크롬박막 스트레인 게이지의 열처리 특성 (Anneling Characteristics of Chromium Thin Film Strain Gauges)

  • 강경두;김순철;박정도;정귀상
    • 대한전기학회:학술대회논문집
    • /
    • 대한전기학회 1998년도 하계학술대회 논문집 D
    • /
    • pp.1540-1542
    • /
    • 1998
  • This paper presents the deposition and anneling characteristics of Cr thin film strain gaugs, which were deposited on glass by DC magnetron sputtring. The optimzed deposition conditions of Cr thin films were the input DC power, 7 W/$cm^2$ and the Ar vacuuming pressure, 9 mTorr, GF, TCR and TCS of Cr thin film strain gauges were 5.86, 400 ppm/$^{\circ}C$ and $\approx$0 ppm/$^{\circ}C$ respectively. The anneling conditions were investigated with the thinkness rang (1200 $\sim$ 3500$\AA$) of Cr thin films, anneling temperature (100 $\sim$ $300^{\circ}C$) and anneling time (24 $\sim$ 72hr). The maximum resistivity and the minimum TCR value were 1757.03 ${\mu}{\Omega}$cm, -194.07 ppm/$^{\circ}C$, respectively.

  • PDF

고효율 마그네트론 스퍼트링 캐소드의 설계 및 박막 제작 특성 (Thin films made by magnetron sputtering cathode with wide target erosion)

  • 박장식;이원건;정민기;박이순;안창규
    • 한국전기전자재료학회:학술대회논문집
    • /
    • 한국전기전자재료학회 2007년도 추계학술대회 논문집
    • /
    • pp.365-366
    • /
    • 2007
  • High quality cathode with high deposition rate of thin films and long target life time is required for manufacturing TFT-LCD and semiconductor. We developed WV(wide view) sputtering cathode with wide erosion area and high deposition rate. Ti thin film thickness variation in WV cathode is below 5% for 380 kWh target life time. Al thin film thickness using normal cathode is decreased about 20%. By using WV cathode, target using efficiency was improved 40%. in comparison with normal cathode.

  • PDF

Possibility of Magnetocapacitor for Multilayered Thin Films

  • Hong, Jong-Soo;Yoon, Sung-Wook;Kim, Chul-Sung;Shim, In-Bo
    • Journal of Magnetics
    • /
    • 제17권2호
    • /
    • pp.78-82
    • /
    • 2012
  • CoNiFe(CNF)/$BaTiO_3(BTO)$/CoNiFe(CNF) multilayered thin films were deposited on Pt/Ti/$SiO_2$/Si substrates by using pulsed laser deposition (PLD) system. We fabricated three different thin films of BTO, BTO/CNF and CNF/BTO/CNF for magneto-capacitor and studied their crystalline structure, surface and interface morphology, and magnetic and electrical properties. When three different structures of multilayered thin film were compared, magnetization of CNF/BTO/CNF thin films was decreased by magnetic and dielectric interaction. Also we confirmed that capacitance of CNF/BTO/CNF multilayered thin film was enhanced as being near tetragonal structure with increasing of c/a ratio because of atomic bonding at interface between BTO dielectric and CNF magnetic materials. Finally, we studied the change of the capacitance of CNF/BTO/CNF multilayered thin film with magnetic field for emergence of magnetocapacitance and suggested a possibility of enhanced capacitance.

Preparation of Novel Magnesium Precursors and MgO Thin Films Growth by Atomic Layer Deposition (ALD)

  • Kim, Hyo-Suk;park, Bo Keun;Kim, Chang Gyoun;Son, Seung Uk;Chung, Taek-Mo
    • 한국진공학회:학술대회논문집
    • /
    • 한국진공학회 2014년도 제46회 동계 정기학술대회 초록집
    • /
    • pp.364.2-364.2
    • /
    • 2014
  • Magnesium oxide (MgO) thin films have attracted great scientific and technological interest in recent decades. Because of its distinguished properties such as a wide band gap (7.2 eV), a low dielectric constant (9.8), a low refractive index, an excellent chemical, and thermal stability (melting point=$2900^{\circ}C$), it is widely used as inorganic material in diverse areas such as fire resistant construction materials, optical materials, protective layers in plasma display panels, buffer layers of multilayer electronic/photonic devices, and perovskite ferroelectric thin films. Precursor used in the ALD requires volatility, stability, and low deposition temperature. Precursors using a heteroleptic ligands with different reactivity have advantage of selective reaction of the heteroleptic ligands on substrate during ALD process. In this study, we have synethesized new heteroleptic magnesium precursors ${\beta}$-diketonate and aminoalkoxide which have been widely used for the development of precursor because of the excellent volatility, chelating effects by increasing the coordination number of the metal, and advantages to synthesize a single precursor. A newly-synthesized Mg(II) precursor was adopted for growing MgO thin films using ALD.

  • PDF

다공성 니켈 나노 구조체를 이용한 3차원 그래핀의 합성 (Synthesis of Three-Dimensional Graphene Using Porous Nickel Nanostructure)

  • 송우석;명성;이선숙;임종선;안기석
    • Composites Research
    • /
    • 제29권4호
    • /
    • pp.151-155
    • /
    • 2016
  • 그래핀은 저차원 구조에서 기인하는 우수한 특성으로 인해 슈퍼커패시터의 전극소재로 응용이 가능한 소재이다. 본 연구에서는 2차원 구조인 그래핀의 비 표면적 향상을 위해 다공성 니켈 나노구조체 표면에 열 화학기상증착법과 마이크로웨이브 플라즈마 화학기상증착법을 이용하여 3차원의 그래핀을 합성하였다. 주사전자현미경, 라만 분광법, X-선 광전자 분광법을 통해 합성된 그래핀의 구조적, 화학적 특성을 분석한 결과, 3차원 구조의 우수한 결정성을 지니는 다중층 그래핀이 다양한 기판 위에 합성된 것을 확인할 수 있었다.

TiN 나노 박막을 코팅한 AL7075-T7351 알루미늄 합금의 트라이볼로지 특성에 관한 연구 (A Study on the Tribological Characteristics of AL7075-T7351 Aluminum Alloy Coated with TiN Nano Thin Film)

  • 김광수;임성훈;김도현;박형준;허선철
    • 한국산업융합학회 논문집
    • /
    • 제26권5호
    • /
    • pp.743-750
    • /
    • 2023
  • Aluminum alloy is a material widely used in the aircraft industry. However, since it has relatively low hardness, strength and tribological properties, it is necessary to improve these properties. In this paper, a TiN thin film was coated on the surface of AL7075-T7351 using DC magnetron sputtering. The coating was performed by setting different deposition pressure, deposition time, and applied power. Then, the tribological properties of the thin film were investigated. As a result of the experiment, the hardness of the thin film was higher than that of the base material, and the specimen with the highest hardness had excellent friction coefficient, wear amount, and adhesive strength characteristics. Through this study, it was confirmed that the tribological characteristics of aluminum alloy can be improved by depositing thin films using DC magnetron sputtering.

Feature Scale Simulation of Selective Chemical Vapor Deposition Process

  • Yun, Jong-Ho
    • 한국진공학회지
    • /
    • 제4권S1호
    • /
    • pp.190-195
    • /
    • 1995
  • The feature scale model for selective chemical vapor deopsition process was proposed and the simulation was performed to study the selectivity and uniformity of deposited thin film using Monte Carlo method and string algorithm. The effect of model parameters such as sticking coefficient, aspect ratio, and surface diffusion coefficient on the deposited thin film pattern was improved for lower sticking coefficient and higher aspect ratio. It was revealed that the selectivity loss ascrives to the surface diffusion. Different values of sticking coefficients on Si and on SiO2 surface greatly influenced the deopsited thin film profile. In addition, as the lateral wall angle decreased, the selectively deposited film had improved uniformity except the vicinity of trench wall. The optimum eondition for the most flat selective film deposition pattern is the case with low sticking coefficient and slightly increased surface diffusion coefficient.

  • PDF

Microwave Plasma Process에 의한 N-Hexane으로부터 다이아몬드 박막제작 및 특성 (Fabrication and Properties of Diamond Thin-Film from N-Hexane by Using Microwave Plasma Process)

  • 한상보;권태진;박상현;박재윤;이승지
    • 조명전기설비학회논문지
    • /
    • 제25권4호
    • /
    • pp.79-87
    • /
    • 2011
  • In this paper, the best conditions for the deposition of the high quality diamond thin-film from N-hexane as a carbon source in the microwave plasma process was carried out. Major parameters are the deposition time, flow rates of oxygen and hexane. The deposition time for the steady state thin-film was required more than 4[h], and the suitable flow rates of hexane and oxygen for the high-quality thin-film are 0.4[sccm] and 0.1~0.2[sccm], respectively. In addition, amorphous carbons such as DLC and graphite were grown by increasing the flow rate of hexane, and it decreased by increasing the flow rate of oxygen. Specifically, the growth rate is about 1.5[${\mu}mh-1$] under no addition of oxygen and it decreased about 60[%] as ca. 1.0[${\mu}mh-1$] with oxygen.

Influence of $TiO_2$ Thin Film Thickness and Humidity on Toluene Adsorption and Desorption Behavior of Nanoporous $TiO_2/SiO_2$ Prepared by Atomic Layer Deposition (ALD)

  • Sim, Chae-Won;Seo, Hyun-Ook;Kim, Kwang-Dae;Park, Eun-Ji;Kim, Young-Dok;Lim, Dong-Chan
    • 한국진공학회:학술대회논문집
    • /
    • 한국진공학회 2012년도 제42회 동계 정기 학술대회 초록집
    • /
    • pp.268-268
    • /
    • 2012
  • Adsorption and desorption of toluene from bare and $TiO_2$-coated silica with a mean pore size of 15 nm was studied using breakthrough curves and temperature programmed desorption. Thicknesses of $TiO_2$ films prepared by atomic layer deposition on silica were < 2 nm, and ~ 5 nm, respectively. For toluene adsorption, both dry and humid conditions were used. $TiO_2$-thin film significantly improved toluene adsorption capacity of silica under dry condition, whereas desorption of toluene from the surface as a consequence of displacement by water vapor was more pronounced for $TiO_2$-coated samples with respect to the result of bare ones. In the TPD experiments, silica with a thinner $TiO_2$ film (thickness < 2 nm) showed the highest reactivity for toluene oxidation to $CO_2$ in the absence and presence of water. We show that the toluene adsorption and oxidation reactivity of silica can be controlled by varying thickness of $TiO_2$ thin films.

  • PDF

Synthesis of Li2PtO3 Thin Film Electrode by an Electrostatic Spray Deposition Technique

  • Oh, Heung-Min;Kim, Ji-Young;Lee, Kyung-Keun;Chung, Kyung-Yoon;Kim, Kwang-Bum
    • Journal of Electrochemical Science and Technology
    • /
    • 제1권1호
    • /
    • pp.45-49
    • /
    • 2010
  • $Li_2PtO_3$ thin film electrodes, which might be possible candidate for the cathode materials for implantable batteries, were synthesized using an electrostatic spray deposition (ESD) technique onto a platinum foil substrate. Single phase $Li_2PtO_3$with a structure similar to layered $LiCoO_2$ structure were synthesized by spraying a precursor solution of $CH_3CO_2Li2H_2O$ in ethanol onto a Pt substrate at temperatures ranging from 200 to $400^{\circ}C$ followed by annealing at above $600^{\circ}C$. Lithium carbonate was the only major phase at temperatures up to $500^{\circ}C$. The X-ray diffraction (XRD) peaks of the Pt foil substrate and lithium carbonate disappeared at temperatures >$600^{\circ}C$. The volumetric capacity of the $Li_2PtO_3$ thin film synthesized using the ESD technique was approximately 817 mAh/$cm^3$, which exceeded that of $LiCoO_2$ (711 mAh/$cm^3$).