• Title/Summary/Keyword: Stress-relieving treatment

Search Result 47, Processing Time 0.027 seconds

A Study on Mechanical Stress Relleving in a Butt-Welded Pipe (파이프 용접에서 기계적 잔류응력 이완법에 관한 연구)

  • 양영수
    • Journal of Welding and Joining
    • /
    • v.14 no.1
    • /
    • pp.75-81
    • /
    • 1996
  • The heat transfer and thermal stress-distribution were numerically determined by using the finite element method for a butt-welded pipe. A mechanical stress relieving(MSR) treatment which has been frequently used in the fabrication of pressure vessels instead of the post weld heat treatment (PWHT) was also simulated to investigate its effect of reducing the residual stress in the welded zone by a mechanical loading.

  • PDF

The Influence of Stress Relieving on Microstructures and Mechanical Properties of Weld Metal in 60kg/mm2 Quenched and Tempered High Strength Steel (응력제거 열처리가 60kg/mm2급 조질 고장력강의 용접부 미세조직과 기계적 특성에 미치는 영향)

  • Kim, O.S.;Chung, I.S.;Park, K.C.
    • Journal of the Korean Society for Heat Treatment
    • /
    • v.6 no.3
    • /
    • pp.144-151
    • /
    • 1993
  • For the purpose of studying the influence of stress relieving on microstructures and mechanical properties of weld metal, manual arc welding, onepole and twopole submerged arc welding were accomplished on $60kg/mm^2$ quenched and tempered high strength steel. After stress relieving, a lot of carbides were precipitated, developed and subsequently coarsened at the grain boundaries and within matrix due tn multiple tempering effect in manual arc welding, resulting in deterioated toughness. Meanwhile pearlite and cementite films were spheroidized and shortened in submerged arc welding, resulting in improved considerable toughness. It was observed that main effect of stress relieving was to reduce solut supersaturation by nucleation and growth of carbide precipitates, and stress relieving led to some reduction in the yield and tensile strenath but did not significantly affect elongation.

  • PDF

A Study on the Characteristics of Residual Stress in the Manufacturing Process of AISI 1536V and AISI A387 (제조공정에 따른 강종별 잔류응력 특성에 관한 연구; AISI 1536V, AISI A387)

  • Hwang, Sung-Kug;Moon, Jeong-Su;Kim, Han Joo
    • Journal of the Korean Society of Manufacturing Process Engineers
    • /
    • v.19 no.9
    • /
    • pp.100-106
    • /
    • 2020
  • This study analyzes the residual stress of AISI 1536V for an engine shaft of the shipbuilding industry and AISI A387 for a reactor shell of the chemical refining industry by the hole drilling method with a strain gauge rosette, which transforms fine mechanical changes into electrical signals. Tensile residual stress is generated in the forging and heat treatment process because specimens are affected by thermal stress and metal transformation stress. In the heat treatment process, the residual stress of AISI A387 is almost 170% the yield strength at 402 MPa. Since during the machining process, variable physical loads are applied to the material, compressive residual stress is generated. Under the same condition, the mechanical properties greatly affect the residual stress during the machining process. After the stress-relieving heat treatment process, the residual stress of AISI A387 is reduced below the yield strength at 182 MPa. Therefore, it is necessary to control the temperature, avoid rapid heat change, and select machining conditions depending on the mechanical properties of materials during manufacturing processes. In addition, to sufficiently reduce the residual stress, it is necessary to study the optimum condition of the stress-relieving heat treatment process for each material.

Combination of Green Tea Extract and L-Theanine Alleviates Electric Foot Shock Induced Stress by Modulating Neurotransmitters in Mice (녹차추출물과 테아닌 복합물의 신경전달물질 조절을 통한 항스트레스 효과)

  • Park, Sang-Ki;Kim, Tae-Il;Lee, Won-Kyung;Park, Hyoung-Kook;Hong, Jin-Tae
    • YAKHAK HOEJI
    • /
    • v.53 no.5
    • /
    • pp.241-249
    • /
    • 2009
  • Various neurotransmitters are involved in regulating stress systems. In this study, we investigated the combination relieving effect of green tea extract(GTE) and L-theanine on the stress induced by electric foot shock. Four week oral administration of GTE (24 mg/kg), L-theanine (4 mg/kg) or their combination reduced the levels of dopamine, noradrenaline and corticosterone in blood, brain cortex, hippocampus, and striatum, wherease increased serotonin level. The combination of GTE and L-theanine showed much greater effects than single treatment of each component, and the effects are comparable to diazepam (2 mg/kg). Therefore, this study suggests that the combination of GTE and L-theanine may act effective and be useful for stress relieving treatment.

Effect of Stress Relieving Heat Treatment on Tensile and Impact Toughness Properties of AISI 316L Alloy Manufactured by Selective Laser Melting Process (선택적 레이저 용융 공정으로 제조된 AISI 316L 합금의 인장 및 충격 인성 특성에 미치는 응력 완화 열처리의 영향)

  • Yang, Dong-Hoon;Ham, Gi-Su;Park, Sun-Hong;Lee, Kee-Ahn
    • Journal of Powder Materials
    • /
    • v.28 no.4
    • /
    • pp.301-309
    • /
    • 2021
  • In this study, an AISI 316 L alloy was manufactured using a selective laser melting (SLM) process. The tensile and impact toughness properties of the SLM AISI 316 L alloy were examined. In addition, stress relieving heat treatment (650℃ / 2 h) was performed on the as-built SLM alloy to investigate the effects of heat treatment on the mechanical properties. In the as-built SLM AISI 316 L alloy, cellular dendrite and molten pool structures were observed. Although the molten pool did not disappear following heat treatment, EBSD KAM analytical results confirmed that the fractions of the low- and high-angle boundaries decreased and increased, respectively. As the heat treatment was performed, the yield strength decreased, but the tensile strength and elongation increased only slightly. Impact toughness results revealed that the impact energy increased by 33.5% when heat treatment was applied. The deformation behavior of the SLM AISI 316 L alloy was also examined in relation to the microstructure through analyses of the tensile and impact fracture surfaces.

A Study on the Reduction of Spring Back for Precision Forming of Steam Generator Tube (증기발생기 전열관의 정밀성형을 위한 스프링 백 저감에 관한 연구)

  • Suh Y. S.;Kim Y. W.;Kim J. I.
    • Proceedings of the Korean Society for Technology of Plasticity Conference
    • /
    • 2001.10a
    • /
    • pp.102-105
    • /
    • 2001
  • The spring back taking place after the coiling process of steam generator tube leads to the dimensional inaccuracy. In order to reduce the spring back, tension force was applied to the one end of the tube during forming. In this work, parametric study using FEM was performed to find the appropriate magnitude of tension force. The force that induces minimum suing back was found by simultaneously taking account of suing back amount, cross-sectional ovality, and thickness of the tube wall after deformation. In addition, stress relieving by heat treatment was also simulated as an alternative to the former method. The latter was found to be more effective under the given constraints.

  • PDF

A Study on the Control of Spring Back for the Precision Forming of the Steam Generator Helical Tube (나선형 증기 발생기 튜브의 정밀성형을 위한 스프링백 제어 연구)

  • 서영성;김용완;김종인
    • Transactions of Materials Processing
    • /
    • v.11 no.3
    • /
    • pp.238-245
    • /
    • 2002
  • The spring back taking place after the coiling process of steam generator tube leads to the dimensional inaccuracy. In order to reduce the spring back, tension force was applied to the one end of the tube during forming. In this work, parametric study using FEM was performed to find the appropriate magnitude of tension force. The force that induces minimum spring back was found by simultaneously taking account if spring back amount, cross-sectional ovality, and thickness of the tube wall after deformation. In addition, stress relieving by heat treatment was also simulated as an alternative to the former method. The latter was found to be more effective under the given constraints.

The Effect of Aroma Inhalation Method on Stress Responses of Nursing Students (향기 흡입법이 간호대학생의 스트레스 반응에 미치는 효과)

  • 박미경;이은숙
    • Journal of Korean Academy of Nursing
    • /
    • v.34 no.2
    • /
    • pp.344-351
    • /
    • 2004
  • Purpose: The purpose of this study is to identify the effect of aroma inhalation on stress responses (physical symptoms, levels of anxiety, perceived stresses)of nursing students. Method: This study was a quasi-experimental research using anon-equivalent pre-post design and was conducted from June 1 to June 5, 2002. The subjects consisted of 77 junior nursing students who were divided into 39 experimental group members and 38 control group members. A pretest and Post-test were conducted to measure body symptoms, the level of anxiety, and the level of perceived stress. In the experimental group, aromas were given using an aroma lamp, lavender, peppermint, rosemary and Clary-Sage. In the control group, the treatment was not administered. Result: As a result of administering aroma inhalation to nursing students, their physical symptoms decreased, their anxiety scores were low, and their perceived stress scores were low, showing that aroma inhalation could be a very effective stress management method. Conclusion: Nursing educators should play an important role in contributing to college students' physical and psychological health by helping enhance their recognition of stress management and effectively relieving their stress using essential oils.

A Study on the Explosive Sleeving of A Repair for Defective Tube/Tubeplate on the Nuclear Steam Generator (원자력 증기발생기 결함 세관 보수용 폭발 sleeving에 관한 연구)

  • 이병일;강정윤;이상래
    • Explosives and Blasting
    • /
    • v.17 no.4
    • /
    • pp.8-17
    • /
    • 1999
  • Unfortunately leaks occur in heat exchangers periodically, usually at the tube to tubeplate joint. The usual method of repair is to plug off the defective area and isolate the tubes of concern from the circuit. If the leaks continua the thermal capacity of the units is progressively reduced and for this reason the alternative of using an internal bridging sleeve has been examined. This paper discusses the overall development activities that has been found necessary to bring this repair procedure to a successful conclusion for use on the nuclear steam generator. In this work we have investigated optimum explosives and explosive quality, explosive sleeving's thickness, the design of sheath stress relieving heat treatment pull-out load, hydraulic leakage, stress corrosion cracking properties. The results obtain are as follows : (1) The optimum explosives and explosive qualities are PETN and about 15~40 gr/ft of explosive sleeving in nuclear steam generator. (2) Explosive sleeving's thickness is 1.1~l.4mm, If groove of 0.35mm formed in sleeve outside existed, For the hydraulic leakage is go up, explosive sleeving of formed groove are applicate tube and turnplate. (3) If the stress relieving heat treatment are experiment in $750^\circ{C}$, $850^\circ{C}$, 15 minutes Pull-out strength of sleeving 1,500~2,300kg, hydraulic leakage is $250kg/cm^2$.

  • PDF

The Repeat Heat Treatment Behavior of Double Remelted Fe-Co Ultra-high Strength Steel. - Part. 1 Microstructure Control (Fe-Co기 고인성 고강도강의 반복 열처리 거동 - Part 1. 조직제어)

  • Yoon, Bo-Hee;Park, Kyoung-Tae;Lee, Tae-Hyuk;Kim, Jae-Hoon;Kim, Hong-Kyu;Lee, Seong;Lee, Jong-Hyeon
    • Journal of Korea Foundry Society
    • /
    • v.32 no.1
    • /
    • pp.32-37
    • /
    • 2012
  • In this study, microstructural evaluation was carried out on secondary hardening type ultrahigh strength steel, Fe-Co-Ni composition. This paper as a first part of whole research presented the microstructural behavior by cyclic heat treatment. The cyclic heat treatment method includes normalizing, stress relieving, solution treatment and aging. Especially, solution treatments performed triple times to get maximized solution hardening. Phase transformation and microstructure were observed by using optical microscope (OM), Electron back-scattered diffraction (EBSD) and X-ray stress analyzer. During the triple solution treatment, size of grain boundary was dramatically decreased by generating a packet from the martensite transformation of residual austenite in the inner part of grain, whereas the hardness increase was not significant.