Proceedings of the Korea Institute of Applied Superconductivity and Cryogenics Conference
/
1999.02a
/
pp.18-21
/
1999
The effects of joining process such as contact method, shape of joined area and pressure on the properties of Bi-2223 superconducting tape have been optimized. In the process tapes were etched to expose the superconductor core in the shape of 'ㅁ' and 'ㄷ'. The exposed cores of the two tapes were brought into contact, uniaxially pressed and sintered. Subsequently, the current capacity of the joined tape was measured as a function of uniaxial pressure. It was observed that the current capacity was significantly dependent on uniaxial pressure. The joined tape, fabricated with a pressure of 1,600 MPa, showed the highest value of current capacity(90%) of highest value of current capacity is resulted from improvements in core density, contacting area and grain alignment, etc. In addition the effect of processing variables on microstructural evolution and mechanical property of joined tape will be presented.
[ $YBa_2Cu_3O_{7-\delta}$ ] thin films were deposited by laser ablation using modified melt-textured grown targets. As the laser energy density was increased, the films showed an increasing c-axis orientation and an improvement of superconducting properties. However, at 4 $J/cm^2$, the degree of c-axis alignment and $J_c$ of the film were considerably reduced. These were attributed to the enhanced a-axis outgrowths. It was shown that the increased laser energy density resulted in the formation of $Y_2O_3$ inclusions during the c-axis film growth, and that these inclusions nucleated the a-axis outgrowths.
Evaluation of the mechanical properties of Bi-2223/Ag HTS tapes was carried out by the tension and bending tests. Most of the Bi-2223/Ag tapes retained critical current up to 10 kgf/mm$_2$ axial tension stress, and 0.2% tension strain at room temperature. Applied tension strain exceeding 0.3% in superconducting tapes at 77 K leaded to rapid degradation of the critical current. It was observed that the more filaments, the better axial tension property at 77 K, self-field The influence of bending strain on critical current degradation was revealed to be less sensitive for Bi-2223/Ag HTS tapes with a more number of filaments and higher silver ratio.
We investigate the electrical and thermal transport properties of a sesquicarbide superconductor $La_2C_3$, including electrical resistivity, thermoelectric power, and thermal conductivity. The electrical resistivity exhibits a typical metallic character with a saturation behavior at high temperatures. The thermoelectric power shows a metallic behavior with pronounced phonon-drag effect, comparable with pure metals. The broad peak of the thermal conductivity is observed in the superconducting state, which is rapidly suppressed by magnetic fields. These observations suggest that the electron-phonon scattering is significant in $La_2C_3$, which is relevant with the relatively high-$T_c$ in $La_2C_3$ through strong electron-phonon coupling with low frequency phonon modes.
123 초전도체에 마그네틱 모멘트가 큰 Ni불순물을 도핑하여 제작한 $Y_{1}$ Ba(C $u_{2.9}$$N_{0.1}$) $O_{7-{\delta}}$ 초전도체의 X-ray diffraction pattern, susceptibility, 온도변화등에 따른 전류-전압관계, 임계온도 등에 대하여 연구하였다. 제작된 시료는 매우 뚜렷한 orthorhombic 피크를 가진 123상을 나타내고 있었다. N=0.1의 시료에서는 적은 양의 Ni 불순물과 단면적인 무정형상태의 잘 반응된 YBa(Cu, Ni)$_{3}$$O_{7-{\delta}}$의 orthorhombic구조를 나타내고 있다. 전반적인 실험 결과로 부터 Ni는 Y-Ba-Cu-O 초전도 시스템에서 초전도에 중요한 역할을 담당하지 않는다는 결론을 얻었다.얻었다.다.
The various type Ag sheathed Bi-2223 tapes have been were fabricated by Powder-in-tube(PIT) process. The critical current density could be improved with the value of $23,000\;A/cm^2$(77 K, zero field) in the single concentric Bi-2223 tape. The bending property dependence of $I_c$ was improved in the double concentric Bi-2223 tape compared with single filamentary and single concentric one.
The evaluation of the electromechanical properties of HTS CC tapes is one of the foremost procedures to be done to ensure the applicability of superconducting wires to electric devices. A precise measurement of the stress and strain is important in deriving the mechanical properties under operating environment. Up to now, there is no standard test method yet for the electromechanical property evaluation of HTS tapes under self field and external magnetic field although there are already reports on the different devices used to evaluate these properties. Strain can be measured by adopting a strain gauge or a high resolution double extensometer. In this study, strain effect on $I_c$ in HTS CC tapes under magnetic fields was evaluated. Comparison of advantages and setback of strain measuring devices were discussed. In addition, a dual strain measurement system using both the SG and extensometer may be practical to lessen the burden in case one of the measuring devices does not work well.
Journal of the Korean Institute of Electrical and Electronic Material Engineers
/
v.34
no.5
/
pp.333-336
/
2021
Oxide YBCO bulk superconductors are manufactured using the melt process. Because seed crystal growth method utilizes a slow-spreading layer-by-layer reaction, a long-term heat treatment is required to manufacture a single-crystal specimen of several cm. In this study, the melt process method was applied to compensate for the shortcomings of the seed crystal growth method. The thickness of the upper and lower pellets of the YBCO bulk was molded to 40 mm, and YBCO superconductor was produced by heat treatment. The measurement results of capture magnetism was in line with the literature. This results in a relationship that the higher the growth of Y211 particle in the YBCO, the higher the superconducting properties. We analyzed the YBCO superconductor, focusing on the Y2BaCuO5 particle distribution.
In superconducting coil applications particularly in wet wound coils, coated conductor (CC) tapes are subjected to different type of stresses that could affect its electromechanical transport property. These include hoop stress acting along the length of the CC tape and the Lorentz force acting perpendicular to the CC tape's surface. Since the latter is commonly associated with the delamination problem of multi-layered REBCO CC tapes, more understanding and attention on the delamination phenomena induced in the case of coil applications are needed. Difference on the coefficient of thermal expansion (CTE) of each constituent layer of the CC tape, the bobbin, and the impregnating materials is the main causes of delamination in CC tapes when subjected to thermal and mechanical cycling. In the design of degradation-free superconducting coils, therefore, characterization of the delamination behaviors including mechanism and strength in the multi-layered REBCO CC tapes becomes a critical issue. Various trials to increase the delamination strength by improving interface characteristics at interlayers have been performed. In this study, in order to investigate the influences of laser cleaning and Ag annealing treated at the substrate side surface, transverse tensile tests were conducted under different sample configurations using $4.5mm{\times}8mm$ upper anvil. The mechanical delamination strength of differently processed CC samples was examined at room temperature (RT). As a result, the Sample 1 with the additional laser cleaning and Ag annealing processes and the Sample 2 with additional Ag annealing process only showed higher mechanical delamination strength as compared to the Sample 3 without such additional treatments. Sample 3 showed quite different behavior when the loading direction is to the substrate side where the delamination strength much lower as compared to other cases.
본 웹사이트에 게시된 이메일 주소가 전자우편 수집 프로그램이나
그 밖의 기술적 장치를 이용하여 무단으로 수집되는 것을 거부하며,
이를 위반시 정보통신망법에 의해 형사 처벌됨을 유념하시기 바랍니다.
[게시일 2004년 10월 1일]
이용약관
제 1 장 총칙
제 1 조 (목적)
이 이용약관은 KoreaScience 홈페이지(이하 “당 사이트”)에서 제공하는 인터넷 서비스(이하 '서비스')의 가입조건 및 이용에 관한 제반 사항과 기타 필요한 사항을 구체적으로 규정함을 목적으로 합니다.
제 2 조 (용어의 정의)
① "이용자"라 함은 당 사이트에 접속하여 이 약관에 따라 당 사이트가 제공하는 서비스를 받는 회원 및 비회원을
말합니다.
② "회원"이라 함은 서비스를 이용하기 위하여 당 사이트에 개인정보를 제공하여 아이디(ID)와 비밀번호를 부여
받은 자를 말합니다.
③ "회원 아이디(ID)"라 함은 회원의 식별 및 서비스 이용을 위하여 자신이 선정한 문자 및 숫자의 조합을
말합니다.
④ "비밀번호(패스워드)"라 함은 회원이 자신의 비밀보호를 위하여 선정한 문자 및 숫자의 조합을 말합니다.
제 3 조 (이용약관의 효력 및 변경)
① 이 약관은 당 사이트에 게시하거나 기타의 방법으로 회원에게 공지함으로써 효력이 발생합니다.
② 당 사이트는 이 약관을 개정할 경우에 적용일자 및 개정사유를 명시하여 현행 약관과 함께 당 사이트의
초기화면에 그 적용일자 7일 이전부터 적용일자 전일까지 공지합니다. 다만, 회원에게 불리하게 약관내용을
변경하는 경우에는 최소한 30일 이상의 사전 유예기간을 두고 공지합니다. 이 경우 당 사이트는 개정 전
내용과 개정 후 내용을 명확하게 비교하여 이용자가 알기 쉽도록 표시합니다.
제 4 조(약관 외 준칙)
① 이 약관은 당 사이트가 제공하는 서비스에 관한 이용안내와 함께 적용됩니다.
② 이 약관에 명시되지 아니한 사항은 관계법령의 규정이 적용됩니다.
제 2 장 이용계약의 체결
제 5 조 (이용계약의 성립 등)
① 이용계약은 이용고객이 당 사이트가 정한 약관에 「동의합니다」를 선택하고, 당 사이트가 정한
온라인신청양식을 작성하여 서비스 이용을 신청한 후, 당 사이트가 이를 승낙함으로써 성립합니다.
② 제1항의 승낙은 당 사이트가 제공하는 과학기술정보검색, 맞춤정보, 서지정보 등 다른 서비스의 이용승낙을
포함합니다.
제 6 조 (회원가입)
서비스를 이용하고자 하는 고객은 당 사이트에서 정한 회원가입양식에 개인정보를 기재하여 가입을 하여야 합니다.
제 7 조 (개인정보의 보호 및 사용)
당 사이트는 관계법령이 정하는 바에 따라 회원 등록정보를 포함한 회원의 개인정보를 보호하기 위해 노력합니다. 회원 개인정보의 보호 및 사용에 대해서는 관련법령 및 당 사이트의 개인정보 보호정책이 적용됩니다.
제 8 조 (이용 신청의 승낙과 제한)
① 당 사이트는 제6조의 규정에 의한 이용신청고객에 대하여 서비스 이용을 승낙합니다.
② 당 사이트는 아래사항에 해당하는 경우에 대해서 승낙하지 아니 합니다.
- 이용계약 신청서의 내용을 허위로 기재한 경우
- 기타 규정한 제반사항을 위반하며 신청하는 경우
제 9 조 (회원 ID 부여 및 변경 등)
① 당 사이트는 이용고객에 대하여 약관에 정하는 바에 따라 자신이 선정한 회원 ID를 부여합니다.
② 회원 ID는 원칙적으로 변경이 불가하며 부득이한 사유로 인하여 변경 하고자 하는 경우에는 해당 ID를
해지하고 재가입해야 합니다.
③ 기타 회원 개인정보 관리 및 변경 등에 관한 사항은 서비스별 안내에 정하는 바에 의합니다.
제 3 장 계약 당사자의 의무
제 10 조 (KISTI의 의무)
① 당 사이트는 이용고객이 희망한 서비스 제공 개시일에 특별한 사정이 없는 한 서비스를 이용할 수 있도록
하여야 합니다.
② 당 사이트는 개인정보 보호를 위해 보안시스템을 구축하며 개인정보 보호정책을 공시하고 준수합니다.
③ 당 사이트는 회원으로부터 제기되는 의견이나 불만이 정당하다고 객관적으로 인정될 경우에는 적절한 절차를
거쳐 즉시 처리하여야 합니다. 다만, 즉시 처리가 곤란한 경우는 회원에게 그 사유와 처리일정을 통보하여야
합니다.
제 11 조 (회원의 의무)
① 이용자는 회원가입 신청 또는 회원정보 변경 시 실명으로 모든 사항을 사실에 근거하여 작성하여야 하며,
허위 또는 타인의 정보를 등록할 경우 일체의 권리를 주장할 수 없습니다.
② 당 사이트가 관계법령 및 개인정보 보호정책에 의거하여 그 책임을 지는 경우를 제외하고 회원에게 부여된
ID의 비밀번호 관리소홀, 부정사용에 의하여 발생하는 모든 결과에 대한 책임은 회원에게 있습니다.
③ 회원은 당 사이트 및 제 3자의 지적 재산권을 침해해서는 안 됩니다.
제 4 장 서비스의 이용
제 12 조 (서비스 이용 시간)
① 서비스 이용은 당 사이트의 업무상 또는 기술상 특별한 지장이 없는 한 연중무휴, 1일 24시간 운영을
원칙으로 합니다. 단, 당 사이트는 시스템 정기점검, 증설 및 교체를 위해 당 사이트가 정한 날이나 시간에
서비스를 일시 중단할 수 있으며, 예정되어 있는 작업으로 인한 서비스 일시중단은 당 사이트 홈페이지를
통해 사전에 공지합니다.
② 당 사이트는 서비스를 특정범위로 분할하여 각 범위별로 이용가능시간을 별도로 지정할 수 있습니다. 다만
이 경우 그 내용을 공지합니다.
제 13 조 (홈페이지 저작권)
① NDSL에서 제공하는 모든 저작물의 저작권은 원저작자에게 있으며, KISTI는 복제/배포/전송권을 확보하고
있습니다.
② NDSL에서 제공하는 콘텐츠를 상업적 및 기타 영리목적으로 복제/배포/전송할 경우 사전에 KISTI의 허락을
받아야 합니다.
③ NDSL에서 제공하는 콘텐츠를 보도, 비평, 교육, 연구 등을 위하여 정당한 범위 안에서 공정한 관행에
합치되게 인용할 수 있습니다.
④ NDSL에서 제공하는 콘텐츠를 무단 복제, 전송, 배포 기타 저작권법에 위반되는 방법으로 이용할 경우
저작권법 제136조에 따라 5년 이하의 징역 또는 5천만 원 이하의 벌금에 처해질 수 있습니다.
제 14 조 (유료서비스)
① 당 사이트 및 협력기관이 정한 유료서비스(원문복사 등)는 별도로 정해진 바에 따르며, 변경사항은 시행 전에
당 사이트 홈페이지를 통하여 회원에게 공지합니다.
② 유료서비스를 이용하려는 회원은 정해진 요금체계에 따라 요금을 납부해야 합니다.
제 5 장 계약 해지 및 이용 제한
제 15 조 (계약 해지)
회원이 이용계약을 해지하고자 하는 때에는 [가입해지] 메뉴를 이용해 직접 해지해야 합니다.
제 16 조 (서비스 이용제한)
① 당 사이트는 회원이 서비스 이용내용에 있어서 본 약관 제 11조 내용을 위반하거나, 다음 각 호에 해당하는
경우 서비스 이용을 제한할 수 있습니다.
- 2년 이상 서비스를 이용한 적이 없는 경우
- 기타 정상적인 서비스 운영에 방해가 될 경우
② 상기 이용제한 규정에 따라 서비스를 이용하는 회원에게 서비스 이용에 대하여 별도 공지 없이 서비스 이용의
일시정지, 이용계약 해지 할 수 있습니다.
제 17 조 (전자우편주소 수집 금지)
회원은 전자우편주소 추출기 등을 이용하여 전자우편주소를 수집 또는 제3자에게 제공할 수 없습니다.
제 6 장 손해배상 및 기타사항
제 18 조 (손해배상)
당 사이트는 무료로 제공되는 서비스와 관련하여 회원에게 어떠한 손해가 발생하더라도 당 사이트가 고의 또는 과실로 인한 손해발생을 제외하고는 이에 대하여 책임을 부담하지 아니합니다.
제 19 조 (관할 법원)
서비스 이용으로 발생한 분쟁에 대해 소송이 제기되는 경우 민사 소송법상의 관할 법원에 제기합니다.
[부 칙]
1. (시행일) 이 약관은 2016년 9월 5일부터 적용되며, 종전 약관은 본 약관으로 대체되며, 개정된 약관의 적용일 이전 가입자도 개정된 약관의 적용을 받습니다.