Improving Smoothness of Hydrophilic Natural Polymer Coating Layer by Optimizing Composition of Coating Solution and Modifying Chemical Properties of Cobalt-Chrome Stent Surface (코팅 용액의 조성 최적화 및 코발트-크롬 금속스텐트의 화학적 표면개질을 통한 친수성 천연 고분자 코팅층의 표면 거칠기 개선)

  • Kim, Dae Hwan;Kum, Chang Hun
    • Journal of Chitin and Chitosan
    • /
    • v.23 no.4
    • /
    • pp.256-261
    • /
    • 2018
  • Recently, the number of cardiovascular disease-related deaths worldwide has increased. Therefore, the importance of percutaneous cardiovascular intervention and drug-eluting stents (DES) has been highlighted. Despite the great clinical success of DES, the re-endothelialization at the site of stent implantation is retarded owing to the anti-proliferative effect from the coated drug, resulting in late thrombosis or very late restenosis. In order to solve this problem, studies have been actively carried out to excavate new drugs that promote rapid re-endothelialization. In this study, we introduced hydrophilic drug, tauroursodeoxycholate (TUDCA), that improves the proliferation of endothelial progenitor cells and promotes apoptosis of vascular smooth muscle cells. In addition, we utilized shellac, which is a natural resin from lac bug to coat TUDCA on the surface of the metal. When using conventional coating method including biodegradable polymers and organic solvents, phase separation between polymer and drug occurred in the coating layer that caused incomplete incorporation of drug into the polymer layer. However, when using shellac as a coating polymer, no phase separation was observed and drug was fully covered with the polymer matrix. In addition, by adjusting the composition of coating solution and modifying the hydrophilicity of the metal surface using oxygen plasma, the surface roughness decreased due to the increased affinity between coating solution and metal surface. This result provides a method of depositing a hydrophilic drug layer on the stent.

Hydrodynamic Characteristics of Self-expandable Graft Stents in Steady Flow (정상유동에서 자가팽창성 그래프트 스텐트의 수력학적 특성)

  • 이홍철;김철생;박복춘;박복춘
    • Journal of Biomedical Engineering Research
    • /
    • v.24 no.1
    • /
    • pp.37-44
    • /
    • 2003
  • This experimental study is aimed at evaluating the hydrodynamic performance of newly designed self-expandable graft stents under steady flow condition. Two graft stents with different coating materials and a bare TiNi metallic stent for comparison test were used in the experiment. Pressure variation and velocity distribution at the upstream and downstream of the stents were measured at flow rates of 5, 10, and 15 l/min, respectively. Pressure loss due to insertion of the stent increased with increasing flow rate exponentially as expected. At a flow rate of 15 l/min, pressure loss of Polyure-thane(PU)-coated graft stent was 6 times higher than that of TiNi metallic stent, while the pressure loss of a porous Polytetrafluoroethylene(PTFE)-coated graft stent was comparable to a bare TiNi metallic stent. Velocity profiles of the porous PTFE-coated graft stent were similar to those of a bare TiNi metallic stent regardless of flow rate. Furthermore, the velocity profile of PU-coated graft stent revealed an asymmetrical and relatively low central velocity at a higher flow rate than 10 1/min, expecially, where the effects resulted in increases of wall shear stress and normal stress. The worse hydrodynamic behavior of PU-coated graft stent than the other two stents might be attributed to formation of folds due to poor flexibility of coated material when inserting the graft stent into the pipe with a more smaller size, which later gave rise non-symmetry of flow area, increase of surface roughness and jet flow via the crevice between the stent and cylinder wall.

Effect of Electropolishing Process on Corrosion Resistance of Co-Cr Alloy (Co-Cr alloy의 전해연마에 따른 부식의 영향)

  • Park, Je-Min;Kim, Wan-Cheol
    • Journal of the Korean institute of surface engineering
    • /
    • v.43 no.4
    • /
    • pp.199-204
    • /
    • 2010
  • The Co-Cr alloys have clinical histories as dental and orthopaedic implants, and recently as cardiovascular stent applications because they exhibit a high elastic modulus and radiopacity. In order to improve their mechanical and corrosion resistance, electropolishing is employed as the final process. Electropolishing, an anodic dissolution process in the transpassive state, is sensitively affected by process conditions such as current density, machining time, and electrode gap. In this study, the effect of the electropolishing conditions on surface roughness and corrosion resistance is investigated for Co-Cr alloys (L605). The most smooth surface is obtained when electropolishing is performed at 15-20 V for 15-30 sec with a electrode gap of 3.5 mm. It is found out that electropolishing reduces corrosion rate about one-tenth as much.

Effect of Surface Modification by Heat Treatment of Co-Cr Alloy (Co-Cr alloy의 열처리에 따른 표면개질의 영향)

  • Park, J.M.;Kim, W.C.
    • Journal of the Korean Society for Heat Treatment
    • /
    • v.23 no.3
    • /
    • pp.137-141
    • /
    • 2010
  • The Co-Cr alloys have clinical histories in dental and orthopaedic implants, and recently in cardiovascular stent applications because the alloys exhibit a high elastic modulus and radiopacity. In order to improve mechanical property of the Co-Cr alloys, electropolishing is employed as the final process. Electropolishing, an anodic dissolution process in the transpassive state, is sensitively affected by process conditions such as current density, machining time, electrode gap. In this study, the effect of heat treatment conditions on surface roughness and inclusion analysis is investigated in Co-Cr alloy (L605). The most smooth surface of Co-Cr alloy is obtained when electropolishing is performed at 15-20 V for 15-30 sec with a electrode gap of 3.5 mm.

Application of Ultrasonic Nano Crystal Surface Modification into Nitinol Stent Wire to Improve Mechanical Characteristics (나이티놀 스텐트 와이어의 기계적 특성 향상을 위한 초음파 나노표면 개질 처리에 대한 연구)

  • Kim, Sang-Ho;Suh, Tae-Suk;Lee, Chang-Soon;Park, In-Gyu;Cho, In-Sik;Pyoun, Young-Shik;Kim, Seong-Hyeon
    • Progress in Medical Physics
    • /
    • v.20 no.2
    • /
    • pp.80-87
    • /
    • 2009
  • Phase transformation, superelastic characteristics and variation of surface residual stress were studied for Nitinol shape memory alloy through application of UNSM technology, and life extension methods of stent were also studied by using elastic resilience and corrosion resistance. Nitinol wire of ${\phi}1.778$ mm showed similar surface roughness before and after UNSM treatment, but drawing traces and micro defects were all removed by UNSM treatment. It also changed the surface residual stress from tensile to compressive values, and XRD result showed less intensive austenite peak and clear martensite and additional R-phase peaks after UNSM treatment. Fatigue resistance could be greatly improved through removal of surface defects and rearrangement of surface residual stress from tensile to compressive state, and development of surface modification system to improve not only bio-compatability but also resistance to corrosion and wear will make it possible to develop vascular stent which can be used for circulating system diseases which run first cause of death of recent Koreans.

  • PDF

Metal Surface Coating Using Electrospray of Biodegradable Polymers and $\alpha$-Lipoic Acid Release Behavior for Drug-Eluting Stents (생분해성 고분자의 전기분사를 이용한 약물방출 스텐트용 금속표면 코팅 및 ALA방출 거동)

  • Kim, Dong-Min;Lee, Bong-Soo;Park, Cheol-Ho;Park, Kwi-Deok;Son, Tae-Il;Jeong, Myeong-Ho;Han, Dong-Keun
    • Polymer(Korea)
    • /
    • v.34 no.2
    • /
    • pp.178-183
    • /
    • 2010
  • Medical metal stents inserted to patients with a cardiovascular disease associated with coronary artery system have relatively increased the survival rate. The development of new stents is, however, urgently required due to restenosis and late thrombosis generated in metal stents. To solve these problems, the biodegradable polymers such as poly(lactide-co-glycolide) (PLGA), poly(L-lactide)(PLLA), and poly ($\varepsilon$-caprolactone)(PCL) were mixed with alpha lipoic acid (ALA), which is well known to inhibit the proliferation of neointimal hyperplasia. Subsequently, the ALA-loaded polymers were coated on stainless steel by electrospray. The drug-eluting behaviors from the coated polymers were investigated according to kinds and concentrations of polymers, spray rates, and kinds of solvents. The drug-eluting rate from PCL with the lowest glass transition temperature was the fastest among three polymers and followed by PLGA and PLLA. The surface roughness increased as the spray rate was increased and also the drug-eluting rate was affected by kinds of solvents with different boiling point. It is expected that drug-eluting stent (DES) coated with ALA-loaded polymers can be applied practically for clinical applications by controlling the behavior of drug release.