전기화학적 방법에 의한 내열강의 열화도측정 제2보 : 열화도측정치에 미치는 측정조건들의 영향과 기계적성질 변화에 대해서 (Degradation Degree Evaluation of Heat Resisting Steel by Electrochemical Technique Part 2 : Effect of Testing Conditions on Evaluation Value of Degradation Degree and Changes of Mechaical Properties)

  • 정희돈;권영각;장래웅
    • 대한기계학회논문집
    • /
    • 제17권2호
    • /
    • pp.300-312
    • /
    • 1993
  • The material deterioration of service-exposed boiler tube steels in fossil power plant was evaluated by using the electrochemical technique namely, modified electrochemical potentiokinetic reactivation(EPR). It was focused that the passivation of Mo$_{6}$C carbide which governs the mechanical properties of Mo alloyed steels did not occur even in the passivity region of steel in sodium molybdate solution and the reactivation peak current (Ip) observed as the result of non-passivation indicating the precipitation of Mo$_{6}$C carbides. To obtain the optimal test conditions for the field test by using the specially designed electrochemical cell, the effects of scan rate, the surface roughness and the pH of electrolyte on Ip value were also investigated. Furthermore, the change of mechanical properties occurred during the long time exposure at high temperature was evlauated quantitatively by small punch(SP) tests and micro hardness test taking account of the metallurgical changes. It is known that reactivation peak current (Ip) has a good relationship with Larson-Miller Parameter(LMP) which represents the information about material deterioration occurred at high temperature environment. In addition it was possible to estimate the ductile-brittle transition temperature (DBTT) by means of the SP test. The Sp test could be, therefore, suggested as a reliable test method for evaluating the material degradation of boiler tube steels. From the good correaltion between the SP DBTT and Ip values shown in this study, it was knows that the change of mechanical properties could be evaluated non-destructively by measurring only Ip values.ues.

National Genetic Evaluation (System) of Hanwoo (Korean Native Cattle)

  • Park, B.;Choi, T.;Kim, S.;Oh, S.H.
    • Asian-Australasian Journal of Animal Sciences
    • /
    • 제26권2호
    • /
    • pp.151-156
    • /
    • 2013
  • Hanwoo (Also known as Korean native cattle; Bos taurus coreanae) have been used for transportation and farming for a long time in South Korea. It has been about 30 yrs since Hanwoo improvement began in earnest as beef cattle for meat yield. The purpose of this study was to determine the trend of improvement as well as to estimate genetic parameters of the traits being used for seedstock selection based on the data collected from the past. Hanwoo proven bulls in South Korea are currently selected through performance and progeny tests. National Hanwoo genetic evaluations are implemented with yearling weight (YW), carcass weight (CW), eye muscle area (EMA), backfat thickness (BF) and marbling score (MS). Yearling weights and MS are used for selecting young bulls, and EMA, BF, and MS are used for selecting proven bulls. One individual per testing room was used for performance tests, and five individuals per room for progeny tests. Individuals tested were not allowed to graze pasture, but there was enough space for them to move around in the testing room. Feeds including roughages and minerals were fed ad libitum, and concentrates were provided at the rate of about 1.8% of individual weight. Overall means of the traits were $352.8{\pm}38.56$ kg, $335.09{\pm}44.61$ kg, $77.85{\pm}8.838\;cm^2$, $8.6{\pm}3.7$ mm and $3.293{\pm}1.648$ for YW, CW, EMA, BF and MS. Heritabilities estimated in this study were 0.30, 0.30, 0.42, 0.50 and 0.63 in YW, CW, EMA, BF and MS, respectively, which are similar to results from previous research. Yearling weight was 315.54 kg in 1998, and had increased to 355.06 kg in 2011, resulting in about 40 kg of improvement over 13 yrs. YW and CW have improved remarkably over the past 15 yrs. Breeding values between 1996 and 2000 decreased or did not change much, but have moved in a desirable direction since 2001. These improvements correspond with the substantial increase in use of animal models since the late 1990s in Korea. Hanwoo testing programs have practically contributed to the improvement in aspects of quality and quantity. In sum, the current selection system is good enough to accommodate circumstances where fewer sires are used on many more cows. Although progeny tests take longer and cost more, they seem to be appropriate under the circumstances of the domestic market with its higher requirement for better meat quality. Consequently, accumulative data collection, genetic evaluation model development, revision of selection indices, as well as cooperation among farms, associations, National Agricultural Cooperative Federation, universities, research institutes, and government agencies must be applied to the Hanwoo selection program. All these efforts will assist the domestic market to secure a competitive position against imported beef under Free Trade Agreement trade system and will provide farmers with higher profits as well as the public with a higher quality of beef.

Lomax 분포의 형상모수에 근거한 소프트웨어 신뢰성 비용모형에 관한 연구 (A Software Reliability Cost Model Based on the Shape Parameter of Lomax Distribution)

  • 양태진
    • 한국정보전자통신기술학회논문지
    • /
    • 제9권2호
    • /
    • pp.171-177
    • /
    • 2016
  • 소프트웨어 개발과정에서 소프트웨어 신뢰성은 매우 중요한 이슈이다. 소프트웨어 고장분석을 위한 무한고장 비동질적인 포아송과정에서 고장발생률이 상수이거나, 단조 증가 또는 단조 감소하는 패턴을 가질 수 있다. 본 연구에서는 소프트웨어 제품 테스팅 과정에서 고장 수명분포의 형상모수를 고려한 소프트웨어 신뢰성 비용 모형에 대하여 연구 하였다. 소프트웨어 신뢰성 분야에서 많이 사용되는 Lomax-NHPP 신뢰 성장 모형에 대한 비용 비교 문제를 제시하였다. 소프트웨어 고장모형은 무한고장 비동질적인 포아송과정을 이용하고 모수추정법은 최우추정법을 이용 하였다. 따라서 본 논문에서는 형상모수를 고려한 소프트웨어 비용모형 분석을 위하여 소프트웨어 고장시간 자료를 적용하여 비교 분석하였다. 대용량 소프트웨어가 수정과 변경하는 과정에서 결함의 발생을 거의 피할 수 없는 상황이 현실이다. 신뢰성 요구를 만족하고 총비용을 최소화하는 상황이 최적방출시간이다. 경우에 따라서는 왜도와 첨도 측면에서 효율적인 카파분포, 지수화지수분포 등 업데이트된 분포에 대한 방출 시기 문제를 비교 분석하는 연구도 가치 있는 일이라 판단된다. 이 연구를 통하여 소프트웨어 개발자들은 최적방출시간과 경제적 개발 비용을 파악 하는데 도움을 줄 수 있으리라 사료 된다.

Influences of luting cement shade on the color of various translucent monolithic zirconia and lithium disilicate ceramics for veneer restorations

  • Ghada Alrabeah;Nawaf Alamro;Atif Alghamdi;Ahmed Almslam;Meshari Azaaqi
    • The Journal of Advanced Prosthodontics
    • /
    • 제15권5호
    • /
    • pp.238-247
    • /
    • 2023
  • PURPOSE. The purpose of this study was to assess the effect of resin cement shade on the color of different novel ultratranslucent monolithic zirconia and lithium disilicate veneer materials. MATERIALS AND METHODS. For a total of 40 specimens, flat cylindrical discs with a 9-mm diameter and 0.5-mm thickness were created using CAD/CAM technology. The specimens were divided into five groups according to their material (n = 8) (e.max, Prettau, Aidite, Shofu and Dima) using A1 shade. Resin discs with the same diameter and shade as the specimens served as tooth-colored substructures. Three shades (neutral, light and warm) of resin cement try-in pastes (Variolink Esthetic LC) were used as the luting cement material. The color of each material group was measured before and after cementation using the three cement shades, and the CIE L*a*b* coordinates were obtained with a spectrophotometer. Values for the translucency parameter (TP) and color change delta E (E) before (baseline) and after cementation of each specimen were determined. To compare differences among the material groups within each shade of cement and among various shades of cement within each material, the data were analyzed using one-way ANOVA and post hoc testing. RESULTS. Color coordinates L*, a* and b* significantly changed after the application of try-in pastes relative to baseline values, with a noticeable decrease in lightness (L*) (P < .05). A significant color change (ΔE) was observed in all tested materials after cementation, with ΔE values exceeding 3.3 (P < .05). Although TP changed after cementation for most materials tested, these changes were not statistically significant (P > .05). Shofu and Dima ceramics showed the lowest TP values, while Aidite and Prettau showed the highest TP values. For e.max, translucency decreased after cementation with neutral and warm shades, and it significantly increased after cementation with a light shade. CONCLUSION. The shade of cement significantly altered the final color of the ceramic veneer material to a level above the threshold at which the clinical perception of color change occurred (> 3.3). The TP was not influenced by the cement shade. The translucency levels of the novel ultratranslucent multilayer monolithic zirconia ceramics Aidite and Prettau were higher than that of the lithium disilicate e.max material.

혼성동력계에서 주요 설계변수가 제동성능에 미치는 효과분석 (Effect of the Design Parameters Change on the Hybrid Dynamometer Braking Performance)

  • 이종훈;황재혁;정민지;권준용
    • 한국항공우주학회지
    • /
    • 제44권11호
    • /
    • pp.981-988
    • /
    • 2016
  • 브레이크 동력계는 브레이크의 성능을 시험하는 장치로 시험구역, 기계적 관성구역, 전기모터 및 제어구역으로 구성된다. 혼성동력계는 기계적 관성 구역의 크기를 줄이고 전기모터를 이용하여 브레이크 작동에 따른 기계적 관성의 손실을 보상하는 방식으로 상대적으로 작은 기계적 관성 크기와 적은 비용으로 시험이 가능한 장점이 있다. 본 논문에서는 공간적 제약이 있는 실험실에 적절한 혼성동력계를 설계하였고, 설계된 혼성동력계에서 마찰계수 변화 등 주요 설계변수가 혼성동력계 제동성능에 미치는 영향을 분석하였다. 본 연구를 통해 축소된 기계적 관성에 의한 에너지 손실을 보상하기 위한 전기 모터의 토크를 측정하면 마찰재의 불량여부를 판단 할 수 있는 결과를 얻었다.

인공신경망을 활용한 동착강도 예측 (Prediction of Adfreeze Bond Strength Using Artificial Neural Network)

  • 고성규;신휴성;최창호
    • 한국지반공학회논문집
    • /
    • 제27권11호
    • /
    • pp.71-81
    • /
    • 2011
  • 동착강도는 동토지반 말뚝기초 설계시 지지력을 결정하는 주요 설계정수이다. 동착강도는 동결온도, 구속응력, 말뚝표면 특성, 토사종류 등 다양한 인자들에 의해 동시다발적인 영향을 받는 것으로 보고되고 있다. 하지만 동착강도에 대한 연구는 소수의 인자들만 반영할 수 있는 실험연구를 중심으로 수행되어온 경향이 있으며, 설계정수로서 동착강도를 산정하기 위한 방법들은 동결온도, 말뚝재료 등의 주요 인자들만을 고려할 수 있는 한계가 있어 왔다. 본 연구는 인공신경망 이론을 동착강도 산정에 활용함으로서 다양한 영향인자 조건에서 동착강도를 예측할 수 있는 방안을 모색하기 위한 목적으로 수행되었다. 인공신경망 학습을 위하여 총 5종류의 연구사례로부터 137개의 자료를 수집하였으며, 그 중 100개를 학습자료로, 37개를 실증자료로 구분하였다. 연구결과 단계적 인공신경망 학습을 통하여 동착강도 산정 시 다양한 영향인지를 다차원적으로 고려하여 예측하는 방법이 병행되어야 할 필요성을 확인하였으며, 5개 영향인자를 동시에 고려하여 동착강도를 예측할 수 있는 신뢰성 높은 학습결과를 도출 및 검증하였다. 또한, 매개변수 연구결과 동착강도는 동결온도와 말뚝재료의 변화에 가장 민감하게 반응하는 것으로 나타났고 수직응력에 의한 영향은 일부 온도구간에서만 뚜렷하게 나타나며 토사종류와 재하속도의 변화에 따라 동착강도가 증가하는 경향이 변화하는 특성을 나타내었다.

집중형 모형 IHACRES와 GR4J를 이용한 강수 및 기온 변동성에 대한 유출 해석 민감도 평가 (Assessing the Sensitivity of Runoff Projections Under Precipitation and Temperature Variability Using IHACRES and GR4J Lumped Runoff-Rainfall Models)

  • 우동국;조지현;강부식;이송희;이가림;노성진
    • 대한토목학회논문집
    • /
    • 제43권1호
    • /
    • pp.43-54
    • /
    • 2023
  • 기후변화가 고착화되면서 강수와 기온 변동으로 인한 가뭄 및 홍수 발생이 증가하고 있다. 유역 단위의 유출량 예측은 기후변화로 인한 자연재해에 대비하기 위한 수자원 관리의 시작이라 할 수 있다. 하지만, 기후변화와 유출모형의 불확실성은 정확한 유출 분석을 어렵게 한다. 본 연구에서는 이러한 불확실성을 완화하기 위하여 기후 스트레스 시나리오에 따른 두 개의 집중형 수문모형, 즉 IHACRES와 GR4J를 이용하여 강수 및 기온 변화에 따른 유출량 변화를 비교, 분석하였다. 연구 대상 지역은 합천댐과 섬진강댐 유역이며, Nash-Sutcliffe Efficiency (NSE) 및 Kling Gupta Efficiency (KGE)를 목적함수로 하여 각 모형의 매개변수를 최적화하였다. 모형의 보정과 검정은 20년(1995년-2014년)의 유출자료를 활용하였으며, 보정 및 검정 기간은 각각 7:3 비율로 설정하였다. 두 모형 모두 보정과 검정 기간에 비교적 높은 신뢰도(NSE>0.74, KGE>0.75)를 보여, 모형이 과거 사상을 재현하기에 적합하고, 모의 결과가 비교적 유사함을 확인하였다. 다음으로, 기후변동이 유출에 미치는 영향을 평가하기 위해 동일한 모의 기간에 대해 강수는 -50 %에서 +50 %의 범위를 1 %씩, 기온은 0 ℃에서 8 ℃까지 0.1 ℃씩 구분하여 총 8,181개의 기후조건 시나리오를 구축하였다. 이후, 기후 스트레스 시나리오에 따른 두 모형의 최대유량, 풍수량, 평수량을 비교 및 분석하였다. 기후 스트레스 영향을 반영한 연최대유량과 풍수량의 경우, 강수 감소에 따른 유출 패턴은 두 모형에서 비슷하였으나, 강수와 기온이 증가할수록 상이한 결과를 얻었다. 이와 반대로, 풍수량의 경우 강수와 기온 변화의 차이가 커질수록 두 모형은 유사한 결과를 얻었다. 즉, 유역의 탄력적 기후변화 대응을 위해서는 모형의 불확실성에 대한 정량적 평가가 필요하다는 것을 시사한다.

2.25Cr-1Mo 강 인공 열화재의 고주파수 초음파 감쇠특성에 관한 연구 (A Study on the High Frequency Ultrasonic Attenuation Characterization in Artificially Aging Degraded 2.25Cr-1Mo Steel)

  • 박익근;박은수;김정석;김현묵;권숙인;변재원
    • 비파괴검사학회지
    • /
    • 제21권4호
    • /
    • pp.439-445
    • /
    • 2001
  • 재료나 설비의 고온 장시간 사용으로 인하여 발생되는 재질열화 평가에는 파괴적인 방법이 널리 사용되고 있으며, 신뢰도가 높다. 그러나, 시험편의 채취가 어렵고 많은 경비와 시간이 소요된다. 전기저항법, 레프리카법, 바크하우젠 노이즈법, 전기화학적방법, 초음파법 등과 같은 비파괴적인 열화손상 평가 방법이 주목을 받고 있다. 본 연구에서는 2.25Cr-1Mo 강을 $630^{\circ}C$에서 장시간 등온열처리로 모의 열화시험편을 제작하고, 고온설비부재에서 발생되는 미세조직의 변화와 고주파 초음파의 전파특성(감쇠계수)과의 일대일 상관관계를 규명하여 초음파 비파괴평가에 의한 열화도 평가의 유용성 유모를 실험적으로 검증하였다. 그 결과 2.25Cr-1Mo 인공열화재의 경우 열화가 진행됨에 따라 탄화물의 석출 및 조대화가 일어나며 초음파 감쇠계수는 증가하는 경향을 나타내었으며, 그 정도는 침상의 탄화물이 거의 소멸되는 1,000시간 이후에 초음파 감쇠계수가 급격히 증가하는 매우 좋은 상관성을 나타내었다.

  • PDF

안경착용자 방진마스크 착용 시 밀착계수와 착용시력에 미치는 영향 (Effects of Fit Factor and Visual Acuity of Eyeglasses Wearers when Wearing Particulate Filtering Facepiece Respirators)

  • 어원석;신창섭
    • 한국안전학회지
    • /
    • 제35권3호
    • /
    • pp.105-115
    • /
    • 2020
  • This study compares the difference of fit factors (FF) and visual acuity according to masks and eyeglasses preferences for 54 participants. We the precautions and behaviors of discomfort when wearing masks of eyewear wearers. Contact lens discomfort and priority action of complaints was investigated Glasses fitting factors is Optical Center Height(OH), Vertex Distance(VD) and Pantoscopic Angle(PA). We measured those factors and expressed by the ratio of standard point and change point. Quantitative fit factor was measured by Portacount Pro+ 8038. Also, we selected to 6 exercises among 8 exercises OSHA QNFT (Quantitative Fit testing) protocol to measure the fit factors. The pass/ fail criterion of FF was set at 100. Visual acuity(VA) test chart is developed by Chunsuk Han was used, Descriptive statistics was performed. Descriptive statistics(SAS ver 9.2), it is used geometric means, Wilcoxon analysis(P=0.05) When wearing the mask preferentially, fit factor(FF) was high according to the step of glasses fitting parameter. on the other hand, when the glasses first choice, the visual acuity(VA) was high. there was no significant difference. In the case of fit factor (FF), mask first choice/ glasses first choice is OH (p=0.671/ p=0.332), VD (p=0.602/ p=0.571) and PA (p=0.549/ p=0.607). Visual acuity (VA), mask first choice/ glasses first choice is OH (p=0.753/ p=0.386), VD (p=0.815/ p=0.557) and PA (p=0.856/ p=0.562). The workers of workplace and office chose glasses but occupational health workers and students chose mask. In case of discomforts, it was suggested to remove the mask and tolerate discomforts. The main discomforts and usual action of lens were dryness, hyperemia, foreign body sensation, ophthalmodynia, decreased vision and glasses wearing. Therefore, it is necessary to develop a mask wearing method education program considering glasses fitting and develop a hybrid model that minimizes inconvenience when wearing glasses and a mask at the same time.

토양의 함수율에 따른 전기비저항 반응 모형 실험 연구 (Study on Electrical Resistivity Pattern of Soil Moisture Content with Model Experiments)

  • 지윤수;오석훈;이희순
    • 지구물리와물리탐사
    • /
    • 제16권2호
    • /
    • pp.79-90
    • /
    • 2013
  • 지반조사에서 비파괴 조사 기술은 시추조사보다 경제적으로 비용이 덜 들고 광역에 걸친 지반정보를 제공하는 장점이 있다. 하지만 지반설계정수로서 적용하기에는 어려운 한정된 정보만을 제공하게 된다. 이를 극복하기 위해, 비파괴 조사 방법 중 하나인 전기비저항 탐사를 모형토조실험에 적용하여, 토질상태에 따른 비저항 반응과 함수비에 따른 비저항 반응을 분석하여 비저항 거동 양상에 대한 연구를 수행하였다. 실험에 사용한 토질은 주문진 표준사, 마사토이며 각 토질의 입도 분포, 균등계수를 구하여 실험에 있어 실험재료의 균질한 상태를 유지하였다. 실험에 사용한 모형의 제원은 $160{\times}100{\times}50$ (cm)의 아크릴 재질 토조이며, 각 토질의 높이는 30 cm를 유지하였다. 5TE(함수비측정센서)센서를 7 ~ 8cm 간격으로 수직하게 꽂아 층별 함수비를 측정하였다. 모형실험 결과 주문진 표준사는 비저항 거동 양상이 함수비에 민감하게 반응하는 것을 알 수 있었으며, 마사토는 함수비에 따라 비저항이 낮아진 후에도 시간경과에 따른 거동 양상에 큰 변화가 없는 것을 관찰하였다. 또한 토조 실험에 사용된 토양과 유사한 테스트 베드를 선정하여 그 반응을 비교 분석하였다. 이러한 실험을 통해 토질 상태와 함수비에 따른 다양한 비저항 거동 양상 자료를 수집하고, 비파괴 조사기술의 정확도를 향상 시켜 나간다면 지반설계정수를 산정하는데 있어 기초적인 연구가 될 수 있음을 확인하였다.