Crystallization Mechanisms of Joule-Heating-Induced Crystallization

  • Park, Doo-Jung;Ro, Jae-Sang
    • Journal of Information Display
    • /
    • 제10권2호
    • /
    • pp.76-79
    • /
    • 2009
  • In Joule-heating-induced crystallization, solid-to-solid or liquid-to-solid phase transformation could occur. It was found that novel physical phenomena that randomly nucleated liquid seeds, followed by rapid solidification in an amorphous matrix, during the Joule-heating-up period play an important role especially in liquid-to-solid transformation. Under some processing conditions, super-grains sized 6-8 ${\um}m$ were produced by the lateral growth from the initial seeds, without any artificially control.

SLS 공정을 이용한 p-type poly-Si TFT 제작에 관한 연구 (A Study on the Fabrication of p-type poly-Si Thin Film Transistor (TFT) Using Sequential Lateral Solidification(SLS))

  • 이윤재;박정호;김동환
    • 대한전기학회논문지:전기물성ㆍ응용부문C
    • /
    • 제51권6호
    • /
    • pp.229-235
    • /
    • 2002
  • This paper presents the fabrication of polycrystalline thin film transistor(TFT) using sequential lateral solidification(SLS) of amorphous silicon. The fabricated SLS TFT showed high Performance suitable for active matrix liquid crystal display(AMLCD). The SLS process involves (1) a complete melting of selected area via irradiation through a patterned mask, and (2) a precisely controlled pulse translation of the sample with respect to the mask over a distance shorter than the super lateral growth(SLG) distance so that lateral growth extended over a number of iterative steps. The SLS experiment was performed with 550$\AA$ a-Si using 308nm XeCl laser having $2\mu\textrm{m}$ width. Irradiated laser energy density is 310mJ/$\textrm{cm}^2$ and pulse duration time was 25ns. The translation distance was 0.6$\mu$m/pulse, 0.8$\mu$m/pulse respectively. As a result, a directly solidified grain was obtained. Thin film transistors (TFTs) were fabricated on the poly-Si film made by SLS process. The characteristics of fabricated SLS p -type poly-Si TFT device with 2$\mu\textrm{m}$ channel width and 2$\mu\textrm{m}$ channel length showed the mobility of 115.5$\textrm{cm}^2$/V.s, the threshold voltage of -1.78V, subthreshold slope of 0.29V/dec, $I_{off}$ current of 7$\times$10$^{-l4}$A at $V_{DS}$ =-0.1V and $I_{on}$ / $I_{off}$ ratio of 2.4$\times$10$^{7}$ at $V_{DS}$ =-0.1V. As a result, SLS TFT showed superior characteristics to conventional poly-Si TFTs with identical geometry.y.y.y.

비정질 실리콘의 ELC 공정에 대한 광학적 연구 (An Optical Study on ELC Process of Amorphous Silicon)

  • 김우진;윤창환;박승호;김형준
    • 한국레이저가공학회지
    • /
    • 제6권2호
    • /
    • pp.9-17
    • /
    • 2003
  • Due to the heat confinement in the shallow region of the target for a short time scale, pulsed laser annealing has received an increasing interest for the fabrication of poly-Si thin film transistors(TFTs) on glass as a low cost substrate in the flat panel displays. The formation and growth mechanisms of poly silicon(poly-Si) grains in thin films are investigated using an excimer laser crystallization system. To understand the crystallization mechanism, the grain formations are observed by FESEM photography. The optical reflectance and transmittance during the crystallization process are measured using HeNe laser optics. A two-step ELC(Excimer Laser Crystallization) process is applied to enhance the grain formation uniformity.

  • PDF

다공질 양극산화 피막을 이용한 고균일 다결정 살리콘의 성장 (Growth of High Uniform Polycrystalline Grain on the Highly Ordered Porous Anodic Alumina)

  • 김종연;한진우;김영환;김병용;서대식
    • 한국전기전자재료학회:학술대회논문집
    • /
    • 한국전기전자재료학회 2007년도 하계학술대회 논문집 Vol.8
    • /
    • pp.375-375
    • /
    • 2007
  • In the conventional crystallization method, thepoly-Si TFTs show poor device-to-device uniformity because of the random location of the grain boundaries. However, our new crystallization method introduced in this paper employed substrate-embedded seeds on the highly ordered anodic alumina template to control both the location of seeds and the number of grain boundaries intentionally. In the process of excimer laser crystallization (ELC), a-Si film deposited on the anodic alumina by low pressure chemical vapor deposition (LPCVD) is transformed into fine poly-Si grains by explosive crystallization (XC) prior to primary melting. At the higher energy density, the film is nearly completely melted and laterally grown by super lateral growth (SLG) from remained small part of the fine poly-Si grains as seeds at the Si/anodic alumina interface. Resultant grain boundaries have almost linear functions of the number of seeds in concavities of anodic alumina which have a constant spacing. It reveals the uniformity of. device can be enhanced prominently by controlling location and size of pores which contains fine poly~Si seeds under artificial anodizing condition.

  • PDF

정렬된 다공질 산화알루미늄을 이용한 새로운 다결정 실리콘 결정화 방법 (Novel Method of Poly-silicon Crystallization using Ordered Porous Anodic Alumina)

  • 김종연;김미정;김병용;오병윤;한진우;한정민;서대식
    • 한국전기전자재료학회:학술대회논문집
    • /
    • 한국전기전자재료학회 2007년도 추계학술대회 논문집
    • /
    • pp.396-396
    • /
    • 2007
  • Highly ordered pore structures as a template for formation of seeds have been prepared by the self-organization process of aluminum oxidation. The a-Si films were deposited on the anodic alumina films and crystallized by laser irradiation. It was found that un-melted part of fine poly-Si grain formed by explosive crystallization (EX) lead super lateral growth(SLG) and occluded with neighbor grains. The crystallized grains along the distribution of seeds were obtained. This results show a great potential for use in novel crystallization for decently uniform polycrystalline Si thin film transistors (poly-Si TFTs).

  • PDF