• Title/Summary/Keyword: T-peel 강도

Search Result 33, Processing Time 0.03 seconds

A Study on the CFRP Treatment by ion Assisted Reaction Method to Improve T-peel Strength of CFRP/Aluminum Composites (CFRP/알루미늄 복합재에서 이온도움반응법을 적용한 CFRP의 표면처리가 T-peel 강도에 미치는 영향에 대한 연구)

  • Lee, Gyeong-Yeop;Yang, Jun-Ho;Yun, Chang-Seon;Choe, Nak-Sam
    • Transactions of the Korean Society of Mechanical Engineers A
    • /
    • v.26 no.3
    • /
    • pp.570-575
    • /
    • 2002
  • It is well-known that the bond strength between CFRP(Carbon Fiber Reinforced Plastic) and aluminum is significantly affected by the surface treatment of the CFRP and the aluminum. This study investigates the surface treatment of CFRP to improve the T-peel strength of CFRP/aluminum composites. The surface of %CFRP([0^0]_{14})$ was treated by the ion assisted reaction method under oxygen environment. T-peel strength tests were performed based on the procedure of ASTM D1876-95. The T-peel strength of surface-treated CFRP/aluminum composites was compared with that of untreated CFRP/aluminum composites. The results showed that the T-peel strength of surface-treated CFRP/aluminum composites was about 5.5 times higher than that of untreated CFRP/aluminum composites. SEM examination showed that the improvement of T-peel strength was attributed to the uniform spread and fracture of epoxy adhesive.

The Effect of Resin Mixture Ratio on Characteristics of Tensile and T-peel Strength in Al/AFRP Laminates (Al/APRP 적층재의 수지혼합비가 인장 및 티-필(T-peel) 강도 특성에 미치는 영향)

  • Song, Sam-Hong;Kim, Cheol-Woong
    • Transactions of the Korean Society of Mechanical Engineers A
    • /
    • v.26 no.11
    • /
    • pp.2374-2382
    • /
    • 2002
  • Aluminum alloy/aramid fiber reinforced plastic(Al/AFRP) laminates consists of high strength metal(A15052) and laminated aramid fiber with structural adhesive bond. The mixture ratio effect of epoxy resin curing agent accelerator on the tensile strength and T-peel strength characteristic in Al AFRP laminates were investigated in this study. The epoxy. diglycidylether of bisphenol A(DCEBA), It'as cured by methylene dianiline(MDA) with or without an accelerator(K-54). Eight different kinds of resin mixture ratios were selected for the test , five kinds of Al/AFRP laminates were named as Al/AFRP(1) and three others of Al/AFRP laminates were named as Al/AFRP(2). The comparison of tensile strength and T-peel strength with variation of resin mixture ratio were studied. Respectively. Al/AFRP(1) and Al/AFRP(2) indicated approximately 6.0 times and 7.0 times more improved maximum tensile strength in comparison with those of monolithic A15052. Al/AFRP(2) indicated approximately 1.5 times more impoved maximum T-peel strengths in comparison with those of Al/AFRP(1). As results. Al/AFRP(2) turned out to have more effective characteristics on the tensile strength and T-peel strength than those of Al/AFRP(1).

Strength Evaluation of Adhesive Bonded Joint for Light Weight Structure by T-Peel Joint Test (T형 이음 접합에 의한 경량구조물용 접착이음강도의 평가)

  • 이강용;공병석;우형표
    • Transactions of the Korean Society of Automotive Engineers
    • /
    • v.6 no.4
    • /
    • pp.56-65
    • /
    • 1998
  • The bonding strength evaluation of the light weight materials for an electrical vehicle has been performed through the T-peel joint test in which the design paramete- rs such as joint style, adherend type, adherend thickness, adhesive thickness, and adhesive type are considered. It is experimentally observed that the peel strength of joint increases with the increase of the adherend thickness. With the increase of the adhesive thickness, however, the peel strength of joint increases a little. Aluminum-FRP adherend combination shows such higher peel strength than that of Aluminum-Aluminum adherend combination. For the adhesive bonded joint, the results of FEM analysis agree with those of experiment. The adhesive bonded joint reinfored with a rivet gives higher peel strength than that of the joint without rivet.

  • PDF

Effect of Aluminum Treatment by Plasma on the Bonding Strength Between Aluminum and CFRP Composites (플라즈마를 적용한 알루미늄의 표면처리가 알루미늄/CFRP 복합재의 접합강도에 미치는 영향)

  • Lee, Gyeong-Yeop;Yang, Jun-Ho;Choe, Nak-Sam
    • Transactions of the Korean Society of Mechanical Engineers A
    • /
    • v.25 no.12
    • /
    • pp.1981-1987
    • /
    • 2001
  • This paper documents the effect of surface treatment of aluminum on the bonding strength of aluminum/CFRP composites. The surface of aluminum panel was treated by DC plasma. The optimal treatment condition of the aluminum was determined by measuring the contact angle and T-peel strength as functions of mixture ratio of acetylene gas to nitrogen gas. The mixture ratios used were 1:9, 3:7, 5:5, 7:3, and 9:1 Lap shear tests and T-peel tests were performed using surface-treated alumiunm/CFRP composites and regular alumiunm/CFRP composites. The results showed that the contact angle was minimized and the T-peel strength was maximized iota the mixture ratio of 5:5. The results also showed that the shear strength of surface-treated alumiunm/CFRP composites was 34% greater than that of regular alumiunm/CFRP composites. The T-peel strength of surface-treated alumiunm/CFRP composites was also 5 times greater than that of regular alumiunm/CFRP composites.

A Study on the Curing Method to Improve Bonding Strength of Aluminum/CFRP Composites (알루미늄/CFRP 복합재의 접착강도 향상을 위한 경화방법에 관한 연구)

  • 이경엽;양준호;최낙삼
    • Transactions of the Korean Society of Automotive Engineers
    • /
    • v.10 no.3
    • /
    • pp.130-135
    • /
    • 2002
  • This study investigates the effect of curing method on the bonding strength of aluminum/CFRP composites. The surface of aluminum panel was treated by DC plasma. Lap shear tests and T-peel tests were performed based on the procedure of ASTM 906-94a and ASTMD1876-95, respectively. Test samples were fabricated by using the co-curing method and the secondary curing method. The results showed that the shear strength of test samples made by the co-curing method was 2.5 times greater than that of test samples made by the secondary curing method. The T-peel strength of the co-curing method case was almost 2 times greater than that of the secondary curing method case.

Fatigue Strength Evaluation of T-Peel Adhesive Joing for Light Weight Material (경량 재료의 T형 접합이음의 피로강도 평가)

  • Lee, K.Y.;Kong, B.S.;Choi, H.S.
    • Transactions of the Korean Society of Automotive Engineers
    • /
    • v.6 no.6
    • /
    • pp.166-173
    • /
    • 1998
  • The evaluation of joint fatigue strength of light weight materials for an electrical vehicle body has been performed through T-peel joint tests with the design parameters such as joint style, adherend type, adherend thickness, adhesive thickness, and various adhesives. Fatigue strength was evaluated through 5-Hz, tension-tension, load controlled test with the zero stress ratio. It was observed that the fatigue strength of the joint increases with the increase of the adherend thickness. With the increase of the adhesive thickness, however, the fatigue strength of the joint increases insignificantly. An aluminum-FRP adherend combination shows much higher fatigue strength than an aluminum-aluminum adherend combination. The results of fatigue tests were found to be consistent with those of static tests.

  • PDF

Peel-tension Fatigue Strength of Mechanical Press Joints of Cold Rolled Steel Sheet (냉간 압연강 판재 기계적 접합부의 인장-박리 피로 강도)

  • Lee, Man-Suk;Park, Jong-Min;Kim, Taek-Young;Kim, Ho-Kyung
    • Journal of the Korean Society of Safety
    • /
    • v.27 no.5
    • /
    • pp.42-48
    • /
    • 2012
  • Peel-tension fatigue experiments were conducted for investigating on fatigue strength of mechanical press joints of SPCC steel sheet used in the field of the automobile industry. In addition, finite element method analysis on the peel-tension specimen was conducted using HyperMesh and ABAQUS softwares. The cold rolled mild steel was used to join the T-shaped peel-tension specimen with a button diameter of 5.4 mm and a punch diameter of 8.3 mm. The fatigue limit load amplitude was found to be 112.4 N at the number of cycles 106, indicating that the ratio of fatigue limit load to static peel-tension strength was about 8%. This value suggests that the mechanical press joint is highly vulnerable to peel-tension load rather than to tensile-shear load, considering that the ratio of fatigue limit load to static tensile-shear strength was about 43%. Fatigue failure mode was found to be interface-failure mode.

Effects of Temperature/Humidity Treatment Conditions on the Peel Strength between Screen-printed Ag and Polyimide Films (고온/고습 조건이 스크린 프린팅 Ag와 Polyimide의 필 강도에 미치는 영향)

  • Lee, Hyeonchul;Bae, Byeong-Hyun;Son, Kirak;Kim, Gahui;Park, Young-Bae
    • Journal of the Microelectronics and Packaging Society
    • /
    • v.29 no.2
    • /
    • pp.43-48
    • /
    • 2022
  • Effect of temperature/humidity (T/H) treatment conditions on the peel strength of screen-printed Ag/polyimide (PI) structures was evaluated by peeling PI films in 90° peel test. Initial peel strength was 25.99±1.47 gf/mm, and then decreased to 6.05±0.54 gf/mm after 500 h at 85℃/85% relative humidity T/H condition. And, the peeled locus was changed from Ag/PI interface to shallow cohesive inside PI near interface. X-ray photoelectron spectroscopy analysis on the peeled surfaces showed that the long-term moisture penetration into the Ag/PI interface during T/H treatment led to hydrolytic degradation of PI to form weak boundary layer inside PI near Ag/PI interface, which are responsible for large decrease in peel strength.

SPRC 강판의 표면전처리 공정에 따른 에폭시 접착부 특성 평가

  • Kim, Hae-Yeon;Kim, Min-Su;Kim, Jong-Hun;Kim, Mok-Sun;Kim, Jun-Gi
    • Proceedings of the Materials Research Society of Korea Conference
    • /
    • 2011.05a
    • /
    • pp.56.2-56.2
    • /
    • 2011
  • 최근 철강, 알루미늄, 이종재료의 접합 등 용접이 어려운 부분에 구조용 접착제의 적용이 증가하고 있는 추세이다. 이를 위해 변성 에폭시레진을 활용한 고접합 강도, 고인성의 구조용 접착제가 연구되어 지고 있다. 피착제의 표면처리는 접합부의 접합강도를 향상시키는 방법으로 알려져 있으나 최근의 구조용 접착제는 표면 전처리 없이도 우수한 접착 특성을 보이는 것으로 기대되고 있다. 본 연구에서는 변성레진에 대해서 각종 표면처리가 접합부 특성에 미치는 영향을 조사하였다. 피착제로는 자동차용 냉연강판인 SPRC440을 사용하였고, 전처리로는 무처리 상태, SiC연마지를 이용한 연마, 아르곤 및 산소가스를 이용한 마이크로웨이브 플라즈마 표면처리, 산세 등의 표면처리를 실시하였다. 에폭시 접착제는 변성 에폭시 레진과 경화제 및 촉매제를 이용하여 직접 포뮬레이션하였다. 단일 겹치기 전단강도 시험과 T-Peel 시험은 각각 ASTM D 1002 규격에 따라 준비하였으며 인장 시험 후 파면은 SEM으로 관찰하였다.

  • PDF

Analysis for Strength Estimation of Adhesive Joints (접착이음의 강도평가에 대한 해석)

  • 박성완;이장규
    • Proceedings of the Korean Society of Machine Tool Engineers Conference
    • /
    • 2004.10a
    • /
    • pp.98-107
    • /
    • 2004
  • The objectives of this research are to establish the criteria of peel occurrence considering the shape of bond terminus and to compare the strength properties of some adhesive joints. The criteria of feel occurrence at the bond terminus was suggested. Peel loads of some adhesive joint(butt joint, T -shape specimen, single lap joint) were determined from tensile tests. Principal stress distributions of these joints were determined from finite element method analysis. Then, peel occurrence was estimated with intensity of stress singularity ' $K_{prin.}$' when the terminus shape was square, with average principal stress when the terminus shape was rounded. The conclusions are summarized as follows; (1) In the non-filleted model(e.g., butt joint, T-shape specimen), principal stress shows singularity at the bond terminus, intensity of stress(principal stress) singularity ' $K_{prin.}$&apso; can use as the criteria of peel occurrence at the bond terminus. (2) In the filleted model(e.g., single lap joint), principal stress doesn't show singularity at the bond terminus. Average principal stress can use as the criteria of peel occurrence at the bond terminus.'t show singularity at the bond terminus. Average principal stress can use as the criteria of peel occurrence at the bond terminus.

  • PDF