up to $150^{\circ}C$ and then rapidly down to $0.869MN/m^{1.5}$ at $450^{\circ}C$ for 4-hour exposure time, $0.812MN/m^{1.5}$ for 8-hour exposure time and $0.771MN/m^{1.5}$ for 16-hour exposure time. In general, the $K_{IC}$ values for the hot concrete up to $200^{\circ}C$ were larger than those for the cold concrete, and an inverse trend was observed thereafter. The increase in heating rate slightly decreased $K_{IC}$, and at $450^{\circ}C$ $K_{IC}$ decreased from $0.893MN/m^{1.5}$ for $1^{\circ}C/min$ to $0.839MN/m^{1.5}$ for $10^{\circ}C/min$ for the hot concrete and from $0.792MN/m^{1.5}$ for $1^{\circ}C/min$ to $0.743MN/m^{1.5}$ for $10^{\circ}C/min$ for the cold concrete after an exposure time of 16 hours. The increase in cooling rate also slightly decreased $K_{IC}$, and at $450^{\circ}C$ $K_{IC}$ decreased from $0.771MN/m^{1.5}$ for slow cooling to $0.739MN/m^{1.5}$ for fast cooling after an exposure time of 16 hours. The fracture energy-based fracture toughness $K_{IC}$' was also assessed, and similar decrease trends with the heating temperature and exposure time existed for both hot and cold concretes. The relationships of two fracture toughness parameters with the weight loss and the modulus of rapture were also evaluated.

Numerical Simulation of 72m-Long Ultra High Performance Concrete Pre-Stressed Box Girder (72m 초고강도 콘크리트 프리스트레스트 박스 거더의 수치 해석)

  • Mai, Viet-Chinh;Han, Sang Mook
    • Journal of the Computational Structural Engineering Institute of Korea
    • /
    • v.35 no.2
    • /
    • pp.73-82
    • /
    • 2022
  • The study presents a three-dimensional approach to simulate the nonlinear behavior of a 72 m long Ultra High Performance Fiber Reinforced Concrete (UHPFRC) pre-stressed box girder for a pedestrian bridge in Busan, South Korea. The concrete damage plasticity (CDP) model is adopted to model the non-linear behavior of the UHPFRC material, in which the material properties are obtained from uniaxial compressive and tensile tests. The simulation model based on the proposed stress-strain curve is validated by the results of four-point bending model tests of a 50 m UHPFRC pre-stressed box girder. The results from the simulation models agree with the experimental observations and predict the flexural behavior of the 50 m UHPFRC pre-stressed box girder accurately. Afterward, the validated model is utilized to investigate the flexural behavior of the 72 m UHPFRC pre-stressed box girder. Here, the load-deflection curve, stress status of the girder at various load levels, and connection details is analyzed. The load-deflection curve is also compared with design load to demonstrate the great benefit of the slender UHPFRC box girder. The obtained results demonstrate the applicability of the nonlinear finite element method as an appropriate option to analyze the flexural behavior of pre-stressed long-span girders.